Light Microscopy (LM) of Carbides in Steels

(Cr, Fe)23C6 carbides in Cr-Co steel
(Cr, Fe)23C6 carbides in Cr-Co steel
(Cr, Fe)23C6 carbides in Cr-Co steel
(Cr, Fe)23C6 carbides in Cr-Co steel
(Cr, Fe)23C6 carbides in Cr25 cast steel
(Cr, Fe)7C3 carbides in Cr-Co steel
(Cr, Fe)7C3 carbides in chromium cast iron
(Cr, Fe)7C3 carbides in chromium cast iron
(Cr,Fe)7C3 carbides in K110, PM steel K390 steels
(Cr,Fe)7C3 carbides in X180CrMo12-1 steel
(Cr,Fe)7C3 carbides in bainitic steels
(Cr,Fe)7C3, Fe3C and Fe23(C,B)6 carbides in white cast irons
(Cr15.58Fe7.42)23C6 and V8C7 carbides in PM AISI M2 steel
(Fe,Cr)7C3 carbides in ferritic stainless steel
(FeCrMo)C and (FeCrMoMn)C carbides in 10CrMo9-10 steel
(Ti,Mo)C, M23C6 carbides in AIM1 steel
(Ti,W)C and (Fe,W)6C carbides in LIME steel sample
Alloy carbide in white cast iron
Alloy carbide in white cast iron
Austenite and carbides in 1.4841 steel
Borides in Fe-Cr-Ni-B alloy
Borides in Fe-Cr-Ni-B alloy
Borides in Fe-Cr-Ni-B alloy
C2C, Cr3C2, Cr7C2, Cr7C3 and Cr23C6 carbides in AISI 446 steel
Carbide band analysis
Carbide bands in 1.3343 steel
Carbide morphology of M2 tool steel
Carbide network in 1.2362 steel
Carbide network in 1.2379 steel
Carbide network in 1.3539 steel
Carbide network on the grains in 1.2344 steel
Carbide phases in high speed steels
Carbide segregation in M2 high speed steel
Carbide segregation in T1 high speed steel
Carbides cracking during plane grinding
Carbides in 1.3343 steel
Carbides in 0.13C, 5Cr, 4Mo, 0.2V, 0.5C, 5Cr, 5Mo, 0.6V and 0.7C, 1.5Mn, 1.39Si, 6Cr, 2Mo steels
Carbides in 0.79C-0.84Si-4.96Cr-0.31Mo steel
Carbides in 1.06C-7.37Cr-2.29V-1.43Mo steel
Carbides in 1.07C-1.21Si-8.02Cr-2.63V-1.14W-1.53Mo steel
Carbides in 1.08C-1.04Si-7.32Cr-2.28V-0.98W-1.44Mo steel
Carbides in 1.0C-10.0Cr-90.25V steel, overheated microstructure
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1000 C/air
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1000 C/oil
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1020 C/air
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1020 C/oil
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1040 C/air
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1040 C/oil
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1060 C/air
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1060 C/oil
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1080 C/air
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1080 C/oil
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1120 C/air
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1120 C/oil
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1160 C/air
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1160 C/oil
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1200 C/air
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1200 C/oil
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1240 C/air
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1240 C/oil
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 900 C/air
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 900 C/oil
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 940 C/air
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 940 C/oil
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 980 C/air
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 980 C/oil
Carbides in 1.10C-1.0Si-7.90Cr-2.20V-1.15W-1.45Mo steel
Carbides in 1.2080 steel
Carbides in 1.2080 steel
Carbides in 1.2080 steel
Carbides in 1.2080 steel
Carbides in 1.2080 steel
Carbides in 1.2080 steel
Carbides in 1.2080 steel
Carbides in 1.2080 steel
Carbides in 1.2080 steel
Carbides in 1.2080 steel
Carbides in 1.2080 steel
Carbides in 1.2080 steel
Carbides in 1.2080 steel
Carbides in 1.2080 steel
Carbides in 1.2080 steel
Carbides in 1.2080 steel, quenched from 1000 C/air
Carbides in 1.2080 steel, quenched from 1000 C/oil
Carbides in 1.2080 steel, quenched from 1020 C/air
Carbides in 1.2080 steel, quenched from 1020 C/oil
Carbides in 1.2080 steel, quenched from 1040 C/air
Carbides in 1.2080 steel, quenched from 1040 C/oil
Carbides in 1.2080 steel, quenched from 1060 C/air
Carbides in 1.2080 steel, quenched from 1060 C/oil
Carbides in 1.2080 steel, quenched from 1080 C/air
Carbides in 1.2080 steel, quenched from 1080 C/oil
Carbides in 1.2080 steel, quenched from 1120 C/air
Carbides in 1.2080 steel, quenched from 1120 C/oil
Carbides in 1.2080 steel, quenched from 1160 C/air
Carbides in 1.2080 steel, quenched from 1160 C/oil
Carbides in 1.2080 steel, quenched from 1200 C/air
Carbides in 1.2080 steel, quenched from 1200 C/oil
Carbides in 1.2080 steel, quenched from 1240 C/oil
Carbides in 1.2080 steel, quenched from 1240 C/oil
Carbides in 1.2080 steel, quenched from 900 C/air
Carbides in 1.2080 steel, quenched from 900 C/oil.
