Mo2C carbides in molybdenum steel


Figure 1: Mo2C carbides in molybdenum steel, Mag. 20,000x.

Carbide name: Mo2C
Record No.: 64
Carbide formula: Mo2C
Carbide type: M2C
Carbide composition in weight %: No data
Image type: TEM
Steel name: Molybdenum steel
Mat.No. (Wr.Nr.) designation: No data
DIN designation: No data
AISI/SAE/ASTM designation: No data
Other designation: No data
Steel group: Molybdenum steels
Steel composition in weight %: 0.14% C, 0.65% Mn, 0.26% Si, 2.05% Mo, 0.0020% B.
Heat treatment/condition: 970 C/water quenched; tempered at 700 C for 1h.
Note: Single stage carbon extraction replica. Mo2C rods in Widmanstatten pattern.
Links: No. 64 and No. 65.