Chemical Composition of Steels in Weight %
0.005% C, 0.05% Si, 0.10% Mn, 5.00% Mo, 18.50% Ni, 9.00% Co, 0.70% Ti, 0.10% Al
0.005% C, 4.85% Mo, 18.00% Ni, 9.25% Co, 1.00% Ti
0.02% C, 0.25% Si, 0.25% Mn, 0.015% P, 0.010% S, 9.50-10.50% Cr, 1.75-2.25% Mo, 11.50-13.00% Ni, 0.95-1.50% Ti, 1.30-1.70% Al, 0.01% N
0.02% C, 0.25% Si, 0.25% Mn, 11.00-12.50% Cr, 1.75-2.25% Mo, 10.25-11.25% Ni, 0.20-0.50% Ti, 1.35-1.75% Al
0.02% C, 5.00% Mo, 18.00% Ni, 10.00% Co, 1.00% Ti
0.02% C, 5.00% Mo, 18.00% Ni, 10.00% Co, 1.00% Ti
0.02% C, 5.00% Mo, 18.00% Ni, 10.00% Co, 1.00% Ti
0.020% C, 0.70% Si, 0.90% Mn, 0.040% P, 0.030% S, 11.75% Cr, 0.40% Ni, 0.030% N
0.025% C, 0.40% Si, 0.70% Mn, 12.00% Cr, 0.50% Mo, 4.10% Ni
0.025% C, 0.40% Si, 0.70% Mn, 12.00% Cr, 0.50% Mo, 4.10% Ni
0.03% C, 0.10% Si, 0.15% Mn, 5.20% Mo, 18.00% Ni, 9.50% Co, 0.95% Ti
0.03% C, 0.10% Si, 0.15% Mn, 9.50% Co, 5.20% Mo, 18.00% Ni, 0.95% Ti, + special additions
0.03% C, 0.10% Si, 0.15% Mn, 9.50% Co, 5.20% Mo, 18.00% Ni, 0.95% Ti, + special additions
0.03% C, 0.10% Si, 0.15% Mn, 9.50% Co, 5.20% Mo, 18.00% Ni
0.03% C, 0.30% Si, 0.30% Mn, 12.00% Cr, 1.40% Mo, 1.60% Al
0.03% C, 0.30% Si, 0.30% Mn, 12.00% Cr, 1.40% Mo, 9.20% Ni, 1.60% Al
0.03% C, 17.00-18.00% Cr, 2.50-3.00% Mo, 12.50-13.50% Ni
0.03% C, 3.00% Mo, 18.00% Ni, 10.00% Co, 1.00% Ti
0.03% C, 5.00% Mo, 18.00% Ni, 10.00% Co, 1.00% Ti
0.03% C, 5.00% Mo, 18.00% Ni, 10.00% Co, 1.00% Ti
0.03% C, 5.00% Mo, 18.00% Ni, 9.50% Co, 1.00% Ti
0.030% C, 0.20% Si, 12.00% Cr, 2.00% Mo, 8.90% Ni, 1.60% Ti, 0.030% N
0.03% C, 0.40% Mn, 0.014% P, 0.018% S, 0.07% Cr, 9.00% Ni
0.03% C, 0.40% Mn, 0.014% P, 0.018% S, 0.07% Cr, 9.00% Ni
0.04% C, 0.25% Si, 12.00% Cr, 7.80% Ni, 1.50% Mo, 1.20% Al
0.04% C, 0.40% Si, 0.40% Mn, 15.40% Cr, 5.30% Ni, 0.90% Mo, 0.04% N
0.04% C, 0.70% Mn, 16.50% Cr, 4.50% Ni, 0.30% Cu, 0.30% Nb
0.05% C, 0.02% Si, 0.13% Mn, 0.012% P, 0.010% S, 3.98% Cr, 0.54% Mo
0.05% C, 0.20% Si, 0.90% Mn, 0.12% S, 12.80% Cr, + Ni
0.05% C, 0.35% Si, 0.35% Mn, 53.00% Ni, 19.00% Cr, 5.00% Nb, 3.00% Mo, 0.90% Ti, 0.50% Al, Fe balance
0.05% C, 0.70% Si, 1.50% Mn, 0.040% P, 0.015% S, 12.00-14.00% Cr, 0.30-0.70% Mo, 3.50-4.50% Ni
0.05% C, 13.00% Cr, 1.50% Mo, 6.00% Ni
0.05% C, 15.00% Cr, 4.50% Ni, 3.50% Cu, + Nb
0.05% C, 15.00% Cr, 4.50% Ni, 3.50% Cu, +Nb
0.05% C, 16.50-17.50% Cr, 2.50-3.00% Mo, 10.00-12.00% Ni
0.05% C, 4.50% Ni, 3.50% Cu, 15.00% Cr, +Nb
0.05% C, 0.90% Mn, 12.70% Cr, 0.14% S, 0.40% Ni
0.06% C, 0.70% Si, 1.50% Mn, 0.040% P, 0.015% S, 15.00-17.00% Cr, 0.80-1.50% Mo, 4.00-6.00% Ni
0.06% C, 15% Mo, 25% Co
0.06% C, 16.00% Cr, 1.10% Mo, 5.00% Ni
0.06-0.11% C, 0.15-0.40% Si, 0.70-1.00% Mn, 0.025% P, 0.015% S, 0.25-0.50% Cr, 0.020-0.050% Ti, 0.0008-0.0040% B
0.06-0.11% C, 0.15-0.40% Si, 0.70-1.00% Mn, 0.025% P, 0.015% S, 0.25-0.50% Cr, 0.020-0.050% Ti, 0.0008-0.0040% B
0.06-0.15% C, 1.00% Si, 1.00% Mn, 0.040% P, 0.020% S, 12.00-14.00% Cr, 0.60% Mo
0.06-0.15% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.15-0.35% S, 12.00-14.00% Cr, 0.60% Mo
0.06-0.15% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.15-0.35% S, 12.00-14.00% Cr, 0.60% Mo
0.07% C, 0.70% Si, 1.50% Mn, 16.00% Cr, 4.00% Ni, 3.50% Cu
0.07% C, 15.00% Cr, 4.50% Ni, 3.50% Cu, 0.30% Nb
0.08% C, 0.20-0.40% Mn, 0.040% P, 0.040% S, 0.007% N
0.08% C, 0.80% Si, 1.50% Mn, 0.020% P, 0.010% S, 15.00% Cr, 1.30% Mo, 26.00% Ni, 0.40% V, 2.00%Ti
0.08% C, 1.00% Si, 1.0% Mn, 15.00-17.00% Cr, 3.00-5.00% Ni, 3.00-5.00% Cu
0.08% C, 1.00% Si, 1.10% Mn, 15.00% Cr, 1.50% Mo, 26.00% Ni, 2.10% Ti
0.08% C, 1.00% Si, 1.10% Mn, 15.00% Cr, 1.50% Mo, 26.00% Ni
0.08% C, 1.00% Si, 1.50% Mn, 0.045% P, 0.020% S, 21.00-23.00% Cr, 2.00-3.00% Mo, 20.00-23.00% Ni, 0.15-0.60% Al, 0.15-0.60% Ti
0.08% C, 17.00-19.00% Cr, 9.00-12.00% Ni, >5C (0.7) Ti
0.08-0.12% C, 0.50% Si, 0.30-0.60% Mn, 0.020% P, 0.005% S, 0.040% Al, 8.00-9.50% Cr, 0.30% Cu, 0.85-1.05% Mo, 0.030-0.070% N, 0.060-0.10% Nb, 0.30% Ni, 0.18-0.25% V
0.08-0.14% C, 0.50% Si, 0.40-0.80% Mn, 0.020% P, 0.010% S, 2.00-2.50% Cr, 0.30% Ni, 0.030% Cu, 0.90-1.10% Mo
0.08-0.15% C, 1.00% Si, 1.00% Mn, 0.040% P, 0.030% S, 11.50-13.50% Cr, 0.75 Ni
0.08-0.15% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.015% S, 11.50-13.50% Cr, 0.75% Ni
0.08-0.15% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.030% S, 11.50-13.50% Cr, 0.75% Ni
0.08-0.15% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.030% S, 11.50-13.50% Cr, 0.75% Ni
0.08-0.15% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.15-0.35% S, 12.00-14.00% Cr, 0.60% Mo
0.08-0.18% C, 0.35% Si, 0.40-1.00% Mn, 0.025% P, 0.010% S, 0.70-1.15% Cr, 0.40-0.60% Mo, 0.30% Cu
0.081% C, 8.94% Cr, 0.476% Mo, 0.19% V, 0.061% Nb, 1.91% W, 0.037% N, 0.005% B
0.09% C, 0.41% Mn, 8.62% Cr, 0.35% Mo, 0.23% Ni, 0.10% V, 1.11% W, 0.050% Nb, 0.0063% B, 0.0345% N
0.09-0.15% C, 0.15-0.40% Si, 0.30-0.60% Mn, 0.035% P, 0.020-0.035% S, 0.40-0.70% Cr, 0.10% Mo, 0.50-0.80% Ni, 0.020-0.050% Al, 0.15-0.30% Pb
0.10% C, 0.30% Si, 2.50% Mn, 3.00% Cr, 0.30% Mo, 1.00% Ni
0.10% C, 0.30% Si, 2.50% Mn, 3.00% Cr, 0.30% Mo, 1.00% Ni
0.10% C, 0.30% Si, 2.50% Mn, 3.00% Cr, 0.30% Mo, 1.00% Ni
0.10% C, 0.30% Si, 2.50% Mn, 3.00% Cr, 0.30% Mo, 1.00% Ni
0.10% C, 0.30% Si, 2.50% Mn, 3.00% Cr, 0.30% Mo, 1.00% Ni
0.10% C, 2.50% Mn, 3.00% Cr, 1.00% Ni
0.10% C, 2.50% Mn, 3.00% Cr, 1.00% Ni
0.10-0.17% C, 0.20-0.30% Si, 0.30-0.50% Mn, 0.030% P, 0.030% S, 0.90-1.20% Cr, 4.20-4.70% Ni
0.10-0.17% C, 0.20-0.35% Si, 0.30-0.50% Mn, 0.030% P, 0.030% S, 0.65-0.85% Cr, 3.30-3.60% Ni
0.10-0.17% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.15-0.35% S, 15.50-17.50% Cr, 0.20-0.60% Mo
0.10-0.17% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.15-0.35% S, 15.50-17.50% Cr, 0.20-0.60% Mo
0.10-0.17% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.15-0.35% S, 15.50-17.50% Cr, 0.20-0.60% Mo
0.10-0.25% C, 1.00% Si, 1.00% Mn, 0.035% P, 0.035% S, 15.50-18.00% Cr, 1.00-2.50% Ni
0.11% C, 0.40% Si, 0.40% Mn, 12.00% Cr
0.11% C, 0.40% Si, 0.40% Mn, 12.00% Cr
0.11% C, 8.16% Cr, 0.91% Mo, 0.206% V, 0.067% Nb
0.11% C, 8.80% Cr, 0.98% Mo, 0.19% V, 0.067% Nb, 0.95% W, 0.063% N
0.115% C, 0.49% Si, 0.35% Mn, 0.018% P, 0.001% S, 11.50% Cr, 0.29% Mo, 0.29% Ni, 0.26% V, 1.50% W, 0.008% Al, 0.050% Nb, 1.62% Co, 0.0049% B, 0.065% N
0.12% C, 0.17% Si, 0.47% Mn, 0.016% P, 0.003% S, 8.62% Cr, 0.94% Mo, 0.93% W, 0.20% V, 0.0018% B, 0.067% N, 0.08% Nb, 0.007% Al
0.12% C, 0.20% Si, 1.30% Mn, 0.10% S, 13.40% Cr, 0.50% Mo, 1.60% Ni, 0.20% V
0.12% C, 0.21% Si, 0.42% Mn, 0.011% P, 0.011% S, 2.17% Cr, 0.93% Mo, 0.16% Ni, 0.003% Al
0.12% C, 0.40% Si, 0.40% Mn, 0.03% P, 0.13% S, 12.50% Cr, 0.40% Mo
0.12% C, 0.40% Si, 0.40% Mn, 0.13% S, 12.50% Cr, 0.40% Mo
0.12% C, 0.40% Si, 0.50% Mn, 12.50% Cr
0.12% C, 0.40% Si, 0.50% Mn, 12.50% Cr
0.12% C, 0.40% Si, 0.60% Mn, 0.025% P, 0.005% S, 12.00% Cr, 0.30% Ni
0.12% C, 0.40% Si, 0.60% Mn, 0.025% P, 0.025% S, 12.00% Cr, 0.30% Ni
0.12% C, 0.40% Si, 0.60% Mn, 0.025% P, 0.025% S, 12.00% Cr, 0.30% Ni
0.12% C, 0.75% Cr, 3.30% Ni
0.12% C, 0.85% Cr, 1.60% Ni
0.12% C, 14.00% Cr, 4.75% Mo, 0.60% V, 2.00% Ni, 12.50% Co, 0.02% Nb
0.12-0.18% C, 0.15-0.40% Si, 0.30-0.60% Mn, 0.025% P, 0.020-0.035% S, 0.60-0.90% Cr, 0.10% Mo, 2.50-3.00% Ni, 0.020-0.050% Al
0.12-0.18% C, 0.15-0.40% Si, 0.30-0.60% Mn, 0.035% P, 0.035% S, 0.60-0.90% Cr, 2.50-3.00% Ni
0.12-0.18% C, 0.35% Si, 0.30-0.60% Mn, 0.035% P, 0.035% S, 2.50-3.00% Ni, 0.60-0.90% Cr
0.12-0.18% C, 0.35% Si, 0.30-0.60% Mn, 0.035% P, 0.035% S, 2.50-3.00% Ni, 0.60-0.90% Cr
0.12-0.22% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.015% S, 15.00-17.00% Cr, 1.50-2.50% Ni
0.12-0.22% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.015% S, 15.00-17.00% Cr, 1.50-2.50% Ni
0.12-0.22% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.015% S, 15.00-17.00% Cr, 1.50-2.50% Ni
0.12-0.22% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.030% S, 15.00-17.00% Cr, 1.50-2.50% Ni
0.12-0.22% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.030% S, 15.00-17.00% Cr, 1.50-2.50% Ni
0.12% C, 0.24% Si, 0.19% Mn, 0.021% P, 0.024% S, 11.90% Cr, 0.027% Nb
0.13% C, 0.20% Si, 0.25% Mn, 4.20% Cr, 4.25% Mo, 1.20% V, 3.40% Ni
0.13% C, 0.30% Si, 2.00% Mn, 0.35% Cr, 3.50% Ni, 1.20% Cu, 1.20% Al, + addions
0.13% C, 0.30% Si, 2.00% Mn, 0.35% Cr, 3.50% Ni, 1.20% Cu, 1.20% Al, +S
0.13% C, 0.40% Si, 0.50% Mn, 12.00% Cr
0.13% C, 0.40% Si, 1.20% Mn, 0.030% P, 0.32% S, 12.50% Cr, 0.30% Mo
0.13% C, 0.40% Si, 1.20% Mn, 0.030% P, 0.32% S, 12.50% Cr, 0.30% Mo
0.13-0.18% C, 0.40% Si, 0.80-1.10% Mn, 0.025% P, 0.030% S, 1.20-1.50% Cr, 0.80-1.10% Mo, 0.20-0.30% V
0.13-0.18% C, 0.40% Si, 0.80-1.10% Mn, 0.025% P, 0.030% S, 1.20-1.50% Cr, 0.80-1.10% Mo, 0.20-0.30% V
0.13-0.18% C, 0.40% Si, 0.80-1.10% Mn, 0.025% P, 0.030% S, 1.20-1.50% Cr, 0.80-1.10% Mo, 0.20-0.30% V
0.13-0.19% C, 0.15-0.40% Si, 0.40-0.70% Mn, 0.035% P, 0.035% S, 0.80-1.10% Cr, 2.70-3.20% Ni, 0.30-0.40% Mo
0.13-0.19% C, 0.15-0.40% Si, 0.40-0.70% Mn, 0.035% P, 0.035% S, 2.70-32.0% Ni, 0.80-1.10% Cr, 0.30-0.40% Mo
0.13-0.19% C, 0.15-0.40% Si, 0.40-0.70% Mn, 0.035% P, 0.035% S, 2.70-32.0% Ni, 0.80-1.10% Cr, 0.30-0.40% Mo
0.13-0.19% C, 0.15-0.40% Si, 0.70-1.00% Mn, 0.020% P, 0.040% S, 0.60-1.00% Cr, 0.80-1.10% Ni, 0.40% Cu
0.13-0.19% C, 0.15-0.40% Si, 0.70-1.00% Mn, 0.025% P, 0.020-0.040% S, 0.60-1.00% Cr, 0.80-1.10% Ni, 0.40% Cu, 0.020-0.050% Al, 0.15-0.30% Pb
0.13-0.19% C, 0.40% Si, 0.70-1.00% Mn, 0.035% P, 0.035% S,
0.13-0.19% C, 0.40% Si, 0.70-1.00% Mn, 0.60-1.00% Cr, 0.80-1.10% Ni
0.14% C, 0.15% Si, 0.70% Mn, 12.00% Cr, 1.75% Mo, 0.30% V, 2.75% Ni, 0.035% N
0.14% C, 0.25% S, 16.50% Cr, 0.40% Mo
0.14% C, 0.38% Si, 1.09% Mn, 0.012% P, 0.002% Si, 0.20% Cr, 0.28% Mo, 1.10% Ni, 0.58% Cu
0.14% C, 1.40% Mn, 0.30% Cr, 0.30% Mo, 2.80% Ni, 0.90% Cu, 0.90% Al
0.14-0.17% C, 0.15% Si, 1.20-1.40% Mn, 0.020% P, 0.020-0.030% S, 2.10-2.30% Cr, 0.45-0.55% Mo, 0.45-0.55% Ni, 0.15-0.25% V
0.14-0.17% C, 0.15-0.30% Si, 1.20-1.40% Mn, 0.020% P, 0.002 S, 2.10-2.30% Cr, 0.45-0.55% Mo, 0.45-0.55% Ni, 0.15-0.25% V
0.14-0.17% C, 0.30% Si, 1.20-1.40% Mn, 0.020% P, 0.002% S, 2.10-2.30% Cr, 0.45-0.55% Mo, 0.45-0.55% Ni, 0.15-0.25% V
0.14-0.17% C, 0.30% Si, 1.20-1.40% Mn, 0.020% P, 0.002% S, 2.10-2.30% Cr, 0.45-0.55% Mo, 0.45-0.55% Ni
0.14-0.17% C, 0.30% Si, 1.20-1.40% Mn, 0.020% P, 0.002% S, 2.10-2.30% Cr, 0.45-0.55% Mo, 0.45-0.55% Ni
0.14-0.19% C, 0.15-0.40% Si, 1.00-1.30% Mn, 0.025% P, 0.020-0.035% S, 0.80-1.10% Cr, 0.40% Cu, 0.020-0.040% Al, 0.15-0.30% Pb
0.14-0.19% C, 0.40% Si, 1.00-1.30% Mn, 0.025% P, 0.035% S, 0.80-1.10% Cr
0.14-0.19% C, 0.40% Si, 1.00-1.30% Mn, 0.035% P, 0.035% S, 0.80-1.10% Cr
0.14-0.19% C, max.0.40% Si, 1.00-1.30% Cr, 0.80-1.10% Cr
0.14-0.20% C, 0.15-0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.020-0.040% S, 0.80-1.10% Cr, 0.15-0.25% Mo, 1.20-1.60% Ni, 0.40% Cu, 0.020-0.050% Al
0.14-0.20% C, 0.40% Si, 0.60-0.90% Mn, 0.80-1.10% Cr, 0.15-0.25% Mo, 1.20-1.50% Ni
0.15% C, 0.10% Si, 1.30% Mn, 2.20% Cr, 0.50% Mo, 0.50% Ni, 0.20% V
0.15% C, 0.20% Si, 0.88% Mn, 0.53% Cr, 0.50% Mo, 0.86% Ni
0.15% C, 0.25% Si, 0.90% Mn, 0.80% Cr, 0.10% Mo, 1.20% Ni
0.15% C, 0.30% Si, 0.40% Mn, 14.00% Cr, 0.60% Ni, +N
0.15% C, 0.30% Si, 0.50% Mn, 4.00% Cr, 1.10% Mo, 3.00% Ni
0.15% C, 0.85% Cr, 1.60% Ni
0.15% C, 1.10% Si, 1.00% Cr, 2.00% Mo, 2.50% Ni
0.15% C, 1.25% Cr, 0.90% Mo, 0.25% V
0.15-0.21% C, 0.15-0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.70-1.00% Cr, 0.15-0.25% Mo, 1.20-1.50% Ni
0.15-0.21% C, 0.15-0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.70-1.00% Cr, 0.15-0.25% Mo, 1.20-1.50% Ni
0.15-0.21% C, 0.15-0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.70-1.00% Cr, 0.15-0.25% Mo, 1.20-1.50% Ni
0.15-0.21% C, 0.40% Si, 0.50-0.90% Mn, 0.025% P, 0.035% S, 1.50-1.80% Cr, 0.25-0.35% Mo, 1.40-1.70% Ni
0.16% C, 0.20% Si, 0.20% Mn, 10.00% Cr, 5.10% Mo, 0.50% V, 10.00% Co
0.16% C, 1.00% Cr, 0.25% Mo, 3.20% Ni
0.16% C, 1.20% Cr, 0.20% Mo, 4.25% Ni
0.16-0.19% C, 0.20-0.40% Si, 0.75-1.00% Mn, 0.020% P, 0.030% S, 1.75-2.00% Cr, 0.50-0.60% Mo, 0.30% Ni, 0.10% V
0.16-0.22% C, 0.10-0.40% Si, 0.15-0.45% Mn, 0.030% P, 0.030% S, 1.10-1.40% Cr, 0.15-0.25% Mo, 3.80-4.30% Ni
0.16-0.23% C, 0.20-0.40% Si, 0.20-0.40% Mn, 0.025% P, 0.025% S, 2.30-2.60% Cr, 0.30-0.40% Mo
0.16-0.25% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.015% S, 12.00-14.00% Cr
0.16-0.25% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.015% S, 12.00-14.00% Cr
0.16-0.25% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.015% S, 12.00-14.00% Cr
0.16-0.25% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.015% S, 12.00-14.00% Cr
0.16-0.25% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.030% S, 12.00-14.00% Cr
0.16-0.25% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.030% S, 12.00-14.00% Cr
0.16-0.25% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.030% S, 12.00-14.00% Cr
0.16-0.25% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.030% S, 12.00-14.00% Cr
0.16-0.25% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.030% S, 12.00-14.00% Cr
0.17% C, 0.85% Mn, 1.85% Cr, 0.55% Mo
0.17% C, 1.00% Si, 1.50% Mn, 16.00% Cr, 2.00% Ni
0.17% C, 16.00% Cr, 2.00% Ni
0.17% C, 16.00% Cr, 2.00% Ni
0.17-0.21% C, 0.20-0.30% Si, 0.30-0.50% Mn, 0.020% P, 0.015-0.030% S, 1.20-1.40% Cr, 0.20-0.26% Mo, 2.50-2.90% Ni
0.17-0.22% C, 0.15-0.40% Si, 1.10-1.40% Mn, 0.025% P, 0.020-0.040% S, 1.00-1.30% Cr, 0.40% Cu, 0.020-0.050% Al, 0.15-0.30% Pb
0.17-0.22% C, 0.30-0.50% Si, 0.20-0.40% Mn, 0.035% P, 0.035% S, 12.50-13.50% Cr
0.17-0.22% C, 0.40% Si, 1.10-1.40% Mn, 0.025% P, 0.035% S, 1.00-1.30% Cr
0.17-0.22% C, 0.40% Si, 1.10-1.40% Mn, 0.025% P, 0.035% S, 1.00-1.30% Cr
0.17-0.22% C, 0.40% Si, 1.10-1.40% Mn, 1.00-1.30% Cr
0.17-0.22% C, 1.00% Si, 1.00% Mn, 0.040% P, 0.015% S, 12.00-14.00% Cr, 0.90-1.30% Mo, 1.00% Ni
0.17-0.22% C, 1.00% Si, 1.00% Mn, 0.040% P, 0.015% S, 12.00-14.00% Cr, 0.90-1.30% Mo, 1.00% Ni
0.17-0.23% C, 0.15-0.35% Si, 0.40-0.60% Mn, 0.035% P, 0.035% S, 9.00-10.00% Cr, 1.80-2.20% Mo, 5.00-6.00% W, 9.50-10.50% Co
0.17-0.23% C, 0.15-0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.35-0.65% Cr, 0.15-0.25% Mo, 0.40-0.70% Ni
0.17-0.23% C, 0.15-0.40% Si, 0.65-0.95% Mn, 0.025% P, 0.020-0.040% S, 0.35-0.70% Cr, 0.15-0.25% Mo, 0.40-0.70% Ni, 0.40% Cu
0.17-0.23% C, 0.15-0.40% Si, 1.10-1.40% Mn, 0.035% P, 0.035% S, 1.00-1.30% Cr
0.17-0.23% C, 0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.020-0.025% S, 0.90-1.20% Cr, 0.15-0.25% Mo, 0.050% Al, 0.30% Cu
0.17-0.23% C, 0.40% Si, 0.65-0.95% Mn, 0.025% P, 0.035% S, 0.35-0.75% Cr, 0.15-0.25% Mo, 0.40-0.0% Ni
0.17-0.23% C, 0.40% Si, 0.65-0.95% Mn, 0.025% P, 0.035% Si, 0.35-0.70% Cr, 0.15-0.25% Mo, 0.40-0.70% Ni
0.17-0.23% C, 0.40% Si, 0.65-0.95% Mn, 0.35-0.75% Cr, 0.15-0.25% Mo, 0.40-0.70% Ni
0.17-0.23% C, 0.40% Si, 1.10-1.40% Mn, 0.025% P, 0.035% S, 0.0008-0.0050% B
0.17-0.23% C, 0.40% Si, 1.10-1.40% Mn, 0.025% P, 0.035% S, 0.0008-0.0050% B
0.17-0.24% C, 0.40% Si, 0.40-0.70% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63%
0.17-0.24% C, 0.40% Si, 0.40-0.70% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63%
0.17-0.24% C, 0.40% Si, 0.40-0.70% Mn, 0.030% P, 0.020-0.040% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.17-0.24% C, 0.40% Si, 0.40-0.70% Mn, 0.030% P, 0.020-0.040% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.17-0.24% C, 0.40% Si, 0.40-0.70% Mn, 0.030% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.17-0.24% C, 0.40% Si, 0.40-0.70% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.17-0.24% C, 0.40% Si, 0.40-0.70% Mn, 0.035% P, 0.035% S,
0.17-0.24% C, 0.40% Si, 0.40-0.70% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Vr+Mo+Ni=0.63
0.17-0.24% C, 0.40% Si, 0.40-0.70% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Vr+Mo+Ni=0.63
0.17-0.24% C, 0.40% Si, 0.40-0.70% Mn, 0.045% P, 0.040% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.17-0.24% C, 0.40% Si, 0.40-0.70% Mn, 0.045% P, 0.040% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.17-0.24% C, 0.40% Si, 0.40-0.70% Mn, 0.045% P, 0.040% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.17-0.24% C, 0.40% Si, 0.80-1.15% Mn, 0.030% P, 0.035% S, min. 0.020% Al, 0.0008-0.0050% B
0.17-0.23% C, 0.30-0.60% Si, 1.30-1.60% Mn, 0.035% P, 0.035% S
0.17-0.24% C, 0.40% Si, 0.40-0.60% Mn, 0.035% P, 0.030% S
0.17-0.24% C, 0.40% Si, 0.40-0.60% Mn, 0.045% P, 0.045% S
0.18% C, 0.40% Si, 0.80% Mn, 0.030% P, 0.015% S, 15.60% Cr, 1.70% Ni
0.18% C, 0.40% Si, 0.80% Mn, 0.030% P, 0.015% S, 15.60% Cr, 1.70% Ni
0.18% C, 0.50% Si, 1.80% Mn, 0.025% P, 0.025% S, 1.00% Cr, 0.30% Mo, 0.80% Ni, 0.08% V, 0.05% Nb, 0.005% B
0.18% C, 0.50% Si, 1.80% Mn, 0.025% P, 0.025% S, 1.00% Cr, 0.30% Mo, 0.80% Ni, 0.08% V, 0.05% Nb, 0.005% B
0.18-0.22% C, 0.30% Si, 0.30-0.60% Mn, 0.025% P, 0.025% S, 0.25% Cu
0.18-0.23% C, 0.15-0.35% Si, 0.90-1.20% Mn, 0.035% P, 0.035% S, 1.10-1.40% Cr, 0.20-0.30% Mo
0.18-0.23% C, 0.15-0.35% Si, 0.90-1.20% Mn, 0.035% P, 0.035% S, 1.10-1.40% Cr, 0.20-0.30% Mo
0.18-0.23% C, 0.15-0.40% Si, 0.80-1.10% Mn, 0.035% P, 0.020-0.035% S, 0.90-1.20% Cr, 0.10% Mo, 0.90-1.20% Ni, 0.15-0.30% Pb
0.18-0.23% C, 0.15-0.40% Si, 0.80-1.10% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.90-1.20% Ni
0.18-0.24% C, 0.15-0.35% Si, 1.10-1.40% Mn, 0.030% P, 0.030% S, 1.00-1.30% Cr
0.18-0.24% C, 0.15-0.40% Si, 0.40-0.80% Mn, 0.035% P, 0.035% S
0.18-0.24% C, 1.00% Si, 0.30-0.60% Mn, 0.040% P, 0.040% S
0.19% C, 0.25% Si, 0.40% Mn, 15.60% Cr, 1.60% Ni
0.19% C, 0.30% Si, 0.55% Mn, 10.75% Cr, 0.20% V, 0.33% Nb 0.55% Ni, 0.080% N, 0.0015% B
0.19% C, 0.40% Si, 1.25% Mn, 1.15% Cr
0.19% C, 1.30% Cr, 0.20% Mo, 4.10% Ni
0.19% C, 1.30% Cr, 0.20% Mo, 4.10% Ni
0.19% C, 1.30% Cr, 0.20% Mo, 4.10% Ni
0.19% C, 1.30% Cr, 0.20% Mo, 4.10% Ni
0.19-0.25% C, 0.40% Si, 1.10-1.40% Mn, 0.025% P, 0.015% S, 0.15-0.35% Cr, 0.020-0.050% Ti, 0.020-0.060% Al, 0.0008-0.0050% B
0.19-0.25% C, 0.40% Si, 1.10-1.40% Mn, 0.025% P, 0.015% S, 0.15-0.35% Cr, 0.020-0.050% Ti, 0.020-0.060% Al, 0.0008-0.0050% B
0.20% C, 0.09% Si, 0.89% Mn, 0.015% P, 0.015% Ti, 0.03% Al, 0.005% B
0.20% C, 0.20% Si, 0.50% Mn, 0.00% Cr, 0.025% P, 0.025% S, 0.25% Cu
0.20% C, 0.20% Si, 0.50% Mn, 9.50% Cr, 2.00% Mo, 5.50% W, 10.00% Co
0.20% C, 0.20% Si, 0.50% Mn, 9.50% Cr, 2.00% Mo, 5.50% W, 10.00% Co
0.20% C, 0.20% Si, 0.50% Mn, 9.50% Cr, 2.00% Mo, 5.50% W, 10.00% Co
0.20% C, 0.20% Si, 0.70% Mn, 0.15% Cr, 3.35% Mo, 0.08% V, 3.15% Ni
0.20% C, 0.25% Si, 0.40% Mn, 1.20% Cr, 0.20% Mo, 4.00% Ni, or 0.40% W
0.20% C, 0.30% Si, 0.40% Mn, 0.010% P, 0.005% S, 2.50% Cr, 0.40% Mo
0.20% C, 0.30% Si, 1.20% Mn, 1.10% Cr
0.20% C, 0.35% Si, 0.40% Mn, 13.20% Cr, 1.10% Mo
0.20% C, 0.40% Si, 0.40% Mn, 12.50% Cr
0.20% C, 0.40% Si, 0.50% Mn, 0.025% P, 0.030% S, 13.00% Cr
0.20% C, 0.40% Si, 0.50% Mn, 0.030% P, 0.025% S, 13.00% Cr
0.20% C, 0.40% Si, 0.55% Mn, 0.10% Mo, 0.40% Ni, (Cr+Mo+Ni) = 0.63
0.20% C, 0.50% Cr, 0.20% Mo, 0.50% Ni
0.20% C, 0.50% Si, 1.00% Mn, 11.25% Cr, 1.00% Mo, 0.30% V, 0.55% Ni
0.20% C, 0.50% Si, 1.15% Mn
0.20% C, 0.70% Si, 1.80% Mn, 0.025% P, 0.010% S, 1.50% Cr, 0.50% Mo, 0.80% Ni, 0.08% V, 0.30% Cu, 0.05% Nb, 0.005% B
0.20% C, 1.00% Cr, 0.50% Mo, 3.20% Ni
0.20% C, 1.00% Si, 1.50% Mn, 13.00% Cr
0.20% C, 13.00% Cr
0.20% C, 13.00% Cr
0.20% C, 3.00% Cr, 0.40% Mo
0.20% C, 9.50% Cr, 2.00% Mo, 5.50% W, 10.00% Co
0.20-0.25% C, 0.30% Si, 0.025% P, 0.025% S, 0.30% Cr, 0.25% Cu, 0.0008-0.005% B
0.20-0.30% C, 0.20-0.50% Si, 1.40-1.70% Mn, 1.20-1.60% Cr, 0.55-0.75% Mo, 1.00-1.30% Ni
0.20-0.30% C, 0.20-0.50% Si, 1.40-1.70% Mn, 1.20-1.60% Cr, 0.55-0.75% Mo, 1.00-1.30% Ni
0.20-0.30% C, 0.20-0.50% Si, 1.40-1.70% Mn, 1.20-1.60% Cr, 0.55-0.75% Mo, 1.00-1.30% Ni
0.20-0.35% C, 0.10-0.35% Si, 0.65% Mn, 0.035% P, 0.030% S, 2.50-3.50% Cr, 0.30-0.70% Mn, 0.40% Ni
0.20-0.35% C, 0.15-0.35% Si, 0.50-0.80% Mn, 0.030% P, 0.035% S, 0.90-1.20% Cr, 0.20-0.35% Mo
0.20-0.40% C, 0.40% Si, 0.80-1.40% Mn, 0.025% P, 0.002% S, 1.00-2.00% Cr, 0.20-0.50% Mo
0.20-0.40% C, 0.40% Si, 0.80-1.40% Mn,0.025% P, 0.002% S, 1.00-2.00% Cr, 0.20-0.50% Mo
0.21% C, 0.25% Si, 1.25% Mn, 1.20% Cr
0.21% C, 0.35% Si, 0.35% Mn, 13.30% Cr
0.21% C, 0.90% Si, 0.45% Mn, 13.50% Cr, 0.20% Mo, 0.60% Ni, 0.25% V, +N
0.21% C, 0.90% Si, 0.45% Mn, 13.50% Cr, 0.20% Mo, 0.60% Ni, 0.25% V, +N
0.21% C, 0.90% Si, 0.45% Mn, 13.50% Cr, 0.20% Mo, 0.60% Ni, 0.25% V, +N
0.21% C, 1.30% Mn, 1.20% Cr
0.21% C, 1.30% Mn, 1.20% Cr
0.21% C, 1.30% Mn, 1.20% Cr
0.22% C, 0.25% Si, 0.70% Mn, 0.020% P, 0.025% S, 11.50% Cr, 1.00% Mo, 0.25% V, 0.65% Ni
0.22% C, 0.40% Si, 0.50% Mn, 16.50% Cr, 1.70% Ni
0.22% C, 0.40% Si, 0.55% Mn, 0.10% Mo, 0.40% Ni, (Cr+Mo+Ni) = 0.63
0.22-0.29% C, 0.10-0.40% Si, 0.40-0.70% Mn, 0.025% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, 0.30% Cu
0.22-0.29% C, 0.15-0.35% Si, 0.50-0.80% Mn, 0.020% P, 0.015% S, 0.90-1.20% Cr, 0.15-0.25% Mo, 0.30% Ni
0.22-0.29% C, 0.35% Si, 0.50-0.80% Mn, 0.025% P, 0.020% S, 0.90-1.20% Cr, 0.15-0.30% Mo, 0.30% Cu
0.22-0.29% C, 0.35% Si, 0.50-0.80% Mn, 0.025% P, 0.020% S, 0.90-1.20% Cr, 0.15-0.30% Mo, 0.30% Cu
