Alloy carbide in white cast iron


Figure 1: Alloyed white cast iron (Fe –2.2% C –0.9% Mn –0.5% Si –12.7% Cr –0.4% Mo –0.1% V) with a martensitic matrix and a network of eutectic alloy carbides (white). Etched with Vilella’s reagent. Original at 200x.


Figure 2: Alloyed white cast iron (Fe –2.2% C –0.9%Mn–0.5%Si–12.7% Cr –0.4% Mo –0.1% V) with a martensitic matrix and a network of eutectic alloy carbides (colored). Etched with Groesbeck’s (80 °C –30 sec) reagent to color the alloy carbides. Original at 200x.

Carbide name: Alloy carbide
Record No.: 527
Carbide formula: No data
Carbide type: No data
Carbide composition in weight %: No data
Image type: LM
Steel name: White cast iron
Mat.No. (Wr.Nr.) designation: No data
DIN designation: No data
AISI/SAE/ASTM designation: No data
Other designation: No data
Steel group: Cast iron
Steel composition in weight %: Fe –2.2% C –0.9% Mn –0.5% Si –12.7% Cr –0.4% Mo –0.1% V
Heat treatment/condition: No data
Note: No data
Links: No data
Reference: Not shown in this demo version.