Cadmium Selenide - CdSe

Classification: Selenide
Atomic numbers: 48 & 34
Atomic weight: 191.3
Melting point (C): cca. 1000
Boiling point (C):
Density (g/cm3): cca. 6
Refractive index (n=):
Band gap (eV): 1.8
Hardness (Mosh-scratch): 5-6
Crystal structure: Hexagonal-normal: (10T0) prism
Color (solid): Yellowish
Cleavage: Basal-distinct: (0001)