Ferrite and carbides in 1.28C-1.04Si-24.7Cr-1.14Ni steel


Figure 1: Ferrite and carbides, scale bar: 50 µm.

Carbide name: No data
Record No.: 458
Carbide formula: No data
Carbide type: No data
Carbide composition in weight %: No data
Image type: LM
Steel name: 1.28C-1.04Si-24.7Cr-1.14Ni
Mat.No. (Wr.Nr.) designation: No data
DIN designation: No data
AISI/SAE/ASTM designation: No data
Other designation: No data
Steel group: Cr cast irons
Steel composition in weight %: 1.28% C, 1.05% Si, 0.43% Mn, 0.036% P, 0.025% P, 24.7% Cr, 1.14% Ni, 0.04% V, 0.06% Mo, 0.14% Cu.
Heat treatment/condition: Sample hardness: 313 HB.
Note: No data
Links: No data
Reference: Not shown in this demo version.