0.22-0.29% C, 0.40% Si, 0.40-0.70% Mn, 0.035% P, 0.020-0.040% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.22-0.29% C, 0.40% Si, 0.40-0.70% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.22-0.29% C, 0.40% Si, 0.40-0.70% Mn, 0.045% P, 0.040% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.22-0.29% C, 0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.22-0.29% C, 0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.22-0.29% C, 0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.22-0.29% C, 0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.22-0.29% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.020-0.040% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.22-0.29% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.15-0.30% Mo
0.22-0.29% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.15-0.30% Mo
0.22-0.30% C, 0.30-0.50% Si, 0.20-0.40% Mn, 0.030% P, 0.030% S, 0.60-0.90% Cr, 0.20-0.40% Mo, 1.30-1.60% Ni, 0.15-0.20% V
0.22-0.32% C, 0.15-0.55% Si, 1.20-1.60% Mn, 1.20-1.60% Cr, 0.45-0.70% Mo, 0.80-1.50% Ni, 0.10-0.20% V
0.22-0.50% C, 0.40% Si, 0.50-0.80% Mn, 0.045% P, 0.040% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.22% C, 0.28% Si, 0.70% Mn, 0.07% Cr, 0.25% Mo, 1.97% Ni, 0.010% V, 0.11% Cu
0.23% C, 0.15-0.30% Si, 1.20-1.50% Mn, 0.012% P, 0.008% S, 0.20% Cr, 0.50-0.80% Ni, 0.020% V, 0.12% Cu, 0.010-0.040% Al
0.23% C, 0.30% Si, 0.71% Mn, 0.008% P, 0.003% S, 1.20% Cr, 0.78% Mo, 0.77% Ni, 0.32% V, 0.06% Cu
0.23% C, 0.30% Si, 0.71% Mn, 1.20% Cr, 0.78% Mo, 0.77% Ni, 0.32% V, 0.06% Cu
0.23% C, 0.30-0.70% Si, 1.20-1.70% Mn, 0.025% P, 0.010% S, 1.00-1.60% Cr, 0.50% Mo, 0.60% Ni, 0.20% V, 0.60% Cu, Nb+V+T =20
0.23% C, 16.50% Cr, 1.80% Ni
0.23% C, 16.50% Cr, 1.80% Ni
0.23% C, 3.30% Cr, 1.50% Mo, 13.00% Ni, 0.25% v, 1.50% Al, 5.80% Co
0.23-0.25% C, 0.20-0.35% Si, 0.60-0.60% Mn, 0.020% P, 0.025% S, 3.00-3.50% Cr, 0.45-0.60% Mo, 0.03% Ni, 0.050% V
0.23-0.27% C, 0.20% Si, 1.00-1.60% Mn, 0.020% P, 0.020% S, 1.00-2.50% Cr, 1.00% Ni, 0.60-0.80% Mo
0.23-0.29% C, 0.15-0.40% Si, 1.40-1.70% Mn, 0.025% P, 0.005% S, 1.20-1.80% Cr, 0.30-0.70% Mo, 0.90-1.20% Ni
0.23-0.29% C, 0.15-0.40% Si, 1.40-1.70% Mn, 0.025% P, 0.005% S, 1.20-1.80% Cr, 0.30-0.70% Mo, 0.90-1.20% Ni
0.23% C, 0.60% Si, 1.15-1.60% Mn, 0.045% P, 0.045% S
0.24% C, 0.20% Si, 0.35% Mn, 13.25% Cr, +N, Mo, V, Ni
0.24-0.30% C, 0.40% Si, 1.10-1.40% Mn, 0.025% P, 0.035% S, 0.30-0.60% Cr, 0.0008-0.0050% B
0.24-0.30% C, 0.40% Si, 1.10-1.40% Mn, 0.025% P, 0.035% S, 0.30-0.60% Cr, 0.0008-0.0050% B
0.24-0.30% C, 0.40% Si, 1.10-1.40% Mn, 0.025% P, 0.035% S, 0.30-0.60% Cr, 0.40% Cu, 0.0008-0.005% B
0.24-0.30% C, 0.40% Si, 1.10-1.40% Mn, 0.035% P, 0.040% S, 0.30-0.60% Cr, 0.0008-0.0050% B
0.24-0.30% C, 0.40% Si, 1.10-1.40% Mn, 0.035% P, 0.040% S, 0.30-0.60% Cr, 0.0008-0.0050% B
0.24-0.30% C, 0.40% Si, 1.10-1.40% Mn, 0.035% P, 0.040% S, 0.30-0.60% Cr, 0.0008-0.0050% B
0.24-0.30% C, 0.40% Si, 1.10-1.40% Mn, 0.035% P, 0.040% S, 0.30-0.60% Cr, 0.0008-0.0050% B
0.24-0.31% C, 0.15-0.35% Si, 0.20-0.40% Mn, 0.030% P, 0.030% S, 1.15-1.25% Cr, 4.20-4.70% Ni, 0.15-0.20% V
0.24-0.31% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.025% S, 0.90-1.20% Cr
0.24-0.31% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.025% S, 0.90-1.20% Cr
0.24-0.31% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.025% S, 0.90-1.20% Cr
0.24-0.32% C, 0.30-0.50% Si, 0.20-0.40% Mn, 0.030% P, 0.030% S, 0.60-0.90% Cr, 0.50-0.70% Mo, 2.30-2.60% Ni, 0.25-0.32% V
0.24-0.32% C, 0.30-0.60% Si, 0.20-0.40% Mn, 0.030% P, 0.030% S, 0.60-0.90% Cr, 1.00-1.30% Ni, 0.15-0.20% V
0.242% C, 0.301% Si, 1.26% Mn, 0.018% P, 0.005% S, 0.13% Cr, 0.045% Al, 0.027% Ti, 0.009% N, 0.003% B
0.25% C, 0.25% Si, 0.60% Mn, 1.35% Cr, 0.20% Mo, 2.95% Ni
0.25% C, 0.25% Si, 0.60% Mn, 1.35% Cr, 0.20% Mo, 2.95% Ni
0.25% C, 0.25% Si, 0.70% Mn, 1.05% Cr, 0.25% Mo, + Pb
0.25% C, 0.25% Si, 0.70% Mn, 1.05% Cr, 0.25% Mo
0.25% C, 0.30% Si, 0.50% Mn, 0.008% P, 0.0010% S, 10.00% V, 0.06% Al, 0.0010% B, 0.0030% N
0.25% C, 0.35% Si, 0.55% Mn, 13.30% Cr, 0.35% Mo, 1.35% Ni, 0.35% V
0.25% C, 0.70% Si, 1.60% Mn, 0.025% P, 0.010% S, 1.50% Cr, 0.50% Mo, 0.80% Ni, 0.08% V, 0.30% Cu, 0.05% Nb, 0.005% B
0.25% C, 1.30% Mn, 1.30% Cr, 0.40% Mo, +B
0.25% C, 1.50% Si, 1.35% Mn, 0.025% P, 0.025% S, 0.30% Cr, 1.80% Ni, 0.40% Mo
0.25% C, 1.50% Si, 1.35% Mn, 0.30% Cr, 0.40% Mo, 1.80% Ni
0.25-0.30% C, 0.30% Ni, 12.00-12.50% Cr, 0.50% Mo, + additions
0.25-0.32% C, 0.40% Si, 1.30-1.65% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.25-0.32% C, 0.40% Si, 1.30-1.65% Mn, 0.035% P, 0.035% S, 0.40%Cr, 0.10% Mo, 0.40% Ni, 0.05% V, Cr+Mo+Ni=0.63
0.25-0.32% C, 0.60% Si, 1.20-1.80% Mn, 0.035% P, 0.030% S
0.25-0.32% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.15-0.25% S, 12.00-13.50% Cr, 0.60% Mo
0.25-0.32% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.15-0.25% S, 12.00-13.50% Cr, 0.60% Mo
0.25-0.35% C, 0.10-0.40% Si, 0.15-0.45% Mn, 0.030% P, 0.020% S, 2.50-3.20% Cr, 8.50-9.50% W, 0.30-0.50% V
0.25-0.35% C, 0.15-0.30% Si, 0.20-0.40% Mn, 0.035% P, 0.035% S, 2.20-2.50% Cr, 4.00-4.50% W, 0.50-0.70% V
0.25-0.35% C, 0.15???0.30% Si, 0.20???0.40% Mn, 0.35% P, 0.35% S, 2.50-2.80% Cr, 0.30???0.40% V, 8.00-9.00% W
0.25-0.35% C, 0.30-0.60% Si, 1.40-1.70% Mn, 1.40-1.80% Cr, 0.40-0.60% Mo, 0.20-0.60% Ni
0.25-0.35% C, 0.30-0.60% Si, 1.40-1.70% Mn, 1.40-1.80% Cr, 0.40-0.60% Mo, 0.20-0.60% Ni
0.25-0.35% C, 0.40% Si, 1.10-1.30% Mn, 0.040% P, 0.040% S, 0.50% Cr, 0.0008???0.0040% B
0.25-0.35% C, 0.50-0.80% Si, 1.40-1.70% Mn, 1.40-1.80% Cr, 0.40-0.60% Mo, 0.20-0.60% Ni
0.25-0.35% C, 0.80-1.10% Si, 0.30-0.50% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 3.50-4.00% W, 0.15-0.20% V
0.25-0.35% C, 1.00% Si, 1.00% Mn, 0.030% P, 0.025% S, 14.00-16.00% Cr, 0.85-1.10% Mo, 0.50% Ni
0.25-0.35% C, 1.00% Si, 1.00% Mn, 0.030% P, 0.025% S, 14.00-16.00% Cr, 0.85-1.10% Mo, 0.50% Ni
0.25-0.35% C, 1.00% Si, 1.00% Mn, 14.00-16.00% Cr, 0.85-1.10% Mo, 0.30-0.50% V
0.25-0.35% C, 1.00% Si, 1.00% Mn, 14.00-16.00% Cr, 0.85-1.10% Mo, 0.30-0.50% V
0.25-0.35% C, 1.00% Si, 1.00% Mn, 14.00-16.00% Cr, 0.85-1.10% Mo, 0.30-0.50% V
0.25-0.35% C, 1.00% Si, 1.00% Mn, 14.00-16.00% Cr, 0.85-1.10% Mo, 0.30-0.50% V
0.25-0.35% C, 1.00% Si, 1.00% Mn, 14.00-16.00% Cr, 0.85-1.10% Mo, 0.30-0.50% V
0.25-0.35% C, 1.00% Si, 1.00% Mn, 14.00-16.00% Cr, 0.85-1.10% Mo, 0.50% Ni, 0.30-0.50% N
0.25-0.35% C, 1.00% Si, 1.00% Mn, 14.00-16.00% Cr, 0.85-1.10% Mo, 0.50% Ni, 0.30-0.50% N
0.25% C, 0.25% Si, 0.70% Mn, 1.05% Cr, 0.25% Mo
0.25% C, 0.25% Si, 0.70% Mn, 1.05% Cr, 0.25% Mo
0.25-0.32% C, 0.40% Si, 1.30-1.65% Mn, 0.035% P, 0.030% S
0.26% C, 0.10% Si, 1.45% Mn, 0.015% P, 0.002% S, 1.25% Cr, 0.50% Mo, 1.05% Ni, 0.10% V
0.26% C, 0.10% Si, 1.45% Mn, 0.015% P, 0.002% S, 1.25% Cr, 0.60% Mo, 1.05% Ni, 0.12% V
0.26% C, 0.10% Si, 1.45% Mn, 0.015% P, 0.002% S, 1.25% Cr, 0.70% Mo, 1.05% Ni, 0.15% V
0.26% C, 0.10% Si, 1.45% Mn, 0.015% P, 0.002% S, 1.25% Cr, 1.05% Ni, 0.50% Mo, 0.10% V
0.26% C, 0.20% Si, 0.46% Mn, 0.024% P, 0.019% S, 0.02% Cr, 0.02% Ni, 0.01% Cu
0.26% C, 0.24% Si, 0.24% Mn, 0.007% P, 0.004% S, 0.37% Cr, 0.33% Mo, 2.95% Ni, 0.03% V, 0.05% Cu, 0.010% Al
0.26% C, 0.24% Si, 0.24% Mn, 0.007% P, 0.004% S, 0.37% Cr, 0.33% Mo, 2.95% Ni, 0.030% V
0.26% C, 0.25% Si, 1.50% Mn, 1.40% Cr, 0.70% Mo, 2.00% Ni, + others
0.26% C, 0.35% Si, 1.00% Mn, 1.45% Cr, 0.55% Mo, 0.60% Ni, +others
0.26% C, 0.35% Si, 1.00% Mn, 1.45% Cr, 0.55% Mo, 0.60% Ni, +others
0.26% C, 0.75% Cr, 0.30% Mo, 1.30% Ni, 0.20% V
0.26-0.33% C, 0.15-0.40% Si, 0.30-0.60% Mn, 0.035% P, 0.035% S, 1.80-2.20% Cr, 0.30-0.50% Mo, 1.80-2.20% Ni
0.26-0.34% C, 0.15-0.35% Si, 0.40-0.70% Mn, 0.035% P, 0.035% S, 2.30-2.70% Cr, 0.15-0.25% Mo, 0.10-0.20% V
0.26-0.34% C, 0.15-0.40% Si, 0.30-0.60% Mn, 0.025% P, 0.025% S, 1.80-2.30% Cr, 0.30-0.50% Mo, 1.80-2.30% Ni
0.26-0.34% C, 0.15-0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S, 1.80-2.20% Cr, 1.80-2.20% Ni, 0.15-0.30% Mo
0.26-0.34% C, 0.40% Si, 0.30-0.60% Mn, 0.035% P, 0.035% S, 1.80-2.20% Cr, 0.30-0.50% Mo, 1.80-2.20% Ni
0.26-0.34% C, 0.40% Si, 0.30-0.60% Mn, 0.035% P, 0.035% S, 1.80-2.20% Cr, 0.30-0.50% Mo, 1.80-2.20% Ni
0.26-0.34% C, 0.40% Si, 0.30-0.60% Mn, 0.035% P, 0.035% S, 1.80-2.20% Cr, 0.30-0.50% Mo, 1.80-2.20% Ni
0.26-0.34% C, 0.40% Si, 0.30-0.60% Mn, 0.035% P, 0.035% S, 1.80-2.20% Cr, 0.30-0.50% Mo, 1.80-2.20% Ni
0.26-0.34% C, 0.40% Si, 0.40-0.70% Mn, 0.035% P, 0.035% S, 2.30-2.70% Cr, 0.15-0.25% Mo, 0.60% Ni, 0.10-0.20% V
0.26-0.34% C, 0.40% Si, 0.40-0.70% Mn, 0.035% P, 0.035% S, 2.30-2.70% Cr, 0.15-0.25% Mo, 0.60% Ni, 0.10-0.20% V
0.26-0.34% C, 0.40% Si, 0.40-0.70% Mn, 0.035% P, 0.030% S, 2.30-2.70% Cr, 0.15-0.25% Mo, 0.60% Ni, 0.10-0.20% V
0.26-0.34% C, 0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S, 1.80-2.20% Cr, 0.30-0.50% Mo, 1.80-2.20% Ni
0.26-0.34% C, 0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S, 1.80-2.20% Cr, 0.30-0.50% Mo, 1.80-2.20% Ni
0.26-0.35% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.015% S, 12.00-14.00% Cr
0.26-0.35% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.015% S, 12.00-14.00% Cr
0.26-0.35% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.030% S, 12.00-14.00% Cr
0.26-0.35% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.030% S, 12.00-14.00% Cr
0.26-0.35% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.030% S, 12.00-14.00% Cr
0.26-0.33% C, 0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.025% S, 1.20-1.50% Cr, 0.30-0.60% Mo, 3.30-4.30% Ni
0.26-0.34% C, 0.40% Si, 0.30-0.60% Mn, 0.035% P, 0.030% S, 1.80-2.20% Cr, 0.30-0.50% Mo, 1.80-2.20% Ni
0.26-0.34% C, 0.40% Si, 0.40-0.70% Mn, 0.035% P, 0.030% S, 2.30-2.70% Cr, 0.15-0.25% Mo, 0.10-0.20% V
0.26-0.34% C, 0.40% Si, 0.40-0.70% Mn, 0.035% P, 0.035% S, 2.30-2.70% Cr, 0.15-0.25% Mo, 0.60% Ni, 0.10-0.20% V
0.26-0.34% C, 0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S, 1.80-2.20% Cr, 0.30-0.50% Mo, 1.80-2.20% Ni
0.27% C, 0.23% Si, 1.20% Mn, 0.020% P, 0.020% S, 0.48% Cr, 0.035% Ti, 0.030% Al, 0.005% N, 0.0015% B
0.27% C, 0.25% Si, 1.40% Si, 1.40% Cr, 0.60% Mo, 1.10% Ni, 0.10% V
0.27% C, 0.25% Si, 1.50% Mn, 1.40% Cr, 0.55% Mo, 1.10% Ni, +others
0.27% C, 0.30% Si, 0.65% Mn, 14.50% Cr, 1.00% Mo, 0.85% Ni, + N + others
0.27% C, 0.30% Si, 0.65% Mn, 14.50% Cr, 1.00% Mo, 0.85% Ni, +N and others
0.27% C, 0.30% Si, 0.65% Mn, 14.50% Cr, 1.00% Mo, 0.85% Ni, +N
0.27% C, 0.30% Si, 1.55% Mn, 1.35% Cr, 0.50% Mo, 1.00% Ni, +others
0.27% C, 0.30% Si, 1.55% Mn, 1.35% Cr, 1.00% Ni, +Mo
0.27-0.32% C, 0.15-0.30% Si, 0.20-0.40% Mn, 0.035% P, 0.035% S, 2.20-2.50% Cr, 8.00-9.00% W, 0.20-0.30% V, 1.80-2.30% Co
0.27-0.33% C, 0.30% Si, 1.15-1.45% Cr, 0.025% P, 0.035% S, 0.0008-0.005% B
0.27-0.33% C, 0.40% Si, 1.15-1.45% Mn, 0.025% P, 0.035% S, 0.0008-0.0050% B
0.27-0.33% C, 0.40% Si, 1.15-1.45% Mn, 0.025% P, 0.035% S, 0.0008-0.0050% B
0.27-0.34% C, 0.10-0.40% Si, 0.35-0.60% Mn, 0.035% P, 0.035% S, 0.60-0.90% Cr, 2.50-3.00% Ni
0.27-0.34% C, 0.15-0.40% Si, 0.70-1.00% Mn, 0.035% P, 0.035% S, 0.40-0.60% Cr, 0.15-0.30% Mo, 0.40-0.70% Ni
0.27-0.34% C, 0.30% Si, 0.40-0.70% Mn, 0.025% P, 0.035% S, 2.30-2.70% Cr, 0.15-0.25% Mo, 0.10-0.20% V
0.27-0.34% C, 0.40% Si, 0.40-0.70% Mn, 0.025% P, 0.035% S, 2.30-2.70% Cr, 0.15-0.25% Mo, 0.10-0.20% V
0.27-0.34% C, 0.40% Si, 0.40-0.70% Mn, 0.035% P, 0.035% S, 2.30-2.70% Cr, 0.15-0.25% Mo, 0.10-0.2-% V
0.27-0.34% C, 0.40% Si, 0.40-0.70% Mn, 0.035% P, 0.035% S, 2.30-2.70% Cr, 0.15-0.25% Mo, 0.10-0.2-% V
0.27-0.34% C, 0.40% Si, 0.40-0.80% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.27-0.34% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.020-0.040% S, 0.40% Cr, 0.10% Mo 0.40% Ni
0.27-0.34% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.27-0.34% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.27-0.34% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.27-0.34% C, 0.40% Si, 0.50-0.80% Mn, 0.045% P, 0.045% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.27% C, 0.35% Si, 0.26% Mn, 13.51% Cr, 0.11% N
0.27-0.34% C, 0.40% Si, 0.40-0.70% Mn, 0.025% P, 0.035% S, 2.30-2.70% Cr, 0.15-0.25% Mo, 0.10-0.20% V
0.28% C, 0.10% Si, 1.45% Mn, 0.015% P, 0.002% S, 1.25% Cr, 0.70% Mo, 1.05% Ni, 0.15% V
0.28% C, 0.20% S, 12.80% Cr
0.28% C, 0.30% Si, 0.30% Mn, 13.50% Cr, + N
0.28% C, 0.30% Si, 0.35% Mn, 0.030% P, 0.003% S, 14.20% Cr, 1.10% Mo, 0.50% Ni
0.28% C, 0.30% Si, 0.40% Mn, 14.00% Cr, 0.60% Ni, +N
0.28% C, 0.30% Si, 0.40% Mn, 14.00% Cr, 0.60% Ni, +N
0.28% C, 0.30% Si, 0.70% Mn, 2.80% Cr, 0.60% Mo, 0.40% V, 1.00% Ni
0.28% C, 0.30% Si, 0.70% Mn, 2.80% Cr, 0.60% Mo, 1.00% Ni, 0.40% V
0.28% C, 0.30% Si, 0.95% Mn, 0.030% P, 0.003% S, 14.20% Cr, ~0.50% Ni, 1.10% Mo
0.28% C, 0.70% Cr, 0.60% Mo, 2.50% Ni, 0.30% V
0.28% C, 1.50% Mn, 1.30% Cr, 1.00% Ni, + Mo
0.28-0.32% C, 0.15-0.25% Si, 0.30-0.50% Mn, 0.025% P, 0.0015 S, 1.60-1.80% Cr, 1.80-2.20% Mo, 0.20% Ni, 0.40-0.60% V
0.28-0.35% C, 0.10-0.40% Si, 0.15-0.45% Mn, 0.030% P, 0.020% S, 2.70-3.20% Cr, 2.50-3.00% Mo, 0.40-0.70% V
0.28-0.35% C, 0.10-0.40% Si, 0.15-0.45% Mn, 0.030% P, 0.020% S, 2.70-3.20% Cr, 2.50-3.00% Mo, 0.40-0.70% V
0.28-0.35% C, 0.10-0.40% Si, 0.15-0.45% Mn, 0.030% P, 0.020% S, 2.70-3.20% Cr, 2.50-3.00% Mo, 0.40-0.70% V
0.28-0.35% C, 0.10-0.40% Si, 0.15-0.45% Mn, 0.030% P, 0.030% S, 2.70-3.20% Cr, 2.60-3.00% Mo, 0.40-0.70% V, 2.50-3.00% Co
0.28-0.35% C, 0.10-0.40% Si, 0.15-0.45% Mn, 2.70-3.20% Cr, 2.60-3.00% Mo, 0.40-0.70% V
0.28-0.35% C, 0.10???0.40% Si, 0.15???0.45% Mn, 2.70-3.20% Cr, 2.60-3.00% Mo, 0.40???0.70% V
0.28-0.35% C, 0.15-0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 0.60-1.00% Cr, 0.30-0.50% Mo, 2.60-3.20% Ni
0.28-0.35% C, 0.15-0.40% Si, 0.75-1.00% Mn, 0.025% P, 0.02% S, 0.60-1.20% Cr, 0.45-0.65% Mo, >0.04% V
0.28-0.35% C, 0.15-0.40% Si, 0.95-1.30% Mn, 0.030% P, 0.010-0.040% S, 0.60-0.90% Cr, 0.15-0.25% Mo, >0.02% V
0.28-0.35% C, 0.15-0.40% Si, 0.95-1.30% Mn, 0.030% P, 0.010-0.040% S, 0.60-0.90% Cr, 0.15-0.25% Mo, >0.02% V
0.28-0.35% C, 0.15-0.45% Si, 0.65-0.85% Mn, 0.030% P, 0.020% S, 3.70-3.20% Cr, 2.50-3.00% Mo, 0.40-0.70% V
0.28-0.35% C, 0.25-0.40% Si, 0.40-0.60% Mn, 0.40-0.70% Cr, 0.07-0.12% V, 0.030% P, 0.030% S
0.28-0.35% C, 0.25-0.40% Si, 0.40-0.60% Mn, 0.40-0.70% Cr, 0.07-0.12% V, 0.030% P, 0.030% S
0.28-0.35% C, 0.40% Si, 0.40-0.70% Mn, 0.025% P, 0.035% S, 2.80-3.30% Cr, 0.30-0.50% Mo
0.28-0.35% C, 0.40% Si, 0.40-0.70% Mn, 0.025% P, 0.035% S, 2.80-3.30% Cr, 0.30-0.50% Mo
0.28-0.35% C, 0.40% Si, 0.40-0.70% Mn, 0.025% P, 0.035% S, 2.80-3.30% Cr, 0.30-0.50% Mo
0.28-0.35% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.020-0.040% S, 0.40-0.60% Cr
0.28-0.35% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 0.40-0.60% Cr
0.28-0.38% C, 0.80% Si, 1.40% Mn, 0.03% P, 0.05-0.10% S, 15.00-17.00% Cr,
0.28-0.38% C, 1.00% Si, 1.40% Mn, 0.030% P, 0.030% S, 15.00-17.00% Cr, 1.00% Ni
0.28-0.38% C, 1.00% Si, 1.40% Mn, 0.030% P, 0.050-0.100% S, 15.00-17.00% Cr, 1.00% Ni
0.28-0.38% C, 1.00% Si, 1.40% Mn, 0.030% P, 0.050-0.100% S, 15.00-17.00% Cr, 1.00% Ni
0.28-0.38% C, 1.00% Si, 1.40% Mn, max.0.030% P, 0.050-0.10% S, 15.00-17.00% Cr, 1.00% Ni
0.28-0.40% C, 0.20-0.80% Si, 0.60-1.20% Mn, 0.030% P, 0.030% S, 1.40-2.00% Cr, 0.30-0.55% Mo
0.28-0.35% C, 0.40% Si, 0.40-0.70% Mn, 0.035% P, 0.035% S, 2.80-3.30% Cr, 0.30-0.50% Mo, 0.60% Ni
0.29% C, 0.25% Si, 0.30% Mn, 2.70% Cr, 0.35% V, 8.50% W
0.29-0.35% C, 0.10-0.40% Si, 0.40-0.70% Mn, 0.015% P, 0.007% S, 2.80-3.30% Cr, 0.70-1.20% Mo, 0.030% Ni, 0.15-0.35% V
0.29-0.36% C, 0.30% Si, 0.70-1.20% Mn, 1.10-1.60% Cr, 0.90-1.40% Mo, 0.50-1.00% Ni, 0.20-0.40% V, 0.10-0.30% Al
0.30 - 0.40% C, 0.40% Si, 1.40 - 1.60% Mn, 0.020% P, 0.002% S, 1.00 - 1.40% Cr, 0.30 - 0.60% Mo, 0.30 - 0.60% Ni, 0.30% V
0.30% C, 0.10% Si, 0.30% Mn, 1.00% Cr, 1.00% Mo, 0.10% V, 4.50% Co, 7.50% Ni
0.30% C, 0.10% Si, 0.30% Mn, 1.00% Cr, 1.00% Mo, 0.10% V, 7.50% Ni, 4.50% Co
0.30% C, 0.10% Si, 1.45% Mn, 0.020% P, 0.003% S, 1.35% Cr, 0.50% Mo, 0.65% Ni
0.30% C, 0.10% Si, 1.45% Mn, 0.20% P, 0.003% S, 1.35% Cr, 0.50% Mo, 0.65% Ni
0.30% C, 0.20% Si, 1.20% Mn, 2.30% Cr, 0.80% Mo, 0.80% V, 4.00% Ni
0.30% C, 0.20% Si, 5.00% Cr, 2.30% Mo, 0.50% V
0.30% C, 0.25% Si, 0.20% Mn, 0.003% P, 0.002% S, 1.50% Cr, 0.80% Mo, 3.00% Ni, 0.30% V
0.30% C, 0.25% Si, 0.50% Mn, 1.95% Cr, 1.95% Ni, 0.45% Mo
0.30% C, 0.25% Si, 0.60% Mn, 0.010% P, 0.005% S, 1.10% Cr, 0.25% Mo
0.30% C, 0.25% Si, 0.90% Mn, 0.012% P, 0.005% S, 0.90% Cr, 1.80% Ni, 0.43% Mo, 0.08% V, 20 ppm O2
0.30% C, 0.30% Si, 0.30% Mn, 0.025% P, 0.003% S, 3.00% Cr, 2.80% Mo, 0.60% V
0.30% C, 0.30% Si, 0.30% Mn, 2.35% Cr, 0.60% V, 4.50% W
0.30% C, 0.30% Si, 0.30% Mn, 2.35% Cr, 0.60% V, 4.50% W
0.30% C, 0.30% Si, 0.30% Mn, 2.70% Cr, 0.35% V, 9.00% W
0.30% C, 0.30% Si, 0.30% Mn, 2.70% Cr, 0.35% V, 9.00% W
0.30% C, 0.30% Si, 0.30% Mn, 2.70% Cr, 0.35% V, 9.00% W
0.30% C, 0.30% Si, 0.30% Mn, 3.00% Cr, 2.80% Mo, 0.60% V
0.30% C, 0.30% Si, 0.30% Mn, 3.00% Cr, 2.80% Mo, 0.60% V
0.30% C, 0.30% Si, 0.50% Mn, 2.00% Cr, 0.35% Mo, 2.00% Ni
0.30% C, 0.30% Si, 0.50% Mn, 2.00% Cr, 0.35% Mo, 2.00% Ni
0.30% C, 0.30% Si, 0.50% Mn, 3.00% Cr, 3.00% Mo, 0.90% V, 3.00% Co
0.30% C, 0.30% Si, 0.80% Mn, 0.50% Cr, 0.55% Ni, 0.20% Mo
0.30% C, 0.30% Si, 0.85% Mn, 0.85% Cr, 0.40% Mo, 0.07% V, 1.80% Ni
0.30% C, 0.30% Si, 1.55% Mn, 1.35% Cr, 0.70% Mo, 1.00% Ni, +others
0.30% C, 0.40% Si, 0.50% Mn, 0.025% P, 0.030% S, 13.20% Cr
0.30% C, 0.40% Si, 0.50% Mn, 0.030% P, 0.025% S, 13.20% Cr
0.30% C, 0.40% Si, 0.55% Mn, 2.50% Cr, 0.15% V
0.30% C, 0.40% Si, 0.70% Mn, 0.030% P, 0.20% S, 13.00% Cr, 0.30% Mo
0.30% C, 0.40% Si, 0.70% Mn, 0.030% P, 0.20% S, 13.00% Cr, 0.30% Mo
0.30% C, 0.50% Si, 0.75% Mn, 1.70% Cr, 0.40% Mo
0.30% C, 0.60% Si, 0.40% Mn, 15.00% Cr, 1.00% Mo, 0.40% N
0.30% C, 0.60% Si, 0.40% Mn, 15.00% Cr, 1.00% Mo, 0.40% N
0.30% C, 0.70% Si, 1.60% Mn, 0.025% P, 0.010% S, 1.50% Cr, 0.50% Mo, 1.00% Ni, 0.08% V, 0.30% Cu, 0.05% Nb, 0.005% B
0.30% C, 1.15% Mn, 2.00% Cr, 1.00% Ni, 0.65% Mo
0.30% C, 1.20% Cr, 0.45% Mo, 3.50% Ni
0.30% C, 1.40% Cr, 1.20% Mo, 0.30% V
0.30% C, 13.00% Cr
0.30% C, 13.00% Cr
0.30% C, 3.00% Cr, 0.30% V, 9.00% W
0.30% C, 3.00% Cr, 0.30% V, 9.00% W
0.30% C, 3.00% Cr, 0.40% Mo
0.30% C, 3.00% Cr, 1.00% Mo, 0.20% V
0.30-0.34% C, 0.30% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 0.90-1.20% Cr, 0.0008-0.0050% B
0.30-0.35% C, 0.35% Si, 0.60% Mn, 0.025% P, 0.010% S, 2.80-3.20% Cr, 0.80-1.20%Mo, 0.25-0.35% V
0.30-0.35% C, 0.35% Si, 0.60% Mn, 0.025% P, 0.010% S, 2.80-3.20% Cr, 0.80-1.20% Mo, 0.25-0.35% V
0.30-0.35% C, 20% Si, 0.25% Mn, 0.005% P, 0.005% S, 2.80-3.20% Cr, 0.70-1.20% Mo, 0.30% Ni, 0.15-9.35% V
0.30-0.37% C, 0.15-0.35% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 1.20-1.50% Cr, 0.80-1.10% Al
0.30-0.37% C, 0.40% Si, 0.30-0.60% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr
0.30-0.37% C, 0.40% Si, 0.30-0.60% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr
0.30-0.37% C, 0.40% Si, 0.40-0.70% Mn, 0.025% P, 0.035% S, 1.00-1.30% Cr, 0.15-0.25% Mo, 0.80-1.20% Al
0.30-0.37% C, 0.40% Si, 0.40-0.70% Mn, 0.025% P, 0.035% S, 1.50-1.80% Cr, 0.15-0.25% Mo, 0.85-1.15% Ni, 0.80-1.20% Al
0.30-0.37% C, 0.40% Si, 0.40-0.70% Mn, 0.025% P, 0.035% S, 0.15-0.25% Cr, 0.80-1.20% Al
0.30-0.37% C, 0.40% Si, 0.40-0.70% Mn, 0.025% P, 0.035% S, 0.15-0.25% Cr, 0.80-1.20% Al
0.30-0.37% C, 0.40% Si, 0.40-0.70% Mn, 0.025% P, 0.035% S, 1.50-1.80% Cr, 0.15-0.25% Mn, 0.85-1.15% Ni, 0.80-1.20% Al
0.30-0.37% C, 0.40% Si, 0.40-0.70% Mn, 0.025% P, 0.035% S, 1.50-1.80% Cr, 0.15-0.25% Mo, 0.85-1.15% Ni, 0.80-1.20% Al
0.30-0.37% C, 0.40% Si, 0.40-0.70% Mn, 0.025% P, 0.035% S, 1.50-1.80% Cr, 0.15-0.25% Mo, 0.85-1.15% Ni, 0.80-1.20% Al
0.30-0.37% C, 0.40% Si, 0.40-0.70% Mn, 0.025% P, 0.035% S, 1.50-1.80% Cr, 0.15-0.25% Mo, 0.85-1.15% Ni, 0.80-1.20% Al
0.30-0.37% C, 0.40% Si, 0.40-0.70% Mn, 0.025% P, 0.035% S, 1.50-1.80% Cr, 0.15-0.25% Mo, 0.85-1.15% Ni, 0.80-1.20% Al
0.30-0.37% C, 0.40% Si, 0.40-0.70% Mn, 0.025% P, 0.035% S, 1.50-1.80% Cr, 0.15-0.25% Mo, 0.85-1.15% Ni, 0.80-1.20% Al
0.30-0.37% C, 0.40% Si, 0.40-0.70% Mn, 0.035% P, 0.035% S, 1.50-1.80% Cr, 0.85-1.15% Ni, 0.15-0.25% Mo, 0.80-1.20% Al
0.30-0.37% C, 0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 0.80-1.10% Cr, 1.20-1.60% Ni
0.30-0.37% C, 0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.30-0.37% C, 0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.30-0.37% C, 0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.035% S, 0.90-1.20% Cr
0.30-0.37% C, 0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.035% S, 0.90-1.20% Cr
0.30-0.37% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.020-0.040% S, 0.90-1.20% Cr
0.30-0.37% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.020-0.040% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.30-0.37% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr
0.30-0.38% C, 0.15-0.35% Si, 0.30-0.60% Mn, 0.025% P, 0.020% S, 1.60-1.90% Cr, 0.25-0.45% Mo, 3.80-4.00% Ni
0.30-0.38% C, 0.15-0.40% Si, 0.025% P, 0.035% S, 1.30-1.70% Cr, 0.15-0.30% Mo, 1.30-1.70% Ni
0.30-0.38% C, 0.20-0.40% Si, 0.20-0.50% Mn, 0.035% P, 0.035% S, 1.50-1.90% Cr, 3.50-4.00% Ni
0.30-0.38% C, 0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S, 1.30-1.70% Cr, 0.15-0.30% Mo, 1.30-1.70% Ni
0.30-0.38% C, 0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S, 1.30-1.70% Cr, 0.15-0.30% Mo, 1.30-1.70% Ni
0.30-0.38% C, 0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S, 1.30-1.70% Cr, 0.15-0.30% Mo, 1.30-1.70% Ni