Carbides in 1.2080 steel, quenched from 940 C/air
Carbides in 1.2080 steel, quenched from 940 C/oil
Carbides in 1.2080 steel, quenched from 980 C/air
Carbides in 1.2080 steel, quenched from 980 C/oil
Carbides in 1.2344 steel
Carbides in 1.2360 steel
Carbides in 1.2369 steel
Carbides in 1.2379 and UNIVERSAL steels (Acoustic Emission Test)
Carbides in 1.2379 and Universal steels
Carbides in 1.2379 steel
Carbides in 1.2379 steel
Carbides in 1.2379 steel
Carbides in 1.2379 steel, quenched and tempered
Carbides in 1.2379 steel, quenched from 1000 C/air
Carbides in 1.2379 steel, quenched from 1000 C/oil
Carbides in 1.2379 steel, quenched from 1000 C/oil
Carbides in 1.2379 steel, quenched from 1020 C/air
Carbides in 1.2379 steel, quenched from 1020 C/oil
Carbides in 1.2379 steel, quenched from 1020 C/oil
Carbides in 1.2379 steel, quenched from 1040 C/air
Carbides in 1.2379 steel, quenched from 1040 C/oil
Carbides in 1.2379 steel, quenched from 1040 C/oil
Carbides in 1.2379 steel, quenched from 1060 C/air
Carbides in 1.2379 steel, quenched from 1060 C/oil
Carbides in 1.2379 steel, quenched from 1060 C/oil
Carbides in 1.2379 steel, quenched from 1080 C/air
Carbides in 1.2379 steel, quenched from 1080 C/oil
Carbides in 1.2379 steel, quenched from 1080 C/oil
Carbides in 1.2379 steel, quenched from 1120 C/air
Carbides in 1.2379 steel, quenched from 1120 C/oil
Carbides in 1.2379 steel, quenched from 1120 C/oil
Carbides in 1.2379 steel, quenched from 1160 C/air
Carbides in 1.2379 steel, quenched from 1160 C/oil
Carbides in 1.2379 steel, quenched from 1200 C/air
Carbides in 1.2379 steel, quenched from 1200 C/oil
Carbides in 1.2379 steel, quenched from 1240 C/air
Carbides in 1.2379 steel, quenched from 1240 C/oil
Carbides in 1.2379 steel, quenched from 900 C/air
Carbides in 1.2379 steel, quenched from 900 C/oil
Carbides in 1.2379 steel, quenched from 940 C/air
Carbides in 1.2379 steel, quenched from 940 C/oil
Carbides in 1.2379 steel, quenched from 940 C/oil
Carbides in 1.2379 steel, quenched from 980 C/air
Carbides in 1.2379 steel, quenched from 980 C/oil
Carbides in 1.2379 steel, quenched from 980 C/oil
Carbides in 1.2379, 1.3202 and experimental steels
Carbides in 1.2436 steel, quenched from 1000 C/air
Carbides in 1.2436 steel, quenched from 1000 C/oil
Carbides in 1.2436 steel, quenched from 1020 C/air
Carbides in 1.2436 steel, quenched from 1020 C/oil
Carbides in 1.2436 steel, quenched from 1040 C/air
Carbides in 1.2436 steel, quenched from 1040 C/oil
Carbides in 1.2436 steel, quenched from 1060 C/air
Carbides in 1.2436 steel, quenched from 1060 C/oil
Carbides in 1.2436 steel, quenched from 1080 C/air
Carbides in 1.2436 steel, quenched from 1080 C/oil
Carbides in 1.2436 steel, quenched from 1120 C/air
Carbides in 1.2436 steel, quenched from 1120 C/oil
Carbides in 1.2436 steel, quenched from 1160 C/air
Carbides in 1.2436 steel, quenched from 1160 C/oil
Carbides in 1.2436 steel, quenched from 1200 C/air
Carbides in 1.2436 steel, quenched from 1200 C/oil
Carbides in 1.2436 steel, quenched from 1240 C/air
Carbides in 1.2436 steel, quenched from 1240 C/oil
Carbides in 1.2436 steel, quenched from 900 C/air
Carbides in 1.2436 steel, quenched from 900 C/oil
Carbides in 1.2436 steel, quenched from 940 C/air
Carbides in 1.2436 steel, quenched from 940 C/oil
Carbides in 1.2436 steel, quenched from 980 C/air
Carbides in 1.2436 steel, quenched from 980 C/oil
Carbides in 1.2510 steel
Carbides in 1.2601 steel, quenched from 1000 C/air
Carbides in 1.2601 steel, quenched from 1000 C/oil
Carbides in 1.2601 steel, quenched from 1020 C/air
Carbides in 1.2601 steel, quenched from 1020 C/oil
Carbides in 1.2601 steel, quenched from 1040 C/air
Carbides in 1.2601 steel, quenched from 1040 C/oil
Carbides in 1.2601 steel, quenched from 1060 C/air
Carbides in 1.2601 steel, quenched from 1060 C/oil
Carbides in 1.2601 steel, quenched from 1080 C/air
Carbides in 1.2601 steel, quenched from 1080 C/oil
Carbides in 1.2601 steel, quenched from 1120 C/air
Carbides in 1.2601 steel, quenched from 1120 C/oil
Carbides in 1.2601 steel, quenched from 1160 C/air
Carbides in 1.2601 steel, quenched from 1160 C/oil
Carbides in 1.2601 steel, quenched from 1200 C/air
Carbides in 1.2601 steel, quenched from 1200 C/oil
Carbides in 1.2601 steel, quenched from 1240 C/air
Carbides in 1.2601 steel, quenched from 1240 C/oil
Carbides in 1.2601 steel, quenched from 900 C/air
Carbides in 1.2601 steel, quenched from 900 C/oil
