Correlation of Hardenability and CCT and TTT Curves II

Steel name: Steel
Diagram No.: 2105
Chemical composition in weight %: No data
Steel group: Steels
Applications: No data
Comment: Superposition of cooling curves obtained along a Jominy test bar on the TTT curve of a steel. Note fastest cooling on the water-quenched end yielding a martensitic microstructure and slowest cooling on the air-quenched end yielding a pearlitic microstructure and lowest hardness. Intermediate cooling rates and microstructures are obtained between these two cooling limits.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: No data

Hardenability Diagram

Price: 20.00 US $
Buy Online Hardenability Diagram

Other Steel Data links:
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Transformation Diagrams of Non-Ferrous Alloys
Tempering Diagrams of Steels

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.