0.30-0.38% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 1.30-1.70% Cr, 0.15-0.30% Mo, 1.30-1.70% Ni
0.30-0.38% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 1.30-1.70% Cr, 0.15-0.30% Mo, 1.30-1.70% Ni
0.30-0.38% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 1.30-1.70% Cr, 0.15-0.30% Mo, 1.30-1.70% Ni
0.30-0.38% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 1.30-1.70% Cr, 0.15-0.30% Mo, 1.30-1.70% Ni
0.30-0.38% C, 0.70-1.20% Si, 0.60% Mn, 4.50-5.50% Cr, 1.10-1.80% Mo, 0.50-1.20% V
0.30-0.40% C, 0.15-0.35% Si, 0.40-0.70% Mn, 0.015% P, 0.015% S, 1.00-1.40% Cr, 0.35-0.60% Mo, 1.50-1.80% Ni, 2.50-3.50% Ni, 0.08-0.20% V
0.30-0.40% C, 0.15-0.35% Si, 0.40-0.70% Mn, 0.015% P, 0.015% S, 1.00-1.40% Cr, 0.35-0.65% Mo, 2.50-3.50% Ni, 0.08-0.20% V
0.30-0.40% C, 0.15-0.35% Si, 0.40-0.90% Mn, 0.80-2.00% Cr, 0.35-0.90% Mo, 2.50-4.00% Ni, 0.05-0.25% V
0.30-0.40% C, 0.15-0.55% Si, 0.40-0.90% Mn, 0.80-1.70% Cr, 0.35-0.90% Mo, 3.00-4.00% Ni, 0.05-0.25% V
0.30-0.40% C, 0.15-0.55% Si, 0.40-0.90% Mn, 0.80-2.00% Cr, 0.35-0.90% Mo, 2.50-4.50% Ni, 0.05-0.25% V
0.30-0.40% C, 0.2-1.00% Si, 0.30-1.00% Mn, 0.015% P, 0.003% S, 2.80-3.50% Cr, 2.00-2.40% Mo, 0.20-1.00% V
0.30-0.40% C, 0.20-1.00% Si, 0.30-1.00% Mn, 2.80-3.50% Cr, 2.00-2.40% Mo, 0.20-1.00% V
0.30-0.40% C, 0.30-0.70% Si, 0.60-1.00% Mn, 0.030% P, 0.030% S, 1.50-2.00% Cr, 0.35-0.55% Mo
0.30-0.40% C, 0.30-0.70% Si, 0.60-1.00% Mn, 0.030% P, 0.030% S, 1.50-2.00% Cr, 0.35-0.55% Mo
0.30-0.40% C, 0.30-0.70% Si, 0.60-1.00% Mn, 0.030% P, 0.030% S, 1.50-2.00% Cr, 0.35-0.55% Mo
0.30-0.40% C, 0.40% Si, 1.40-1.60% Mn, 0.020% P, 0.002% S, 1.00-1.40% Cr, 0.30-0.60% Mo, 0.30-0.60% Ni, 0.30% V
0.30-0.40% C, 0.70-1.20% Si, 0.40-0.60% Mn, 0.030% P, 0.030% S, 4.50-5.50% Cr, 1.00-1.20% Mo, 0.80-1.00% V
0.30-0.40% C, 0.75-1.10% Si, 0.40% Mn, 2.80-3.20% Cr, 2.65-2.95% Mo, 0.40% Ni, 0.30-1.10% V, 0.20% Cu
0.30-0.40% C, 0.75-1.10% Si, 0.40% Mn, 2.80-3.20% Cr, 2.65-2.95% Mo, 0.40% Ni, 0.30-1.10% V, 0.20% Cu
0.30-0.40% C, 0.75-1.10% Si, 0.40% Mn, 2.80-3.20% Cr, 2.65-2.95% Mo, 0.40% Ni, 0.30-1.10% V, 0.20% Cu
0.30-0.40% C, 0.80-1.10% Si, 0.20-0.40% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 1.80-2.10% W, 0.15-0.20% V
0.30-0.40% C, 1.00% Si, 0.30-0.60% Mn, 0.05-0.10% S, 15.00-16.50% Cr
0.30% C, 0.25% Si, 1.35% Mn
0.30-0.37% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.020-0.030% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.30-0.37% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.020-0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.30-0.37% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr
0.30-0.38% C, 0.40% Si, 0.40-0.70% Mn, 0.035% P, 0.030% S, 1.40-1.70% Cr, 0.15-0.30% Mo, 1.40-1.70% Ni
0.31% C, 0.25% Si, 0.48% Mn, 0.008% P, 0.002% S, 0.82% Cr, 0.06% Mo, 2.64% Ni, 0.010% Co
0.31% C, 0.25% Si, 0.48% Mn, 0.008% P, 0.002% S, 0.82% Cr, 0.06% Mo, 2.64% Ni, 0.010% Cu
0.31% C, 0.25% Si, 0.60% Mn, 2.55% Cr, 0.15% V, 0.20% Mo
0.31% C, 0.30% Si, 0.35% Mn, 2.90% Cr, 2.70% Mo, 0.50% V
0.31% C, 0.30% Si, 0.35% Mn, 2.90% Cr, 2.80% Mo, 0.50% V
0.31% C, 0.30% Si, 0.35% Mn, 2.90% Cr, 2.80% Mo, 0.50% V
0.31% C, 0.32% Si, 0.58% Mn, 1.07% Cr, 0.21% Mo, 0.15% Ni, 0.025% V, 0.028% Nb
0.31% C, 0.40% Si, 0.55% Mn, 3.05% Cr, 0.40% Mo, 0.30% Ni
0.31% C, 1.00% Si, 1.50% Mn, 13.00% Cr
0.31% C, 2.50% Cr, 0.20% Mo, 0.15% V
0.31-0.38% C, 0.150.40% Si, 0.30-0.60% Mn, 0.035% P, 0.035% S, 1.60-1.20% Cr, 0.25-0.45% Mo, 3.70-4.20% Ni
0.31-0.38% C, 0.150.40% Si, 0.30-0.60% Mn, 0.035% P, 0.035% S, 1.60-1.20% Cr, 3.70-4.20% Ni, 0.25-0.45% Mo
0.31-0.38% C, 0.40% Si, 1.20-1.50% Mn, 0.040% P, 0.030% S, 0.50% Cr, 0.0008???0.0040% B
0.31% C, 0.27% Si, 0.64% Mn, 0.020% P, 0.022% S, 0.79% Cr, 2.89% Ni
0.31% C, 0.40% Si, 0.55% Mn, 3.05% Cr, 0.40% Mo, 0.30% Ni
0.32% C, 0.20% Si, 0.30% Mn, 5.20% Cr, 1.20% Mo, 0.50% V, 3.80% W
0.32% C, 0.25% Si, 0.53% Mn, 0.013% P, 0.001% S, 1.27% Cr, 0.33% Mo, 3.87% Ni, 0.08% Cu
0.32% C, 0.30% Si, 0.50% Mn, 1.10% Cr, 0.20% Mo
0.32% C, 0.40% Si, 0.40% Mn, 3.00% Cr, 2.80% Mo, 0.60% V, 3.00% Co
0.32% C, 0.40% Si, 0.40% Mn, 3.00% Cr, 2.80% Mo, 0.60% V
0.32% C, 0.40% Si, 0.40% Mn, 3.00% Cr, 2.80% Mo, 0.60% V
0.32% C, 0.40% Si, 0.40% Mn, 3.00% Cr, 2.80% Mo, 0.50% V
0.32% C, 0.40% Si, 0.40% Mn, 3.00% Cr, 2.80% Mo, 0.60% V, 3.00% Co
0.32% C, 0.90% Si, 0.40% Mn, 1.10% Cr, 0.20% V, 4.00% W
0.32% C, 3.0% Cr, 2.8% Mo, 0.5% V
0.32% C, 3.00% Cr, 2.80% Mo, 0.50% V, 3.00% Co
0.32% C, 3.00% Cr, 2.80% Mo, 0.50% V, 2.80% Co
0.32% C, 3.00% Cr, 2.80% Mo, 0.50% V, 3.00% Co
0.32% C, 3.00% Cr, 2.80% Mo, 0.50% V
0.32% C, 3.00% Cr, 2.80% Mo, 0.50% V
0.32% C, 3.00% Cr, 2.80% Mo, 0.50% V
0.32% C, 3.00% Cr, 2.80% Mo, 0.50% V
0.32% C, 3.00% Cr, 2.80% Mo, 0.50% V
0.32-0.39% C, 0.10-0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.020-0.040% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, 0.30% Cu
0.32-0.39% C, 0.15-0.35% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S
0.32-0.39% C, 0.30% Si, 0.50-0.80% Mn, 0.025% P, 0.025% S, 0.025% Cu
0.32-0.39% C, 0.40% Si, 0.30-0.60% Mn, 0.030% P, 0.025% S, 1.60-2.00% Cr, 0.25-0.45% Mo, 3.60-4.10% Ni
0.32-0.39% C, 0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.025% S, 1.60-2.00% Cr, 0.25-0.45% Mo, 3.60-4.10% Ni
0.32-0.39% C, 0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.025% S, 1.60-2.00% Cr, 0.25-0.45% Mo, 3.60-4.10% Ni
0.32-0.39% C, 0.40% Si, 0.50-0.80% Mn, 0.030% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.32-0.39% C, 0.40% Si, 0.50-0.80% Mn, 0.030% P, 0.020-0.040% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.32-0.39% C, 0.40% Si, 0.50-0.80% Mn, 0.030% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.32-0.39% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.32-0.39% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.32-0.39% C, 0.40% Si, 0.50-0.80% Mn, 0.045% P, 0.040% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.32-0.39% C, 0.40% Si, 0.50-0.80% Mn, 0.045% P, 0.040% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.32-0.39% C, 0.40% Si, 0.50-0.80% Mn, 0.045% P, 0.045% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.32-0.39% C, 0.40% Si, 0.70-1.10% Mn, 0.060% P, 0.15-0.25% S
0.32-0.39% C, 0.40% Si, 1.30-1.70% Mn, 0.06% P, 0.10-0.18% S
0.32-0.39% C, 0.40% Si, 1.30-1.70% Mn, 0.06% P, 0.10-0.18% S
0.32-0.40% C, 0.10-0.30% Si, 0.30-0.50% Mn, 0.015% P, 0.003% S, 4.80-5.50% Cr, 1.20-1.50% Mo, 0.30-0.50% V
0.32-0.40% C, 0.10-0.30% Si, 0.30-0.50% Mn, 0.015% P, 0.003% S, 4.80-5.50% Cr, 1.20-1.50% Mo, 0.30-0.50% V
0.32-0.40% C, 0.10-0.30% Si, 0.30-0.50% Mn, 0.015% P, 0.003% S, 4.80-5.50% Cr, 1.20-1.50% Mo, 0.30-0.50% VBR>
0.32-0.40% C, 0.10-0.30% Si, 0.30-0.50% Mn, 0.015% P, 0.003% S, 4.80-5.50% Cr, 2.80-3.20% Mo, 0.40-0.70% V
0.32-0.40% C, 0.10-0.30% Si, 0.30-0.50% Mn, 0.003% S, 0.015% P, 4.80-5.50% Cr, 1.50-2.00% Mo, +W
0.32-0.40% C, 0.10-0.30% Si, 0.30-0.50% Mn, 0.003% S, 0.015% P, 4.80-5.50% Cr, 1.50-2.00% Mo, 0.40-0.70% V, +W
0.32-0.40% C, 0.10-0.30% Si, 0.30-0.50% Mn, 0.003% S, 0.015% P, 4.80-5.50% Cr, 2.00-2.40% Mo, +W
0.32-0.40% C, 0.10-0.30% Si, 0.30-0.50% Mn, 0.015% P, 0.003% S, 4.80-5.50% Cr, 1.20-1.50% Mo, 0.30-0.50% V
0.32-0.40% C, 0.10-0.30% Si, 0.30-0.50% Mn, 0.015% P, 0.003% S, 4.80-5.50% Cr, 1.20-1.50% Mo, 0.30-0.50% V
0.32-0.40% C, 0.10-0.30% Si, 0.30-0.50% Mn, 0.015% P, 0.003% S, 4.80-5.50% Cr, 1.20-1.50% Mo, 0.30-0.50% V
0.32-0.40% C, 0.10-0.30% Si, 0.30-0.50% Mn, 0.015% P, 0.003% S, 4.80-5.50% Cr, 2.00-2.40% Mo, 0.40-0.70% V
0.32-0.40% C, 0.10-0.30% Si, 0.30-0.50% Mn, 0.015% P, 0.003% S, 4.80-5.50% Cr, 2.80-3.20% Mo, 0.40-0.70% V
0.32-0.40% C, 0.10-0.30% Si, 0.30-0.50% Mn, 4.80-5.50% Cr, 1.20-1.50% Mo, 0.30-0.50% V
0.32-0.40% C, 0.10-0.30% Si, 0.30-0.50% Mn, 4.80-5.50% Cr, 1.20-1.50% Mo, 0.30-0.50% V
0.32-0.40% C, 0.10-0.30% Si, 0.30-0.50% Mn, 4.80-5.50% Cr, 2.80-3.20% Mo, 0.40-0.70% V
0.32-0.40% C, 0.10-0.30% Si, 0.30-0.50% Mn, 4.80-5.50% Cr, 2.80-3.20% Mo, 0.40-0.70% V
0.32-0.40% C, 0.10-0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo, 0.90-1.20% Ni, 0.40% Cu
0.32-0.40% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo, 0.90-1.20% Ni
0.32-0.40% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo, 0.90-1.20% Ni
0.32-0.40% C, 0.40% Si, 1.20-1.50% Mn, 0.035% P, 0.035% S
0.32-0.40% C, 0.80-1.20% Si, 0.20-0.50% Mn, 0.030% P, 0.020% S, 4.75-5.50% Cr, 1.25-1.60% Mo, 1.10-1.60% W, 0.20-0.50% V
0.32-0.40% C, 0.90-1.20% Si, 0.30-0.60% Mn, 0.030% P, 0.030% S, 5.00-5.60% Cr, 1.30-1.60% Mo, 1.20-1.40% W, 0.15-0.40% V
0.32-0.41% C, 0.80-1.20% Si, 0.25-0.50% Mn, 0.025% P, 0.005% S, 4.80-5.50% Cr, 1.10-1.50% Mo, 0.30-0.50% V
0.32-0.42% C, 0.80-0.12% Si, 0.50% Mn, 0.00% Ni, 4.50-5.50% Cr, 1.00-1.50% Mo, 0.80-1.20% V
0.32-0.42% C, 0.80-1.20 C, 0.50% Mn, 4.50-5.50% Cr, 1.00-1.50% Mo, 0.80-1.20% V
0.32-0.42% C, 0.80-1.20% Si, 0.50% Mn, 4.50-5.50% Cr, 1.00-1.50% Mo, 0.80-1.00% V
0.32-0.42% C, 0.80-1.20% Si, 0.50% Mn, 4.50-5.50% Cr, 1.00-1.50% Mo, 0.80-1.20% V
0.32-0.42% C, 0.80-1.20% Si, 0.50% Mn, 4.50-5.50% Cr, 1.00-1.50% Mo, 0.80-1.20% V
0.32-0.42% C, 1.50% Si, 1.50% Mn, 4.50-5.50% Cr, 1.00-1.50% Mo, 0.40-1.20% V, + free machining elemenets
0.32-0.42% C, 1.50% Si, 1.50% Mn, 4.50-5.50% Cr, 1.00-1.50% Mo, 0.40-1.20% V, + free machining elemenets
0.32-0.42% C, 1.50% Si, 1.50% Mn, 4.50-5.50% Cr, 1.00-1.50% Mo, 0.40-1.20% V
0.32-0.45% C, 0.80-1.20% Si, 0.20-0.50% Mn, 0.030% P, 0.030% S, 4.75-5.50% Cr, 1.10-1.75% Mo, 0.80-1.20% V
0.32-0.45% C, 0.80-1.20% Si, 4.75-5.50% Cr, 1.10-1.75% Mo, 0.80-1.20% V
0.32-0.45% C, 0.80-1.20% Si, 4.75-5.50% Cr, 1.10-1.75% Mo, 0.80-1.20% V
0.32-0.45% C, 0.80-1.20% Si, 4.75-5.50% Cr, 1.10-1.75% Mo, 0.80-1.20% V
0.32-0.45% C, 0.80-1.20% Si, 4.75-5.50% Cr, 1.10-1.75% Mo, 0.80-1.20% V
0.32-0.45% C, 0.80-1.20% Si, 4.75-5.50% Cr, 1.10-1.75% Mo, 0.80-1.20% V
0.32-0.45% C, 0.80-1.20% Si, 4.75-5.50% Cr, 1.10-1.75% Mo, 0.80-1.20% V
0.32-0.45% C, 0.80-1.20% Si, 4.75-5.50% Cr, 1.10-1.75% Mo, 0.80-1.20% V
0.32-0.45% C, 0.80-1.20% Si, 4.75-5.50% Cr, 1.10-1.75% Mo, 0.80-1.20% V
0.32-0.45% C, 0.80-1.25% Si, 0.20-0.60% Mn, 4.75-5.50% Cr, 1.10-1.75% Mo, 0.80-1.20% V
0.32-0.37% C, 0.20-0.40% Si, 0.60-0.80% Mn, 0.90-1.00% Cr, 0.20-0.25% Mo
0.32-0.39% C, 0.40% Si, 0.50-0.80% Mn, 0.030% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.32-0.39% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.020-0.035% S
0.32-0.39% C, 0.40% Si, 0.50-0.80% Mn, 0.045% P, 0.045% S
0.32-0.40% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.030% S, 0.90-1.20% Cr, 0.15-0.30% Mo, 0.90-1.20% Ni
0.32-0.40% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo, 0.90-1.20% Ni
0.32-0.40% C, 0.40% Si, 1.20-1.50% Mn, 0.035% P, 0.035% S
0.33% C, 0.05% S, 16.00% Cr, 0.50% Ni
0.33% C, 0.08% S, 16.00% Cr
0.33% C, 0.20% Si, 0.30% Mn, 13.70% Cr
0.33% C, 0.25% Si, 0.20% Mn, 0.003% P, 0.002% S, 1.50% Cr, 0.80% Mo, 3.00% Ni, 0.30% V
0.33% C, 0.30% Si, 0.80% Mn, 0.06% S, 16.00% Cr, 0.30% Ni
0.33% C, 0.34% Si, 0.92% Mn, 0.011% P, 0.02% S, 5.43% Cr, 2.36% Mo, 0.53% V, 0.06% Cu. Patent pending.
0.33% C, 0.35% Si, 0.36% Mn, 0.028% P, 0.07% S, 15.08% Cr, 0.07% Mo, 0.03% V, 0.19% Ni, 0.07% Cu
0.33% C, 0.35% Si, 0.36% Mn, 15.08% Cr, 0.07% Mo, 0.19% Ni, 0.03% V
0.33% C, 0.35% Si, 0.85% Mn, 1.55% Cr, 0.50% Mo, 0.55% Ni
0.33% C, 0.35% Si, 1.35% Mn, 16.70% Cr, 0.12% S
0.33% C, 0.45% Si, 0.25% Mn, 3.30% Cr, 0.45% V, 9.15% W
0.33% C, 0.45% Si, 0.25% Mn, 3.30% Cr, 9.15% W, 0.45% V
0.33% C, 0.45% Si, 0.80% Mn, 1.80% Cr, 0.45% Mo, 0.40% Ni, 0.00% W
0.33% C, 0.92% Mn, 0.011% P, 0.002% S, 5.43% Cr, 2.36% Mo, 0.14% Ni, 0.53% V, 0.06% Cu
0.33% C, 1.00% Si, 1.00% Mn, 0.08% S, 16.00% Cr, 1.00% Ni
0.33% C, 1.00% Si, 1.00% Mn, 16.00% Cr, 1.00% Ni, 0.07% S
0.33% C, 16.00% Cr, 0.050% S, 0.50% N
0.33% C, 16.00% Cr, 0.050% S, 0.50% Ni
0.33-0.39% C, 0.15-0.35% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S
0.33-0.39% C, 0.15-0.35% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S
0.33-0.39% C, 0.15-0.35% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S
0.33-0.40% C, 0.15-0.40% Si, 0.80-1.20% Mn, 0.035% P, 0.035% S, 1.00-1.30% Cr
0.33-0.41% C, 0.80-1.20% Si, 0.25-0.50% Mn, 0.025% P, 0.005% S, 4.80-5.50% Cr, 1.10-1.50% Mo, 0.30-0.50% V
0.33-0.41% C, 0.80-1.20% Si, 0.25-0.50% Mn, 0.030% P, 0.020% S, 4.80-5.50% Cr, 1.10-1.50% Mo, 0.30-0.50% V
0.33-0.41% C, 0.80-1.20% Si, 0.25-0.50% Mn, 0.030% P, 0.020% S, 4.80-5.50% Cr, 1.10-1.50% Mo, 0.30-0.50% V
0.33-0.41% C, 0.80-1.20% Si, 0.25-0.50% Mn, 0.030% P, 0.030% S, 5.80-5.50% Cr, 1.10-1.50% Mo, 0.30-0.50% V
0.33-0.41% C, 0.80-1.20% Si, 0.25-0.50% Mn, 0.030% P, 0.030% S, 5.80-5.50% Cr, 1.10-1.50% Mo, 0.30-0.50% V
0.33-0.41% C, 0.80-1.20% Si, 0.25-0.50% Mn, 0.030% P, 0.030% S, 5.80-5.50% Cr, 1.10-1.50% Mo, 0.30-0.50% V
0.33-0.41% C, 0.80-1.20% Si, 0.25-0.50% Mn, 0.030% P, 0.030% S, 5.80-5.50% Cr, 1.10-1.50% Mo, 0.30-0.50% V
0.33-0.41% C, 0.80-1.20% Si, 0.25-0.50% Mn, 0.030% P, 0.030% S, 5.80-5.50% Cr, 1.10-1.50% Mo, 0.30-0.50% V
0.33-0.41% C, 0.80-1.20% Si, 0.25-0.50% Mn, 0.030% P, 0.030% S, 5.80-5.50% Cr, 1.10-1.50% Mo, 0.30-0.50% V
0.33-0.41% C, 0.80-1.20% Si, 0.30-0.50% Mn, 0.015% P, 0.002% S, 4.80-5.20% Cr, 1.10-1.40% Mo, 0.30-0.50% V
0.33-0.41% C, 1.10-1.40% Si, 1.10-1.40% Mn, 0.035% P, 0.035% S
0.33-0.43% C, 1.00% Si, 0.30-0.60% Mn, 12.50-13.50% Cr
0.33-0.43% C, 1.00% Si, 1.0% Mn, 12.50-13.50% Cr
0.33-0.43% C, 1.00% Si, 1.00% Mn, 12.50-13.50% Cr, 0.30-0.60% Mo
0.33-0.43% C, 1.00% Si, 1.00% Mn, 15.00-17.50% Cr, 1.00-1.30% Mo, 1.00% Ni
0.33-0.43% C, Max. 1.00% Si, 1.00% Mn, 15.00-17.50% Cr, 1.00-1.30% Mo, 1.00% Ni
0.33-0.45% C, 1.00% Si, 1.50% Mn, 0.030% P, 0.030% S, 15.50-17.50% Cr, 0.80-1.30% Mo, 1.00% Ni
0.33-0.45% C, 1.00% Si, 1.50% Mn, 0.030% P, 0.030% S, 15.50-17.50% Cr, 0.80-1.30% Mo, 1.00% Ni
0.33-0.45% C, 1.00% Si, 1.50% Mn, 0.030% P, 0.030% S, 15.50-17.50% Cr, 0.80-1.30% Mo, 1.00% Ni
0.33-0.45% C, 1.00% Si, 1.50% Mn, 0.030% P, 0.030% S, 15.50-17.50% Cr, 0.80-1.30% Mo, 1.00% Ni
0.33-0.45% C, 1.00% Si, 1.50% Mn, 0.030% P, 0.030% S, 15.50-17.50% Cr, 0.80-1.30% Mo, 1.00% Ni
0.33-0.45% C, 1.00% Si, 1.50% Mn, 0.030% P, 0.030% S, 15.50-17.50% Cr, 0.80-1.30% Mo, 1.00% Ni
0.33-0.45% C, 1.00% Si, 1.50% Mn, 0.030% P, 0.030% S, 15.50-17.50% Cr, 0.80-1.30% Mo, 1.00% Ni
0.33-0.45% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.015% S, 15.50-17.50% Cr, 0.80-1.30% Mo, 1.00% Ni
0.33-0.45% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.015% S, 15.50-17.50% Cr, 0.80-1.30% Mo, 1.00% Ni
0.33-0.45% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.030% S, 15.50-17.50% Cr, 0.80-1.30% Mo, 1.00% Ni
0.33-0.45% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.030% S, 15.50-17.50% Cr, 0.80-1.30% Mo, 1.00% Ni
0.33-0.39% C, 0.15-0.35% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S
0.34% C, 0.25% Si, 0.50% Mn, 1.15% Cr, 0.75% Mo, 2.85% Ni, 0.10% V
0.34% C, 0.25% Si, 0.50% Mn, 1.50% Cr, 0.25% Mo, 1.55% Ni, + Pb
0.34% C, 0.25% Si, 0.50% Mn, 1.50% Cr, 1.55% Ni, 0.25% Mo
0.34% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.25% Mo
0.34% C, 0.25% Si, 0.85% Mn, 1.05% Cr, 0.035% S
0.34% C, 0.28% Mn, 0.56% Si, 0.008% P, 0.001% S, 1.57% Cr, 0.20% Mo, 1.58% Ni, 0.11% Cu
0.34% C, 0.30% Si, 0.50% Mn, 1.50% Cr, 0.20% Mo, 1.50% Ni
0.34% C, 0.30% Si, 0.50% Mn, 1.70% Cr, 0.20% Mo, 1.00% Ni, 0.95% Al
0.34% C, 0.30% Si, 0.95% Mn, 0.025% P, 0.10% S, 15.00% Cr
0.34% C, 0.30% Si, 0.95% Mn, 0.025% P, 0.100% S, 15.00% Cr
0.34% C, 0.35% Si, 1.40% Mn, 0.12% S, 16.00% Cr, 0.15% Mo, + special additions
0.34% C, 0.35% Si, 1.40% Mn, 0.12% S, 16.00% Cr, 0.15% Mo, plus others
0.34% C, 0.40% Si, 0.55% Mn, 1.65% Cr, 0.20% Mo, 1.00% Ni, 1.00% Al
0.34% C, 0.40% Si, 0.95% Mn, 0.020% P, 0.005-0.020% S, 1.90% Cr, 0.40% Mo, Ni dpends on thickness
0.34% C, 0.80% Mn, 1.70% Cr, 0.40% Mo, 0.50% Ni
0.34% C, 1.50% Cr, 0.25% Mo, 1.50% Ni
0.34% C, 1.50% Cr, 0.25% Mo, 1.50% Ni
0.34% C, 1.70% Cr, 0.20% Mo, 1.00% Ni, 1.00% Al
0.34-0.40% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr
0.34-0.40% C, 0.40% Si, 0.80-1.10% Mn, 0.025% P, 0.015% S, 0.15-0.35% Cr, 0.020-0.050% Ti, 0.020-0.060% Al, 0.0008-0.0050% B
0.34-0.40% C, 0.40% Si, 0.80-1.10% Mn, 0.025% P, 0.015% S, 0.15-0.35% Cr, 0.020-0.050% Ti, 0.020-0.060% Al, 0.0008-0.0050% B
0.34-0.41% C, 0.10-0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.035% S, 0.90-1.20% Cr, 0.40% Cu
0.34-0.41% C, 0.15-0.80% Si, 1.20-1.60% Mn, 0.025% P, 0.020-0.060% S, 0.30% Cr, 0.08% Mo, 0.08-0.20% V, 0.010-0.020% N
0.34-0.41% C, 0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.035% S, 0.90-1.20% Cr
0.34-0.41% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.020-0.040% S, 0.90-1.20% Cr
0.34% C, 0.23% Si, 0.55% Mn, 0.011% P, 0.022% S, 1.39% Cr, 4.59% Ni
0.34% C, 0.40% Si, 0.75% Mn, 1.05% Cr
0.34-0.41% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.020-0.035% S, 0.90-1.20% Cr
0.34-0.41% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.030% S, 0.90-1.20% Cr
0.34% C, 0.25% Si, 0.55% Mn, 1.65% Cr, 1.00% Al, 0.20% Mo, 1.00% Ni
0.34% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.25% Mo
0.34% C, 0.25% Si, 0.75% Mn, 1.50% Cr, 1.00% Al
0.34% C, 0.29% Si, 0.59% Mn, 0.012% P, 0.007% S, 1.54% Cr, 0.24% Mo, 1.52% Ni
0.35 - 0.45% C, 0.20-0.40% Si, 1.30 - 1.60% Mn, 0.020% P, 0.002% S, 1.80 - 2.10% Cr, 0.15 - 0.25% Mo, 0.90 - 1.10% Ni, 0.05% V
0.35 - 0.45% C, 0.30 - 0.50% Si, 1.40 - 1.60% Mn, 0.030% P, 0.050 - 1.100% S, 1.80 - 2.00% Cr, 0.15 - 0.25% Mo
0.35% C, 0.10-0.35% Si, 0.60-1.05% Mn, 0.035% P, 0.040% S, 0.30% Cu, 0.12% Cu, 0.40% Ni, 0.08% V, 0.03% Nb, 0.40% Cu
0.35% C, 0.20% Si, 0.30% Mn, 0.012% P, 0.003% S, 5.20% Cr, 1.40% Mo, 0.55% V, + Nb
0.35% C, 0.20% Si, 0.30% Mn, 0.012% P, 0.003% S, 5.20% Cr, 1.40% Mo, 0.55% V, + Nb
0.35% C, 0.20% Si, 0.30% Mn, 5.20% Cr, 1.40% Mo, 0.55% V, +Nb
0.35% C, 0.20% Si, 0.30% Mn, 5.20% Cr, 1.40% Mo, 0.55% V, +Nb
0.35% C, 0.20% Si, 0.50% Mn, 5.00% Cr, 2.30% Mo, 0.60% V
0.35% C, 0.20% Si, 0.50% Mn, 5.00% Cr, 2.30% Mo, 0.60% V
0.35% C, 0.20% Si, 0.50% Mn, 5.00% Cr, 2.30% Mo, 0.60% V
0.35% C, 0.20% Si, 0.50% Mn, 5.00% Cr, 2.30% Mo, 0.60% V
0.35% C, 0.20% Si, 0.50% Mn, 5.00% Cr, 2.30% Mo, 0.60% V
0.35% C, 0.20% Si, 0.70% Mn, 0.025% P, 0.025% S, 0.25% Cu
0.35% C, 0.22% Si, 0.63% Mn, 0.094% Cr, 0.010% V, 0.014% Al, 0.081% Cu, 0.004% B
0.35% C, 0.25% Si, 0.00% Mn, 0.65% Cr, 0.020-0.035% S, + Pb
0.35% C, 0.25% Si, 0.50% Mn, 0.025% P, 0.010% S, 1.35% Cr, 0.30% Mo, 4.00% Ni
0.35% C, 0.25% Si, 0.50% Mn, 1.35% Cr, 0.30% Mo, 4.10% Ni
0.35% C, 0.30% Si, 0.003% S, 5.00% Cr, 1.35% Mo, 0.45% V
0.35% C, 0.30% Si, 0.10% S, 16.00% Cr, 1.00% Mo
0.35% C, 0.30% Si, 0.30% Mn, 0.003% S, 5.00% Cr, 1.35% Mo, 0.45% V
0.35% C, 0.30% Si, 0.30% Mn, 0.003% S, 5.00% Cr, 1.75% Mo, 0.80% V, + additions
0.35% C, 0.30% Si, 0.40% Mn, 0.010% P, 0.003% S, 5.00% Cr, 1.35% Mo, 0.50% V
0.35% C, 0.30% Si, 0.40% Mn, 0.010% P, 0.003% S, 5.00% Cr, 1.35% Mo, 0.50% V
0.35% C, 0.30% Si, 3.00% Cr, 1.80% Mo, 0.70% V, 2.20% W, 2.20% Co
0.35% C, 0.30% Si, 5.00% Cr, 1.30% Mo, 0.45% V
0.35% C, 0.30% Si, 5.00% Cr, 1.30% Mo, 0.45% V
0.35% C, 0.35% Si, 0.40% Mn, 4.80% Cr, 2.90% Mo, 0.60% V, 2.75% Co
0.35% C, 0.35% Si, 0.40% Mn, 4.80% Cr, 2.90% Mo, 0.60% V, 2.75% Co
0.35% C, 0.35% Si, 0.50% Mn, 0.0040% P, 0.006% S, 13.00% Cr, 0.50% Mo
0.35% C, 0.35% Si, 0.50% Mn, 0.025% P, 0.003% S, 2.70% Cr, 1.00% Mo, 0.60% Ni, 0.20% V, + others
0.35% C, 0.35% Si, 0.70% Mn, 15.50% Cr, 1.00% Mo, 0.50% Ni
0.35% C, 0.35% Si, 0.70% Mn, 15.50% Cr, 1.00% Mo, 0.50% Ni
0.35% C, 0.35% Si, 1.40% Mn, 0.30% P, 0.018% S, 2.00% Cr, 0.20% Mo, 0.00% V
0.35% C, 0.40% Si, 0.30% Mn, 13.00% Cr
0.35% C, 0.40% Si, 0.65% Mn, 0.10% Mo, 0.40% Ni, (Cr+Mo+Ni) = 0.63
0.35% C, 0.40% Si, 1.00% Al, 1.70% Cr, 0.20% Mo, 1.00% Ni
0.35% C, 0.50% Si, 0.50% Mn, 5.00% Cr, 2.20% Mo, 0.55% V
0.35% C, 0.50% Si, 1.20% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.08% Mo, 0.30% Ni, 0.020% Al, 0.012% N
0.35% C, 0.50% Si, 1.20% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.08% Mo, 0.30% Ni, 0.020% Al, 0.012% N
0.35% C, 0.80% Si, 0.70% Mn, 13.30% Cr, 0.20% Mo, 0.40% Ni, + others
0.35% C, 0.80% Si, 5.00% Cr, 1.00% Mo, 0.85% V
0.35% C, 0.80% Si, 5.00% Cr, 1.00% Mo, 0.85% V
0.35% C, 0.85% Cr, 1.20% Ni
0.35% C, 1.00% Cr, 0.20% Mo
0.35% C, 1.00% Si, 0.30% Mn, 3.30% Cr, 2.45% Mo, 0.65% V, 2.00% Co
0.35% C, 1.00% Si, 0.30% Mn, 3.30% Cr, 2.45% Mo, 0.65% V, 2.00% Co
0.35% C, 1.00% Si, 0.30% Mn, 3.30% Cr, 2.45% Mo, 0.65% V, 2.00% Co
0.35% C, 1.00% Si, 0.30% Mn, 3.30% Cr, 2.45% Mo, 0.65% V, 2.00% Co
0.35% C, 1.00% Si, 0.30% Mn, 5.00% Cr, 1.40% Mo, 0.30% V, 1.30% W
0.35% C, 1.00% Si, 0.30% Mn, 5.00% Cr, 1.40% Mo, 0.30% V, 1.30% W
0.35% C, 1.00% Si, 0.50% Mn, 0.025% P, 0.003% S, 5.20% Cr, 1.50% Mo, 0.30% V, 1.30% W
0.35% C, 1.70% Cr, 0.30% Mo, 3.80% Ni
0.35% C, 1.70% Cr, 0.30% Mo, 3.80% Ni
0.35% C, 3.00% Cr, 1.00% Mo, 0.25% V
0.35% C, 5.00% Cr, 1.30% Mo, 0.40% V
0.35% C, 5.00% Cr, 1.50% Mo, 1.00% V
0.35-0.30% C, 0.30% Ni, 12-12.50% Cr,0.50% Mo, +other elements
0.35-0.40% C, 0.10-0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.85-1.15% Cr
0.35-0.40% C, 0.30-0.50% Si, 0.30-0.50% Mn, 0.030% P, 0.020% S, 4.80-5.20% Cr, 2.70-3.20% Mo, 0.40-0.60% V
0.35-0.40% C, 0.30-0.50% Si, 0.30-0.50% Mn, 0.030% P, 0.020% S, 4.80-5.20% Cr, 2.70-3.20% Mo, 0.40-0.60% V