Carbides in 1.2601 steel, quenched from 940 C/air
Carbides in 1.2601 steel, quenched from 940 C/oil
Carbides in 1.2601 steel, quenched from 980 C/air
Carbides in 1.2601 steel, quenched from 980 C/oil
Carbides in 1.3207 steel, as cast and soft annealed condition
Carbides in 1.3207 steel, as cast and soft annealed condition
Carbides in 1.3207 steel, as cast and soft annealed condition
Carbides in 1.3243 steel
Carbides in 1.3255 steel, 2 x quenched from 1280 C/oil
Carbides in 1.3255 steel, 2 x quenched from 1300 C/oil
Carbides in 1.3255 steel, 3 x quenched from 1260 C/oil
Carbides in 1.3255 steel, 3 x quenched from 1280 C/oil
Carbides in 1.3255 steel, 3 x quenched from 1320 C/oil
Carbides in 1.3255 steel, 3x quenched from 1300 C/oil
Carbides in 1.3255 steel, as cast condition, bottom of the ingot
Carbides in 1.3255 steel, as cast condition, head of the ingot
Carbides in 1.3255 steel, as cast condition, middle of the ingot
Carbides in 1.3255 steel, quenched from 1200 C/oil
Carbides in 1.3255 steel, quenched from 1240 C/oil
Carbides in 1.3255 steel, quenched from 1240 C/oil and tempered at 560 C
Carbides in 1.3255 steel, quenched from 1240 C/thermal bath
Carbides in 1.3255 steel, quenched from 1260 C/oil
Carbides in 1.3255 steel, quenched from 1260 C/oil and tempered at 560 C
Carbides in 1.3255 steel, quenched from 1280 C/oil
Carbides in 1.3255 steel, quenched from 1280 C/oil and 2 x tempered at 560 C
Carbides in 1.3255 steel, quenched from 1280 C/oil and 3 x tempered at 560 C
Carbides in 1.3255 steel, quenched from 1280 C/oil and tempered at 560 C
Carbides in 1.3255 steel, quenched from 1300 C/oil
Carbides in 1.3255 steel, quenched from 1300 C/oil and 2 x tempered at 560 C
Carbides in 1.3255 steel, quenched from 1300 C/oil and 3 x tempered at 560 C
Carbides in 1.3255 steel, quenched from 1300 C/oil and tempered at 560 C
Carbides in 1.3255 steel, quenched from 1320 C/oil
Carbides in 1.3255 steel, quenched from 1320 C/oil and 3 x tempered at 560 C
Carbides in 1.3255 steel, quenched from 1320 C/oil and tempered at 560 C
Carbides in 1.3255 steel, quenched from 1340 C/oil
Carbides in 1.3255 steel, soft annealed microstructure
Carbides in 1.3318 steel, quenched from 1240 C, 2 min/hot bath
Carbides in 1.3318 steel, quenched from 1240 C, 3 min/hot bath
Carbides in 1.3318 steel, quenched from 1250 C, 2 min/hot bath
Carbides in 1.3318 steel, quenched from 1250 C, 3 min/hot bath
Carbides in 1.3318 steel, quenched from 1260 C, 2 min/hot bath
Carbides in 1.3318 steel, quenched from 1260 C, 3 min/hot bath
Carbides in 1.3318 steel, quenched from 1270 C, 2 min/hot bath
Carbides in 1.3318 steel, quenched from 1270 C, 3 min/hot bath
Carbides in 1.3318 steel, quenched from 1280 C, 2 min/hot bath
Carbides in 1.3318 steel, quenched from 1280 C, 3 min/hot bath
Carbides in 1.3318 steel, quenched from 1290 C, 3 min/hot bath
Carbides in 1.3318 steel, quenched from 1300 C, 2 min/hot bath
Carbides in 1.3318 steel, quenched from 1300 C, 3 min/hot bath
Carbides in 1.3318 steel, quenched from 1310 C, 2 min/hot bath
Carbides in 1.3318 steel, quenched from 1310 C, 3 min/hot bath
Carbides in 1.3318 steel, quenched from 1320 C, 2 min/hot bath
Carbides in 1.3318 steel, quenched from 1320 C, 3 min/hot bath
Carbides in 1.3318 steel, quenched from 1330 C, 2 min/hot bath
Carbides in 1.3318 steel, quenched from 1330 C, 3 min/hot bath
Carbides in 1.3318 steel, quenched from 1340 C, 2 min/hot bath
Carbides in 1.3318 steel, quenched from 1340 C, 3 min/hot bath
Carbides in 1.3318 steel, quenched from 1350 C, 2 min/hot bath
Carbides in 1.3318 steel, quenched from 1350 C, 3 min/hot bath
Carbides in 1.3318 steel, quenched from 1360 C, 2 min/hot bath
Carbides in 1.3318 steel, quenched from 1360 C, 3 min/hot bath
Carbides in 1.3343 steel
Carbides in 1.3343 steel, 2 x quenched from 1240 C/oil
Carbides in 1.3343 steel, 2 x quenched from 1280 C/oil
Carbides in 1.3343 steel, 2 x quenched from 1300 C/oil
Carbides in 1.3343 steel, as cast condition
Carbides in 1.3343 steel, quenched from 1140 C/oil
Carbides in 1.3343 steel, quenched from 1140 C/oil and tempered at 540 C
Carbides in 1.3343 steel, quenched from 1240 C/oil
Carbides in 1.3343 steel, quenched from 1240 C/oil and 2 x tempered at 540 C
Carbides in 1.3343 steel, quenched from 1240 C/oil and tempered at 540 C
Carbides in 1.3343 steel, quenched from 1280 C/oil
Carbides in 1.3343 steel, quenched from 1280 C/oil and 2 x tempered at 540 C
