Citric Acid:H2O2 - InGaAs/AlGaAs/GaAs - Wet Etchant by Chemical Composition

Material Name: InGaAs/AlGaAs/GaAs
Recipe No.: 4955
Primary Chemical Element in Material: In, Al, Ga
Sample Type: Wafer
Uses: Etching
Etchant Name: None
Etching Method: Wet etching
Etchant (Electrolyte) Composition: Citric acid:H2O2 (4:1)
Procedure (Condition): No data
Note: Wet etchant by chemical composition. GaAs selective etch from AlxGa1ÿxAs (Table 1). Ref. (Tong, N., 1992b).
Reference: A.R. Clawson, Guide to references on III-V semiconductor chemical etching, Materials Science and Engineering (Original Reference List), 31 (2001), p. 157.

Table 1: Etch rates.