0.35-0.40% C, 0.30-1.00% Si, 0.30-1.0% Mn, 0.003% S, 0.015% P, 2.80-3.50% Cr, 2.00-2.40% Mo, 0.30-1.00% V
0.35-0.40% C, 0.30-1.00% Si, 0.30-1.00% Mn, 2.80-3.50% Cr, 2.00-2.40% Mo, 0.30-1.00% V
0.35-0.40% C, 0.80-1.10% Si, 0.30-0.50% Mn, 0.015% P, 0.003% S, 4.80-5.50% Cr, 1.20-1.50% Mo, 0.80-1.00% V
0.35-0.40% C, 0.80-1.10% Si, 0.30-0.50% Mn, 0.015% P, 0.003% S, 4.80-5.50% Cr, 1.20-1.50% Mo, 0.80-1.00% V
0.35-0.40% C, 0.80-1.10% Si, 0.30-0.50% Mn, 0.015% P, 0.003% S, 4.80-5.50% Cr, 1.20-1.50% Mo, 0.80-1.00% V
0.35-0.40% C, 0.80-1.10% Si, 0.30-0.50% Mn, 0.015% P, 0.003% S, 5.00-5.50% Cr, 1.20-1.50% Mo, 0.30-0.50% V
0.35-0.40% C, 0.80-1.10% Si, 0.30-0.50% Mn, 0.015% P, 0.003% S, 5.00-5.50% Cr, 1.20-1.50% Mo, 0.30-0.50% V
0.35-0.40% C, 0.80-1.10% Si, 0.30-0.50% Mn, 0.015% P, 0.003% S, 5.00-5.50% Cr, 1.20-1.50% Mo, 0.30-0.50% V
0.35-0.40% C, 0.80-1.10% Si, 0.30-0.50% Mn, 0.015% P, 0.003% S, 4.80-5.50% Cr, 1.20-1.50% Mo, 0.80-1.00% V
0.35-0.40% C, 0.80-1.10% Si, 0.30-0.50% Mn, 0.015% P, 0.003% S, 5.00-5.50% Cr, 1.20-1.50% Mo, 0.30-0.50% V
0.35-0.40% C, 0.80-1.10% Si, 0.30-0.50% Mn, 0.015% P, 0.003% S, 5.00-5.50% Cr, 1.20-1.50% Mo, 0.30-0.50% V
0.35-0.40% C, 0.80-1.10% Si, 0.30-0.50% Mn, 4.80-5.50% Cr, 1.10-1.50% Mo, 0.30-0.50% V
0.35-0.40% C, 0.80-1.10% Si, 0.30-0.50% Mn, 4.80-5.50% Cr, 1.20-1.50% Mo, 0.80-1.00% V
0.35-0.40% C, 0.80-1.10% Si, 0.30-0.50% Mn, 4.80-5.50% Cr, 1.20-1.50% Mo, 0.80-1.00% V
0.35-0.40% C, 0.80-1.10% Si, 0.30-0.50% Mn, 5.00-5.50% Cr, 1.20-1.50% Mo, 0.30-0.50% V
0.35-0.40% C, 1.00% Si, 1.00% Mn, 0.040% P, 0.030% S, 14.00-15.00% Cr, 0.40-0.60% Mo, 0.10-0.15% V
0.35-0.42% C, 0.30-0.50% Si, 0.30-0.50% Mn, 0.030% P, 0.020% S, 4.80-5.20% Cr, 2.70-3.20% Mo, 0.40-0.60% V
0.35-0.42% C, 0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S, 0.40-0.60% Cr
0.35-0.42% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.020-0.040% S, 0.40-0.60% Cr
0.35-0.42% C, 0.80-1.20% Si, 0.25-0.50% Mn, 0.025% P, 0.005% S, 4.80-5.50% Cr, 1.20-1.50% Mo, 0.85-1.15% V
0.35-0.42% C, 0.80-1.20% Si, 0.25-0.50% Mn, 0.025% P, 0.005% S, 4.80-5.50% Cr, 1.20-1.50% Mo, 0.85-1.15% V
0.35-0.42% C, 0.80-1.20% Si, 0.25-0.50% Mn, 0.025% P, 0.005% S, 4.80-5.50% Cr, 1.20-1.50% Mo, 0.85-1.15% V
0.35-0.42% C, 0.80-1.20% Si, 0.25-0.50% Mn, 0.030% P, 0.020% S, 4.80-5.50% Cr, 1.20-1.50% Mo, 0.85-1.15% V
0.35-0.42% C, 0.80-1.20% Si, 0.25-0.50% Mn, 0.030% P, 0.020% S, 4.80-5.50% Cr, 1.20-1.50% Mo, 0.85-1.15% V
0.35-0.42% C, 0.80-1.20% Si, 0.25-0.50% Mn, 0.030% P, 0.020% S, 4.80-5.50% Cr, 1.20-1.50% Mo, 0.85-1.15% V
0.35-0.42% C, 1.30-1.60% Si, 0.30-0.50% Mn, 0.035% P, 0.035% S, 1.30-1.60% Cr, 0.07-0.12% V
0.35-0.42% C, 1.50-1.80% Si, 0.50-0.80% Mn, 0.025% P, 0.025% S
0.35-0.43% C, 0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S, 0.60-1.00% Cr, 0.15-0.25% Mo, 0.70-1.00% Ni
0.35-0.43% C, 0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S, 0.60-1.00% Cr, 0.15-0.25% Mo, 0.70-1.00% Ni
0.35-0.43% C, 0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S, 0.60-1.00% Cr, 0.15-0.25% Mo, 0.70-1.00% Ni
0.35-0.43% C, 0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S, 0.60-1.00% Cr, 0.15-0.25% Mo, 0.70-1.00% Ni
0.35-0.45% C, 0.10-0.40% Si, 0.20-0.55% Mn, 0.030% P, 0.025% S, 1.40-1.70% Cr, 0.35-0.60% Mo, 4.30-4.90% Ni
0.35-0.45% C, 0.10-0.40% Si, 0.35-0.75% Mn, 0.030% P, 0.030% S, 1.60-2.00% Cr, 0.40-0.60% Mo, 3.40-4.10% Ni, 0.05-0.20% V
0.35-0.45% C, 0.15-0.30% Si, 0.20-0.50% Mn, 0.030% P, 0.020% S, 4.00-4.70% Cr, 0.30-0.50% Mo, 3.80-4.50% W, 1.70-2.10% V, 4.0-4.50% Co
0.35-0.45% C, 0.20-0.40% Si, 0.20-0.40% Mn, 0.025% P, 0.005% S, 1.80-2.10% Cr, 0.15-0.25% Mo
0.35-0.45% C, 0.20-0.40% Si, 1.30-1.60% Mn, 0.025% P, 0.005% S, 1.80-2.10% Cr, 0.15-0.25% Mo, 1.00-1.20% V
0.35-0.45% C, 0.20-0.40% Si, 1.30-1.60% Mn, 0.025% P, 0.002% S, 1.80-2.10% Cr, 0.15-0.25% Mo, 0.90-1.10% Ni
0.35-0.45% C, 0.20-0.40% Si, 1.30-1.60% Mn, 0.025% P, 0.002% S, 1.80-2.10% Cr, 0.15-0.25% Mo
0.35-0.45% C, 0.20-0.40% Si, 1.30-1.60% Mn, 0.025% P, 0.002% S, 1.80-2.10% Cr, 0.15-0.25% Mo
0.35-0.45% C, 0.20-0.40% Si, 1.30-1.60% Mn, 0.025% P, 0.005% S, 1.80-2.10% Cr, 0.15-0.25% Mo, 1.00-1.20% Ni
0.35-0.45% C, 0.20-0.40% Si, 1.30-1.60% Mn, 0.025% P, 0.005% S, 1.80-2.10% Cr, 0.15-0.25% Mo
0.35-0.45% C, 0.20-0.40% Si, 1.30-1.60% Mn, 0.030% P, 0.030% S, 1.80-2.10% Cr, 0.15-0.25% Mo, 0.90-1.20% Ni
0.35-0.45% C, 0.20-0.40% Si, 1.30-1.60% Mn, 0.035% P, 0.035% S, 1.80-2.10% Cr, 0.15-0.25% Mo, 0.90-1.20% Ni
0.35-0.45% C, 0.20-0.40% Si, 1.30-1.60% Mn, 0.035% P, 0.035% S, 1.80-2.10% Cr, 0.15-0.25% Mo
0.35-0.45% C, 0.20-0.40% Si, 1.30-1.60% Mn, 0.035% P, 0.035% S, 1.80-2.10% Cr, 0.15-0.25% Mo
0.35-0.45% C, 0.20-0.40% Si, 1.30-1.60% Mn, 0.035% P, 0.035% S, 1.80-2.10% Cr, 0.15-1.25% Mo, 0.90-1.20% V
0.35-0.45% C, 0.20-0.40% Si, 1.30-1.60% Mn, 0.05-0.10% S, 1.80-2.10% Cr, 0.15-0.30% Mo
0.35-0.45% C, 0.20-0.40% Si, 1.30-1.60% Mn, 1.80-2.10% Cr, 0.15-0.25% Mo
0.35-0.45% C, 0.20-0.40% Si, 1.30-1.60% Mn, 1.80-2.10% Cr, 0.15-0.25% Mo
0.35-0.45% C, 0.20-0.40% Si, 1.30-1.60% Mn, 1.80-2.10% Cr, 0.15-0.30% Mo
0.35-0.45% C, 0.20-0.40% Si, 1.40-1.70% Mn, 1.80-2.20% Cr, 0.15-0.30% Mo, 0.90-1.30% Ni
0.35-0.45% C, 0.30-0.50% Si, 1.40-1.60% Mn, 0.030% P, 0.05-0.10% S, 1.80-2.00% Cr, 0.15-0.25% Mo
0.35-0.45% C, 0.30-0.50% Si, 1.40-1.60% Mn, 0.030% P, 0.05-0.10% S, 1.80-2.10% Cr, 0.15-0.25% Mo
0.35-0.45% C, 0.30-0.50% Si, 1.40-1.60% Mn, 0.030% P, 0.05-0.10% S, 1.80-2.20% Cr, 0.15-0.25% Mo
0.35-0.45% C, 0.30-0.50% Si, 1.40-1.60% Mn, 0.030% P, 0.05-0.100% S, 1.80-2.00% Cr, 0.15-0.25% Mo
0.35-0.45% C, 0.30-0.50% Si, 1.40-1.60% Mn, 0.030% P, 0.050-0.10% S, 1.80-2.00% Cr, 0.15-0.25% Mo
0.35-0.45% C, 0.30-0.50% Si, 1.40-1.60% Mn, 0.030% P, 0.050-0.100% S, 1.80-2.00% Cr, 0.15-0.25% Mo
0.35-0.45% C, 0.30-0.50% Si, 1.40-1.60% Mn, 0.05-0.10% S, 1.80-2.00% Cr, 0.15-0.25% Mo
0.35-0.45% C, 1.00% Si, 1.0% Mn, 12.50-13.50% Cr, 0.50% V
0.35-0.45% C, 1.30-1.50% Si, 0.20-0.60% Mn, 0.035% P, 0.035% S, 1.80-2.10% Cr, 0.15-0.25% Mo
0.35% C, 0.26% Si, 0.50% Mn, 0.010% P, 0.020% S, 0.49% Cr, 1.54% Ni
0.35% C, 0.30% Si, 3.00% Cr, 1.80% Mo, 0.70% V, 2.20% W, 2.20% Co
0.35-0.42% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.030% S, 0.40-0.60% Cr
0.35-0.42% C, 0.80-1.20% Si, 0.25-0.50% Mn, 0.03% P, 0.02% S, 4.80-5.50% Cr, 1.20-1.50% Mo, 0.85-1.15% V
0.35-0.45% C, 0.10-0.40% Si, 0.20-0.55% Mn, 0.030% P, 0.025% S, 1.40-1.70% Cr, 0.35-0.60% Mo, 4.30-4.90% Ni
0.36% C, 0.20% Si, 0.30% Mn, 5.00% Cr, 1.35% Mo, 0.45% V
0.36% C, 0.20% Si, 0.30% Mn, 5.00% Cr, 1.35% Mo, 0.45% V
0.36% C, 0.22% Si, 0.75% Mn, 0.01% P, 0.01% S, 1.55% Cr, 0.25% Mo
0.36% C, 0.23% Si, 0.80% Mn, 0.026% P, 0.013% S, 15.59% Cr, 1.04% Mo, 0.84% Ni, 0.050% Cu
0.36% C, 0.25% Si, 0.35% Mn, 5.00% Cr, 1.50% Ni, 1.75% Mo, 0.65% V
0.36% C, 0.25% Si, 0.35% Mn, 5.00% Cr, 1.75% Mo, 1.50% Ni, 0.65% V
0.36% C, 0.25% Si, 0.40% Mn, 5.20% Cr, 1.90% Mo, 0.55% V
0.36% C, 0.25% Si, 0.40% Mn, 5.20% Cr, 1.90% Mo, 0.55% V
0.36% C, 0.25% Si, 0.40% Mn, 5.20% Cr, 1.90% Mo, 0.55% V
0.36% C, 0.25% Si, 0.40% Mn, 5.20% Cr, 1.90% Mo, 0.55% V
0.36% C, 0.25% Si, 0.65% Mn, 1.05% Cr, 0.20% Mo, 1.05% Ni, + Pb
0.36% C, 0.25% Si, 0.70% Mn, 1.40% Cr, 0.20% Mo, 1.40% Ni
0.36% C, 0.25% Si, 1.25% Mn, + Pb
0.36% C, 0.30% Si, 0.30% Mn, 18.20% Cr, 1.10% Mo, 1.55% Ni, 3.50% V
0.36% C, 0.30% Si, 0.30% Mn, 18.20% Cr, 1.10% Mo, 3.50% V, 1.55% N
0.36% C, 0.30% Si, 0.30% Mn, 5.00% Cr, 1.30% Mo, 0.50% V, 0.00% W
0.36% C, 0.30% Si, 0.30% Mn, 5.00% Cr, 1.30% Mo, 0.45% V
0.36% C, 0.30% Si, 0.30% Mn, 5.00% Cr, 1.30% Mo, 0.50% V
0.36% C, 0.30% Si, 0.40% Mn, 0.012% P, 0.003% S, 5.20% Cr, 1.90% Mo, 0.55% V
0.36% C, 0.30% Si, 0.40% Mn, 0.012% P, 0.003% S, 5.20% Cr, 1.90% Mo, 0.55% V
0.36% C, 0.30% Si, 0.40% Mn, 5.20% Cr, 1.90% Mo, 0.55% V
0.36% C, 0.30% Si, 0.50% Mn, 0.005% S, 4.90% Cr, 1.94% Mo, 1.51% Ni, 0.66% V
0.36% C, 0.30% Si, 0.55% Mn, 1.70% Cr, 0.20% Mo, 1.00% Ni, 0.95% Al
0.36% C, 0.30% Si, 1.50% Mn, 0.020% P, 0.003% S, 2.00% Cr, 0.20% Mo, 1.00% Ni
0.36% C, 0.30% Si, 1.50% Mn, 0.020% P, 0.003% S, 2.00% Cr, 0.20% Mo, 1.00% Ni
0.36% C, 0.30% Si, 1.50% Mn, 1.80% Cr, 0.20% Mo, 1.10% Ni
0.36% C, 0.30% Si, 5.0% Cr, 1.4% Mo, 0.40% V
0.36% C, 0.30% Si, 5.00% Cr, 1.40% Mo, 0.40% V
0.36% C, 0.35% Si, 0.35% Mn, 5.10% Cr, 2.80% Mo, 0.55% V
0.36% C, 0.40% Si, 0.45% Mn, 0.020% P, 0.003% S, 5.00% Cr, 3.00% Mo, 0.65% V
0.36% C, 0.40% Si, 0.45% Mn, 0.030% P, 0.020% S, 13.50% Cr, 1.00% Mo
0.36% C, 0.50% Si, 0.50% Mn, 1.50% Cr, 0.50% Mo, 1.20% Ni, 0.75% Cu
0.36% C, 0.90% Mn, 1.90% Cr, 0.50% Mo, 0.50% Ni, + additions
0.36% C, 0.90% Si, 0.60% Mn, 5.00% Cr, 2.85% Mo, 0.25% V
0.36% C, 1.00% Si, 0.35% Mn, 5.00% Cr, 1.20% Mo, 0.40% V
0.36% C, 1.00% Si, 0.35% Mn, 5.00% Cr, 1.20% Mo, 0.40% V
0.36% C, 1.00% Si, 0.40% Mn, 5.20% Cr, 1.40% Mo, 0.30% V, 1.40% W
0.36% C, 1.00% Si, 0.40% Mn, 5.20% Cr, 1.40% Mo, 0.30% V, 1.40% W
0.36% C, 1.00% Si, 0.40% Mn, 5.20% Cr, 1.40% Mo, 0.30% V, 1.40% W
0.36% C, 1.60% Mn, 1.80% Cr, 0.20% Mo, 0.70% Ni
0.36% C, 1.60% Mn, 1.80% Cr, 0.20% Mo, 0.80% Ni
0.36% C, 16.00% Cr, 1.20% Mn
0.36% C, 16.00% Cr, 1.20% Mn
0.36% C, 16.00% Cr, 1.20% Mo
0.36% C, 16.00% Cr, 1.20% Mo
0.36% C, 16.00% Cr, 1.20% Mo
0.36-0.42% C, 0.30-0.50% Si, 0.50-0.80% Mn, 0.030% P, 0.030% S, 4.80-5.50% Cr, 1.10-1.40% Mo, 0.25-0.50% V
0.36-0.42% C, 0.80-1.20% Si, 0.30-0.50% Mn, 0.015% P, 0.002% S, 4.80-5.50% Cr, 1.10-1.40% Mo, 0.30-0.50% V
0.36-0.42% C, 0.90-1.20% Si, 0.30-0.50% Mn, 0.03% P, 0.03% S, 4.80-5.50% Cr, 1.10-1.40% Mo, 0.25-0.50% V
0.36-0.42% C, 0.90-1.20% Si, 0.30-0.50% Mn, 0.030% P, 0.030% S, 4.80-5.80% Cr, 1.10-1.40% Mo, 0.25-0.50% V
0.36-0.42% C, 0.90-1.20% Si, 0.30-0.50% Mn, 4.80-5.50% Cr, 1.10-1.40% Mo, 0.25-0.50% V
0.36-0.42% C, 1.0% Si, nax. 1.0% Mn, 0.025% P, 0.005% S, 12.50-14.50% Cr
0.36-0.42% C, 1.00% Si, 1.00% Mn, 0.025% P, 0.005% S, 12.50-14.50% Cr
0.36-0.42% C, 1.00% Si, 1.00% Mn, 0.030% P, 0.020% S, 12.50-14.50% Cr
0.36-0.42% C, 1.00% Si, 1.00% Mn, 0.030% P, 0.030% S, 12.50-14.50% Cr
0.36-0.42% C, 1.00% Si, 1.00% Mn, 0.030% P, 0.030% S, 12.50-14.50% Cr
0.36-0.42% C, 1.00% Si, 1.00% Mn, 0.030% P, 0.030% S, 12.50-14.50% Cr
0.36-0.42% C, 1.00% Si, 1.00% Mn, 0.030% P, 0.030% S, 12.50-14.50% Cr
0.36-0.42% C, 1.00% Si, 1.00% Mn, 0.040% P, 0.015% S, 12.50-14.50% Cr
0.36-0.42% C, 1.00% Si, 1.00% Mn, 0.040% P, 0.030% S, 12.50-14.50% Cr
0.36-0.42% C, 1.00% Si, 1.00% Mn, 0.040% P, 0.030% S, 12.50-14.50% Cr
0.36-0.44% C, 0.25-0.50% Si, 0.80-1.10% Mn, 0.035% P, 0.035% S
0.36-0.44% C, 0.40% Si, 0.45-0.85% C, 0.040% P, 0.040% S, 0.90-1.20% Cr, 0.50-0.65% Mo, 0.25-0.35% V, 0.015% Al
0.36-0.44% C, 0.40% Si, 0.45-0.85% Mn, 0.030% P, 0.030% S, 0.90-1.20% Cr, 0.50-0.65% Mo, 0.25-0.35% V, 0.015% Al
0.37% C, 0.20% Si, 0.30% Mn, 5.00% Cr, 1.30% Mo, 0.05% V
0.37% C, 0.30% Si, 1.40% Mn, 0.010% S, 2.00% Cr, 1.00% Ni, 0.20% Mo,
0.37% C, 0.30% Si, 1.40% Mn, 0.010% S, 2.00% Cr, 1.00% Ni, 0.20% Mo
0.37% C, 0.30% Si, 1.40% Mn, 2.00% Cr, 0.20% Mo, 1.00% Ni, 0.010% S
0.37% C, 0.35% Si, 1.93% Mn, 1.60% Cr, 0.43% Mo, 0.12% V
0.37% C, 0.40% Si, 0.003% S, 5.00% Cr, 3.00% Mo, 0.60% V
0.37% C, 0.42% Si, 0.45% Mn, 4.90% Cr, 2.90% Mo, 0.61% V
0.37% C, 0.42% Si, 0.45% Mn, 4.90% Cr, 2.90% Mo, 0.616% V
0.37% C, 0.60% Si, 16.00% Cr, 0.50% Ni, 1.90% Mo, 0.25% N, +additions
0.37% C, 0.90% Si, 0.50% Mn, 13.60% Cr, 0.30% V
0.37% C, 0.90% Si, 0.50% Mn, 13.60% Cr, 0.30% V
0.37% C, 1.00% Si, 0.30% Mn, 5.00% Cr, 1.30% Mo, 1.00% V
0.37% C, 1.00% Si, 0.35% Mn, 5.00% Cr, 1.25% Mo, 1.00% V
0.37% C, 1.00% Si, 0.40% Mn, 5.00% Cr, 1.30% Mo, 0.40% V
0.37% C, 1.00% Si, 0.40% Mn, 5.30% Cr, 1.35% Mo, 0.28% V
0.37% C, 1.00% Si, 0.40% Mn, 5.30% Cr, 1.35% Mo, 0.38% V
0.37% C, 1.00% Si, 5.30% Cr, 1.30% Mo, 0.40% V
0.37% C, 1.00% Si, 5.30% Cr, 1.30% Mo, 0.40% V
0.37% C, 1.25% Si, 1.25% Mn, +Pb
0.37% C, 1.80% Cr, 0.30% Mo, 3.70% Ni
0.37% C, 5.00% Cr, 3.00% Mo, 0.60% V
0.37% C, 5.00% Cr, 3.00% Mo, 0.60% V
0.37% C, 5.00% Cr, 3.00% Mo, 0.60% V
0.37-0.42% C, 0.85-1.20% Si, 0.20-0.50% Mn, 5.00-5.50% Cr, 1.20-1.70% Mo, 0.85-1.20% V
0.37-0.42% C, 0.90-1.20% Si, 0.30-0.50% Mn, 0.030% P, 0.080-0.120% S, 5.00-5.50% Cr, 1.20-1.15% Mo, 0.90-1.10% V
0.37-0.43% C, 0.90-1.20% Si, 0.90-1.20% Mn, 4.80-5.50% Cr, 1.20-1.50% Mo, 0.90-1.10% V
0.37-0.44% C, 0.10-0.35% Si, 0.55-0.90% Mn, 0.040% P, 0.040% S, 0.65-0.95% Cr, 0.20-0.35% Mo, 1.55-2.00% Ni
0.37-0.44% C, 0.10-0.35% Si, 0.55-0.90% Mn, 0.040% P, 0.040% S, 0.65-0.95% Cr, 0.20-0.35% Mo, 1.55-2.00% Ni
0.37-0.44% C, 0.10-0.35% Si, 0.65-1.10% Mn, 0.040% P, 0.040% S, 0.75-1.20% Cr, 0.15-0.30% Mo
0.37-0.44% C, 0.10-0.35% Si, 0.65-1.10% Mn, 0.040% P, 0.045% S, 0.75-1.20% Cr, 0.15-0.30% Mo
0.37-0.44% C, 0.14-0.35% Si, 0.75-1.00% Mn, 0.040% P, 0.040% S, 0.75-1.20% Cr, 0.15-0.25% Mo
0.37-0.44% C, 0.15-0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 0.60-0.90% Cr, 0.20-0.30% Mo, 1.60-1.90% Ni
0.37-0.44% C, 0.15-0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 0.60-0.90% Cr, 0.20-0.30% Mo, 1.60-1.90% Ni
0.37-0.44% C, 0.15-0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 0.60-0.90% Cr, 0.20-0.30% Mo, 1.60-1.90% Ni
0.37-0.44% C, 0.15-0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S
0.37-0.44% C, 0.15-0.40% Si, 0.70-1.00% Mn, 0.035% P, 0.035% S, 0.40-0.60% Cr, 0.15-0.30% Mo, 0.40-0.70% Ni
0.37-0.44% C, 0.25-0.35% Si, 0.70-0.90% Mn, 0.020% P, 0.015% S, 0.70-0.95% Cr, 0.30-0.40% Mo, 1.65-2.00% Ni, 0.005-0.050% Al
0.37-0.44% C, 0.40% Si, 0.50-0.80% Mn, 0.030% P, 0.035% S, 0.40% Cr, 0.40% Ni
0.37-0.44% C, 0.40% Si, 0.50-0.80% Mn, 0.030% P, 0.035% S, 0.40% Cr, 0.40% Ni
0.37-0.44% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.020-0.040% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.37-0.44% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.37-0.44% C, 0.40% Si, 0.50-0.80% Mn, 0.045% P, 0.045% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.37-0.45% Mn, 0.60% Si, 0.60% Mn, 15.00-16.50% Cr, 1.50-1.90% Mo, 0.30% Ni, 0.20-0.40% V, 0.16-0.25% N
0.37-0.45% Mn, 0.60% Si, 0.60% Mn, 15.00-16.50% Cr, 1.50-1.90% Mo, 0.30% Ni, 0.20-0.40% V, 0.16-0.26% N
0.37% C, 1.25% Si, 1.25% Mn
0.38% C+N, 0.40% Si, 0.45% Mn, 13.60% Cr, 0.30% V
0.38% C, 0.20% Si, 0.25% Mn, 5.00% Cr, 2.80% Mo, 0.65% V
0.38% C, 0.20% Si, 0.25% Mn, 5.00% Cr, 2.80% Mo, 0.65% V
0.38% C, 0.20% Si, 0.30% Mn, 5.00% Cr, 1.30% Mo, 0.50% V
0.38% C, 0.20% Si, 0.55% Mn, 5.00% Cr, 1.75% Mo, 0.55% V, +N
0.38% C, 0.20% Si, 0.55% Mn, 5.00% Cr, 1.75% Mo, 0.55% V, N
0.38% C, 0.30% Si, 0.35% Mn, 14.00% Cr, 0.80% Mo
0.38% C, 0.30% Si, 0.75% Mn, 2.60% Cr, 2.25% Mo, 0.90% V
0.38% C, 0.30% Si, 0.75% Mn, 2.60% Cr, 2.25% Mo, 0.90% V
0.38% C, 0.30% Si, 1.50% Mn, 0.020% P, 0.003% S, 2.00% Cr, 0.20% Mo, 1.00% Ni
0.38% C, 0.30% Si, 1.50% Mn, 0.020% P, 0.003% S, 2.00% Cr, 0.20% Mo
0.38% C, 0.30% Si, 1.50% Mn, 0.020% P, 0.003% S, 2.00% Cr, 0.20% Mo
0.38% C, 0.30% Si, 1.50% Mn, 0.020% P, 0.003% S, 2.00% Cr, 0.20% Mo
0.38% C, 0.30% Si, 1.50% Mn, 0.020% P, 0.07% S, 2.00% Cr, 0.20% Mo
0.38% C, 0.30% Si, 1.50% Mn, 0.020% P, 0.070% S, 2.00% Cr, 0.20% Mo
0.38% C, 0.30% Si, 1.50% Mn, 1.90% Cr, 0.20% Mo
0.38% C, 0.30% Si, 1.50% Mn, 2.00% Cr, 0.20% Mo, 1.10% Ni
0.38% C, 0.30% Si, 1.50% Mn, 2.00% Cr, 0.20% Mo, 1.10% Ni
0.38% C, 0.30% Si, 1.50% Mn, 2.00% Cr, 0.20% Mo, 1.10% Ni
0.38% C, 0.40% Si, 0.25% Mn, 16.00% Cr, 0.80% Ni, 1.00% Mo
0.38% C, 0.40% Si, 0.40% Mn, 5.00% Cr, 2.80% Mo, 0.60% V
0.38% C, 0.40% Si, 0.40% Mn, 5.00% Cr, 2.80% Mo, 0.60% V
0.38% C, 0.40% Si, 0.40% Mn, 5.00% Cr, 2.80% Mo, 0.55% V
0.38% C, 0.40% Si, 0.40% Mn, 5.00% Cr, 2.80% Mo, 0.55% V
0.38% C, 0.40% Si, 0.40% Mn, 5.00% Cr, 2.80% Mo, 0.60% V
0.38% C, 0.40% Si, 0.45% Mn, 13.60% Cr, 0.30% V
0.38% C, 0.40% Si, 0.45% Mn, 13.60% Cr, 0.30% V
0.38% C, 0.40% Si, 0.45% Mn, 5.00% Cr, 3.00% Mo, 0.55% V
0.38% C, 0.40% Si, 0.45% Mn, 5.00% Cr, 3.00% Mo, 0.55% V
0.38% C, 0.40% Si, 0.65% Mn, 0.50% Cr
0.38% C, 0.40% Si, 0.65% Mn, 16.00% Cr, 1.00% Mo, 0.80% Ni
0.38% C, 0.40% Si, 0.75% Mn, 1.05% Cr
0.38% C, 0.40% Si, 5.00% Cr, 3.00% Mo, 0.50% V
0.38% C, 0.50% Si, 0.30% Mn, 5.00% Cr, 1.70% Mo, 0.45% V
0.38% C, 0.70% Si, 0.45% Mn, 14.25% Cr, 0.20% V
0.38% C, 0.70% Si, 0.45% Mn, 14.30% Cr, 0.20% V
0.38% C, 0.75% Si, 0.50% Mn, 13.60% Cr, 0.30% V
0.38% C, 0.80% Si, 0.40% Mn, 0.020% P, 0.003% S, 5.00% Cr, 1.40% Mo, 1.00% V
0.38% C, 0.80% Si, 0.40% Mn, 0.020% P, 0.030% S, 5.00% Cr, 1.30% Mo, 0.40% V
0.38% C, 0.80% Si, 0.50% Mn, 13.60% Cr, 0.30% V
0.38% C, 0.90% Si, 0.50% Mn, 13.60% Cr, 0.30% V, 0.00% W
0.38% C, 0.90% Si, 0.50% Mn, 13.60% Cr, 0.30% V
0.38% C, 0.90% Si, 0.50% Mn, 13.60% Cr, 0.30% V
0.38% C, 0.90% Si, 0.50% Mn, 13.60% Cr, 0.30% V
0.38% C, 0.90% Si, 0.50% Mn, 13.60% Cr, 0.30% V
0.38% C, 0.90% Si, 0.50% Mn, 13.60% Cr, 0.30% V
0.38% C, 0.90% Si, 0.50% Mn, 13.60% Cr, 0.30% V
0.38% C, 1.00% Si, 0.30% Mn, 3.50% Cr, 2.55% Mo, 0.75% V, 3.00% Co
0.38% C, 1.00% Si, 0.30% Mn, 3.50% Cr, 2.55% Mo, 0.75% V, 3.00% Co
0.38% C, 1.00% Si, 0.40% Mn, 5.00% Cr, 1.30% Mo, 0.40% V, 0.00% W
0.38% C, 1.00% Si, 0.40% Mn, 5.00% Cr, 1.30% Mo, 0.40% V
0.38% C, 1.00% Si, 0.40% Mn, 5.00% Cr, 1.30% Mo, 0.40% V
0.38% C, 1.00% Si, 0.40% Mn, 5.00% Cr, 1.30% Mo, 0.40% V
0.38% C, 1.00% Si, 0.40% Mn, 5.20% Cr, 1.30% Mo, 0.40% V
0.38% C, 1.00% Si, 0.40% Mn, 5.20% Cr, 1.30% Mo, 0.40% V
0.38% C, 1.00% Si, 0.40% Mn, 5.20% Cr, 1.30% Mo, 0.40% V
0.38% C, 1.00% Si, 0.40% Mn, 5.20% Cr, 1.30% Mo, 0.40% V
0.38% C, 1.00% Si, 0.40% Mn, 5.30% Cr, 1.20% Mo, 0.40% V
0.38% C, 1.00% Si, 0.50% Mn, 13.00% Cr, 0.25% V
0.38% C, 1.00% Si, 1.00% Mn, 13.00% Cr
0.38% C, 1.00% Si, 5.30% Cr, 1.30% Mo, 0.40% V
0.38% C, 1.00% Si, 5.30% Cr, 1.30% Mo, 0.40% V
0.38% C, 1.00% Si, 5.30% Cr, 1.30% Mo, 0.40% V
0.38% C, 1.00% Si, 5.30% Cr, 1.40% Mo, 0.40% V
0.38% C, 1.05% Si, 0.40% Mn, 0.025% P, 0.003% S, 5.20% Cr, 1.30% Mo, 0.40% V
0.38% C, 1.05% Si, 0.40% Mn, 0.025% P, 0.003% S, 5.20% Cr, 1.30% Mo, 0.30% V
0.38% C, 1.10% Si, 0.40% Mn, 5.00% Cr, 1.30% Mo, 0.40% V
0.38% C, 1.10% Si, 0.40% Mn, 5.00% Cr, 1.30% Mo, 0.40% V
0.38% C, 16.50% Cr, 1.20% Mo
0.38% C, 16.50% Cr, 1.20% Mo
0.38% C, 5.00% Cr, 3.00% Mo, 0.50% V
0.38% C, 5.10% Cr, 1.35% Mo, 0.40% V
0.38% C, ~1.00% Si, ~0.35% Mn, ~5.00% Cr, ~1.30% Mo, ~0.40% V, patent pending
0.38-0.42% C, 1.65-1.68% Si, 1.40-1.55% Mn, 0.020% P, 0.004% S, 1.50-1.60% Cr, 0.43-0.47% Mo, 0.30% Ni, 9 ppm O, 30 ppm Ti
0.38-0.42% C, 1.65-1.68% Si, 1.40-1.55% Mn, 0.020% P, 0.010-0.020% S, 1.50-1.60% Cr, 0.43-0.47% Mo, 0.30% Ni, 11 ppm O, 30 ppm Ti
0.38-0.42% C, 1.65-1.80% Si, 1.40-1.55% Mn, 0.020% P, 0.012-0.020% S, 1.50-1.60% Cr, 0.43-0.47% Mo, 0.30% Ni
0.38-0.42% C, 1.65-1.80% Si, 1.40-1.55% Mn, 0.020% P, 0.012-0.020% S, 1.50-1.60% Cr, 0.43-0.47% Mo, 0.30% Ni
0.38-0.43% C, 0.14-0.35% Si, 0.75-1.00% Mn, 0.040% P, 0.040% S, 0.80-1.10% Cr, 0.15-0.25% Mo
0.38-0.43% C, 0.20-0.50% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 1.50-1.80% Cr, 0.25-0.40% Mo, 0.80-1.20% Al
0.38-0.43% C, 0.40% Si, 0.70-1.00% Mn, 0.015% P, 0.010% S, 0.90-1.10% Cr, 0.20-0.30% Mo, 0.30-0.60% Ni, 0.020-0.040% Al
0.38-0.44% C, 0.15-0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.38-0.44% C, 0.15-0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.38-0.44% C, 0.15-0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S, 0.90-1.20% Cr
0.38-0.45% C, 0.15-0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.25% Mo
0.38-0.45% C, 0.20-0.50% Si, 0.60-0.90% Mn, 0.90-1.20% Cr, 0.20-0.30% Mo
0.38-0.45% C, 0.40% Si, 0.40-0.70% Mn, 0.025% P, 0.035% S, 1.50-1.80% Cr, 0.20-0.35% Mo, 0.80-1.20% Al
0.38-0.45% C, 0.40% Si, 0.40-0.70% Mn, 0.025% P, 0.035% S, 1.50-1.80% Cr, 0.20-0.35% Mo, 0.80-1.20% Al
0.38-0.45% C, 0.40% Si, 0.40-0.70% Mn, 0.025% P, 0.035% S, 1.50-1.80% Cr, 0.20-0.35% Mo, 0.80-1.20% Al
0.38-0.45% C, 0.40% Si, 0.40-0.70% Mn, 0.025% S, 0.035% S, 1.50-1.80% Cr, 0.20-0.35% Mo, 0.80-1.20% Al
0.38-0.45% C, 0.40% Si, 0.60-0.80% Mn, 0.025% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.38-0.45% C, 0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.38-0.45% C, 0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.035% S, 0.90-1.20% Cr
0.38-0.45% C, 0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.035% S, 0.90-1.20% Cr
0.38-0.45% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.020-0.040% S, 0.90-1.20% Cr
0.38-0.45% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.020-0.040% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.38-0.45% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.38-0.45% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.38-0.45% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr
0.38-0.45% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr
0.38-0.48% C, 0.20-0.50% Si, 1.40-1.70% Mn, 1.90-2.30% Cr, 0.15-0.30% Mo, 0.30-0.60% Ni
0.38-0.48% C, 0.20-0.50% Si, 1.40-1.70% Mn, 1.90-2.30% Cr, 0.15-0.30% Mo, 0.30-0.60% Ni
0.38-0.45% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.020-0.030% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.38-0.45% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.030% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.38-0.45% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr
0.38-0.45% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr
0.39% C, 0.30% Si, 0.35% Mn, 2.90% Cr, 2.80% Mo, 0.65% V, 2.90% Co
0.39% C, 0.30% Si, 0.35% Mn, 2.90% Cr, 2.80% Mo, 2.90% Co