Carbides in 1.3343 steel, quenched from 1300 C/oil
Carbides in 1.3343 steel, quenched from 1300 C/oil and 2 x tempered at 540 C
Carbides in 1.3343 steel, quenched from 1300 C/oil and 2 x tempered at 540 C
Carbides in 1.3343 steel, soft annealed condition
Carbides in 1.3344 steel
Carbides in 1.3344 steel
Carbides in 1.3344 steel
Carbides in 1.3344 steel
Carbides in 1.3355 steel
Carbides in 1.3395 PM steel
Carbides in 1.4034 steel
Carbides in 1.4108 steel
Carbides in 1.4110 stee
Carbides in 1.4112 steel
Carbides in 1.4112 steel
Carbides in 1.4122 steel
Carbides in 1.93C-20.9Cr-1.35W-0.57V steel
Carbides in 12Cr and 8Cr steels
Carbides in 16MnCr5 steel - As-received steel
Carbides in 16MnCr5 steel - Heat treated steel II
Carbides in 16MnCr5 steel - Heat treated steel III
Carbides in 1C-1.10Si-8Cr-2.70Mo-0.30V steel
Carbides in 2.25Cr-1Mo steel
Carbides in 2.25Cr-1Mo weld/mild steel interface
Carbides in 316 stainless steel
Carbides in 4Cr5MoSiV1 steel
Carbides in 51CrV4 steel
Carbides in AISI 1045, 5150 and 52100 steels
Carbides in AISI 2367 steel
Carbides in AISI D2 steel
Carbides in AISI D2 steel
Carbides in AISI H13 steel
Carbides in AISI H13 steel
Carbides in AISI M1 high speed steels
Carbides in AISI M2 steel
Carbides in APM 23 steel
Carbides in C45 carbon steel
Carbides in D2 steel
Carbides in DC01EK and DC04EK low alloyed carbon steels
Carbides in DC01EK and DC04EK low carbon steels
Carbides in Damascus steel
Carbides in Fe-30.8Ni-26.6Cr alloy
Carbides in Fe-5Cr-5W-5Mo-V-C cast high speed steel
Carbides in HK30 cast steel
Carbides in Hadfield Mn steel
Carbides in Hadfield steel
Carbides in HiCr iron rolls
Carbides in L1, S2, S5, S7, H13 and M2 steels
Carbides in M2 steel
Carbides in MM23 PM steel
Carbides in NCWV/D3 steel
Carbides in O6 steel
Carbides in P/M T15 high speed steel
Carbides in P/M T15 high speed steel
Carbides in P92 steel
Carbides in Roltec PM steel
Carbides in Rp5 high speed steel
Carbides in S5 tool steel
Carbides in S7 shock resisting tool steel
Carbides in SAE 8620 steel
Carbides in SDK11 steel
Carbides in Str?mhard austenitic manganese steel
Carbides in T1 steel
Carbides in T15 PM steel
Carbides in T91 and T92 heat resistant steels
Carbides in TRIP steel
Carbides in UTOP 38 and UTOP 55 steels (filler materials)
Carbides in Vanadis 23 and AISI M3;2 PM steels
Carbides in Vanadis 6 PM steel
Carbides in Vanadis 6 steel
Carbides in Vanadis PM steel
Carbides in W1 steel
Carbides in W2 steel
Carbides in X155CrVMo121 steel
Carbides in X46Cr13 steel
Carbides in alloyed steel
Carbides in annealed microstructure of M4 high speed steel
Carbides in annealed microstructure of M42 high speed steel
Carbides in annealed microstructure of T1 high speed steel
Carbides in annealed microstructure of T15 high speed steel
Carbides in annealing quality in A6 tool steel
Carbides in austempered ductile iron (ADI)
Carbides in carbon, chromium and high speed steel recoreded by AFM
Carbides in carburized microstructures of P5 steel
Carbides in cast and hot-deformed S 6-5-2-5 high speed steel
Carbides in cast martensitic stainless steel
Carbides in cold work tool steel
Carbides in cold work tool steel
Carbides in cold work tool steels (A2, D2, O1, S7, A8 and A11)
Carbides in creep resistant steel
Carbides in high speed steel
Carbides in high speed steel rolls
Carbides in high speed steels
Carbides in high strength spring steel
Carbides in hot bands in low carbon steel
Carbides in hot work tool steel
Carbides in hot work tool steels
Carbides in plastic mould steel
Carbides in quenched and tempered microstructures of S1, O1 and M2 steels
Carbides in quenched microstructure of D2, D3, M1 and M4 steels
Carbides in quenched microstructure of P20, H11, H13 and H21 steels
Carbides in quenched microstructure of W1 steel
Carbides in quenched microstructures of A2 steel
Carbides in quenched microstructures of O1 steel
Carbides in quenched microstructures of S7 steel
Carbides in spray-formed AISI M32 high-speed steel
Carbides in tempered martensitic tool steels D3, H13, L6, H21, M42 and T15
Carbides in tempered microstructure of D2 steel
Carbides in the cryogenic treated AISI M2 steel
Carbides in the microstructure of 1.3247 steel
Carbides in the quenched microstructure of 1.3346 steel
Carbides in the soft annealed microstructure of 1.4034 steel
Carbides in the white layer of AISI 52100 steel
Carbides in tool steels with high chromium content
Carbides shape, size - Mean free path
