M2C Cabides in Steels

(Cr15.58Fe7.42)23C6 and V8C7 carbides in PM AISI M2 steel
(FeCrMo)C and (FeCrMoMn)C carbides in 10CrMo9-10 steel
(Mo,Cr)2C carbides in Fe-1.7C-1.2Si-l.1Mn-0.8Ni-3.6Cr-1.7Mo-4.7V alloy
(Mo,V)2C, (Fe,Mo)6C and VC carbides in high speed steel produces by CDC process
C2C, Cr3C2, Cr7C2, Cr7C3 and Cr23C6 carbides in AISI 446 steel
Carbides in 0.10C-1.99Mn-1.60Mo steel
Carbides in 2.25Cr-1Mo weld/mild steel interface
Carbides in AISI M1 high speed steels
Carbides in HSS7 steel
Carbides in HiCr iron rolls
Carbides in M50 high speed steel
Carbides in annealed microstructure of M42 high speed steel
Carbides in annealed, hardened and tempered S 6-5-2-5 high speed steel
Carbides in cast and hot-deformed S 6-5-2-5 high speed steel
Carbides in high speed steel
Carbides in semi-high-speed steel (HSS)
Cementite in Dillidur 690 steel
Cementite in martensitic steel
Characteristic carbides (MC, M2C, M3C, M7C3, M23C6) in white cast iron
Cr23C6, VC, Fe3C, Mo2C, Nb4C3 carbides in R7, R47, R102A, R147, R191, R192 and R206N steels
Cr2C, Cr3C2, Cr23C6 and Cr7C3 carbides in AISI 446 steel
Cr7C3 and Cr23C6 carbides in D3 steel
Cr7C3 and Mo2C carbides in high Cr cast iron
Cr7C3 and Mo2C carbides in high chromium cast iron
Cr7C3, V8C7, V4C3; Mo2C, (Fe3W3)C-(Fe4W2)C carbides in HS7-7-7-10 - Annealed condition
Epsilon and M3C carbides in 35MnCrMoV8-6-4-1 steel
Epsilon, M3C, M2C carbides in 30CrMoNiV10-25-6-2 steel
Epsilon, M3C, MC and M2C carbides in 0.30C-2.50Cr-2.60Mo-1.59Ni-0.18V hot work tool steel
Epsilon, M3C, MC and M2C carbides in 30CrMoNiV10-25-6-2 hot work tool steel
Epsilon, M3C, MC, M2C carbides in HS18-0-1 steel
Epsilon, MC and M2C carbides in HS18-0-1 and HS6-5-2 steels
Etchants for carbides in steels
Fe2MoC carbides in grade P11 SA335 steel
Fe3C and Mo2C carbides in SA 508 Cl. 3 steel
Fe3C, Cr7C3, Mo2C, and (Mn,Mo)2C carbides in 20MoCrS4 steel
Fe3C, M23(C,B)6 carbides in microalloyed constructional steels
M23C6 and M2X carbides in 9Cr-1Mo steel
M23C6 and M7C3 carbides in 2.25Cr–1.0Mo steel
M23C6 carbides in P91 steel
M23C6 carbides in P92 creep resistants steel
M23C6 carbides in austenitic stainless steel
M23C6, M2C and M6C carbides in low alloy Cr-Mo-Ni-V steel
M23C6, M3C, M2C and M6C carbides in ASTM A387-22-CL2 steel
M23C6, M6C and M2C carbides in Cr-Mo-Ni-V steel for turbine rotor
M23C6, M6C and MC carbides in 2.25Cr–1Mo steel
M23C6, NbC and M7C3 carbides in steels for nuclear industry
M23C6, V8C7, MC and M2C carbides in spray formed AISI M2 steel
M2C and M23C6 carbides in 0.5Mo-0.5Cr-0.25V low alloy creep resistant steel
M2C and M3C carbides in Ni-Hard Iron class I Type B white cast iron
M2C and M3C carbides in the cryogenic quenching of AISI A2 steel
M2C and M6C carbides in M42 steel
M2C and M6C carbides in M42 steel
M2C and M7C3 carbides in high-chromium white iron
M2C carbides in 2.25Cr1Mo steel
M2C carbides in M2 steel
M2C carbides in martensitic steel
M2C, M3C and M7C3 carbides in Caldie hot work tool steel
M2C, M3C, M23C6 and Cr7C3 carbides in 2.25Cr–1Mo (ASTM A387-22-CL2) steel
M2C, M3C, M23C6 and M7C3 carbides in 13CrMo4-5 steel
M2C, M3C, M7C3 and M23C6 carbides in 1.25Cr–0.5Mo steel
M2C, M6C and M7C3 carbides in Fe3Al alloy
M2C, M6C carbides M23C6 in 10% Cr steel
M2C, M6C, M7C3 and M23C6 carbides 2.25Cr1Mo steel
M2C, M6C, M7C3 carbides in Fe3Al-based alloy
M2C, M6C, TiC, VC and NbC carbides in AISI M7 cast high speed steel
M2C, M7C3, M23C6 and M6C carbides in 2.25Cr-1Mo steel
M2C, MC and M6C carbides in AISI M2 high speed steel
M2C6 cabides in P92 martensitic chromium steel
M3C and M7C3 carbides in 3Cr1.5Mo power plant steel
M3C, M2C, M7C3 and M23C6 carbides in 3Cr1.5Mo and 21–4 Cr1Mo steels
M6C and M7C3 carbides in 0.86%C, 7.6%Cr, 0.48%(Nb + V) semi high speed cast steel
M6C and Mo2C carbides in Fe-2.2C-20.5Mo steel