0.39% C, 0.35% Si, 1.50% Mn, 0.055% S, 1.87% Cr, 0.40% Ni, 0.18% Mo, + others
0.39% C, 0.90% Si, 0.40% Mn, 5.20% Cr, 1.40% Mo, 0.95% V
0.39% C, 0.97% Si, 0.43% Mn, 0.015% P, 0.006% S, 5.01% Cr, 1.14% Mo, 0.21% Ni, 0.35% V
0.39% C, 0.97% Si, 0.43% Mn, 0.015% P, O.006% S, 5.0% Cr, 1.14% Mo, 0.21% Ni, 0.35% V
0.39% C, 1.0% Si, 0.40% Mn, 0.030% P, 0.010% S, 5.15% Cr, 1.40% Mo, 0.80% V
0.39% C, 1.00% Si, 0.40% Mn, 5.20% Cr, 1.40% Mo, 0.90% V
0.39% C, 1.00% Si, 0.40% Mn, 5.20% Cr, 1.40% Mo, 0.90% V
0.39% C, 1.00% Si, 0.40% Mn, 5.20% Cr, 1.40% Mo, 0.90% V
0.39% C, 1.00% Si, 0.40% Mn, 5.20% Cr, 1.40% Mo, 0.90% V
0.39% C, 1.00% Si, 0.40% Mn, 5.30% Cr, 1.30% Mo, 0.90% V
0.39% C, 1.00% Si, 0.40% Mn, 5.30% Cr, 1.30% Mo, 0.90% V
0.39% C, 1.00% Si, 0.40% Mn, 5.30% Cr, 1.30% Mo, 0.90% V
0.39% C, 1.00% Si, 0.40% Mn, 5.30% Cr, 1.30% Mo, 0.90% V
0.39% C, 1.00% Si, 0.40% Mn, 5.30% Cr, 1.30% Mo, 0.90% V
0.39% C, 1.00% Si, 0.40% Mn, 5.30% Cr, 1.30% Mo, 0.90% V
0.39% C, 1.00% Si, 0.65% Mn, 0.030% P, 0.130% S, 5.15% Cr, 1.40% Mo, 0.55% V
0.39% C, 1.00% Si, 1.00% Mn, 16.50% Cr, 1.05% Mo, 1.00% Ni
0.39% C, 1.06% Si, 0.32% Mn, 0.019% P, 0.004% S, 4.91% Cr, 1.17% Mo, 0.11% Ni, 0.37% V, 0.011% Ti
0.39% C, 1.06% Si, 0.32% Mn, 0.019% P, 0.004% S, 4.91% Cr, 1.17% Mo, 0.11% Ni, 0.37%, 0.011% Ti
0.39% C, 1.10% Si, 0.40% Mn, 5.20% Cr, 1.40% Mo, 0.95% V
0.39% C, 16.50% Cr, 1.10% Mo
0.39% C, 16.50% Cr, 1.10% Mo
0.39-0.44% C, 1.50-1.80% Si, 0.60-0.90% Mn, 0.015% P, 0.001% S, 0.70-0.95% Cr, 0.30-0.45% Mo, 0.65-2.00% Ni, 0.05-0.10% V
0.39-0.44% C, 1.50-1.80% Si, 0.60-0.90% Mn, 0.015% P, 0.001% S, 0.70-0.95% Cr, 0.30-0.45% Mo, 1.65-2.00% Ni, 0.06-0.10% V
0.39-0.45% C, 0.15-0.40% Si, 0.80-1.10% Mn, 0.025% P, 0.015% S, 0.25-0.50% Cr, 0.60-0.90% Ni, 0.020-0.050% Ti, 0.60-0.90% Ni, 0.0008-0.0040% B
0.39-0.45% C, 0.15-0.40% Si, 0.80-1.10% Mn, 0.025% P, 0.015% S, 0.25-0.50% Cr, 0.60-0.90% Ni, 0.020-0.050% Ti, 0.60-0.90% Ni, 0.0008-0.0040% B
0.40% C 0.25% Si 5.30% Cr 1.80% Mo 0.65% V
0.40% C, 0.20% Si, 0.50% Mn, 12.00% Cr, 0.50% V, +N
0.40% C, 0.20% Si, 0.77% Mn, 0.030% P, 0.020% S, 0.04% Cr
0.40% C, 0.20% Si, 0.80% Mn, 0.025% P, 0.025% S, 1.00% Cr, 0.25% Mo
0.40% C, 0.25% Si, 0.40% Mn, 1.35% Cr, 0.25% Mo, 4.00% Ni, or 0.50% W
0.40% C, 0.25% Si, 0.65% Mn, 0.03% Cr, + Pb
0.40% C, 0.25% Si, 0.70% Mn, 0.025% P, 0.025% S, 0.80% Cr, 1.80% Ni, 0.25% Mo
0.40% C, 0.25% Si, 1.00% Mn, 1.00% Cr, 0.20% Mo
0.40% C, 0.25% Si, 1.00% Mn, 1.00% Cr, 0.20% Mo
0.40% C, 0.30% Si, 0.30% Mn, 3.30% Cr, 1.20% Mo, 1.25% V, 2.40% W, 1.60% Co
0.40% C, 0.30% Si, 0.30% Mn, 4.25% Cr, 2.00% V, 4.25% W, 4.25% Co
0.40% C, 0.30% Si, 0.30% Mn, 4.25% Cr, 0.45% Mo, 2.10% V, 4.25% W
0.40% C, 0.30% Si, 0.30% Mn, 4.25% Cr, 2.00% V, 4.25% Co, 5.25% W
0.40% C, 0.30% Si, 0.40% Mn, 4.50% Cr, 0.50% Mo, 2.10% V, 4.50% Co
0.40% C, 0.30% Si, 0.40% Mn, 4.50% Cr, 0.50% Mo, 2.10% V, 4.50% Co
0.40% C, 0.30% Si, 0.60% Mn, 1.60% Cr, 0.35% Mo, 1.15% Al
0.40% C, 0.30% Si, 0.60% Mn, 1.60% Cr, 0.35% Mo, 1.15% V
0.40% C, 0.30% Si, 0.75% Mn, 0.80% Cr, 0.25% Mo, 1.80% Ni
0.40% C, 0.30% Si, 0.75% Mn, 0.80% Cr, 0.25% Mo, 1.80% Ni
0.40% C, 0.30% Si, 0.90% Mn, 0.50% Cr, 0.55% Ni, 0.20% Mo
0.40% C, 0.30% Si, 1.40% Mn, 1.90% Cr, 0.20% Mo
0.40% C, 0.30% Si, 1.45% Mn, 1.95% Cr, 0.20% Mo, 1.05% Ni
0.40% C, 0.30% Si, 1.50% Mn, 0.003% S, 1.90% Cr, 1.20% Ni, 0.20% Mo, + others
0.40% C, 0.30% Si, 1.50% Mn, 0.012% P, 0.005% S, 1.90% Cr, 0.20% Mo
0.40% C, 0.30% Si, 1.50% Mn, 0.012% P, 0.005% S, 1.90% Cr, 0.20% Mo
0.40% C, 0.30% Si, 1.50% Mn, 0.012% P, 0.060% S, 1.90% Cr, 0.20% Mo
0.40% C, 0.30% Si, 1.50% Mn, 0.012% P, 0.060% S, 1.90% Cr, 0.20% Mo
0.40% C, 0.30% Si, 1.50% Mn, 0.05% S, 1.90% Cr, 0.20% Mo
0.40% C, 0.30% Si, 1.50% Mn, 0.06% S, 2.00% Cr, 0.20% Mo
0.40% C, 0.30% Si, 1.50% Mn, 1.90% Cr, 0.20% Mo, 1.10% Ni
0.40% C, 0.30% Si, 1.50% Mn, 2.00% Cr, 0.20% Mo, 1.00% Ni
0.40% C, 0.30% Si, 1.50% Mn, 2.00% Cr, 0.20% Mo
0.40% C, 0.30% Si, 1.50% Mn, 2.00% Cr, 0.20% Mo
0.40% C, 0.35% Si, 0.60-0.90% Mn, 0.050% P, 0.050% S
0.40% C, 0.35% Si, 0.80% Mn, 0.030% P, 0.070% S, 16.00% Cr, 1.030% Mo
0.40% C, 0.35% Si, 0.90% Mn, 0.030% P, 0.005% S, 16.00% Cr, 1.030% Mo
0.40% C, 0.35% Si, 1.50% Mn, 0.05% S, 1.90% Cr, 0.20% Mo
0.40% C, 0.40% Si, 0.20% Mn, 4.20% Cr, 5.00% Mo, 1.90% V, 6.50% W
0.40% C, 0.40% Si, 0.30% Mn, 13.00% Cr
0.40% C, 0.40% Si, 0.70% Mn, 13.00% Cr
0.40% C, 0.40% Si, 1.20% Mn, 0.08% S, 1.90% Cr, 0.20% Mo
0.40% C, 0.40% Si, 1.50% Mn, 0.06% S, 1.90% Cr, 0.20% Mo
0.40% C, 0.40% Si, 1.50% Mn, 0.07% S, 1.90% Cr, 0.20% Mo
0.40% C, 0.40% Si, 1.50% Mn, 0.080% S, 1.90% Cr, 0.20% Mo
0.40% C, 0.40% Si, 1.50% Mn, 1.90% Cr, 0.20% Mo, 0.07% S
0.40% C, 0.40% Si, 1.50% Mn, 1.90% Cr, 0.20% Mo
0.40% C, 0.70% Mn, 0.80% Cr, 0.25% Mo, 1.80% Ni
0.40% C, 0.70% Mn, 0.80% Cr, 0.25% Mo, 1.80% Ni
0.40% C, 0.70% Mn, 0.80% Cr, 0.25% Mo, 1.85% Ni
0.40% C, 0.80% Cr, 0.25% Mo, 1.80% Ni
0.40% C, 0.80% Mn, 0.95% Cr, 0.25% Mo
0.40% C, 0.80% Si, 0.50% Mn, 14.50% Cr, 0.30% V
0.40% C, 0.80% Si, 1.00% Mn, 13.50% Cr, 0.25% V
0.40% C, 0.80% Si, 1.00% Mn, 13.50% Cr, 0.25% V
0.40% C, 0.90% Si, 0.30% Mn, 5.00% Cr, 1.30% Mo, 0.50% V
0.40% C, 0.90% Si, 5.00% Cr, 1.30% Mo, 0.45% V
0.40% C, 0.95% Si, 0.35% Mn, 5.20% Cr, 1.50% Mo, 0.90% V
0.40% C, 0.95% Si, 0.35% Mn, 5.20% Cr, 1.50% Mo, 0.90% V
0.40% C, 0.95% Si, 0.35% Mn, 5.20% Cr, 1.50% Mo, 0.90% V
0.40% C, 0.95% Si, 0.35% Mn, 5.20% Cr, 1.50% Mo, 0.90% V
0.40% C, 1.00% Si, 0.03% S, 5.30% Cr, 1.40% Mo, 1.00% V
0.40% C, 1.00% Si, 0.003% S, 5.30% Cr, 1.30% Mo, 0.95% V
0.40% C, 1.00% Si, 0.005% S, 5.20% Cr, 1.30% Mo, 0.95% V
0.40% C, 1.00% Si, 0.10% S, 5.25% Cr, 1.35% Mo, 1.00% V
0.40% C, 1.00% Si, 0.25% Mn, 5.25% Cr, 1.35% Mo, 4.75% W
0.40% C, 1.00% Si, 0.25% Mn, 5.25% Cr, 4.75% W
0.40% C, 1.00% Si, 0.30% Mn, 5.00% Cr, 1.30% Mo, 0.50% V
0.40% C, 1.00% Si, 0.30% Mn, 5.00% Cr, 1.30% Mo, 0.50% V
0.40% C, 1.00% Si, 0.40% Mn, 0.09% S, 5.00% Cr, 1.30% Mo, 0.95% V
0.40% C, 1.00% Si, 0.40% Mn, 5.20% Cr, 1.30% Mo, 1.00% V
0.40% C, 1.00% Si, 0.40% Mn, 5.20% Cr, 1.30% Mo, 1.00% V
0.40% C, 1.00% Si, 0.40% Mn, 5.20% Cr, 1.30% Mo, 1.00% V
0.40% C, 1.00% Si, 0.40% Mn, 5.20% Cr, 1.30% Mo, 1.00% V
0.40% C, 1.00% Si, 0.40% Mn, 5.20% Cr, 1.30% Mo, 1.00% V
0.40% C, 1.00% Si, 0.40% Mn, 5.20% Cr, 1.30% Mo, 1.00% V
0.40% C, 1.00% Si, 0.40% Mn, 5.20% Cr, 1.40% Mo, 1.00% V
0.40% C, 1.00% Si, 0.40% Mn, 5.25% Cr, 1.35% Mo, 1.00% V, 0.001% S
0.40% C, 1.00% Si, 0.40% Mn, 5.25% Cr, 1.35% Mo, 1.00% V
0.40% C, 1.00% Si, 0.40% Mn, 5.25% Cr, 1.35% Mo, 1.00% V
0.40% C, 1.00% Si, 0.40% Mn, 5.25% Cr, 1.00% V, 1.35% Mo
0.40% C, 1.00% Si, 0.40% Mn, 5.25% Cr, 1.35% Mo, 1.00% V
0.40% C, 1.00% Si, 0.40% Mn, 5.26% Cr, 1.35% Mo, 1.00% V, 0.001% S
0.40% C, 1.00% Si, 0.40% Mn, 5.30% Cr, 1.40% Mo, 1.00% V
0.40% C, 1.00% Si, 0.60% Mn, 5.25% Cr, 1.50% Mo, 1.00% V
0.40% C, 1.00% Si, 0.60% Mn, 5.25% Cr, 1.50% Mo, 1.00% V
0.40% C, 1.00% Si, 0.80% Mn, 0.12% S, 5.25% Cr, 1.35% Mo, 1.00% V
0.40% C, 1.00% Si, 1.00% Mn, 16.00% Cr, 1.20% Mo, 1.00% N
0.40% C, 1.00% Si, 5.00% Cr, 1.50% Mo, 0.40% V
0.40% C, 1.00% Si, 5.20% Cr, 1.30% Mo, 0.95% V
0.40% C, 1.00% Si, 5.25% Cr, 1.40% Mo, 1.00% V
0.40% C, 1.00% Si, 5.25% Cr, 1.40% Mo, 1.00% V
0.40% C, 1.00% Si, 5.30% Cr, 1.40% Mo, 0.10% V
0.40% C, 1.00% Si, 5.30% Cr, 1.40% Mo, 1.00% V
0.40% C, 1.00% Si, 5.30% Cr, 1.40% Mo, 1.00% V
0.40% C, 1.00% Si, 5.30% Cr, 1.40% Mo, 1.00% V
0.40% C, 1.00% Si. 5.30% Cr, 1.40% Mo, 1.00% V
0.40% C, 1.05% Si, 0.40% Mn, 0.025% P, 0.003% S, 5.20% Cr, 1.40% Mo, 1.00% V
0.40% C, 1.05% Si, 0.40% Mn, 0.025% P, 0.003% S, 5.20% Cr, 1.40% Mo, 1.00% V
0.40% C, 1.05% Si, 5.00% Cr, 1.30% Mo, 1.10% V
0.40% C, 1.50% Cr, 0.50% Mo, 4.50% Ni
0.40% C, 1.50% Mn, 0.05% S, 1.90% Cr, 0.20% Mo
0.40% C, 1.50% Mn, 0.05% S, 1.90% Cr, 0.20% Mo
0.40% C, 1.50% Mn, 0.05% S, 1.90% Cr, 0.20% Mo
0.40% C, 1.50% Mn, 1.90% Cr, 0.20% Mo, 0.05% S, 0.00% W
0.40% C, 1.50% Mn, 1.90% Cr, 0.20% Mo, 1.00% Ni
0.40% C, 1.50% Mn, 1.90% Cr, 0.20% Mo, 1.00% Ni
0.40% C, 1.50% Mn, 1.90% Cr, 0.20% Mo
0.40% C, 1.50% Mn, 1.90% Cr, 0.20% Mo
0.40% C, 1.50% Mn, 1.90% Cr, 0.20% Mo
0.40% C, 1.50% Mn, 1.90% Cr, 0.20% Mo
0.40% C, 1.50% Mn, 1.90% Cr, 0.20% Mo
0.40% C, 1.50% Mn, 1.90% Cr, 0.20% Mo
0.40% C, 1.50% Mn, 1.90% Cr, 0.20% Mo
0.40% C, 1.50% Mn, 1.90% Cr, 0.20% Mo
0.40% C, 1.50% Mn, 1.90% Cr, 0.20% Mo
0.40% C, 1.50% Mn, 1.90% Cr, 1.00% Ni, 0.20% Mo
0.40% C, 1.50% Mn, 1.90% Cr, 1.00% Ni, 0.20% Mo
0.40% C, 1.50% Mn, 1.90% Cr, 1.00% Ni, 0.20% Mo
0.40% C, 1.69% Si, 0.85% Cr, 0.40% Mo, 1.80% Ni
0.40% C, 1.80% Cr, 0.25% Mo, 1.00% Al
0.40% C, 13.00% Cr
0.40% C, 13.00% Cr
0.40% C, 13.50% Cr
0.40% C, 14.50% Cr, 0.30% Mo
0.40% C, 15.50% Cr, 2.00% Mo, 0.30% V, 0.20% N
0.40% C, 3.00% Cr, 1.00% Mo, 0.20% V
0.40% C, 3.00% Cr, 1.20% Mo, 0.20% V
0.40% C, 5.00% Cr, 1.30% Mo, 0.40% V
0.40% C, 5.00% Cr, 1.30% Mo, 0.45% V
0.40% C, 5.00% Cr, 1.30% Mo, 1.00% V
0.40% C, 5.00% Cr, 3.00% Mo, 0.50% V, 2.70% Co
0.40% C, 5.00% Cr, 3.00% Mo, 0.50% V
0.40% C, 5.30% Cr, 1.40% Mo, 1.00% V
0.40% C, 5.30% Cr, 1.40% Mo, 1.00% V
0.40% C, 5.30% Cr, 1.40% Mo, 1.00% V
0.40-0.46% C, 0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.015% S, 0.90-1.20% Cr, 0.15-0.30% Mo, 0.30% Cu, 0.050% Al
0.40-0.48% C, 0.40% Si, 1.30-1.70% Mn, 0.06% P, 0.24-0.33% S
0.40-0.50% C, 0.10-0.30% Si, 0.20-0.50% Mn, 0.030% P, 0.030% S, 1.20-1.50% Cr, 3.80-4.30% Ni
0.40-0.50% C, 0.10-0.40% Si, 0.15-0.45% Mn, 1.20-1.50% Cr, 0.15-0.35% Mo, 3.80-4.30% Ni
0.40-0.50% C, 0.10-0.40% Si, 0.20--0.50% Mn, 0.030% P, 0.030% S, 1.20-1.50% Cr, 0.15-0.35% Mo, 3.80-4.30% Ni
0.40-0.50% C, 0.10-0.40% Si, 0.20-0.50% Mn, 0.030% P, 0.030% S, 1.20-1.50% Cr, 0.15-0.35% Mo, 3.80-4.30% Ni
0.40-0.50% C, 0.10-0.40% Si, 0.20-0.50% Mn, 0.030% P, 0.030% S, 1.20-1.50% Cr, 0.15-0.35% Mo, 3.80-4.30% Ni
0.40-0.50% C, 0.10-0.40% Si, 0.20-0.50% Mn, 0.030% P, 0.030% S, 1.20-1.50% Cr, 0.15-0.35% Mo, 3.80-4.30% Ni
0.40-0.50% C, 0.15-0.35% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 1.20-1.50% Cr, 1.50-1.80% Ni
0.40-0.50% C, 0.15-0.35% Si, 0.60-0.90% Mn, 0.030% P, 0.030% S, 1.30-1.60% Cr, 0.25-0.35% Mo
0.40-0.50% C, 0.15-0.40% Si, 0.60-1.00% Mn
0.40-0.50% C, 0.15-0.40% Si, 0.60-1.00% Mn
0.40-0.50% C, 0.20-0.40% Si, 0.30-0.50% Mn, 0.015% P, 0.003% S, 2.70-3.40% Cr, 4.80-5.20% Mo, 0.90-1.10% V
0.40-0.50% C, 0.30-0.50% Si, 0.30-0.50% Mn, 0.025% P, 0.025% S, 4.00-5.00% Cr, 0.40-0.60% Mo, 4.00-5.00% W, 1.80-2.10% V, 4.00-5.00% Co
0.40-0.50% C, 0.50-0.70% Si, 0.30-0.50% Mn, 0.035% P, 0.035% S, 1.30-1.60% Cr, 0.40-0.60% Mo, 0.40-0.60% W, 0.75-0.90% V
0.40-0.50% C, 0.50-0.80% Si, 0.90-1.30% Mn, 0.80-1.20% Cr, 0.30% Mo, 0.50% Ni
0.40-0.50% C, 0.80-1.10% Si, 0.20-0.40% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 1.80-2.10% W, 0.15-0.20% V
0.40-0.50% C, 1.30-1.60% Si, 0.50-0.70% Mn, 0.035% P, 0.035% S, 1.30-1.60% Cr, 0.07-0.12% V
0.40-0.60% C, 0.10-0.40% Si, 0.20-0.50% Mn, 0.030% P, 0.030% S, 1.20-1.50% Cr, 0.15-0.35% Mo, 3.80-4.30% Ni
0.40% C, 0.38% Si, 0.95% Mn
0.4% C, 4.5% Cr, 2% Mo, 0.5% W, 0.5% V
0.41% C, 0.30% Si, 0.70% Mn, 1.10% Cr, 0.20% Mo
0.41% C, 0.40% Si, 0.65% Mn, 1.65% Cr, 0.33% Mo, 1.00% Al
0.41-0.49% C, 0.15-0.35% Si, 0.60-0.80% Mn, 0.025% P, 0.020% S, 1.40-1.60% Cr, 3.80-4.20% Ni, 0.73-0.85% Mo, 0.45-0.55% V
0.41-0.49% C, 0.15-0.35% Si, 0.60-0.80% Mn, 0.025% P, 0.020% S, 1.40-1.60% Cr, 0.73-0.75% Mo, 3.80-4.20% Ni, 0.45-0.55% V
0.42% C, 0.25% Si, 0.70% Mn, 1.05% Cr
0.42% C, 0.25% Si, 0.75% Mn, 1.05% Cr, 0.20% Mo
0.42% C, 0.25% Si, 0.75% Mn, 1.10% Cr, 0.22% Mo
0.42% C, 0.25% Si, 0.76% Mn, 0.035% S, 1.10% Cr, 0.22% Mo
0.42% C, 0.30% Si, 0.50% Mn, 0.025% P, 0.015% S, 16.20% Cr, 0.95% Mo, 0.30% Ni
0.42% C, 0.30% Si, 0.80% Mn, 0.85% Cr, 0.30% Mo, 1.90% Ni, 0.06% V, 0.03% Al
0.42% C, 0.40% Si, 0.30% Mn, 0.01% P, 0.001% S, 13.00% Cr
0.42% C, 0.40% Si, 0.30% Mn, 0.01% P, 0.001% S, 13.00% Cr
0.42% C, 0.40% Si, 0.30% Mn, 13.00% Cr
0.42% C, 0.40% Si, 0.30% Mn, 13.00% Cr
0.42% C, 0.40% Si, 0.40% Mn, 0.030% P, 0.003% S, 13.00% Cr
0.42% C, 0.40% Si, 0.40% Mn, 0.030% P, 0.003% S, 13.00% Cr
0.42% C, 0.50% Si, 0.40% Mn, 6.50% Cr, 1.30% Mo, 0.80% V
0.42% C, 0.50% Si, 0.75% Mn, 2.50% Cr, 1.00% Mo, 0.80% Ni, 0.05% V
0.42% C, 1.00% Cr, 0.20% Mo
0.42% C, 1.00% Si, 0.55% Mn, 3.15% Cr, 2.15% Mo, 0.35% V
0.42% C, 1.00% Si, 0.55% Mn, 3.15% Cr, 2.15% Mo, 0.35% V
0.42% C, 1.10% Cr, 0.25% Mo
0.42% C, 1.10% Cr, 0.25% Mo
0.42% C, 1.60% Cr, 0.50% Mo, 4.40% Ni
0.42% C, 1.65% Si, 0.75% Mn, 0.80% Cr, 0.40% Mo, 0.07% V, 1.80% Ni
0.42% C, 1.65% Si, 0.75% Mn, 0.80% Cr, 0.40% Mo, 0.07% V, 1.80% Ni
0.42% C, 13.00% Cr
0.42% C, 13.00% Cr
0.42% C, 16.00% Cr, 1.80% Mo, 0.35% V, 0.20% N
0.42% Mn, 1.25% Mo, 1.40% Ni. Mix 2-1: 0.0% Cu, 0.8% graphite. Mix 2-2: 1.0% Cu, 0.7% graphite. Mix 2-3: 1.5% Cu, 0.8% graphite. Mix 2-4: 2.0% Cu, 0.9% graphite
0.42-0.47% C, 0.20-0.30% Si, 0.85-1.00% Mn, 0.030% P, 0.030% S, 1.70-1.90% Cr, 0.20-0.30% Mo, 0.05-0.15% V
0.42-0.48% C, 0.15-0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S, 0.40-0.60% Cr
0.42-0.48% C, 0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S, 0.40-0.60% Cr, 0.30% Cu
0.42-0.50% C, 0.15-0.30% Si, 0.60-0.80% Mn, 0.030% P, 0.030% S
0.42-0.50% C, 0.15-0.35% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S
0.42-0.50% C, 0.15-0.40% Si, 0.60-0.70% Mn, 0.040% P, 0.030% S
0.42-0.50% C, 0.15-0.40% Si, 0.60-0.80% Mn, 0.030% P, 0.030% S
0.42-0.50% C, 0.15-0.40% Si, 0.60-0.80% Mn, 0.030% P, 0.030% S
0.42-0.50% C, 0.15-0.40% Si, 0.60-0.80% Mn, 0.030% P, 0.030% S
0.42-0.50% C, 0.15-0.40% Si, 0.60-0.80% Mn, 0.030% P, 0.030% S
0.42-0.50% C, 0.15-0.40% Si, 0.60-0.80% Mn, 0.030% P, 0.030% S
0.42-0.50% C, 0.15-0.40% Si, 0.60-0.80% Mn, 0.030% P, 0.030% S
0.42-0.50% C, 0.30% Si, 0.50-0.80% Mn, 0.025% P, 0.025% S, 0.25% Cu
0.42-0.50% C, 0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.010% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni = 0.63
0.42-0.50% C, 0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.010% S
0.42-0.50% C, 0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S, 0.40-0.60% Cr
0.42-0.50% C, 0.40% Si, 0.50-0.80% Mn, 0.030% P, 0.020-0.040% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.42-0.50% C, 0.40% Si, 0.50-0.80% Mn, 0.030% P, 0.035% S
0.42-0.50% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.020-0.040% S, 0.40-0.60% Cr
0.42-0.50% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.42-0.50% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.42-0.50% C, 0.40% Si, 0.50-0.80% Mn, 0.045% P, 0.045% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.42-0.50% C, 0.40% Si, 0.50-0.80% Mn, 0.045% P, 0.045% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.42-0.50% C, 0.40% Si, 0.50-0.80% Mn, 0.045% P, 0.045% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.42-0.50% C, 0.40% Si, 0.50-0.80% Mn, 0.045% P, 0.045% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.42-0.50% C, 0.40% Si, 0.70-1.10% Mn, 0.006% P, 0.15-0.25% S, Pb
0.42-0.50% C, 1.50-1.80% Si, 0.50-0.80% Mn, 0.050% P, 0.050% S, 0.007% N
0.42-0.50% C, 1.50-1.80% Si, 0.50-0.80% Mn, 0.050% P, 0.050% S, 0.0070% N
0.42% C, 0.25% Si, 0.70% Mn, 1.05% Cr
0.42% C, 0.25% Si, 0.75% Mn, 1.10% Cr, 0.22% Mo
0.42-0.50% C, 0.40% Si, 0.50-0.80% Mn, 0.030% P, 0.035% S
0.42-0.50% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.020-0.035% S
0.42-0.50% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.030% S, 0.40-0.60% Cr
0.42-0.50% C, 0.40% Si, 0.50-0.80% Mn, 0.045% P, 0.045% S
0.42-0.50% C, 1.50-1.80% Si, 0.50-0.80% Mn, 0.050% P, 0.050% S, 0.0070% N
0.43% C, 0.18% Si, 0.69% Mn, 0.010% P, 0.016% S, 1.46% Cr, 0.78% Mo, 3.91% Ni, 0.50% V, 0.08% Cu
0.43% C, 0.30% Si, 0.40% Mn, 6.40% Cr, 1.30% Mo, 0.90% V
0.43% C, 0.30% Si, 0.70% Mn, 3.70% Ni, 1.70% Cr, 0.40% Mo, 0.10% V
0.43% C, 0.35% Si, 1.50% Mn, 0.001% S, 1.87% Cr, 0.5% Ni, 0.18% Mo, + others
0.43% C, 0.90% Mn, 1.50% Mo, 0.90% Ni, 1.30% V
0.43% C, 1.00% Cr, 0.20% Mo
0.43-0.46% C, 1.00% Si, 1.00% Mn, 0.040% P, 0.0180-0.026% S, 12.50-14.50% Cr
0.43-0.48% C, 0.60-0.75% Si, 0.65-0.85% Mn, 0.025% P, 0.025% S, 1.65-1.85% Cr, 0.25-0.35% Cr, 0.45-0.65% Ni, 0.17-0.22% V, 0.30% Cu
0.43-0.48% C, 0.60-0.75% Si, 0.65-0.85% Mn, 0.025% P, 0.025% S, 1.65-1.85% Cr, 0.25-0.35% Mo, 0.45-0.60% Ni, 0.17-0.22% V, 0.30% Cu
0.43-0.49% C, 0.15-0.35% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S
0.43-0.49% C, 0.15-0.35% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S
0.43-0.49% C, 0.15-0.35% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S
0.43-0.50% C, 1.00% Si, 1.00% Mn, 0.040% P, 0.030% S, 12.50-14.50% Cr
0.43-0.50% C, 1.00% Si, 1.00% Mn, 0.040% P, 0.015% S, 12.50-14.50% Cr
0.43-0.50% C, 1.00% Si, 1.00% Mn, 0.040% P, 0.015% S, 12.50-14.50% Cr
0.43-0.50% C, 1.00% Si, 1.00% Mn, 0.040% P, 0.030% S, 12.50-14.50% Cr
0.43-0.50% C, 1.00% Si, 1.00% Mn, 0.040% P, 0.035% S, 12.00-14.50% Cr
0.43-0.50% C, 1.00% Si, 2.00% Mn, 0.040% P, 0.15-0.35% S, 12.50-14.00% Cr
0.43% C, 0.30% Si, 1.78% Mn, 0.019% P, 0.017% S, 0.10% V
0.43-0.49% C, 0.15-0.35% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S
0.44% C, 0.25% Si, 0.55% Mn, 0.95% Cr, 0.50% Mo, 0.28% V
0.44% C, 0.25% Si, 0.55% Mn, 0.95% Cr, 0.50% Mo, 0.28% V
0.44% C, 1.60% Mn, 0.007% S, 1.88% Cr, 0.25% Mo
0.44-0.54% C, 0.60-0.90% Si, 0.70-1.00% Mn, 1.70-2.10% Cr, 0.25-0.45% Mo, 0.50-0.80% Ni, 0.15-0.25% V
0.44-0.54% C, 0.60-0.90% Si, 0.70-1.00% Mn, 1.70-2.10% Cr, 0.25-0.45% Mo, 0.50-0.80% Ni, 0.15-0.25% V
0.44% C, 0.29% Si, 1.30% Mn, 0.020% P, 0.025% S, 0.08% Cr, 0.02% Ni, 0.14% Cu
0.45% C, 0.30% Si, 0.70% Mn
0.45% C, 0.20% Si, 0.40% Mn, 1.30% Cr, 0.30% Mo, 4.00% Ni
0.45% C, 0.20% Si, 0.40% Mn, 1.30% Cr, 0.30% Mo, 4.00% Ni
0.45% C, 0.20% Si, 0.70% Mn, 0.025% P, 0.025% S, 0.25% Cu
0.45% C, 0.20% Si, 0.70% Mn
0.45% C, 0.25% Si, 0.30% Mn, 0.025% P, 0.003% S, 1.30% Cr, 0.25% Mo, 4.00% Ni
0.45% C, 0.25% Si, 0.30% Mn, 0.025% P, 0.003% S, 1.30% Cr, 0.25% Mo, 4.00% Ni
0.45% C, 0.25% Si, 0.35% Mn, 1.25% Cr, 0.20% Mo, 3.90% Ni
0.45% C, 0.25% Si, 0.35% Mn, 1.35% Cr, 0.25% Mo, 4.05% Ni
0.45% C, 0.25% Si, 0.35% Mn, 1.40% Cr, 0.20% Mo, 4.00% Ni
0.45% C, 0.25% Si, 0.35% Mn, 1.40% Cr, 4.00% Ni
0.45% C, 0.25% Si, 0.40% Mn, 1.30% Cr, 0.25% Mo, 4.00% Ni
0.45% C, 0.25% Si, 0.40% Mn, 1.35% Cr, 0.25% Mo, 4.00% Ni
0.45% C, 0.25% Si, 0.40% Mn, 1.35% Cr, 0.25% Mo, 4.00% Ni
0.45% C, 0.25% Si, 0.70% Mn, 1.50% Cr, 0.79% Mo, 0.50% V, 4.00% Ni
0.45% C, 0.25% Si, 0.70% Mn, 1.50% Cr, 0.80% Mo, 0.40% V, 4.00% Ni
0.45% C, 0.30% Si, 0.30% Mn, 3.00% Cr, 5.00% Mo, 1.00% V
0.45% C, 0.30% Si, 0.30% Mn, 3.00% Cr, 5.00% Mo, 1.00% V
0.45% C, 0.30% Si, 0.40% Mn, 4.50% Cr, 3.00% Mo, 2.00% V, 4.50% Co
0.45% C, 0.30% Si, 0.40% Mn, 4.50% Cr, 3.00% Mo, 2.00% V, 4.50% Co
0.45% C, 0.30% Si, 0.40% Mn, 4.50% Cr, 3.00% Mo, 2.00% V, 4.50% Co
0.45% C, 0.30% Si, 0.70% Mn, 1.50% Cr, 0.75% Mo, 0.30% V
0.45% C, 0.30% Si, 0.70% Mn, 1.50% Cr, 0.75% Mo, 0.30% V
0.45% C, 0.30% Si, 0.70% Mn, 1.50% Cr, 0.75% Mo, 0.30% V
0.45% C, 0.30% Si, 0.70% Mn
0.45% C, 0.30% Si, 0.70% Mn
0.45% C, 0.30% Si, 0.70% Mn
0.45% C, 0.30% Si, 0.70% Mn
0.45% C, 0.30% Si, 0.70% Mn
0.45% C, 0.30% Si, 0.75% Mn, 0.025% P, 0.010% S, 1.50% Cr, 0.50% Mo, 0.30% V
0.45% C, 0.35% Si, 0.70% Mn, 0.020% P, 0.005% S
0.45% C, 0.40% Si, 0.40% Mn, 0.020% P, 0.010% S, 4.50% Cr, 0.50% Mo, 2.00% V, 4.50% W, 4.50% Co
0.45% C, 0.40% Si, 0.50% Mn, 0.030% P, 0.003% S, 13.00% Cr
0.45% C, 0.42% Si, 0.42% Mn, 1.35% Cr, 0.70% Mo, 4.10% Ni, 0.20% V
0.45% C, 0.50% Si, 0.50% Mn, 0.025% P, 0.030% S, 13.00% Cr
0.45% C, 0.50% Si, 0.50% Mn, 0.030% P, 0.025% S, 13.00% Cr
0.45% C, 0.50% Si, 1.20% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.08% Mo, 0.30% Ni, 0.020% Al, 0.012% N
0.45% C, 0.50% Si, 1.20% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.08% Mo, 0.30% Ni, 0.020% Al, 0.012% N
0.45% C, 0.60% Si, 0.40% Mn, 1.60% Cr, 0.60% Mo, 0.80% V, 0.50% W
0.45% C, 0.60% Si, 0.40% Mn, 1.60% Cr, 0.60% Mo, 0.80% V, 0.50% W
0.45% C, 0.60% Si, 0.40% Mn, 1.60% Cr, 0.60% Mo, 0.80% V, 0.50% W
0.45% C, 0.70% Si, 0.80% Mn, 1.80% Cr, 0.30% Mo, 0.60% Ni, 0.20% V
0.45% C, 0.85% Si, 0.35% Mn, 7.40% Cr, 1.40% Mo, 1.35% V
0.45% C, 0.90% Mn, 1.80% Cr, 0.30% Mo, 0.05% V
0.45% C, 0.90% Si, 1.80% Cr, 0.30% Mo, 0.05% V
0.45% C, 1.00% Cr, 0.55% Mo, 0.30% V
0.45% C, 1.00% Si, 0.30% Mn, 1.10% Cr, 0.20% V, 2.00% W
0.45% C, 1.00% Si, 0.30% Mn, 1.10% Cr, 0.20% V, 2.00% W
0.45% C, 1.30% Cr, 0.30% Mo, 4.10% Ni
0.45% C, 1.35% Si, 1.35% Cr, 0.10% V
0.45% C, 1.40% Cr, 0.30% Mo, 4.00% Ni
0.45% C, 1.40% Cr, 0.25% Mo, 4.00% Ni
0.45% C, 1.40% Cr, 0.30% Mo, 4.00% Ni
0.45% C, 1.40% Cr, 0.30% Mo, 4.00% Ni
0.45% C, 1.40% Cr, 0.30% Mo, 4.00% Ni
0.45% C, 1.45% Cr, 0.25% Mo, 4.00% Ni
0.45% C, 1.60% Si, 0.60% Mn, 0.60% Cr, 0.25% Mo
0.45% C, 13.50% Cr
0.45-0.50% C, 0.70-0.90% Si, 0.35-0.45% Mn, 0.020% P, 0.005% S, 7.30-7.80% Cr, 1.30-1.50% Mo, 1.30-1.50% V
0.45-0.55% C, 0.15-0.35% Si, 0.40-0.60% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 3.00-3.50% Ni
0.45-0.55% C, 0.20-0.50% Si, 0.50-0.80% Mn, 0.030% P, 0.030% S, 3.00-3.60% Cr, 1.20-1.60% Mo, 0.05-0.25% V
0.45-0.55% C, 0.20-0.80% Si, 0.50-0.90% Mn, 0.030% P, 0.020% S, 3.00-3.50% Cr, 1.30-1.70% Mo, 0.15-0.35% V
0.45-0.55% C, 0.20-1.00% Si, 0.20-0.80% Mn, 0.030% P, 0.030% S, 3.00-3.50% Cr, 1.30-1.80% Mo, 0.35% V
0.45-0.55% C, 0.20-1.00% Si, 0.20-0.90% Mn, 3.00-3.50% Cr, 0.35% V.