Cementite in Fe ?0.16% C ?1.26% Mn?0.22% Si?0.15% Cr steel
Cementite in 0.17C-0.74Mn steel
Cementite in 1.2 wt% C steel
Cementite in 1.31C-0.35Mn-0.25Si steel
Cementite in 100Cr6 steel
Cementite in 100CrMn6 steel
Cementite in 8620 steel
Cementite in 9310 alloy steel
Cementite in AISI 5160 steel
Cementite in Fe ? 0.94% C ? 0.51% Mn ? 0.32% Si ? 1.34% Cr steel
Cementite in Fe ?0.11% C ?0.85% Mn?0.21% S steel
Cementite in Fe-1% C
Cementite in Ni-Hard cast iron
Cementite in Ni-Hard cast iron
Cementite in Nihard cast iron
Cementite in O6 steel
Cementite in S10C low carbon steel
Cementite in TWIP steel
Cementite in W1 steel I
Cementite in W1 steel II
Cementite in W2 carbon tool steel
Cementite in chill cast hypoeutecic gray
Cementite in ductile cast iron
Cementite in ductile cast iron
Cementite in eutectoid steel
Cementite in eutectoid steel
Cementite in high carbon tool steel
Cementite in high strength steel
Cementite in hyper-eutectic white cast iron
Cementite in hyper-eutectoid steel
Cementite in hyper-eutectoid steel
Cementite in ledeburite in Ni-Hard cast iron
Cementite in ledeburite in pearlitic ductile iron
Cementite in low-carbon steel
Cementite in pearlitic ductile iron
Cementite in spheroidize annealed W1 tool steel
Cementite in unalloyed white iron
Cementite in white cast iron
Cementite in white cast iron
Cementite particles in W1 carbon tool steel
Chi and Laves phases in Cr-Co-Mn steel
Chi and Laves phases in Cr-Co-Mn steel
Chi and Laves phases in Cr-Co-Mo steel
Chromium carbides in 3% chromium steel for rolls
Chromium carbides in high speed tool steel
Coarse acicular chromium carbides in Fe ? 2.95% C ? 0.61% Mn ? 29.3% Cr cast iron
Coarse intergranular and intragranular proeutectoid cementite in Fe ? 1.4% C binary alloy
Coarse intergranular proeutectoid cementite in a hot-rolled Fe ?1.2% C binary alloy
Complex carbides in hard faced surface double layer hard faced Cera metal sheet
Cr23C6 and Cr3C2 carbides in low carbon steel
Cr23C6 and Cr7C3 carbides in CA6NM cast stainless steel
Cr23C6 and Cr7C3 carbides in heat resistant steel
Cr23C6 carbides in 1Cr22Mn16N steel
Cr23C6 carbides in LDX 2101 steel
Cr2C, Cr3C2, Cr23C6 and Cr7C3 carbides in AISI 446 steel
Cr7C3 and Cr23C6 carbides in D3 steel
Cr7C3 and Cr3C2 carbides in the chromium carbide coated on AISI D2 steel
Cr7C3 and Mo2C carbides in high Cr cast iron
Cr7C3 and Mo2C carbides in high chromium cast iron
Distribution of nitro-carbides in VANCRON 40 steel
Epsilon carbides in AISI 4340 ultrahigh-strength martensitic steel
Epsilon, M3C, MC, M2C carbides in HS18-0-1 steel
Etchants for cast iron
Eutectic carbides in alloyed white cast iron
Fe2MoC carbides in grade P11 SA335 steel
Fe3C and Mo2C carbides in SA 508 Cl. 3 steel
Fe3C and NbC carbides in 0.14C-1.48Mn-0.78Si-0.052Nb steel
Fe3C and NbC carbides in 3.4C?0.9Si?0.7Mn?4.4Ni?1.8Cr?0.4Mo cast steel roll
Fe3C and V4C3 carbides in 60CrV7 steel
Fe3C carbides in 0.6C-10.8Mn-1.44Cr steel
Fe3C carbides in Fe-0.85Mo-2Ni-0.6C PM steel
Fe3C carbides in Fe?0.17C steel
Fe3C carbides in Ni Resist
Fe3C carbides in W1 steel
Fe3C carbides in spheroidized microstructure of W1 tool steel
Fe3C, Cr7C3, Mo2C, and (Mn,Mo)2C carbides in 20MoCrS4 steel
Fe3C, M23(C,B)6 carbides in microalloyed constructional steels
Fe3Mo3C carbides in sinter-hardening steel
Ferrite and carbides in 1.28C-1.04Si-24.7Cr-1.14Ni steel
Ferrite and carbides in 1.4138 steel
Ferrite and carbides in 1.4138 steel
Fine carbides of chromium, molybdenium and vanadium in the microstructure of TENASTEEL steel
Grain boundary carbide networks in 420 stainless steel
Grain boundary carbide networks in 420 stainless steel
Grain boundary carbide networks in P5 tool steel
Hardness of various carbide types in HiCr cast steel rolss
Heavy grain boundary carbide networks in failed 8620 mold
High Speed Tool Steels - Heat-Treated Microstructures & Surface Conditions
Hot rolled and slowly cooled Hadfield manganese steel
Influence of austenitizing temperature on the microstructure of 440C martensitic stainless steel
Influence of austenitizing temperature on the microstructure of D2 tool steel
Influence of austenitizing temperature on the microstructure of D2 tool steel
Influence of excessive austenitizing temperature on the microstructure of 440C martensitic stainless steel
Influence of starting microstructure on spheroidize annealed microstructure of W1 tool steel
Influence of starting microstructure on the spheroidize annealed microstructure of S5 tool steel
