Mg-Al-Zn-Mn alloys - General macrostructure

Material Name: Mg-Al-Zn-Mn alloys
Recipe No.: 9598
Primary Chemical Element in Material: Mg
Sample Type: Bulk
Uses: General macrostructure
Etchant Name: None
Type (Macro/Micro): Macro
Etching Method: Chemical
Etchant (Electrolyte) Composition: 100 ml ethanol saturated with picric acid, 10 ml acetic acid.
Procedure (Condition): Use fresh solution to reveal grain structure.
Note: Montgomery
Reference: Vander Voort, Metallography Principles and Practice, McGraw-Hill, Inc., 1984, p. 524.