0.45-0.55% C, 0.70-1.00% Si, 0.15-0.45% Mn, 0.030% P, 0.030% S, 0.90-1.20% Cr, 1.70-2.20% W, 0.10-0.20% V
0.45-0.55% C, 0.80-1.00% Si, 0.40-0.60% Mn, 0.035% P, 0.035% S, 8.00-9.00% Cr, 1.10-1.30% Mo, 1.10-1.30% W
0.45-0.55% C, 0.80-1.00% Si, 0.40-0.60% Mn, 0.035% P, 0.035% S, 8.00-9.00% Cr, 1.10-1.30% Mo, 1.10-1.30% W
0.45-0.55% C, 1.00% Si, 1.00% Mn, 0.040% P, 0.015% S, 14.00-15.00% Cr, 0.50-0.80% Mo, 0.10-0.20% V
0.45-0.55% C, 1.00% Si, 1.00% Mn, 0.040% P, 0.030% S, 14.00-15.00% Cr, 0.50-0.80% Mo, 0.10-0.20% V
0.45-0.60% C, 0.40% Si, 0.60-1.10% Mn, 0.70-1.70% Cr, 0.40-1.00% Mo, 1.30-2.70% Ni
0.45-0.60% C, 0.40% Si, 0.60-1.10% Mn, 0.70-1.70% Cr, 1.30-2.50% Ni, 0.40-1.00% Mo
0.45-0.60% C, 1.30-1.70% Si, 0.80% Mn, 15.00-16.50% Cr, 0.20-0.40% Mo, 0.40% Ni, 0.20-0.40% V, 0.05-0.20% N
0.45% C, 0.30% Si, 0.50% Mn, 3.10% Cr, 5.00% Mo, 1.00% V
0.45% C, 0.55% Mn, 1.31% Si, 0.005% S, 0.013% P, 0.60% Cr, 0.22% Mo, 0.21% Ni, 0.27% Cu, 0.05% V, trace Ti
0.46% C, 0.25% Si, 0.75% Mn, 1.10% CR, 0.60% Ni, 1.00% Mo, 0.10% V
0.46% C, 0.25% Si, 0.75% Mn, 1.10% Cr, 1.00% Mo, 0.10% V, 0.60% Ni
0.46% C, 0.25% Si, 0.75% Mn, 1.10% Cr, 1.00% Mo, 0.10% V, 0.60% Ni
0.46% C, 0.35% Si, 0.30% Mn, 13.80% Cr
0.46% C, 0.40% Si, 0.40% Mn, 13.00% Cr, 0.30% V
0.46% C, 0.40% Si, 0.40% Mn, 13.00% Cr, 0.30% V
0.46% C, 0.40% Si, 0.40% Mn, 13.00% Cr
0.46% C, 0.40% Si, 0.65% Mn, 0.10% Mo, 0.40% Ni, (Cr+Mo+Ni) = 0.63
0.46% C, 0.40% Si, 0.65% Mn, 0.10% Mo, 0.40% Ni, (Cr+Mo+Ni) = 0.63
0.46% C, 0.40% Si, 0.65% Mn, 0.50% Cr
0.46% C, 0.45% Si, 0.50% Mn, 6.70% Cr, 1.50% Mo, 0.80% V
0.46% C, 0.45% Si, 0.50% Mn, 6.70% Cr, 1.50% Mo, 0.80% V
0.46% C, 0.50% Si, 0.50% Mn, 0.02% P, 0.015% S, 13.50% Cr
0.46% C, 0.70% Si, 0.80% Mn, 0.00% P, 1.80% Cr, 0.30% Mo, 0.50% Ni, 0.20% V
0.46% C, 13.50% Cr
0.46% C, 13.50% Cr
0.46% C, 3.00% Si, 0.30% Mn, 9.10% Cr
0.46-0.52% C, 0.15-0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.46-0.52% C, 0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.46-0.52% C, 0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo, 0.30% Cu
0.46-0.54% C, 0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.46-0.54% C, 0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.46-0.54% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.46-0.54% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.46-0.54% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.46-0.54% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.46-0.54% C, 0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.46-0.54% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.030% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.47% C, 0.35% Si, 0.35% Mn, 0.015% P, 0.016% S, 1.26% Cr, 0.24% Mo, 4.02% Ni
0.47% C, 0.40% Si, 0.28% Mn, 0.026% P, 0.006% S, 14.60% Cr, 0.13% Mo, 0.07% V, 0.06% W, 0.012% Al
0.47% C, 1.00% Si, 1.50% Mn, 13.50% Cr
0.47-0.50% C, 0.20-0.30% Si, 0.75-0.85% Mn, 0.015% P, 0.015-0.020% S, 1.05-1.20% Cr, 0.93-1.00% Mo, 0.43-0.50% Ni, 0.10-0.13% V
0.47-0.55% C, 0.10-0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.020-0.040% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, 0.30% Cu
0.47-0.55% C, 0.10-1.10% Si, 0.70-1.10% Mn, 0.025% P, 0.025% S, 0.90-1.20% Cr, 0.10-0.25% V
0.47-0.55% C, 0.15-0.40% Si, 0.70-1.10% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.10-0.20% V
0.47-0.55% C, 0.15-0.40% Si, 0.70-1.10% Mn, 0.80-1.20% Cr, 0.07-0.12% V
0.47-0.55% C, 0.40% Si, 0.60-0.90% Mn, 0.030% P, 0.020-0.040% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.47-0.55% C, 0.40% Si, 0.60-0.90% Mn, 0.030% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.47-0.55% C, 0.40% Si, 0.60-0.90% Mn, 0.030% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.47-0.55% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.47-0.55% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.10-0.25% V
0.47-0.55% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.10-0.25% V
0.47-0.55% C, 0.40% Si, 0.60-0.90% Mn, 0.045% P, 0.045% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.47-0.55% C, 0.40% Si, 0.70-1.10% Mn, 0.025% P, 0.025% S, 0.90-1.20% Cr, 0.10-0.25% V
0.47-0.55% C, 0.40% Si, 0.70-1.10% Mn, 0.025% P, 0.025% S, 0.90-1.20% Cr, 0.10-0.25% V
0.47-0.55% C, 0.40% Si, 0.70-1.10% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.10-0.25% V
0.47-0.55% C, 0.40% Si, 0.70-1.10% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.10-0.25% V
0.47-0.55% C, 0.40% Si, 0.70-1.10% Mn, 0.035% P, 0.030% S, 0.90-1.20% Cr, 0.10-0.20% V
0.48% C, 0.23% Si, 0.40% Mn, 1.30% Cr, 0.25% Mo, 4.00% Ni
0.48% C, 0.30% Si, 0.70% Mn, 0.030% P, 0.030% S
0.48% C, 0.30% Si, 0.70% Mn, 0.035% P, 0.035% S
0.48% C, 0.35% Si, 0.30% Mn, 14.40% Cr, 0.60% Mo, 0.12% V
0.48% C, 0.35% Si, 0.35% Mn, 16.50% Cr, 2.00% Mo
0.48% C, 0.40% Si, 0.90% Mn, 1.50% Cr
0.48% C, 0.80% Si, 0.40% Mn, 0.020% P, 0.003% S, 8.00% Cr, 1.40% Mo, 1.40% V
0.48-0.53% C, 0.80-1.10% Si, 0.20-0.40% Mn, 0.030% P, 0.030% S, 4.80-5.20% Cr, 1.25-1.45% Mo, 0.80-1.00% V
0.48-0.54% C, 0.40% Si, 0.70-1.10% Mn, 0.025% P, 0.025% S, 0.90-1.20% Cr, 0.15-0.30% Mo, 0.10-0.20% V
0.48-0.54% C, 0.40% Si, 0.70-1.10% Mn, 0.025% P, 0.025% S, 0.90-1.20% Cr, 0.15-0.30% Mo, 0.10-0.20% V
0.48-0.55% C, 0.15-0.35% Si, 0.60-0.80% Mn, 0.035% P, 0.025% S, 0.30% Cr, 0.10% Mo, 0.30% Ni, 0.10% V
0.48-0.55% C, 0.75-1.05% Si, 0.20-0.50% Mn, 0.030% P, 0.030% S, 7.25-8.75% Cr, 1.25-1.65% Mo, 0.22-0.55% V, 0.50% W
0.48-0.56% C, 0.40% Si, 0.70-1.10% Mn, 0.025% P, 0.025% S, 0.90-1.20% Cr, 0.15-0.30% Mo, 0.10-0.20% V
0.48-0.55% C, 0.15-0.35% Si, 1.60-1.90% Mn, 0.035% P, 0.035% S, 0.07-0.12% V
0.49% C, 0.33% Si, 0.94% Mn, 0.008% P, 0.003% S, 0.97% Cr, 0.08% Mo, 0.10% V, 0.14% Ni, 0.009% Al, 0.013% N
0.49-0.56% C, 1.20-1.50% Si, 0.70-0.90% Mn, 0.70-1.00% Cr, 0.50-0.70% Ni
0.49-0.56% C, 1.20-1.50% Si, 0.70-1.00% Mn, 0.025% P, 0.025% S, 0.70-1.00% Cr, 0.50-0.70% Ni
0.49-0.56% C, 1.20-1.50% Si, 0.70-1.00% Mn, 0.025% P, 0.025% S, 0.70-1.00% Cr, 0.50-0.70% Ni
0.49% C, 0.23% Si, 0.90% Mn, 0.016% P, 0.010% S, 1.03% Cr, 0.12% V
0.50 C, 0.95% Si, 0.45% Mn, 8.00% Cr, 1.30% Mo, 0.45% V
0.50% C, 0.20% Si, 0.25% Mn, 4.50% Cr, 3.00% Mo, 0.55% V
0.50% C, 0.20% Si, 0.25% Mn, 4.50% Cr, 3.00% Mo, 0.55% V
0.50% C, 0.20% Si, 0.50% Mn, 5.00% Cr, 2.30% Mo, 0.50% V
0.50% C, 0.20% Si, 0.50% Mn, 5.00% Cr, 2.30% Mo, 0.50% V
0.50% C, 0.20% Si, 0.50% Mn, 5.00% Cr, 2.30% Mo, 0.50% V
0.50% C, 0.20% Si, 0.50% Mn, 5.00% Cr, 2.30% Mo, 0.50% V
0.50% C, 0.25% Si, 0.50% Mn, 3.25% Ni
0.50% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.20% Mo, + Pb
0.50% C, 0.25% Si, 0.75% Mn, 0.03% S, + Pb
0.50% C, 0.25% Si, 0.75% Mn, 3.25% Cr, 1.40% Mo
0.50% C, 0.25% Si, 0.75% Mn, 3.25% Cr, 1.40% Mo
0.50% C, 0.25% Si, 0.75% Mn, 3.25% Cr, 1.40% Mo
0.50% C, 0.25% Si, 0.85% Mn, 1.30% Cr, 0.50% Mo, 1.65% Ni, 0.10% V
0.50% C, 0.25% Si, 0.90% Mn, 1.10% Cr, 0.12% V, + Pb
0.50% C, 0.25% Si, 0.90% Mn, 1.10% Cr, 0.25% Mo, 0.10% V
0.50% C, 0.30% Si, 0.40% Mn, 5.00% Cr, 1.90% Mo, 0.55% V, + Nb
0.50% C, 0.30% Si, 0.40% Mn, 5.00% Cr, 1.90% Mo, 0.55% V, +Nb
0.50% C, 0.30% Si, 0.40% Mn, 5.00% Cr, 1.90% Mo, 0.55% V, +Nb
0.50% C, 0.30% Si, 0.50% Mn, 1.00% Cr, 3.30% Ni
0.50% C, 0.30% Si, 0.50% Mn, 1.00% Cr, 3.30% Ni
0.50% C, 0.30% Si, 0.60% Mn, 3.30% Cr, 1.50% Mo, 0.25% V
0.50% C, 0.30% Si, 0.70% Mn, 3.25% Cr, 1.40% Mo, 0.25% V
0.50% C, 0.30% Si, 0.70% Mn, 3.25% Cr, 1.40% Mo
0.50% C, 0.30% Si, 0.70% Mn, 3.25% Cr, 1.40% Mo
0.50% C, 0.30% Si, 0.70% Mn, 3.35% Cr, 1.60% Mo, 0.25% V
0.50% C, 0.30% Si, 0.80% Mn, 3.30% Cr, 1.40% Mo
0.50% C, 0.35% Si, 0.70% Mn, 3.20% Cr, 1.40% Mo, 0.07% V
0.50% C, 0.50% Si, 0.50% Mn, 5.00% Cr, 2.20% Mo, 2.80% Ni, 0.70% V, +Ni
0.50% C, 0.50% Si, 0.70% Mn, 3.25% Cr, 1.50% Mo, 0.25% V
0.50% C, 0.75% Si, 0.30% Mn, 1.15% Cr, 0.20% V, 2.50% W
0.50% C, 0.85% Si, 0.30% Mn, 1.05% Cr, 0.15% V, 1.45% W
0.50% C, 0.86% Si, 0.47% Mn, 0.027% P, 0.015% S, 8.15% Cr, 0.16% Ni, 1.14% Mo, 0.12% V, 1.18% W, 0.11% Cu
0.50% C, 0.86% Si, 0.47% Mn, 0.027% P, 0.015% S, 8.15% Cr, 0.16% Ni, 1.14% Mo, 0.12% V, 1.18% W, 0.11% Cu
0.50% C, 0.90% Si, 0.50% Mn, 8.50% Cr, 1.20% Mo, 1.20% W
0.50% C, 0.90% Si, 0.80% Mn, 7.90% Cr, 1.50% Mo, 1.70% V
0.50% C, 0.90% Si, 0.80% Mn, 8.00% Cr, 1.50% Mo, 1.70%
0.50% C, 0.95% Si, 0.45% Mn, 8.00% Cr, 1.30% Mo, 0.45% V
0.50% C, 1.00% Si, 0.40% Mn, 0.50% Mo
0.50% C, 1.00% Si, 0.50% Mn, 8.00% Cr, 1.50% Mo, 0.50% V
0.50% C, 1.00% Si, 0.50% Mn, 8.00% Cr, 1.50% Mo, 0.50% V
0.50% C, 1.00% Si, 0.50% Mn, 8.00% Cr, 1.50% Mo, 0.60% V
0.50% C, 1.00% Si, 1.00% Mn, 14.50% Cr, 0.65% Mo, 0.15% V
0.50% C, 1.00% Si, 5.00% Cr, 1.40% Mo, 1.00% V
0.50% C, 1.05% Si, 0.35% Mn, 5.15% Cr, 1.55% Mo, 1.00% V, 1.50% Ni
0.50% C, 1.05% Si, 0.35% Mn, 5.15% Cr, 1.55% Mo, 1.50% Ni, 1.00% V
0.50% C, 1.05% Si, 0.45% Mn, 8.00% Cr, 1.50% Mo, 0.52% V
0.50% C, 1.10% Cr, 3.20% Ni
0.50% C, 1.20% Si, 0.35% Mn, 7.30% Cr, 1.50% Mo, 0.50% V
0.50% C, 1.20% Si, 0.35% Mn, 7.30% Cr, 1.50% Mo, 0.50% V
0.50% C, 1.40% Si, 0.70% Mn, 13.00% Cr, 13.00% Ni, 0.60% V, 2.40% W
0.50% C, 1.40% Si, 0.70% Mn, 13.00% Cr, 13.00% Ni, 0.60% V, 2.40% W
0.50% C, 1.60% Si, 0.80% Mn, 0.80% Cr, 0.25% Mo
0.50% C, 19.50% Cr, 2.00% Mo, 32.00% TiC, Fe is balance
0.50% C, 5.00% Cr, 1.30% Mo, 1.30% W, 0.40% V
0.50% C, 7.80% Cr, +Mo, +V
0.50% C, 7.80% Cr, 1.50% Mo, 1.50% V
0.50% C, 8.50% Cr, 1.20% Mo, 1.20% W
0.50% C, 8.50% Cr, 1.20% Mo, 1.20% W
0.50-0.56% C, 1.70-2.10% Si, 0.70-0.90% Mn, 0.30% Cr, 0.25-0.45% Mo
0.50-0.57% C, 0.15-0.30% Si, 0.40-0.50% Mn, 0.035% P, 0.035% S, 0.50-0.70% Cr, 2.50-3.00% Ni
0.50-0.57% C, 0.15-0.35% Si, 0.40-0.70% Mn, 0.025% P, 0.035% S
0.50-0.57% C, 0.15-0.35% Si, 0.40-0.70% Mn, 0.025% P, 0.035% S
0.50-0.57% C, 0.15-0.35% Si, 0.40-0.70% Mn, 0.025% P, 0.035% S
0.50-0.57% C, 0.15-0.35% Si, 0.40-0.70% Mn, 0.025% P, 0.035% S
0.50-0.57% C, 0.80-1.00% Si, 0.80-1.20% Mn, 0.035% P, 0.035% S
0.50-0.58% C, 0.15% Si, 0.30-0.50% Mn, 0.030% P, 0.030% S
0.50-0.60% C, 0.10-0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.010% S, 0.80-1.20% Cr, 0.35-0.55% Mo, 1.50-1.80% Ni, 0.05-0.15% V
0.50-0.60% C, 0.10-0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.005% S, 0.80-1.20% Cr, 0.35-0.55% Mo, 0.05-0.15% V, 1.50-1.80% Ni
0.50-0.60% C, 0.10-0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.005% S, 0.80-1.20% Cr, 0.35-0.55% Mo, 1.50-1.80% Ni, 0.05-0.15% V
0.50-0.60% C, 0.10-0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.005% S, 0.80-1.20% Cr, 0.35-0.55% Mo, 1.50-1.80% Ni, 0.05-0.15% V
0.50-0.60% C, 0.10-0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.005% S, 0.80-1.20% Cr, 0.35-0.55% Mo, 1.50-1.80% Ni, 0.05-0.15% V
0.50-0.60% C, 0.10-0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.010% S, 0.80-1.20% Cr, 0.35-0.55% Mo, 0.05-0.15% V, 1.50-1.80% Ni
0.50-0.60% C, 0.10-0.40% Si, 0.60-0.90% Mn, 0.030% P, 0.020% S, 0.80-1.20% Cr, 0.35-0.55% Mo, 1.50-1.80% Ni, 0.05-0.15% V
0.50-0.60% C, 0.10-0.40% Si, 0.60-0.90% Mn, 0.030% P, 0.020% S, 0.80-1.20% Cr, 0.35-0.55% Mo, 1.50-1.80% Ni, 0.05-0.15% V
0.50-0.60% C, 0.10-0.40% Si, 0.60-0.90% Mn, 0.030% P, 0.030% S, 0.80-1.20% Cr, 0.35-0.55% Mo, 1.50-1.80% Ni, 0.05-0.15% V
0.50-0.60% C, 0.10-0.40% Si, 0.60-0.90% Mn, 0.030% P, 0.030% S, 0.80-1.20% Cr, 0.35-0.55% Mo, 1.50-1.80% Ni, 0.05-0.15% V
0.50-0.60% C, 0.10-0.40% Si, 0.65-0.95% Mn, 0.030% P, 0.030% S, 0.60-0.80% Cr, 0.25-0.35% Mo, 1.50-1.80% Ni, 0.070-0.12% V
0.50-0.60% C, 0.10-0.40% Si, 0.65-0.95% Mn, 1.00-1.20% Cr, 0.45-0.55% Mo, 1.50-1.80% Ni, 0.07-0.12% V
0.50-0.60% C, 0.10-0.40% Si, 0.65-0.95% Mn, 1.00-1.20% Cr, 0.56-0.65% Mo, 1.50-1.80% Ni, 0.07-0.12% V
0.50-0.60% C, 0.15-0.35% Si, 0.50-0.80% Mn, 0.025% P, 0.025% S, 0.60-0.80% Cr, 0.25-0.35% Mo, 1.50-1.80% Ni, 0.070-0.12% V
0.50-0.60% C, 0.15-0.35% Si, 0.50-0.80% Mn, 0.025% P, 0.025% S, 0.60-0.80% Cr, 0.25-0.35% Mo, 1.50-1.80% Ni, 0.07-0.12% V
0.50-0.60% C, 0.15-0.35% Si, 0.50-0.80% Mn, 0.025% P, 0.025% S, 0.60-0.80% Cr, 0.50-0.35% Mo, 1.50-1.80% Ni, 0.07-0.12% V
0.50-0.60% C, 0.15-0.35% Si, 0.60-0.80% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.70-0.90% Mo, 1.50-1.80% Ni, 0.07-0.12% V
0.50-0.60% C, 0.15-0.35% Si, 0.60-0.90% Mn, 0.85-1.15% Cr, 0.30-0.55% Mo, 0.07-0.12% V, 1.50-1.80% Ni
0.50-0.60% C, 0.15-0.35% Si, 0.60-0.90% Mn, 0.85-1.15% Cr, 0.30-0.55% Mo, 1.50-1.80% Ni, 0.07-0.12% V
0.50-0.60% C, 0.20-0.60% Si, 1.00-1.25% Mn, 0.025% P, 0.08-0.025% S, 0.15% Cr, 0.02% Mo, 0.10% Ni, 0.030% V, 0.004% Al
0.50-0.60% C, 0.20-0.60% Si, 1.00-1.25% Mn, 0.025% P, 0.08-0.025% S, 0.15% Cr, 0.02% Mo, 0.10% Ni, 0.030% V, 0.004% Al
0.50-0.65 C, 1.70-2.10% Si, 0.70-0.90% Mn, 0.030% P, 0.030% S, 0.30% Cr, 0.25-0.45% Mo
0.50-0.65% C, 1.75-2.25% Si, 0.60-1.00% Mn, 0.10-0.50% Cr, 0.15-0.35% V
0.50% C, 0.20% Si, 0.20% Mn, 4.50% Cr, 3.00% Mo, 0.55% V
0.50-0.57% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S
0.50-0.57% C, 0.80-1.00% Si, 0.80-1.20% Mn, 0.035% P, 0.035% S
0.51% C, 0.90% Si, 0.46% Mn, 0.023% P, 0.004% S, 8.31% Cr, 1.16% Mo, 0.18% Ni, 0.05% V, 0.06% Cu, 1.19% W
0.51% C, 0.90% Si, 0.46% Mn, 0.023% P, 0.004% S, 8.31% Cr, 1.16% Mo, 0.18% Ni, 0.05% V, 0.06% Cu, 1.19% W
0.51% C, 0.90% Si, 0.46% Mn, 0.023% P, 0.004% S, 8.31% Cr, 1.16% Mo, 0.18% Ni, 0.05% V
0.51% C, 0.90% Si, 0.46% Mn, 8.31% Cr, 1.61% Mo, 0.18% Ni, 0.50% V, 1.19% W
0.51% C, 0.95% Si, 0.30% Mn, 5.00% Cr, 1.40% Mo, 1.40% V
0.51% C, 1.10% Cr, 0.20% V
0.51% C, 1.10% Cr, 0.20% V
0.51% C, 1.40% Si, 0.70% Mn, 4.00% Cr, 0.60% Mo, 11.50% Ni, 1.10% V, 1.50% Co, 12.00% W
0.51-0.59% C, 1.20-1.60% Si, 0.50-0.80% Mn, 0.025% P, 0.025% S, 0.50-0.80% Cr
0.52% C, 0.20% Si, 0.70% Mn, 0.020% P, 0.002% S, 0.75% Cr, 0.30% Mo, 1.75% Ni, 0.10% V
0.52% C, 0.25% Si, 0.80% Mn, 0.025% P, 0.004% S, 1.10% Cr, 0.45% Mo, 1.70% Ni, 0.10% V
0.52% C, 0.80% Si, 1.30% Cr, 2.15% W, 0.15% V
0.52% C, 0.85% Si, 0.30% Mn, 5.05% Cr, 1.35% Mo, 0.90% V
0.52% C, 0.93% Mn
0.52% C, 0.95% Si, 0.40% Mn, 8.00% Cr, 1.40% Mo, 0.45% V
0.52-0.50% C, 0.40% Si, 0.60-0.90% Mn, 0.030% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.52-0.50% C, 0.40% Si, 0.60-0.90% Mn, 0.030% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.52-0.59% C, 0.40% Si, 0.70-1.00% Mn, 0.025% P, 0.025% S, 0.70-1.00% Cr
0.52-0.60% C, 0.15-0.35% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.52-0.60% C, 0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.010% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni = 0.63
0.52-0.60% C, 0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.010% S
0.52-0.60% C, 0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.015% S, 0.30% Cu, 0.050% Al
0.52-0.60% C, 0.40% Si, 0.60-0.90% Mn, 0.030% P, 0.020-0.040% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.52-0.60% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.52-0.60% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.52-0.60% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.52-0.60% C, 0.40% Si, 0.60-0.90% Mn, 0.045% P, 0.045% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.52-0.60% C, 1.60-1.20% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S
0.52-0.60% C, 1.60-1.20% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S
0.52-0.60% C, 1.60-2.00% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.52-0.60% C, 1.60-2.00% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.52-0.60% C, 0.40% Si, 0.60-0.0% Mn, 0.045% P, 0.045% S
0.53% C, 0.25% Si, 0.25% Mn, 1.35% Cr, 0.25% V, 2.00% W
0.53% C, 0.25% Si, 0.25% Mn, 1.35% Cr, 0.25% V, 2.00% W
0.53% C, 0.25% Si, 0.40% Mn, 4.00% Cr, 2.00% Mo, 1.10% V, 0.90% Co, 1.50% W, +Nb
0.53% C, 0.30% Si, 0.70% Mn, 3.20% Cr, 1.50% Mo, 0.005% S, 0.00% W
0.53% C, 0.30% Si, 0.70% Mn, max 0.005% S, 3.20% Cr, 1.50% Mo
0.53% C, 0.35% Si, 0.40% Mn, 4.00% Cr, 2.00% Mo, 1.10% V, 1.50% W, 0.90% Co, + Nb
0.53% C, 0.50% Si, 0.30% Mn, 7.50% Cr, 1.60% Mo, 1.50% W
0.53% C, 0.25% Si, 0.55% Mn
0.54% C, 0.25% Si, 0.80% Mn, 0.025% P, 0.004% S, 1.10% Cr, 0.50% Mo, 1.70% Ni, 0.10% V
0.54% C, 0.25% Si, 0.80% Mn, 0.025% P, 0.010% S, 0.75% Cr, 0.30% Mo, 1.70% Ni, 0.10% V
0.54% C, 0.45% Si, 0.40% Mn, 17.30% Cr, 1.10% Mo, 0.10% V, +N
0.54% C, 0.45% Si, 0.40% Mn, 17.30% Cr, 1.10% Mo, 0.10% V
0.54% C, 0.45% Si, 0.40% Mn, 17.30% Cr, 1.10% Mo, 0.10% V
0.55% C, 0.30% Si, 0.80% Mn, 1.10% Cr, 0.50% Mo, 0.10% V, 1.70% Ni
0.55% C, 0.25% Si, 0.25% Mn, 2.00% W, 1.35% Cr, 0.28% V, 0.10% Mo
0.55% C, 0.25% Si, 0.45% Mn, 0.60% Cr, 2.80% Ni
0.55% C, 0.25% Si, 0.45% Mn, 1.00% Cr, 3.10% Ni
0.55% C, 0.25% Si, 0.45% Mn, 1.00% Cr, 3.10% Ni
0.55% C, 0.25% Si, 0.70% Mn, 0.70% Cr, 0.30% Mo, 1.70% Ni, 0.10% V
0.55% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.50% Mo, 1.70% Ni, 0.10% V
0.55% C, 0.25% Si, 0.75% Mn, 0.020-0.035% S, + Pb
0.55% C, 0.25% Si, 0.75% Mn, 1.00% Cr, 0.50% Mo, 0.10% V, 1.65% Ni
0.55% C, 0.25% Si, 0.75% Mn, 1.10% Cr, 0.50% Mo, 1.70% Ni, 0.10% V,
0.55% C, 0.25% Si, 0.95% Mn, 0.001% S, 1.10% Cr, 2.00% Ni, 0.75% Mo + additions
0.55% C, 0.25% Si, 0.95% Mn, 0.015% P,; 0.005% S, 1.10% Cr, 0.75% Mo, 2.00% Ni, 0.10% V