Influence of starting microstructure on the spheroidize annealed microstructure of S5 tool steel
Influence of starting microstructure on the spheroidize annealed microstructure of S5 tool steel
Influence of starting microstructure on the spheroidize annealed microstructure of S5 tool steel
Influence of the normalizing temperature upon the grain size and microstructure of 1040 carbon steel
Intergranular and intragranular cementite in W1 steel
Intergranular carbide network in Fe ?1.31% C ?0.35% Mn?0.25% Si steel
Intergranular cementite film in hypereutectoid steel
Intergranular cementite films in Fe-1.31% C?0.35% Mn?0.25% Si steel
Intergranular cementite grain boundary networks in Fe ?1.31% C ?0.35% Mn?0.25% Si steel
Intergranular cementite in AISI 9310 steel
Intergranular proeutectoid cementite in Fe ? 1.0% C binary alloy
Intermetallic phases in CD3MN duplex stainless steel
Intragranular cementite in high-carbon tool steel
Lamellar pearlite and carbides in 0.82C-5.10Cr-0.28Mo steel
Lamellar pearlite and carbides in 0.95C-3.10Cr-0.14V-0.51Mo steel
Ledeburite in Fe ? 4.0% C ? 0.3% Si ? 0.16% Mn ? 0.91% Cr white cast iron
Ledeburite in eutectic white cast iron
Ledeburite in eutectic white cast iron
Ledeburite in white cast iron
Ledeburitic and secondary carbides in 1.2379 steel
Ledeburitic and secondary carbides in the low tempered microstructure of 1.2379 steel
Ledeburitic carbides ((Fe,Cr,Mo)3C) in nodular cast iron
Ledeburitic carbides in G200CrMoNi4-6-3 cast steel
Ledeburitic carbides in nodular cast iron
Ledeburitic carbides in nodular cast iron
Ledeburitic carbides in nodular cast iron
M(C,N) and M6C in Vancron PM steel
M23(C,B)6 carbides in microalloyed constructional steel
M23(C,B)6, TiC and NbC carbides in 18% Cr ferritic stainless steel
M23C6 and Laves phase in HCM12A steel
M23C6 and VC carbides in HCM12 steel
M23C6 carbides in 12Cr?2W?Cu?V?Nb creep resistant steel
M23C6 carbides in 2205 duplex stainless steel
M23C6 carbides in 316 and 316 L stainless steels
M23C6 carbides in AISI 420 steel
M23C6 carbides in AISI 420 steel
M23C6 carbides in AISI 420 steel - As-received samples
M23C6 carbides in AISI 420 steel - Sub-zero tempering followed by tempering
M23C6 carbides in AISI 420 steel - The effect of austenitising temperature on microstructure
M23C6 carbides in AISI 420 steel - The effect of austenitising temperature on the asquenched microstructure and properties of heats 1 and 2
M23C6 carbides in AISI 420 steel - The effect of double tempering on microstructure
M23C6 carbides in AISI 420 steel - The effect of sub-zero tempering on microstructure
M23C6 carbides in AISI 420 steel - The effect of tempering temperature on microstructure
M23C6 carbides in ASTM A213?T91 steel
M23C6 carbides in ASTM A351 steel
M23C6 carbides in Cr-Co steel
M23C6 carbides in DT4 series steels
M23C6 carbides in E911 creep resisting steel
M23C6 carbides in E911 steel
M23C6 carbides in Fe-12Cr-0.2C
M23C6 carbides in Fe-30.8 Ni-26.6 Cr steel
M23C6 carbides in HCM12A steel
M23C6 carbides in NF709 and NF709R steels
M23C6 carbides in P91 creep resistant steel
M23C6 carbides in P91 steel
M23C6 carbides in P92, HCM12 and X20CrMoV121 steels
M23C6 carbides in TENARIS grade 91 and 911 steels
M23C6 carbides in UNS S31803 steel
M23C6 carbides in X11CrMoWVNb9-1 (T/P911) steel
M23C6 carbides in X11CrMoWVNb9-1 (T/P911) steel
M23C6, M6C and MC carbides in 2.25Cr?1Mo steel
M23C6, M6C and MC carbides in AISI 316, AISI 304, X6CrNiMoTi 17-12-2 steels
M23C6, M7C3 and M6C carbides in 2.25%Cr?Mo?V?Nb and 2.25%Cr?W?V?Nb steels
M23C6, M7C3 carbides in alloyed cast iron
M23C6, MC, M7C3 carbides and sigma phase in austenitic stainless steels
M2C and M23C6 carbides in 0.5Mo-0.5Cr-0.25V low alloy creep resistant steel
M2C and M3C carbides in Ni-Hard Iron class I Type B white cast iron
M2C and M6C carbides in M42 steel
M2C and M6C carbides in M42 steel
M2C carbides in M2 steel
M2C, M3C, M23C6 and M7C3 carbides in 13CrMo4-5 steel
M2C, MC carbides in M42 high speed steel
M2X, M23C6 carbides in 1.4460 steel
M3C and M7C3 carbides in white cast iron
M3C and epsilon carbides in 1.22C-1.93Mn-1.52Cr-0.36Mo steel
M3C carbides in 2CR steel
M3C carbides in 3CR steel
M3C carbides in 3CR50C steel
M3C carbides in 3CRMO steel
M3C carbides in GJN-HV 550 white cast iron
M3C carbides in mottled iron
M3C, M23C6 carbides in P91, P92 and E91 creep resistant steels