M6C, M2C, M23C6 and M7C3 carbides in T24 creep resistant steel
M7C3 and M23C6 carbides in 2.25Cr-1.0Mo steel
M7C3 and M23C6 carbides in MANET steel
M7C3 and M23C6 carbides in Manet steel
M7C3 and M6C carbides in high Cr and semi high speed steels
M7C3 and Mo2C carbides in Fe-0.9C-11.3Cr-0.7Mn-2.95Mo-0.3Si and Fe-1.33C-6.8Cr-2.4Mo-0.2Si steels
M7C3, (Fe,Cr)23C6 and Mo2C carbides in high alloyed chromium cast iron
M7C3, M23C6 and M6C carbides in 13HMF steel
M7C3, M23C6 and M6C carbides in 13HMF steel
M7C3, M23C6, MC and M3C carbides in G21CrMoV4 – 6 (L21HMF) low alloy cast steel
M7C3, M23C6, VC and Mo2C carbides in forged steel rolls
M7C3, M2C and MC carbides in semi-HSS grades
M7C3, MC and M2C carbides in hardfacing steel
MC and M6C carbides in AISI M2 steel
MC and M6C carbides in HS 6-5-3 steel
MC and M6C carbides in cast M2 high speed steel
MC, M2C and M6C carbides in K390 steel
MC, M2C and M6C carbides in AISI M2 high speed steel manufactured by different casting technologies
MC, M2C and M6C carbides in S 6-5-2-5 high speed steel
MC, M2C and M6C carbides in semi high speed steel for rolls
MC, M2C and M7C3 carbides in Wear resistant cast iron for rolls
MC, M2C and M7C3 carbides in cast high speed steel roll
MC, M2C carbides in HSS7 steel for rolls
MC, M2C, M3C, M7C3 and M23C6 carbides in 2CrMoNiWV creep resistant steel III
MC, M2C, M3C, M7C3 and M23C6 carbides in G21CrMoV4 – 6 (L21HMF) cast steel
MC, M2C, M3C, M7C3, M23C6 and M6C carbides in 2CrMoNiWV creep resistant steel II
MC, M2C, M3C, M7C3, M23C6 and M6C carbides in 2CrMoNiWV creep resistant steel IV
MC, M2C, M3C, M7C3, M23C6 and M6C carbides in 2CrMoNiWV creep resistant steel V
MC, M2C, M6C and M7C3 carbides in 2%C–5%Cr–5%V–5%Mo–5%W–5%Co white cast iron
MC, M2C, M6C, M7C3 carbides in cast high speed steels (HSS) for rolls
MC, M2C, M7C3 and M23C6 carbides in Kosmos and Aurora steels
MC, M2C, M7C3 and M23C6 carbides in cast high speed roll
MC, M2C, M7C3 and M23C6 carbides in high speed steel roll
MC, M2C, M7C3, M23C6 carbides in Aurora and Kosmos HSS steels
MC, M2C, M7C3, M23C6 carbides in cast HSS roll
MC, M3C, M6C and M7C3 carbides in SS2541, THG2000, QRO90 and MCG 4M steels
MC, M7C3 and M2C carbides in cast high speed steel roll
MC, M7C3 and M6C carbides in THG2000, MCG2006 and QRO90 steels
Mo2C and (Fe,Cr)7C3 carbides in high Cr white cast iron Fe-21Cr-3Ni-1.7Mo-2.4C
Mo2C and Fe3C carbides in Fe–C–Mo martensitic steel
Mo2C and Ksi carbides in SA508 Gr3 nuclear reactor steel
Mo2C and NbC carbides in Fe–4Mo–0.1Nb–0.2C steel
Mo2C and VC carbides in Cr-Mo-V steel
Mo2C carbides in AISI H13 steel
Mo2C carbides in AISI H13 steel implanted with molybdenum ions
Mo2C carbides in Cr-Mo steel
Mo2C carbides in Cr-Mo steel
Mo2C carbides in Cr-Mo steel
Mo2C carbides in Cr-Mo steel
Mo2C carbides in Cr-Mo steel
Mo2C carbides in Cr-Mo steel
Mo2C carbides in Fe-0.35C-0.9Mo steel
Mo2C carbides in Fe-C-Mo steel
Mo2C carbides in Fe–4Mo–0.2C steel
Mo2C carbides in JAC590R steel
Mo2C carbides in molybdenum steel
Mo2C carbides in molybdenum steel
Mo2C carbides in molybdenum steel
Mo2C carbides in molybdenum steel
Mo2C carbides in molybdenum steel
Mo2C, M7C3 and VC carbides in SHSS II steel
Nanosize cementite in unalloyed steel
NbC, M23(B,C)6 and M2,3C carbides in hardfacing alloys
Primary MC carbide in 0-5-1-2Ti grade cast high speed steel
Some properties of metallic hard materials
Time–temperature–precipitation diagrams (TTP) for low alloyed steels
V6C5 carbides in microalloyed steel
V8C7, Mo2C, (Fe3W3)C – (Fe4W2)C carbides in 1.3344 steel - Annealed condition
VC and Mo2C carbides in Cr-Mo-W-V steel
VC and Mo2C carbides in Cr-Mo-W-V steel
VC and W-Mo carbides in HSS rolls
VC, Mo2C, (Fe,Cr)3C and (Cr,Fe)7C3 carbides in a new hot work tool steel
VC, Mo2C, M7C3 and M23C6 carbides in forged high speed steel roll
W2C carbides in Fe–6W–0.23C steel