0.55% C, 0.25% Si, 1.00% Mn, 1.10% Cr, 0.80% Mo, 2.00% Ni, 0.10% V
0.55% C, 0.30% Si, 0.40% Mn, 1.00% Cr, 0.25% Mo, 3.00% Ni
0.55% C, 0.30% Si, 0.40% Mn, 1.00% Cr, 0.25% Mo, 3.00% Ni
0.55% C, 0.30% Si, 0.50% Mn, 1.00% Cr, 3.00% Ni, 0.30% Mo
0.55% C, 0.30% Si, 0.70% Mn, 1.10% Cr, 0.80% Mo, 0.10% V, 1.70% Ni
0.55% C, 0.30% Si, 0.70% Mn, 1.10% Cr, 0.80% Mo, 1.70% Ni, 0.10% V
0.55% C, 0.30% Si, 0.70% Mn, 1.10% Cr, 0.50% Mo, 0.10% V, 1.70% Ni
0.55% C, 0.30% Si, 0.70% Mn, 1.10% Cr, 0.50% Mo, 1.70% Ni, 0.10% V
0.55% C, 0.30% Si, 0.70% Mn, 1.70% Ni, 1.10% Cr, 0.40% Mo, 0.10% V
0.55% C, 0.30% Si, 0.80% Mn, 1.10% Cr, 0.50% Mo, 0.10% V, 1.70% Ni
0.55% C, 0.30% Si, 0.80% Mn, 1.10% Cr, 0.50% Mo, 1.70% Ni, 0.10% V
0.55% C, 0.30% Si, 0.90% Mn, 0.020% P, 0.005% S, 1.10% Cr, 0.50% Mo, 1.70% Ni, 0.10% V
0.55% C, 0.35% Si, 0.70% Mn, 0.00% P, 3.25% Cr, 1.40% Mo, 0.25% V
0.55% C, 0.35% Si, 0.70% Mn, 3.25% Cr, 1.40% Mo, 0.25% V
0.55% C, 0.50% Si, 0.40% Mn, 4.00% Cr, 4.25% Mo, 1.00% V, 0.50% Ni, 0.010% S
0.55% C, 0.50% Si, 0.60% Mn, 1.00% Cr, 0.80% Mo, 1.55% Ni, 0.05% V
0.55% C, 0.60% Si, 1.90% Mn, 0.025% P, 0.025% S, min. 0.025% Al
0.55% C, 0.95% Si, 0.30% Mn, 5.00% Cr, 1.25% Mo, 1.25% W
0.55% C, 0.95% Si, 0.30% Mn, 5.00% Cr, 1.25% Mo, 1.25% W
0.55% C, 0.95% Si, 0.30% Mn, 5.00% Cr, 1.25% W, 1.25% Mo
0.55% C, 1.00% Si, 0.75% Mn, 2.60% Cr, 2.25% Mo, 0.85% V
0.55% C, 1.00% Si, 0.90% Mn, 0.40% Cr, 0.45% Mo, 0.13% V, 2.70% Ni
0.55% C, 1.00% Si, 0.90% Mn, 0.40% Cr, 0.13% V, 0.45% Mo, 2.70% Ni
0.55% C, 1.10% Cr, 0.50% Mo, 1.70% Ni, 0.10% V
0.55% C, 1.10% Cr, 0.50% Mo, 1.70% Ni, 0.10% V
0.55% C, 1.10% Cr, 1.70% Ni, 0.50% Mo, 0.10% V
0.55% C, 1.40% Si, 0.70% Mn, 1.50% Cr, 0.60% Mo, 1.10% V, 12.00% W, 11.50% Ni
0.55% C, 1.90% Si, 0.80% Mn, 0.25% Cr, 0.40% Mo
0.55% C, 4.50% Cr, 1.00% V, 2.15% W, 2.75% Mo
0.55% C, l.0% Cr, 0.30% Mo, 3.0% Ni
0.55-0.60% C, 0.30-0.50% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 1.00-1.30% Cr, 0.30-0.40% Mo, 2.70-3.00% Ni, 0.07-0.12% V
0.55-0.62% C, 0.15-0.35% Si, 0.80-1.10% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.07-0.12% V
0.55-0.62% C, 0.15-0.35% Si, 0.80-1.10% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.07-0.12% V
0.55-0.62% C, 0.15-0.40% Si, 0.70-1.10% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.10-0.20% V
0.55-0.62% C, 0.15-0.40% Si, 0.70-1.10% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.10-0.20% V
0.55-0.62% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.55-0.63% C, 1.70-2.00% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.35-0.45% Cr
0.55-0.65% C, 0.15-0.40% Si, 0.60-0.80% Mn, 0.035% P, 0.035% S
0.55-0.65% C, 0.15-0.70% Si, 0.15-0.45% Mn, 0.90-1.20% Cr, 0.10-0.20% V, 1.80-2.10% W
0.55-0.65% C, 0.20-0.40% Si, 0.20-0.40% Mn, 0.035% P, 0.035% S, 3.70-4.20% Cr, 0.80-1.00% Mo, 8.50-9.50% W, 0.60-0.80% V
0.55-0.65% C, 0.70-1.00% Si, 0.15-0.45% Mn, 0.030% P, 0.030% S, 0.90-1.20% Cr, 0.10-0.20% V, 1.70-2.20% W
0.55-0.65% C, 0.70-1.00% Si, 0.15-0.45% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 1.70-2.20% Mo, 0.10-0.20% V
0.55-0.65% C, 0.70-1.00% Si, 0.15-0.45% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 1.70-2.20% Mo, 0.10-0.20% V
0.55-0.62% C, 0.15-0.35% Si, 0.80-1.10% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.07-0.12% V
0.55-0.66% C, 1.50-1.80% Si, 0.70-1.00% Mn, 0.035% P, 0.035% S, 0.20-0.40% Cr
0.56% C, 0.17% Si, 0.72% Mn, 0.010% P, 0.005% S, 0.69% Cr, 0.20% Mo, 1.68% Ni, 0.20% Cu
0.56% C, 0.17% Si, 0.72% Mn, 0.010% P, 0.005% S, 0.69% Cr. 1.68% Ni, 0.20% Mo, 0.20% Cu
0.56% C, 0.25% Si, 0.70% Mn, 0.025% P, 0.003% S, 1.10% Cr, 0.80% Mo, 1.70% Ni, 0.10% V
0.56% C, 0.40% Si, 0.75% Mn, 0.10% Mo, 0.40% Ni, (Cr+Mo+Ni) = 0.63
0.56% C, 0.40% Si, 0.75% Mn, 0.10% Mo, 0.40% Ni, (Cr+Mo+Ni) = 0.63
0.56% C, 1.00% Si, 0.40% Mn, 5.20% Cr, 1.30% Mo, 0.30% V, 1.40% W
0.56% C, 1.10% Cr, 0.50% Mo, 1.70% Ni, 0.10% V
0.56% C, 1.10% Cr, 0.50% Mo, 1.70% Ni, 0.10% V
0.56% C, 1.10% Cr, 0.50% Mo, 1.70% Ni, 0.10% V
0.56% C, 1.10% Cr, 0.50% Mo, 1.70% Ni, 0.10% V
0.56% C, 1.10% Cr, 0.50% Mo, 1.70% Ni, 0.10% V
0.56% C, 1.10% Cr, 0.50% Mo, 1.70% Ni, 0.10% V
0.56% C, 1.45% Si, 0.70% Mn, 0.010% P, 0.010% S, 0.65% Cr, 0.16% V
0.56% C, 0.40% Si, 0.75% Mn, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.57% C, 0.30% Si, 0.85% Mn, 0.80% Cr
0.57% C, 1.00% Si, 0.40% Mn, 5.25% Cr, 1.35% Mo, 1.00% V
0.57% C, 2.00% Si, 0.80% Mn, 0.30% Cr, 0.78% Mo, 0.25% V
0.57-0.64% C, 1.60-2.00% Si, 0.70-1.00% Mn, 0.025% P, 0.025% S, 0.20-0.45% Cr
0.57-0.64% C, 1.70-2.20% Si, 0.70-1.00% Mn, 0.035% P, 0.035% S, 0.25-0.40% Cr
0.57-0.64% C, 1.70-2.20% Si, 0.70-1.00% Mn, 0.035% P, 0.035% S, 0.25-0.40% Cr
0.57-0.65% C, 0.15-0.35% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.57-0.65% C, 0.40% Si, 0.60-0.90% Mn, 0.030% P, 0.020-0.040% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.57-0.65% C, 0.40% Si, 0.60-0.90% Mn, 0.030% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.57-0.65% C, 0.40% Si, 0.60-0.90% Mn, 0.030% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.57-0.65% C, 0.40% Si, 0.60-0.90% Mn, 0.030% P, 0.035% S, 0.40% Cr, 0.40% Ni
0.57-0.65% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.57-0.65% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.57-0.65% C, 0.40% Si, 0.60-0.90% Mn, 0.045% P, 0.040% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.57-0.65% C, 0.40% Si, 0.60-0.90% Mn, 0.045% P, 0.045% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.57-0.65% C, 0.70-1.00% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 1.00-1.30% Cr, 0.07-0.12% V
0.57-0.65% C, 1.50-1.80% Si, 0.70-1.00% Mn, 0.030% P, 0.030% S, 0.20-0.40% Cr
0.57-0.65% C, 0.40% Si, 0.60-0.90% Mn, 0.030% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.57-0.65% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.020-0.035% S
0.57-0.65% C, 0.40% Si, 0.60-0.90% Mn, 0.045% P, 0.045% S
0.58% C, 0.25% Si, 0.25% Mn, 4.00% Cr, 0.90% Mo, 0.80% V, 9.00% W
0.58% C, 0.25% Si, 0.25% Mn, 4.00% Cr, 0.90% Mo, 0.80% V, 9.00% W
0.58% C, 0.25% Si, 0.35% Mn, 4.00% Cr, 0.90% Mo, 0.80% V, 9.00% W
0.58% C, 0.25% Si, 0.95% Mn, 1.10% Cr, 0.12% V, + Pb
0.58% C, 0.30% Si, 0.45% Mn, 0.001% S, 0.010% P, 15.00% Cr, 0.50% Mo, 0.17% N2
0.58% C, 0.40% Si, 0.65% Mn, 1.15% Cr, 0.35% Mo, 0.10% V, 2.85% Ni
0.58% C, 0.90% Si, 0.40% Mn, 1.00% Cr, 0.10% V, 2.10% W
0.58% C, 0.90% Si, 1.00% Mn
0.58% C, 1.02% Si, 0.39% Mn, 0.015% P, 0.005% S, 5.16% Cr, 1.05% Mo, 0.11% Ni, 0.27% V, 0.09% Cu
0.58% C, 1.11% Si, 0.50% Mn, 0.018% P, 0.004% S, 7.87% Cr, 1.28% Mo, 0.11% Ni, 0.73% V, 0.09% Cu, 1.17% W, 0.013% Al
0.58-0.62% C, 0.20-0.50% Si, 0.70-0.90% Mn, 0.030% P, 0.030% S, 4.30-4.70% Cr, 0.20-0.30% V, 0.40-0.60% Mo
0.58-0.65% C, 0.80-1.00% Si, 0.80-1.20% Mn, 0.030% P, 0.030% S, 0.20-0.40% Cr
0.58-0.68% C, 0.90-1.20% Si, 0.90-1.20% Mn, 0.030% P, 0.030% S, 0.40-0.70% Cr
0.59% C, 0.90% Mn, 1.00% Cr, 0.10% V
0.60% C, 0.35% Si, 0.80% Mn, 4.50% Cr, 0.50% Mo, 0.20% V
0.60% C, 0.35% Si, 0.80% Mn, 4.50% Cr, 0.50% Mo, 0.20% V
0.60% C, 0.35% Si, 0.80% Mn, 4.50% Cr, 0.50% Mo, 0.20% V
0.60% C, 0.35% Si, 0.80% Mn, 4.50% Cr, 0.50% Mo, 0.20% V
0.60% C, 0.35% Si, 0.80% Mn, 4.50% Cr, 0.50% Mo, 0.20% V
0.60% C, 0.50% Si, 1.20% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.08% Mo, 0.30% Ni, 0.020% Al, 0.012% N
0.60% C, 0.50% Si, 1.20% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.08% Mo, 0.30% Ni, 0.020% Al, 0.012% N
0.60% C, 0.60% Si, 0.30% Mn, 0.025% P, 0.010% S, 1.10% Cr, 0.60% Mo, 0.15% V, 2.00% W
0.60% C, 0.60% Si, 0.30% Mn, 1.10% Cr, 0.15% V, 2.00% W
0.60% C, 0.60% Si, 0.35% Mn, 1.10% Cr, 0.20% V, 2.00% W
0.60% C, 0.60% Si, 0.35% Mn, 1.10% Cr, 0.20% V, 2.00% W
0.60% C, 0.60% Si, 1.10% Cr, 0.20% V, 2.00% W
0.60% C, 0.60% Si, 1.10% Cr, 0.20% V, 2.00% W
0.60% C, 0.60% Si, 1.10% Cr, 0.20% V, 2.00% W
0.60% C, 0.75% Si, 0.30% Mn, 1.10% Cr, 0.15% C, 2.00% W
0.60% C, 0.80% Cr, 0.35% Mo, 0.15% V, 2.70% Ni
0.60% C, 0.85% Si, 0.30% Mn, 1.05% Cr, 0.15% V, 1.45% W
0.60% C, 0.90% Si, 0.80% Mn, 1.10% Cr, 0.10% V
0.60% C, 0.90% Si, 1.00% Mn, 0.30% Cr
0.60% C, 1.0% Si, 0.3% Mn, 4.0% Cr, 2.0% Mo, 1.5% V, 2.1% W
0.60% C, 1.00% Cr, 0.15% V, 2.00% W
0.60% C, 1.00% Cr, 0.15% V, 2.00% W
0.60% C, 1.00% Cr, 2.00% W, 0.15% V
0.60% C, 1.00% Si, 0.30% Mn, 4.00% Cr, 2.00% Mo, 1.50% V, 2.10% W
0.60% C, 1.00% Si, 1.10% Mn, 0.30% Cr
0.60% C, 1.00% Si, 1.10% Mn, 0.30% Cr
0.60% C, 1.50% Si, 0.40% Mn, 4.30% Cr, 2.90% Mo, 1.80% V
0.60% C, 1.90% Si, 0.90% Mn, 0.18% Cr, 0.35% Mo, 0.28% V
0.60% C, 1.90% Si, 0.90% Mn, 0.18% Cr, 0.35% Mo, 0.28% V
0.60% C, 1.90% Si, 0.90% Mn, 0.18% Cr, 0.28% V, 1.28% Mo
0.60% C, 2.00% Si, 0.85% Mn, 0.25% Cr, 0.25% Mo, 0.20% V
0.60% C, 4.50% Cr, 0.50% Mo, 0.20% V
0.60% C, 4.50% Cr, 0.50% Mo, 0.20% V
0.60% C, 5.00% Cr, + Mo, + V
0.60% C, 5.00% Cr, +Mo, +V
0.60-0.65% C, 0.20-0.40% Si, 0.40-0.60% Mn, 0.030% P, 0.030% S, 1.30-1.50% Cr, 0.25-0.30% Mo, 0.07-0.12% V
0.60-0.65% C, 1.00-1.20% Si, 0.30-0.50% Mn, 0.030% P, 0.030% S, 5.00-5.50% Cr, 0.90-1.20% Mo, 0.15-0.35% V
0.60-0.65% C, 1.00-1.20% Si, 0.30-0.50% Mn, 0.030% P, 0.030% S, 5.00-5.50% Cr, 0.90-1.20% Mo, 0.15-0.35% V
0.60-0.65% C, 1.00-1.20% Si, 0.30-0.50% Mn, 0.030% P, 0.030% S, 5.00-5.50% Cr, 1.00-1.30% Mo, 0.25-0.35% V
0.60-0.70% C, 0.30-0.50% Si, 0.40-0.60% Mn, 0.025% P, 0.025% S, 13.50-14.50% Cr, 0.50-0.70% Mo
0.60-0.70% C, 1.50-1.80% Si, 0.70-1.00% Mn, 0.035% P, 0.035% S
0.60-0.75% C, 0.70% Si, 1.00% Mn, 0.030% P, 0.015% S, 14.00-16.00% Cr, 0.40-0.80% Mo
0.60-0.80% C, 0.50-1.10% Si, 0.80-1.20% Mn, 0.020% P, 0.008-0.025% S, 0.80-1.20% Cr, 0.02% Mo, 0.10% Ni, 0.18% V, 0.025% Ti, 0.15% Cu, 0.004% Al, 0.010% Nb
0.60-0.70% C, 1.50-1.80% Si, 0.70-1.00% Mn, 0.035% P, 0.035% S
0.61% C, 0.40% Si, 0.75% Mn, 0.10% Mo, 0.40% Ni, (Cr+Mo+Ni) = 0.63
0.61% C, 0.40% Si, 0.75% Mn, 0.10% Mo, 0.40% Ni, (Cr+Mo+Ni) = 0.63
0.61% C, 0.92% Si, 0.91% Mn, 0.021% P, 0.004% S, 4.90% Cr, 2.20% Mo, 0.19% Ni, 0.46% V, 0.12% Cu
0.61% C, 0.92% Si, 0.91% Mn, 4.90% Cr, 2.20% Mo, 0.19% Ni, 0.46% V, 0.12% Cu
0.62-0.72% C, 1.20-1.40% Si, 0.40-0.60% Mn, 0.035% P, 0.035% S, 0.40-0.60% Cr
0.63% C, 0.34% Si, 0.73% Mn, 0.022% P, 0.002% S, 12.70% Cr, 0.02% Mo
0.63% C, 0.60% Si, 0.30% Mn, 1.10% Cr, 0.18% V, 2.00% W
0.63% C, 0.605 Si, 0.30% Mn, 1.10% Cr, 0.18% V, 2.00% W
0.63% C, 0.80% Si, 1.10% Mn, 0.30% Cr
0.63% C, 0.80% Si, 1.10% Mn, 0.30% Cr
0.63% C, 0.80% Si, 1.10% Mn, 0.30% Cr
0.63% C, 1.10% Si, 0.40% Mn, 5.25% Cr, 1.00% Mo, 0.30% Ni
0.63% C, 1.10% Si, 1.10% Mn, 0.60% Cr
0.63-0.70% C, 1.40-1.60% Si, 1.35-1.55% Mn, 0.025% P, 0.002% S, 1.00-1.20% Cr, 0.23-0.27% Mo, 0.25% Ni
0.64-0.72% C, 0.15-0.40% Si, 0.60-0.80% Mn, 0.035% P, 0.035% S
0.65% C, 0.19% Si, 1.92% Cr, 2.90% Mo, +V, +W
0.65% C, 0.25% Si, 0.75% Mn, 0.020-0.035% S, + Pb
0.65% C, 0.30% Mn, 0.15% Cr, 0.35% Mo, 0.30% Ni
0.65% C, 0.30% Si, 0.65% Mn, 3.05% Cr, 0.50% Mo, 0.13% V
0.65% C, 0.40% Si, 1.10% Mn, 0.025% P, 0.010% S, 0.70% Cr, 0.25% Mo
0.65% C, 1.10% Si, 0.40% Mn, 5.20% Cr, 1.40% Mo, 0.50% V
0.65% C, 1.10% Si, 0.40% Mn, 5.25% Cr, 1.35% Mo, 0.55% V
0.65% C, 1.10% Si, 1.10% Mn, 0.70% Cr
0.65% C, 1.75% Si, 0.80% Mn
0.65% C, 1.75% Si, 0.80% Mn
0.65% C, 2.00% Cr, +Mo, +V, +W
0.65% C, 3.00% Cr, 3.00% Mo, 33.00% TiC, Fe is balance
0.65% C, 4.00% Cr, 4.60% Mo, 1.80% V, 5.80% W
0.65-0.65% C, 0.70-1.00% Si, 0.15-0.45% Mn, 0.030% P, 0.030% S, 0.90-1.20% Cr, 0.10-0.20% V, 1.70-2.20% W
0.65-0.70% C, 1.45-1.60% Si, 1.35-1.55% Mn, 0.025% P, 0.002% S, 1.00-2.00% Cr, 0.23-0.27% Mo, 0.25% Ni, 8 ppm O, 30 ppm Ti
0.65-0.70% C, 1.45-1.60% Si, 1.35-1.55% Mn, 0.025% P, 0.015% S, 1.00-2.00% Cr, 0.23-0.27% Mo, 0.25% Ni, 9 ppm O, 30 ppm Ti
0.65-0.70% C, 1.45-1.60% Si, 1.35-1.55% Mn, 0.025% P, 0.002% S, 1.00-1.20% Cr, 0.23-0.27% Mo, 0.25% Ni, 8 ppm O, 30 ppm Ti
0.65-0.72% C, 0.20% Si, 0.70-1.00% Mn, 0.035% P, 0.15-0.25% S, 0.15-0.25% Pb
0.65-0.75% C, 0.10-0.50% Si, 1.80-2.50% Mn, 0.030% P, 0.030% S, 0.90-1.20% Cr, 0.90-1.40% Mo
0.65-0.75% C, 0.10-0.70% Si, 1.80-2.50% Mn, 0.90-1.40% Cr, 0.90-1.40% Mo
0.65-0.75% C, 0.15-0.30% Si, 0.10-0.40% Mn, 0.030% P, 0.030% S
0.65-0.75% C, 0.15-0.30% Si, 0.10-0.40% Mn, 0.030% P, 0.030% S
0.65-0.75% C, 0.15-0.30% Si, 0.10-0.40% Mn, 0.030% P, 0.030% S
0.65-0.75% C, 0.15-0.30% Si, 0.10-0.40% Mn, 0.030% P, 0.030% S
0.65-0.75% C, 0.15-0.30% Si, 0.10-0.40% Mn, 0.030% P, 0.030% S
0.65-0.75% C, 0.15-0.30% Si, 0.10-0.40% Mn, 0.030% P, 0.030% S
0.65-0.75% C, 0.15-0.30% Si, 0.70% Mn, 0.030% P, 0.030% S
0.65-0.75% C, 0.15-0.35% Si, 0.20-1.10% Mn, 0.025% P, 0.035% S
0.65-0.75% C, 0.15-0.35% Si, 0.20-1.10% Mn, 0.025% P, 0.035% S
0.65-0.75% C, 0.40% Si, 0.60-1.10% Mn, 0.035% P, 0.035% S
0.65-0.75% C, 0.40% Si, 0.60-1.10% Mn, 0.035% P, 0.035% S
0.65-0.75% C, 0.50% Si, 0.25-0.80% Mn, 0.030% P, 0.030% S, 0.60-1.20% Cr, 1.25-2.00% Ni, 0.20-0.30% V
0.65-0.75% C, 0.85-1.15% Si, 0.65-1.05% Mn, 0.030% P, 0.030% S, 0.90-1.20% Cr, 0.20-0.50% Mo, 0.15-0.30% V
0.65-0.75% C, 1.50-1.80% Si, 0.60-0.80% Mn, 0.030% P, 0.030% S
0.65-0.80% C, 0.20-0.40% Si, 0.10-0.40% Mn, 3.75-4.50% Cr, 0.90-1.30% V, 17.25-18.75% W
0.67% C, 1.10% Si, 0.36% Mn, 0.019% P, 0.003% S, 5.47% Cr, 1.24% Mo, 0.55% V
0.68-0.72% C, 0.10-0.30% Si, 0.50-0.70% Mn, 0.020% P, 0.025% S, 0.10% Cr, 0.03% Mo, 0.10% Ni
0.68-0.73% C, 0.10-0.30% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 0.15% Cr, 0.05% Mo, 0.20% Ni
0.68-0.75% C, 0.15-0.35% Si, 0.20-0.35% Mn, 0.025% P, 0.035% S
0.68-0.75% C, 0.15-0.35% Si, 0.20-0.35% Mn, 0.025% P, 0.035% S
0.68-0.75% C, 1.50-1.80% Si, 0.60-0.80% Mn, 0.035% P, 0.035% S
0.68-0.77% C, 0.90-1.10% Si, 0.40-0.60% Mn, 0.025% P, 0.030% S, 0.60-0.80% Cr
0.68-0.78% C, 0.20-0.40% Si, 0.40-0.60% Mn, 0.035% P, 0.035% S, 0.40-0.60% Cr, 0.25-0.40% Mo, 0.40-0.70% W, 0.15-0.30% V
0.68-0.75% C, 0.15-0.35% Si, 0.20-0.35% Mn, 0.025% P, 0.035% S
0.70% C, 0.20% Si, 0.25% Mn
0.70% C, 0.20% Si, 0.50% Mn, 5.00% Cr, 2.30% Mo, 0.50% V
0.70% C, 0.20% Si, 0.50% Mn, 5.00% Cr, 2.30% Mo, 0.50% V
0.70% C, 0.25% Si, 0.25% Mn
0.70% C, 0.25% Si, 0.60% Mn, 0.70% Cr, 1.40% Ni
0.70% C, 0.25% Si, 0.60% Mn, 0.70% Cr, 1.40% Ni
0.70% C, 0.30% Si, 2.00% Mn, 1.00% Cr, 1.25% Mo
0.70% C, 0.30% Si, 2.00% Mn, 1.00% Cr, 1.25% Mo
0.70% C, 1.00% Si, 0.40% Mn, 8.25% Cr, 1.40% Mo, 1.50% Ni, 1.00% V, 0.09% N
0.70% C, 7.50% Cr, 2.00% Mo, 1.50% Ni, 1.00% V
0.70% C, 8.50% Cr, 1.40% Mo, 1.00% V, 1.50% Ni
0.70-0.77% C, 1.00-1.30% Si, 0.40-0.60% Mn, 0.025% P, 0.025% S, 0.45-0.65% Mo, 0.15-0.25% V
0.70-0.80% C, 0.15-0.30% Si, 0.15-0.35% Mn, 0.035% P, 0.035% S, 1.40-1.60% Cr, 0.60-0.80% Mo, 0.40-0.60% Ni, 0.20-0.40% W
0.70-0.80% C, 0.15-0.35% Si, 0.60-0.80% Mn, 0.045% P, 0.045% S
0.70-0.80% C, 0.15-0.35% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.70-0.80% C, 0.25-0.50% Si, 0.60-0.80% Mn, 0.030% P, 0.030% S, 0.30-0.40% Cr
0.70-0.80% C, 0.40% Si, 0.40% Mn, 0.025% P, 0.015% S, 3.90-4.30% Cr, 0.60% Mo, 17.50-19.00% W, 1.00-1.20% V, 0.30% Cu
0.70-1.50% C, 0.10-0.40% Si, 0.10-0.40% Mn, 0.15% Cr, 0.10% Mo, 0.10% V, 0.15% W
0.71% C, 1.37% Si, 0.49% Mn, 0.57% Cr, 0.58% Mo, 1.15% Ni, 0.18% V, 0.05% Co, 0.04% Cu, 0.010% Al
0.72% C, 0.39% Si, 0.27% Mn, 4.09% Cr, 1.25% V, 18.59% W
0.72% C, 1.20% Si, 0.50% Mn, 0.025% P, 0.025% S, 0.60-0.90% Cr, 0.60-0.90% Mo, 1.20% Ni, 0.20% V
0.72% C, 4.0% Cr, 5.0% Mo, 1.0% V, 1.0% W, 8.0% Co
0.72-0.80% C, 0.15-0.58% Si, 0.70-1.20% Mn, 0.020% P, 0.08-0.025% S, 0.15% Cr, 0.02% Mo, 0.10% Ni, 0.030% V, 0.004% Al
0.72-0.82% C, 0.15-0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S
0.73% C, 1.20% Si, 0.50% Mn, 0.55% Mo, 0.20% V
0.73% C, 1.20% Si, 0.50% Mn, 0.55% Mo, 0.20% V
0.73-0.83% C, 0.45% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.80-4.50% Cr, 17.20-18.70% W, 1.00-1.20% V
0.73-0.83% C, 0.45% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.80-4.50% Cr, 17.20-18.70% W, 1.00-1.20% V
0.73-0.83% C, 3.80-4.50% Cr, 0.80-1.20% V, 17.00-19.00% W
0.75% C, 0.25% Si, 0.30% Mn, 4.10% Cr, 1.10% V, 18.00% W
0.75% C, 0.25% Si, 0.45% Mn, 1.00% Cr, 1.70% Ni
0.75% C, 0.25% Si, 0.65% Mn, 0.013% P, 0.003% S, 3.06% Cr, 0.49% Mo, 0.12% V, 0.12% Ni, 0.22% Cu
0.75% C, 13.50% Cr, 3.00% Mo, 33.00% TiC, Fe is balance
0.75% C, 4.1% Cr, 1.1% V, 18.0% W
0.75-0.83% C, 0.45% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.80-4.50% Cr, 0.50-0.80% Mo, 15.50-18.50% W, 1.40-1.70% V, 4.50-5.00% Co
0.75-0.85% C, 0.10-0.30% Si, 0.10-0.35% Mn, 0.030% P, 0.030% S
0.75-0.85% C, 0.10-0.30% Si, 0.10-0.40% Mn, 0.030% P, 0.030% S
0.75-0.85% C, 0.10-0.30% Si, 0.10-0.40% Mn, 0.030% P, 0.030% S
0.75-0.85% C, 0.15-0.30% Si, 0.30-0.50% Mn, 0.025% P, 0.025% S, 0.40-0.60% Cr, 0.15-0.25% V, 0.10% Mo, 0.40% Ni
0.75-0.85% C, 0.15-0.35% Si, 0.30-0.50% Mn, 12.50-13.50% Cr, 0.40-0.60% Mo, 1.65-1.85% V
0.75-0.85% C, 0.15-0.40% Si, 0.30-0.50% Mn, 0.035% P, 0.035% S, 0.40-0.60% Cr, 0.20-0.30% V, 0.60-0.80% W
0.75-0.95% C, 0.90-1.10% Si, 0.70-1.00% Mn, 1.00-1.20% Cr, 0.15-0.30% Mo, 0.07-0.10% V. SKS3 steel: 0.95% C, 0.25% Si, 1.05% Mn, 0.75% Cr, 0.75% W.