M3C, M2C, M7C3 carbides in 6CrC cast steel
M3C, M7C3 and M23C6 carbides in X150CrMoV12-1 steel
M3C, M7C3 carbides in Fe-12Cr-1.6Mn-1.0Ni-0.5Si-4.1C white cast iron
M3C, M7C3 carbides in high-chromium white iron
M3C, M7C3, MC, M6C carbides in steel rolls
M3C/M7C3 carbides in 4CRMO steel
M6C and M7C3 carbides in 0.86%C, 7.6%Cr, 0.48%(Nb + V) semi high speed cast steel
M6C and M7C3 carbides in Cr and semi HSS steels for rolls
M6C carbides in T1 steel
M6C, M2C, M23C6 and M7C3 carbides in T24 creep resistant steel
M6C, VC, (CrFeMoW)7C3 and M23C6 carbides in high speed steels
M7C3 and M23C6 carbides in Manet steel
M7C3 and M23C6 carbides in NCWV/D3 tool steel
M7C3 and M23C6 carbides in Stellites 6 and 21
M7C3 and M23C6 carbides in TENASTEEL steel
M7C3 and M23C6 carbides in high chromium cast iron I
M7C3 and M23C6 carbides in high chromium cast iron II
M7C3 and M23C6 carbides in high chromium cast iron III
M7C3 and M23C6 carbides in high chromium white iron
M7C3 and M6C carbides in high Cr and semi high speed steels
M7C3 carbides in 16% Cr white cast iron
M7C3 carbides in 5CR steel
M7C3 carbides in 5CR80MO steel
M7C3 carbides in 5CRDH steel
M7C3 carbides in 5CRMO steel
M7C3 carbides in AISI 440C martensitic stainless steel
M7C3 carbides in AISI D2 steel (bar diameters of 25.4, 70 and 210 mm)
M7C3 carbides in AISI D3 steel
M7C3 carbides in D2 steel
M7C3 carbides in D3 steel
M7C3 carbides in D3 tool steel
M7C3 carbides in EutecticA white cast iron
M7C3 carbides in Fe-2C-12Cr tool steel
M7C3 carbides in HyperA white cast iron
M7C3 carbides in HyperEXP white cast iron
M7C3 carbides in HypoA white cast iron
M7C3 carbides in PM Vanadis 6 steel
M7C3 carbides in SDS II steel
M7C3 carbides in SKD11 steel
M7C3 carbides in WeldoverlayA white cast iron
M7C3 carbides in WeldoverlayB white cast iron
M7C3 carbides in X210CrW12 steel
M7C3 carbides in hardfacing alloy (Fe- 34Cr-4.5C)
M7C3 carbides in high-chromium white cast iron
M7C3, M23C6 and M6C carbides in 13HMF steel
M7C3, M23C6, VC and Mo2C carbides in forged steel rolls
M7C3, M8C7, M23C6 carbides in 4Cr5MoSiV1 steel
MC (or M4C3), M23C6 and M6C carbides in AISI M2 steel
MC and M23C6 carbides in Armour steel
MC and M6C carbides in M4 high speed steel
MC and M6C carbides in M4 steel
MC and M6C carbides in SINTER 23 PM steel
MC and M6C carbides in cast M2 high speed steel
MC and M7C3 carbides in PM tool steel
MC and M7C3 carbides in Thyrospray 2399 PM steel
MC and M7C3 carbides in Vanadis 6 steel
MC and M7C3 carbides in Vanadis 6 steel
MC and M7C3 carbides in Vanadis 6 steel
MC and M7C3 carbides in Vanadis 6 steel
MC and M7C3 carbides in tool steels made by spray forming
MC carbide segregation in H13 tool steel
MC carbides in 0.17C-1.37Mn-0.24Cr-0.48Mo steel
MC, M2C and M6C carbides in K390 steel
MC, M2C and M6C carbides in S 6-5-2-5 high speed steel
MC, M2C and M6C carbides in semi high speed steel for rolls
MC, M2C and M7C3 carbides in Wear resistant cast iron for rolls
MC, M2C, M6C carbides in AISI M2 high speed steel
MC, M2C, M6C, M7C3 carbides in cast high speed steels (HSS) for rolls
MC, M2C, M7C3 and M23C6 carbides in cast high speed roll
MC, M2C, M7C3 and M23C6 carbides in high speed steel roll
MC, M2C, M7C3 carbides in Fe-5%Cr-5%Mo-5%W-5%V-5%Co-2.0%C cast steel
MC, M2C, M7C3, M23C6 carbides in Aurora and Kosmos HSS steels
MC, M2C, M7C3, M23C6 carbides in cast HSS roll
MC, M6C, M7C3 and M23C6 carbides in 1.2690 steel
MC, M6C, M7C3, M23C6 carbides in HS3-1-2, HS6-5-2 steels
MC, M7C3 carbides in ROLTEC,TOUGHTEC, WEARTEC, AISI A2, D2 and D6 steels
Martensite and carbides in 0.82C-5.10Cr-0.28Mo steel
Martensite and carbides in 1.2436 steel
Martensite and carbides in 1.3255 steel
Martensite and carbides in 1.3355 steel
Martensite and carbides in 1.4112 steel
Martensite and carbides in 1.4122 steel
Martensite and carbides in APM 60 steel
Martensite and carbides in SS 2726 steel
Martensite, delta ferrite and carbides in 1.4000 steel
Martensite, delta ferrite and carbides in 1.4021 steel
Martensite, primary and secondary carbides in 0.8C-8Cr-1.6Mo-0.6V steel
Martensite, primary and secondary carbides in 1.25C-0.90Si-8.75Cr-2.70Mo-1.18V steel
Martensite, primary and secondary carbides in 1.3207 steel
Martensite, retained austenite and carbides in 1.3344 steel
Martensite, retained austenite and carbides in SS 2726 steel
Martensite, up to 5% of bainite, primary and secondary carbides in 1.2063 steel
Massive cementite in Ni-Hard cast iron
