Eutectic carbides in alloyed white cast iron


Figure 1: Alloyed white cast iron (Fe-2.2%C-0.9%Mn- 0.5%Si-12.7%Cr-0.4%Mo-0.1%V) with a martensitic matrix and a network of eutectic alloy carbides (colored). Etched with Groesbeck’s reagent. (80 .C, or 175 .F, for 30 s) to color the alloy carbides. Scale bar: 50 µm.

Carbide name: Eutectic carbide
Record No.: 541
Carbide formula: No data
Carbide type: No data
Carbide composition in weight %: No data
Image type: LM
Steel name: Alloyed white cast iron
Mat.No. (Wr.Nr.) designation: No data
DIN designation: No data
AISI/SAE/ASTM designation: No data
Other designation: No data
Steel group: Cast irons
Steel composition in weight %: Fe-2.2%C-0.9%Mn-0.5%Si-12.7%Cr-0.4%Mo-0.1%V.
Heat treatment/condition: No data
Note: No data
Links: No data