Silicon Carbide - SiC

Classification: Carbide
Atomic numbers: 14 & 6
Atomic weight: 40
Melting point (C): 2700
Boiling point (C): 2100 (sublimes)
Density (g/cm3): 3.21
Refractive index (n=): 2.654-2.697 (2.4-2.8)
Hardness (Mosh-scratch):
Crystal structure: Hexagonal-normal, alpha: (10T0) prism, isometric-normal, beta: (100) cube
Color (solid): Blue-black
Cleavage: Basal/cubic: (0001)/(001)