Massive cementite particles in SAE 8620 alloy steel
Microstructures in a eutectoid steels
Microstructures of D2 steel vs. bar diameters
Microstructures of different commercial grades of M2 steels
Mo2C, (V,Ti)C, (Fe,Mo)6C, Fe7C3, Fe3C carbides in austempered ductile iron (ADI)
Mo2C, M7C3 and VC carbides in SHSS II steel
NbC and Cr23C6 carbides in high Cr (11 wt.%) tempered martensitic steel
NbC carbides in microalloyed Nb-Mo steel
NbC in cast irons
Network of cementite in Fe ?0.94% C ?0.51% Mn?0.32% Si?1.34% Cr steel
Network of eutectic carbides in alloyed white cast iron
Pearlite, primary and secondary carbides in 0.80C-0.85Si-3.0Cr-0.18Mo-0.20V steel
Precipitates in 1.6310 steel
Precipitates in 1.6359 steel
Precipitates in 20Cr-25Ni steel
Precipitates in 9% Cr steel with Co
Precipitates in AISI 347 stainless steel
Precipitates in X2NiCoMo18-12-2 steel
Precipitates in ferritic steels
Precipitates in low carbon steel
Precipitates in micro alloyed steel
Primary and secondary carbides in 1.2063 steel
Primary and secondary carbides in 1.2344 steel
Primary and secondary carbides in 1.2363 steel
Primary and secondary carbides in 1.2379 steel
Primary and secondary carbides in 1.2379 steel
Primary and secondary carbides in 1.3343 steel
Primary and secondary carbides in Cr-Hard (Maxidur) cast iron
Primary carbide particles of MC type in H11 steel
Primary carbides in D3 steel
Primary carbides in white cast iron
Proeutectic cementite in NiHardcast iron
Proeutectic cementite in heat treated Ni-Hard cast iron
Proeutectoid cementite in Fe ?1.31% C water-hardenable tool steel
Proeutectoid cementite in Fe-1% C steel
Proeutectoid cementite in hot rolled Fe-1% C steel
QT microstructure with the carbides in 1.3244 steel
Residual alloy carbide in PM M42 high speed steel
Residual alloy carbides in PM M42 high speed steel
Residual carbides in W1 steel
Residual cementite in 52100 steel
Retained austenite in AISI D2 steel
Segregation in PM stee
Segregations in hot work tool steel
Sigma phase in ASTM A890/A890M Grade 6A steel
Sigma phase in Cr-Co steel
Sigma phase in Cr-Co-Mo steel
Sigma phase in Cr-Ni steel
Sigma phase in Cr-Ni steel
Sigma phase in Cr-Ni steel
Sigma phase in Cr-Ni steel
Sigma phase in Mo stainless steel
Sigma phase in steel specimen removed from a furnace door
Spheroidized cementite in Fe?1% C?1.5% Cr steel
Spheroidized pearlite and carbides in 1.2631 steel
Spheroidized pearlite and carbides in 1.34C-0.85Si-0.67Mn-0.21Mo steel
Spheroidized pearlite and carbides in 1.4125 steel
Spheroidized pearlite and carbides in OH236NI steel
Spheroidized pearlite in 1.2344 steel
Spheroidized pearlite in S5 steel
Spheroidized pearlite in S5 steel
Spheroidized pearlite, Ti(C,N) and carbides in 1.2344 steel
Tantalum carbide powder
Tempered martensite and carbides in 0.85C-3.00Cr-0.13V-0.48Mo steel
Tempered martensite and carbides in 1.2235 steel
Tempered martensite and carbides in 1.2327 steel
Tempered martensite and carbides in 1.2375 steel
Tempered martensite and carbides in 1.2842 steel
Tempered martensite and carbides in 1.3343 steel
Tempered martensite and carbides in 1.4125 steel
Tempered martensite and carbides in 1.4304 steel
Tempered martensite and carbides in X48CrMoV8-1-1 steel
Tempered martensite and carbides in X48CrMoV8-1-1 steel
Tempered martensite and primary and secondary carbides in 1.2379 steel
Tempered martensite, primary and secondary carbides in 0.85C-4.04Cr-17.0W-1.45V-0.85Mo
Tempered martensite, primary and secondary carbides in 1.4122 steel
Tempered martensitic tool steel microstructures of S1, O1 and M2 steels
The Bohler microscope standard chart for the characterization of carbide distributions of high speed steels
TiC carbides in 0.42C?0.30Ti steel
TiC in Fe-10% TiC composite
TiC in Fe-10% TiC composite
TiC in Fe-10% TiC composite
Undissolved cementite in 5160 alloy steel
V4C3, C7C3 and VC carbides in K190 ISOMATRIX PM steel
V4C4 and Cr7C3 carbides in K190 ISOMATRIX PM steel
V8C7, M7C3 carbides in cast high speed steel for rolls
VC and M23C6 carbides in HCM12 steel
VC and W3Fe3C carbides in HSS6-5-2C high speed steel
VC cabides in microalloyed steel
VC carbides in Fe?V?C stel
VC carbides in high vanadium cast iron
VC carbides in medium carbon steel with higher V
VC, Fe3C, M7C3 and M23C6 carbides in 12X1MO steel
Widmanstatten intragranular cementite in Fe ? 1.31% C ? 0.35% Mn ? 0.25% Si steel
Widmanstatten intragranular cementite in water hardenable tool steel