0.75% C, 0.25% Si, 0.70% Mn, 0.035% S
0.76% C, 0.45% Si, 0.40% Mn, 4.15% Cr, 0.65% Mo, 1.55% V, 18.00% W, 9.50% Co
0.76-0.85% C, 3.80-4.50% Cr, 8.00-9.00% Mo, 0.90-1.30% V, 1.30-1.80% W
0.77% C, 0.55% Si, 0.48% Mn, 0.010% P, 0.015% S, 1.19% Cr, 2.00% W, 0.32% V
0.77% C, 0.82% Si, 0.25% Mn, 0.012% P, 0.002% S, 4.91% Cr, 0.29% Mo, 0.19% Ni, 0.15% Cu
0.77-0.85% C, 0.40% Si, 0.15-0.35% Mn, 0.025% P, 0.015% S, 3.90-4.30% Cr, 4.00-4.50% Mo, 0.25% W, 0.90-1.10% V, 0.30% Cu
0.77-0.85% C, 0.65% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.90-4.40% Cr, 4.00-4.50% Mo, 0.90-1.10% V
0.77-0.87% C, 0.70% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.50-4.50% Cr, 8.00-9.00% Mo, 1.40-2.00% W, 1.00-1.40% V
0.78% C, 0.45% Si, 0.45% Mn, 4.15% Cr, 1.10% V, 17.95% W
0.78% C, 4.00% Cr, 1.10% V, 18.00% W
0.78-0.86% C, 0.40% Si, 0.40% Mn, 0.015% P, 0.015% S, 3.80-4.50% Cr, 4.70-5.20% Mo, 6.00-6.70% W, 1.70-2.00% V
0.78-0.86% C, 0.40% Si, 0.40% Mn, 0.025% P, 0.015% S, 3.90-4.10% Cr, 4.70-5.20% Mo, 1.70-2.20% V, 6.00-6.70% W, 0.30% Cu
0.78-0.86% C, 0.40% Si, 0.40% Mn, 0.025% P, 0.015% S, 3.90-4.30% Cr, 4.70-5.20% Mo, 6.00-6.70% W, 1.70-2.00% W, 0.30% Cu
0.78-0.86% C, 0.45% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.50-4.20% Cr, 8.00-9.20% Mo, 1.50-2.00% W, 1.00-1.30% V
0.78-0.88% C, 0.20-0.45% Si, 0.15-0.40% Mn, 0.030% P, 0.030% S, 3.75-4.00% Cr, 4.50-5.50% Mo, 1.75-2.20% V, 5.50-6.75% W
0.78-1.05% C, 0.20-0.45% Si, 0.15-0.40% Mn, 0.030% P, 0.030% S, 3.75-4.50% Cr, 0.30% Ni, 1.75-2.20% V, 5.50-6.75% W
0.79% C, 0.33% Si, 0.45% Mn, 0.016% P, 0.03% S, 2.99% Cr, 0.40% Mo, 0.17% Ni, 0.13% V, 0.13% Cu
0.79% C, 0.33% Si, 0.45% Mn, 2.99% Cr, 0.40% Mo, 0.17% Ni, 0.13% V, 0.13% Cu
0.79% C, 0.45% Si, 0.40% Mn, 4.15% Cr, 0.65% Mo, 1.55% V, 18.00% W, 4.75% Co
0.79-0.86% C, 0.40% Si, 0.40% Mn, 0.025% P, 0.015% S, 3.90-4.30% Cr, 4.70-5.20% Mo, 1.70-2.00% V, 6.00-6.70% W, 0.30% Cu
0.80% C, 0.20% Si, 0.20% Mn
0.80% C, 0.20% Si, 0.30% Mn, 4.00% Cr, 4.30% Mo, 1.00% V
0.80% C, 0.20% Si, 0.50% Mn
0.80% C, 0.30% Si, 0.70% Mn, 0.015% P, 0.015% S, 4.00% Cr, 4.50% Mo, 0.10% Ni, 1.00% V
0.80% C, 0.40% Si, 0.40% Mn, 12.50% Cr, 1.10% Mo, 0.90% V, 0.75% Nb
0.80% C, 0.50% Si, 0.40% Mn, 1.10% Cr, 0.15% Mo, 0.30% V, 1.95% W
0.80% C, 0.60% Cr, 0.20% V
0.80% C, 12.70% Cr, 0.90% V, 1.10% Mo, 0.70% Nb
0.80% C, 4.0% Cr, 1.0% V, 18.00% W, 5.0% Co
0.80% C, 4.0% Cr, 3.0% Mo, 1.0% V, 3.0% W, 8.0% Co, 1.0% Nb
0.80% C, 4.00% Cr, 0.70% Mo, 1.50% V, 18.00% W, 4.80% Co
0.80% C, 4.00% Cr, 1.0% V, 18.00% W
0.80% C, 4.00% Cr, 1.00% V, 18.00% W, 10.00% Co
0.80% C, 4.00% Cr, 4.25% Mo, 1.00% V
0.80% C, 4.00% Cr, 4.25% Mo, 1.00% V
0.80% C, 7.50% Cr, 1.30% Mo, 2.75% V
0.80% C, 7.50% Cr, 2.75% Mo, 1.30% V
0.80-0.88% C, 0.45% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.80-4.50% Cr, 4.70-5.20% Mo, 5.90-6.70% W, 1.70-2.10% V
0.80-0.90% C, 0.25-0.40% Si, 0.50-0.70% Mn, 0.025% P, 0.020% S
0.80-0.90% C, 0.30-0.50% Si, 0.50-0.70% Mn, 0.035% P, 0.035% S, 0.30-0.45% Cr
0.80-0.90% C, 3.80-4.50% Cr, 4.80-5.80% Mo, 1.80-2.30% V, 6.00-7.00% W
0.80-0.90% C, 0.15-0.35% Si, 0.40-0.70% Mn, 0.025% P, 0.025% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.81% C, 0.35% Si, 0.35% Mn, 4.00% Cr, 4.25% Mo, 1.00% V
0.81% C, 0.79% Si, 0.25% Mn, 5.06% Cr, 0.20% Mo, 0.66% Ni, 0.020% V
0.82% C, 0.25% Si, 0.30% Mn, 4.25% Cr, 5.00% Mo, 1.80% V, 6.25% W
0.82% C, 0.25% Si, 0.30% Mn, 4.25% Cr, 5.00% Mo, 1.80% V, 6.25% W
0.82% C, 0.45% Si, 0.40% Mn, 3.85% Cr, 8.60% Mo, 1.15% V, 1.75% W
0.82% C, 0.75% Mn
0.83% C, 0.25% Si, 0.35% Mn, 4.10% Cr, 4.25% Mo, 1.00% V
0.83% C, 0.30% Si, 0.25% Mn, 3.75% Cr, 8.50% Mo, 1.15% V, 1.75% W
0.83% C, 0.45% Si, 0.40% Mn, 1.90% Cr, 0.30% Mo
0.83% C, 1.00% Si, 0.35% Mn, 7.75% Cr, 1.55% Mo, 2.15% V
0.83% C, 3.8% Cr, 8.5% Mo, 1.2% V, 1.8% W
0.83-0.90% C, 0.15-0.35% Si, 0.30-0.45% Mn, 0.030% P, 0.030% S, 1.60-1.90% Cr, 0.20-0.35% Mo, 0.05-0.15% V
0.84% C, 0.40% Si, 0.30% Mn, 3.80% Cr, 8.50% Mo, 1.20% V, 1.80% W
0.84% C, 0.40% Si, 0.30% Mn, 3.80% Cr, 8.60% Mo, 1.20% V, 1.80% W
0.84% C, 0.50% Si, 0.30% Mn, 4.10% Cr, 4.25% Mo, 1.00% V
0.84% C, 0.85% Si, 0.35% Mn, 7.70% C, 1.50% Mo, 2.45% V
0.84% C, 4.0% Cr, 4.2% Mo, 1.1% V
0.85% C, 0.20% Si, 0.30% Mn, 4.10% Cr, 4.25% Mo, 1.00% V
0.85% C, 0.25% Si, 0.33% Mn, 0.20% Cr, 0.13% V, 0.80% Ni
0.85% C, 0.25% Si, 0.35% Mn, 0.025% P, 0.010% S, 4.15% Cr, 6.50% W, 5.30% Mo, 2.05% V
0.85% C, 0.25% Si, 0.65% Mn
0.85% C, 0.25% Si, 2.10% Mn, 0.025% P, 0.010% S, 1.20% Cr, 1.50% Mo
0.85% C, 0.30% Si, 0.20% Mn, 4.00% Cr, 8.00% Mo, 2.00% V
0.85% C, 0.30% Si, 0.28% Mn, 4.15% Cr, 5.00% Mo, 1.85% V, 6.15% W
0.85% C, 0.30% Si, 0.28% Mn, 4.15% Cr, 5.00% Mo, 1.85% V, 6.15% W
0.85% C, 0.30% Si, 0.28% Mn, 4.15% Cr, 5.00% Mo, 1.85% V, 6.15% W
0.85% C, 0.30% Si, 0.30% Mn, 4.25% Cr, 5.00% Mo, 1.85% V, 6.40% W
0.85% C, 0.30% Si, 2.00% Mn, 0.030% P, 0.030% S, 1.00% Cr, 1.40% Mo, 0.25% Ni, 0.25% Cu
0.85% C, 0.35% Si, 0.25% Mn, 4.10% Cr, 5.00% Mo, 1.90% V, 6.40% W
0.85% C, 0.55% Si, 0.40% Mn, 4.35% Cr, 2.80% Mo, 2.10% V, 2.55% W, 4.50% Co
0.85% C, 0.55% Si, 4.35% Cr, 2.80% Mo, 2.10% V, 2.55% W, 4.50% Co
0.85% C, 0.85% Si, 0.35% Mn, 7.70% Cr, 1.50% Mo, 2.45% V
0.85% C, 0.90% Si, 8.40% Cr, 2.50% Mo, 0.00% V, 0.15% Nb
0.85% C, 1.00% Si, 0.30% Mn, 5.00% Cr, 1.35% Mo, 2.75% V
0.85% C, 1.00% Si, 0.50% Mn, 8.00% Cr, 1.50% Mo, 2.50% V
0.85% C, 4.15% Cr, 5.00% Mo, 1.95% V, 6.40% W
0.85% C, 7.70% Cr, 1.50% Mo, 2.30% V
0.85% C, 7.70% Cr, 1.50% Mo, 2.30% V
0.85-0.90% C, 0.25% Mn, 4.10% Cr, 5.00% Mo, 1.90% V, 6.40% W
0.85-0.92% C, 0.45% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.50-4.20% Cr, 8.00-9.20% Mo, 1.50-2.00% W, 1.80-2.20% V, 7.75-8.75% Co
0.85-0.95% C, 0.10-0.30% Si, 0.10-0.40% Mn, 0.030% P, 0.030% S
0.85-0.95% C, 0.10-0.30% Si, 0.10-0.40% Mn, 0.030% P, 0.030% S
0.85-0.95% C, 0.10-0.40% Si, 1.80-2.20% Mn, 0.030% P, 0.030% S, 0.20-0.50% Cr, 0.05-0.20% V
0.85-0.95% C, 0.10-0.40% Si, 1.80-2.20% Mn, 0.030% P, 0.030% S, 0.20-0.50% Cr, 0.05-0.20% V
0.85-0.95% C, 0.10-0.40% Si, 1.80-2.20% Mn, 0.030% P, 0.030% S, 0.20-0.50% Cr, 0.05-0.20% V
0.85-0.95% C, 0.10-0.40% Si, 1.80-2.20% Mn, 0.030% P, 0.030% S, 0.20-0.50% Cr, 0.05-0.20% V
0.85-0.95% C, 0.10-0.40% Si, 1.80-2.20% Mn, 0.030% P, 0.030% S, 0.20-0.50% Cr, 0.15-0.35% Mo, 0.05-0.20% V
0.85-0.95% C, 0.15-0.30% Si, 0.20-0.40% Mn, 0.030% P, 0.030% S, 0.70-0.90% Cr
0.85-0.95% C, 0.15-0.30% Si, 0.40-0.70% Mn, 0.025% P, 0.025% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.85-0.95% C, 0.65% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.90-4.40% Cr, 4.10-4.80% Mo, 1.70-2.20% V, 0.80-1.40% W
0.85-0.95% C, 1.00% Si, 1.00% Mn, 0.040% P, 0.015% S, 17.00-19.00% Cr, 0.90-1.30% Mo, 0.07-0.12% V
0.85-0.95% C, 1.00% Si, 1.00% Mn, 0.040% P, 0.030% S, 17.00-19.00% Cr, 0.90-1.20% Mo, 0.07-0.12% V
0.85-0.95% C, 1.00% Si, 1.00% Mn, 0.040% P, 0.030% S, 17.00-19.00% Cr, 0.90-1.30% Mo, 0.07-0.12% V
0.85-0.95% C, 1.00% Si, 1.00% Mn, 0.045% P, 0.030% S, 15.50-17.50% Cr, 0.40-0.60% Mo, 1.20-1.80% Co
0.85-0.95% C, 1.05-1.25% Si, 0.60-0.80% Mn, 0.035% P, 0.035% S, 1.10-1.30% Cr
0.85-0.95% C, 3.80-4.50% Cr, 4.80-5.80% Mo, 1.80-2.30% V, 6.00-7.00% W, 4.50-5.50% Co
0.85-1.0% C, 0.10-0.50% Si, 1.00-1.40% Mn, 0.40-0.70% Mn, 0.30% V, 0.40-0.60% W
0.86% C, 0.30% Si, 1.20% Mn, 0.030% P, 0.030% S, 0.50% Cr, 0.13% Mo, 0.25% Ni, 0.50% V, + special elements
0.86-0.93% C, 0.45% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.80-4.50% Cr, 4.70-5.20% Mo, 1.70-2.20% V, 5.90-6.70% W
0.86-0.94% C, 0.45% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.80-4.50% Cr, 4.70-5.20% Mo, 5.90-6.70% W, 1.70-2.00% V
0.86-0.94% C, 0.45% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.80-4.50% Cr, 4.70-5.20% Mo, 5.90-6.70% W, 1.70-2.00% V
0.86-0.94% C, 0.45% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.80-4.50% Cr, 4.70-5.20% Mo, 1.70-2.10% V, 5.90-6.70% W
0.86-0.94% C, 3.80-4.50% Cr, 4.70-5.20% Mo, 1.70-2.00% V, 6.00-6.70% W
0.86-0.94% C, 0.45% Si, 0.40% Mn, 0.03% P, 0.03% S, 3.80-4.50% Cr, 4.70-5.20% Mo, 1.70-2.10% V, 5.90-6.70% W
0.87% C, 0.30% Si, 0.30% Mn, 4.00% Cr, 8.00% Mo, 1.90% V, 0.00% W
0.87-0.95% C, 0.45% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.80-4.50% Cr, 4.70-5.20% Mo, 5.90-6.70% W, 1.70-2.10% V, 4.50-5.00% Co
0.87-0.95% C, 0.45% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.80-4.50% Cr, 4.70-5.20% Mo, 1.70-2.10% V, 5.90-6.70% W, 4.50-5.00% Co
0.87-0.97% C, 0.60-0.80% Si, 1.50-1.70% Mn, 0.015% P, 0.015% S, 1.40-1.70% Cr, 0.06-0.10% Mo, 0.10-0.25% Ni
0.88% C, 0.40% Si, 2.00% Mn, 0.13% Cr, 0.10% V
0.88% C, 4.00% Cr, 0.80% Mo, 2.50% V, 12.00% W
0.88% C, 4.00% Cr, 5.00% Mo, 2.00% V, 6.00% W
0.88-0.96% C, 4.50-5.00% Cr, 4.70-5.20% Mo, 1.70-2.00% V, 6.00-6.70% W, 4.50-5.00% Co
0.89% C, 0.30% Si, 0.30% Mn, 4.10% Cr, 4.50% Mo, 1.90% V, 1.20% W
0.89% C, 0.45% Si, 0.25% Mn, 4.00% Cr, 4.50% Mo, 1.85% V, 1.10% W
0.9% C, 3.9% Cr, 2.75% Mo, 1.8% V, 6.0% W, 2.0% Co
0.90% C (for strips), 4.20% Cr, 5.00% Mo, 1.80% V, 6.40% W
0.90% C, 0.20% Si, 2.00% Mn, 0.40% Cr, 0.10% V
0.90% C, 0.20% Si, 2.00% Mn, 0.40% Cr, 0.10% V
0.90% C, 0.20% Si, 2.00% Mn, 0.40% Cr, 0.10% V
0.90% C, 0.20% Si, 2.00% Mn, 0.40% Cr, 0.10% V
0.90% C, 0.20% Si, 2.00% Mn, 0.40% Cr, 0.10% V
0.90% C, 0.25% Si, 0.30% Mn, 0.80% Cr
0.90% C, 0.25% Si, 0.40% Mn, 4.10% Cr, 5.00% Mo, 1.80% V, 6.40% W
0.90% C, 0.25% Si, 0.90% Mn, 0.35% Cr, 0.10% V
0.90% C, 0.25% Si, 2.00% Mn, 0.30% Cr, 0.10% V
0.90% C, 0.25% Si, 2.00% Mn, 0.30% Cr, 0.10% V
0.90% C, 0.25% Si, 2.00% Mn, 0.35% Cr, 0.10% V, 0.00% V
0.90% C, 0.25% Si, 2.00% Mn, 0.35% Cr, 0.13% V
0.90% C, 0.30% Si, 0.30% Mn, 4.00% Cr, 5.00% Mo, 1.90% V, 6.20% W
0.90% C, 0.30% Si, 0.30% Mn, 4.10% Cr, 5.00% Mo, 1.90% V, 6.40% W
0.90% C, 0.30% Si, 0.30% Mn, 4.20% Cr, 5.00% Mo, 1.80% V, 6.40% W
0.90% C, 0.30% Si, 0.60% Mn, 0.55% Cr
0.90% C, 0.30% Si, 2.00% Mn, 0.025% P, 0.015% S, 0.40% Cr, 0.10% V
0.90% C, 0.30% Si, 2.00% Mn, 0.025% P, 0.015% S, 0.40% Cr, 0.10% V
0.90% C, 0.40% Si, 0.45% Mn, 4.15% Cr, 4.95% Mo, 1.90% V, 6.60% W
0.90% C, 0.45% Si, 0.40% Mn, 17.50% Cr, 1.10% Mo, 0.10% V
0.90% C, 0.50% Cr, 1.25% Mo, 0.20% V, 0.50% W
0.90% C, 0.50% Si, 0.33% Mn, 16.00% Cr, 0.30% Mo, 1.00% Co
0.90% C, 0.50% Si, 0.50% Mn, 0.030% P, 0.025% S, 17.00% Cr, 1.00% Mo, 0.10% V
0.90% C, 0.50% Si, 0.50% Mn, 0.030% P, 0.025% S, 17.00% Cr, 1.00% Mo, 0.10% V
0.90% C, 0.90% Si, 0.50% Mn, 7.80% Cr, 2.50% Mo, 0.50% V
0.90% C, 0.90% Si, 0.50% Mn, 7.80% Cr, 2.50% Mo, 0.50% V
0.90% C, 0.90% Si, 0.50% Mn, 7.80% Cr, 2.50% Mo, 0.50% V
0.90% C, 1.00% Si, 1.00% Mn, 18.00% Cr, 1.10% Mo, 0.10% V
0.90% C, 1.00% Si, 1.00% Mn, 18.00% Cr, 1.10% Mo, 0.10% V
0.90% C, 1.00% Si, 1.00% Mn, 19.00% Cr, 1.10% Mo, 0.10% V
0.90% C, 1.00% Si, 18.00% Cr, 1.00% Mn, 0.10% V
0.90% C, 1.20% Mn, 0.50% Cr, 8.00% Mo, 0.20% V, 0.50% W
0.90% C, 12.0% Si, 0.70% Mn, 1.20% Cr
0.90% C, 18.00% Cr, 1.10% Mo, 0.10% V
0.90% C, 18.00% Cr, 1.10% Mo, 0.10% V
0.90% C, 2.00% Mn, 0.40% Cr, 0.10% V
0.90% C, 2.00% Mn, 0.40% Cr, 0.10% V
0.90% C, 2.00% Mn, 0.40% Cr, 0.10% V
0.90% C, 2.00% Mn, 0.40% Cr, 0.10% V
0.90% C, 4.00% Cr, 4.50% Mo, 2.00% V, 1.20% W
0.90% C, 4.00% Cr, 5.00% Mo, 1.80% V, 6.20% W
0.90% C, 4.00% Cr, 5.00% Mo, 1.90% V, 6.40% W
0.90% C, 4.00% Cr, 5.00% Mo, 1.90% V, 6.40% W
0.90% C, 4.00% Cr, 5.50% Mo, 2.00% V, 6.00% W, 5.00% Co
0.90% C, 4.10% Cr, 5.00% Mo, 1.90% V, 6.40% W
0.90% C, 4.10% Cr, 5.00% Mo, 1.90% V, 6.40% W
0.90% C, 4.10% Cr, 5.00% Mo, 1.90% V, 6.40% W
0.90% C, 4.2% Cr, 5.0% Mo, 1.8% V, 6.4% W
0.90% C, 4.20% Cr, 5.00% Mo, 1.80% V, 6.40% W
0.90% C, 4.20% Cr, 5.00% Mo, 1.90% V, 6.10% W
0.90-1.00% C, 0.10-0.40% Si, 1.05-1.35% Mn, 0.030% P, 0.030% S, 0.40-0.65% Cr, 0.40-0.70% W, 0.05-0.20% V
0.90-1.00% C, 0.45% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.80-4.50% Cr, 0.70-1.00% Mo, 11.50-12.50% W, 2.30-2.60% V
0.90-1.05% C, 0.15-0.35% Si, 0.25-0.45% Mn, 0.030% P, 0.025% S, 0.40-0.60% Cr, 0.30% Ni, 0.30% Cu
0.90-1.05% C, 0.15-0.35% Si, 1.00-1.20% Mn, 0.035% P, 0.035% S, 0.50-0.70% Cr, 0.05-0.15% V, 0.50-0.70% W
0.90-1.05% C, 0.15-0.35% Si, 1.00-1.20% Mn, 0.035% P, 0.035% S, 0.50-0.70% Cr, 0.50-0.70% W, 0.050-0.15% V
0.90-1.10% C, 0.15-0.30% Si, 0.20-0.40% Mn, 0.035% P, 0.035% S, 1.10-1.30% Cr, 0.20-0.40% Mo
0.91% C, 0.45% Si, 0.40% Mn, 4.15% Cr, 1.00% Ni, 6.30% V, 4.75% Co
0.91-1.02% C, 0.29% Si, 0.20-0.40% Mn, 0.015% P, 0.005-0.015% S, 1.00-1.15% Cr, 0.06-0.10% Mo, 0.10-0.25% Ni
0.92% C, 0.40% Si, 0.30% Mn, 4.10% Cr, 5.00% Mo, 1.90% V, 6.40% W, 4.80% Co
0.92% C, 4.10% Cr, 5.00% Mo, 1.90% V, 6.40% W, 4.80% Co
0.92% C, 4.15% Cr, 5.00% Mo, 1.85% V, 6.30% W, 4.80% Co
0.92-1.00% C, 0.20-0.40% Si, 0.20-0.40% Mn, 0.030% P, 0.020% S, 11.00-12.00% Cr, 0.80-1.00% Mo, 0.80-1.00% V
0.92-1.05% C, 0.15-0.35% Si, 0.25-0.45% Mn, 0.025% P, 0.015% S, 1.65-1.95% Cr, 0.15-0.30% Mo, 0.30% Cu, 0.050% Al
0.93% C, 0.28% Si, 0.28% Mn, 0.009% P, 0.001% S, 1.47% Cr, 0.02% Mo, 0.10% Ni, 0.10% Cu, 12 ppm Ti, 3.9 ppm O
0.93% C, 0.30% Si, 4.20% Cr, 5.00% Mo, 1.90% V, 6.25% W, 4.90% Co
0.93% C, 4.00% Cr, 5.00% Mo, 1.90% V, 6.20% W, 4.80% Co
0.93% C, 4.2% Cr, 5.0% Mo, 1.8% V, 6.4% W, 4.8% Co
0.93% C, 4.20% Cr, 5.00% Mo, 1.80% V, 6.40% W, 4.80% Co
0.93% C, 4.20% Cr, 5.00% Mo, 1.80% V, 6.40% W, 4.80% Co
0.93-0.98% C, 0.15-0.35% Si, 0.25-0.45% Mn, 0.025% P, 0.003% S, 1.35-1.60% Cr, 0.10% Mo, 0.25% Ni
0.93-0.98% C, 0.50-0.70% Si, 1.00-1.20% Mn, 0.025% P, 0.003-0.008% S, 1.40-1.55% Cr, 0.10% Mo, 0.25% Ni
0.93-1.00% C, 0.29-0.35% Si, 0.25-0.40% Mn, 0.015% P, 0.001% S, 1.40-1.60% Cr, 0.06% Mo, 0.25% Ni
0.93-1.05% C, 0.15-0.35% Si, 0.25-0.45% Mn, 0.025% P, 0.015% S, 1.35-1.60% Cr, 0.10% Mo, 0.050% Al, 0.30% Cu
0.93-1.05% C, 0.15-0.35% Si, 0.25-0.45% Mn, 0.025% P, 0.015% S, 1.65-1.95% Cr, 0.15-0.30% Mo, 0.30% Cu, 0.050% Al
0.93-1.05% C, 0.15-0.35% Si, 0.25-0.45% Mn, 0.025% P, 0.015% S, 1.65-1.95% Cr, 0.15-0.30% Mo, 0.30% Cu, 0.050% Al
0.93-1.05% C, 0.15-0.35% Si, 0.25-0.45% Mn, 0.030% P, 0.030% S, 1.35-1.65% Cr
0.93-1.05% C, 0.15-0.35% Si, 0.60-.80% Mn, 0.025% P, 0.015% S, 1.65-1.95% Cr, 0.20-0.35% Mo, 0.30% Cu, 0.050% Al
0.93-1.05% C, 0.15-0.35% Si, 0.60-0.80% Mn, 0.025% P, 0.015% S, 1.65-1.95% Cr, 0.20-0.35% Mo, 0.30% Cu, 0.050% Al
0.93-1.05% C, 0.20-0.35% Si, 0.25-0.40% Mn, 0.003% S, 1.35-1.60% Cr, 0.20% Ni
0.93-1.05% C, 0.20-0.40% Si, 0.60-0.80% Mn, 0.025% P, 0.005% S, 1.65-1.95% Cr, 0.20-0.35% Mo, 0.25% Ni
0.93-1.05% C, 0.40-0.60% Si, 0.80-1.10% Mn, 0.025% P, 0.015% S, 1.80-2.05% Cr, 0.50-0.60% Mo, 0.30% Cu, 0.050% Al
0.93-1.05% C, 0.45-0.75% Si, 1.00-1.20% Mn, 0.025% P, 0.015% S, 1.45-1.65% Cr, 0.10% Mo, 0.30% Ni, 0.050% Al
0.93-1.05% C, 0.45-0.75% Si, 1.00-1.20% Mn, 0.025% P, 0.05% S, 1.40-1.65% Cr, 0.10% Mo, 0.30% Cu, 0.050% Al
0.93% C, 0.28% Mn, 0.28% Si, 0.009% P, 0.001% S, 1.47% Cr, 0.02% Mo, 0.10% Ni, 0.10 Cu, 12 ppm Ti, 3.9 ppm O.
0.94% C, 0.30% Si, 1.20% Mn, 0.50% Cr, 0.50% W
0.94% C, 0.30% Si, 1.20% Mn, 0.50% Cr, 0.50% W
0.94% C, 0.30% Si, 1.20% Mn, 0.50% Cr, 0.50% W
0.95% C, 0.20% Si, 1.10% Mn, 0.60% Cr, 0.10% V, 0.60% W
0.95% C, 0.20% Si, 1.10% Mn, 0.60% Cr, 0.10% V, 0.60% W
0.95% C, 0.25% Si, 1.05% Mn, 0.025% P, 0.010% S, 0.75% Cr, 0.75% W
0.95% C, 0.25% Si, 1.05% Mn, 0.75% Cr, 0.75% W.
0.95% C, 0.25% Si, 1.10% Mn, 0.55% Cr, 0.10% V, 0.55% W
0.95% C, 0.25% Si, 1.20% Mn, 0.48% Cr, 0.13% V, 0.55% W
0.95% C, 0.30% Si, 1.10% Mn, 0.60% Cr, 0.10% V, 0.55% W
0.95% C, 0.30% Si, 1.10% Mn, 0.60% Cr, 0.10% W, 0.55% W
0.95% C, 1.00% Si, 0.40% Mn, 8.00% Cr, 2.0% Mo, 0.30% V
0.95% C, 1.10% Mn, 0.55% Cr, 0.55% W, 0.10% V
0.95% C, 1.10% Mn, 0.55% Cr, 0.55% W, 0.10% V
0.95% C, 1.10% Mn, 0.60% Cr, 0.60% W, 0.10% V
0.95% C, 1.10% Mn, 0.60% Cr, 0.10% V, 0.60% W
0.95% C, 1.10% Mn, 0.60% Cr, 0.10% V, 0.60% W
0.95% C, 1.10% Mn, 0.60% Cr, 0.10% V, 0.60% W
0.95% C, 1.10% Mn, 0.60% Cr, 0.60% W, 0.10% V, 0.00% W
0.95% C, 1.10% Mn, 0.60% Cr, 0.60% W, 0.10% V
0.95% C, 1.10% Mn, 0.60% Cr, 0.60% W, 0.10% V
0.95% C, 1.10% Mn, 0.60% Cr, 0.60% W
0.95% C, 4.00% Cr, 9.50% Mo, 1.00% V, 1.80% W, 8.00% Co
0.95-1.03% C, 0.45% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.80-4.50% Cr, 2.50-2.90% Mo, 2.70-3.00% W, 2.20-2.50% V
0.95-1.03% C, 0.45% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.80-4.50% Cr, 2.50-2.90% Mo, 2.70-3.00% W, 2.20-2.50% V
0.95-1.03% C, 0.45% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.80-4.50% Cr, 2.50-2.90% Mo, 2.70-3.00% W, 2.20-2.50% V
0.95-1.05% C, 0.10-0.50% Si, 0.40-1.00% Mn, 4.75-5.50% Cr, 0.90-1.40% Mo, 0.15-0.50% V
0.95-1.05% C, 0.15-0.25% Si, 0.15-0.30% Mn, 0.025% P, 0.025% S, 0.10-0.15% V
0.95-1.05% C, 0.15-0.35% Si, 0.60% Mn, 0.025% P, 0.025% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.95-1.05% C, 0.45% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.80-4.50% Cr, 4.70-5.20% Mo, 6.00-6.70% W, 1.70-2.00% V
0.95-1.05% C, 0.70% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.50-4.50% Cr, 8.20-9.20% Mo, 1.50-2.10% W, 1.70-2.20% V
0.95-1.05% C, 0.70% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.50-4.50% Cr, 8.20-9.20% Mo, 1.50-2.10% W, 1.70-2.20% V
0.95-1.10% C, 0.10-0.25% Si, 0.15-0.30% Mn, 0.035% P, 0.035% S, 0.10-0.25% Cr, 0.10-0.20% V, 0.90-1.20% W
0.95-1.10% C, 0.15-0.35% Si, 0.20-0.40% Mn, 0.025% P, 0.025% S, 1.35-1.60% Cr, 0.10% Mo, 0.40% Ni
0.95-1.10% C, 0.15-0.35% Si, 0.20-0.40% Mn, 0.025% P, 0.025% S, 1.35-1.60% Cr, 0.10% Mo, 0.40% Ni
0.95-1.10% C, 0.15-0.35% Si, 0.25-0.45% Mn, 0.015% P, 0.015% S, 1.35-1.65% Cr, 0.40% Ni
0.95-1.10% C, 0.15-0.35% Si, 0.25-0.45% Mn, 0.030% P,
0.95-1.10% C, 0.15-0.35% Si, 0.25-0.45% Mn, 0.030% P, 0.030% S, 1.35-1.65% Cr
0.95-1.10% C, 0.15-0.35% Si, 0.25-0.45% Mn, 0.030% P, 0.030% S, 1.35-1.65% Cr
0.95-1.10% C, 0.20-0.40% Si, 0.25-0.45% Mn, 1.65-1.95% Cr, 0.30-0.40% Mo
0.95-1.20% C, 1.00% Si, 1.00% Mn, 0.040% P, 0.030% S, 16.00-18.00% Cr, 0.40-0.80% Mo
0.95-1.20% C, 1.00% Si, 1.00% Mn, 0.040% P, 0.030% S, 16.00-18.00% Cr, 0.40-0.80% Mo
0.95-1.20% C, 1.00% Si, 1.50% Mn, 0.040% P, 0.015% S, 16.00-18.00% Cr, 0.40-0.80% Mo
0.95???1.05% C, 0.15-0.25% Si, 0.15-0.30% Mn, 0.025% P, 0.025% S, 0.20-0.40% Cr, 0.10-0.15% V
0.96% C, 0.30% Si, 0.30% Mn, 11.50% Cr, 0.90% Mo, 0.90% V
0.96% C, 0.30% Si, 0.30% Mn, 11.50% Cr, 0.90% Mo, 0.90% V
0.97% C, 0.60% Si, 1.10% Mn, 1.53% Cr
0.98% C, 0.30% Si, 0.28% Mn, 4.15% Cr, 5.00% Mo, 1.85% V
0.98% C, 4.00% Cr, 2.60% Mo, 2.40% V, 2.80% W
0.98-1.05% C, 0.20-0.35% Si, 0.30-0.40% Mn, 0.025% P, 0.017-0.023% S, 1.40-1.60% Cr, 0.08% Mo, 0.25% Ni
0.99% C, 0.17% Si, 0.57% Mn, 0.018% P, 0.017% S, 5.25% Cr, 1.02% Mo, 0.16% V
0.99% C, 0.17% Si, 0.57% Mn, 0.018% P, 0.017% S, 5.25% Cr, 1.02% Mo, 0.16% V
0.99% C, 4.1% Cr, 2.7% Mo, 2.4% V, 2.8% W
1.0% C, 1.0% Si, 0.50% Mn, 8.25% Cr, 2.25% Mo, 0.40% V
1.0% C, 3.80% Cr, 8.70% Mo, 2.0% V, 1.80% W
1.00 % C, 1.50% Cr
1.00% C, 0.20% Si, 0.20% Mn, 0.10% V
1.00% C, 0.25% Si, 0.25% Mn, 4.00% Cr, 8.75% Mo, 2.00% V, 1.75% W
1.00% C, 0.25% Si, 0.30% Mn, 0.025% P, 0.010% S, 1.50% Cr
1.00% C, 0.25% Si, 0.33% Mn, 1.50% Cr
1.00% C, 0.25% Si, 0.35% Mn, 0.50% Cr
1.00% C, 0.25% Si, 0.35% Mn, 1.50% Cr
1.00% C, 0.25% Si, 0.35% Mn, 1.50% Cr
1.00% C, 0.25% Si, 0.35% Mn, 1.50% Cr
1.00% C, 0.25% Si, 0.60% Mn, 5.15% Cr, 1.05% Mo, 0.20% V
1.00% C, 0.25% Si, 1.10% Mn, 0.025% P, 0.010% S, 0.60% Cr, 0.10% V, 0.60% W
1.00% C, 0.30% Si, 0.50% Mn, 0.025% P, 0.010% S, 5.00% Cr, 1.00% Mo, 0.20% V
1.00% C, 0.30% Si, 0.50% Mn, 5.00% Cr, 0.95% Mo, 0.20% V
1.00% C, 0.30% Si, 0.50% Mn, 5.00% Cr, 0.95% Mo, 0.20% V
1.00% C, 0.30% Si, 0.50% Mn, 5.20% Cr, 1.10% Mo, 0.20% V
1.00% C, 0.30% Si, 0.50% Mn, 5.25% Cr, 1.10% Mo, 0.30% V
1.00% C, 0.30% Si, 0.55% Mn, 5.20% Cr, 1.10% Mo, 0.25% V
1.00% C, 0.30% Si, 0.55% Mn, 5.20% Cr, 1.10% Mo, 0.25% V
1.00% C, 0.30% Si, 0.60% Mn, 5.25% Cr, 1.10% Mo, 0.20% V
1.00% C, 0.30% Si, 0.60% Mn, 5.25% Cr, 1.10% Mo, 0.20% V
1.00% C, 0.30% Si, 0.60% Mn, 5.30% Cr, 1.10% Mo, 0.20% V
1.00% C, 0.30% Si, 0.60% Mn, 5.30% Cr, 1.10% Mo, 0.20% V
1.00% C, 0.30% Si, 0.60% Mn, 5.30% Cr, 1.10% Mo, 0.20% V
1.00% C, 0.30% Si, 0.60% Mn, 5.30% Cr, 1.10% Mo, 0.20% V
1.00% C, 0.30% Si, 0.70% Mn, 1.80% Cr, 0.30% Mo
1.00% C, 0.30% Si, 0.70% Mn, 1.80% Cr, 0.30% Mo
1.00% C, 0.30% Si, 0.75% Mn, 5.00% Cr, 1.00% Mo, 0.25% V
1.00% C, 0.30% Si, 0.75% Mn, 5.00% Cr, 1.00% Mo, 0.25% V
1.00% C, 0.30% Si, 0.75% Mn, 5.00% Cr, 1.00% Mo, 0.25% V
1.00% C, 0.30% Si, 0.75% Mn, 5.00% Cr, 1.00% Mo, 0.25% V
1.00% C, 0.30% Si, 0.75% Mn, 5.00% Cr, 1.00% Mo, 0.25% V
1.00% C, 0.30% Si, 0.75% Mn, 5.00% Cr, 1.00% Mo, 0.25% V
1.00% C, 0.30% Si, 1.10% Mn, 0.60% Cr, 0.10% V, 0.60% W
1.00% C, 0.35% Mn, 0.005% S, 7.50% Cr, 2.60% Mo, 0.30% V, + Ti
1.00% C, 0.35% Mn, 0.005% S, 7.50% Cr, 2.60% Mo, 0.30% V + Ti
1.00% C, 0.35% Mn, 0.005% S, 7.50% Cr, 2.60% Mo, 0.30% V + Ti
1.00% C, 0.35% Mn, 0.005% S, 7.50% Cr, 2.60% Mo, 0.30% V, +Nb
1.00% C, 0.40% Si, 0.70% Mn, 0.025% P, 0.025% S, 17.00% Cr, 0.45% Mo
1.00% C, 0.40% Si, 0.70% Mn, 0.025% P, 0.025% S, 17.00% Cr, 0.45% Mo
1.00% C, 0.50% Si, 0.30% Mn, 10.00% Cr, 1.05% Mo, 0.25% V
1.00% C, 0.60% Mn, 5.00% Cr, 1.00% Mo, 0.25% V
1.00% C, 0.60% Si, 1.10% Mn, 1.50% Cr
1.00% C, 0.60% Si, 1.10% Mn, 1.50% Cr
1.00% C, 0.85% Mn, 5.25% Cr, 1.10% Mo, 0.25% V
1.00% C, 0.90% Si, 8.00% Cr, 1.10% Mo, 1.60% V
1.00% C, 0.90% Si, 8.00% Cr, 1.60% Mo, 1.60% V
1.00% C, 0.90% Si, 8.00% Cr, 1.60% Mo, 1.60% V
1.00% C, 0.91% Si, 0.32% Mn, 8.00% Cr, 0.32% Mo, 0.28% V
1.00% C, 1.00% Si, 0.40% Mn, 8.00% Cr, 2.00% Mo, 0.30% V
1.00% C, 1.00% Si, 0.40% Mn, 8.00% Cr, 2.00% Mo, 0.30% V
1.00% C, 1.00% Si, 0.50% Mn, 8.25% Cr, 2.25% Mo, 0.40% V
1.00% C, 1.00% Si, 0.50% Mn, 8.25% Cr, 2.25% Mo, 0.40% V
1.00% C, 1.00% Si, 1.00% Mn, 17.00% Cr, 0.60% Mo
1.00% C, 1.08% Si, 0.18% Mn, 8.03% Cr, 2.76% Mo, 0.13% Ni, 0.33% V
1.00% C, 1.10% Si, 0.30% Mn, 8.00% Cr, 2.70% Mo, 0.30% V
1.00% C, 1.20% Mn, 0.60% Cr, 0.10% V, 0.60% W
1.00% C, 1.50% Cr
1.00% C, 1.50% Cr
1.00% C, 1.50% Cr
1.00% C, 1.60% W, 3.75% Cr, 2.00% V, 8.55% Mo
1.00% C, 1.70% Mn, 5.30% Cr, 1.10% Mo, 0.20% V
1.00% C, 1.70% Mn, 5.30% Cr, 1.10% Mo, 0.20% V
1.00% C, 17.00% Cr, 0.50% Mo
1.00% C, 4.00% Cr, 5.00% Mo, 1.80% V, 6.20% W
1.00% C, 4.00% Cr, 8.50% Mo, 2.00% V, 1.50% W
1.00% C, 5.00% Cr, 0.95% Mo, 0.20% V
1.00% C, 5.00% Cr, 1.00% Mo, 0.30% V
1.00% C, 5.30% Cr, 1.10% Mo, 0.20% V
1.00% C, 5.30% Cr, 1.10% Mo, 0.25% V
1.00% C, 5.30% Cr, 1.10% Mo, 0.25% V
1.00% C, 8.00% Cr, 2.50% Mo, 0.30% V, + others
1.00% C, 8.00% Cr, 2.50% Mo, 0.30% V, +others
1.00% C, 8.00% Cr, 2.50% Mo, 0.30% V, +others
1.00-1.10% C, 0.10-0.30% Si, 0.10-0.35% Mn, 0.030% P, 0.030% S
1.00-1.10% C, 0.10-0.30% Si, 0.10-0.35% Mn, 0.030% P, 0.030% S
1.00-1.10% C, 0.10-0.30% Si, 0.10-0.40% Mn, 0.030% P, 0.030% S, 0.10-0.20% V
1.00-1.10% C, 0.10-0.30% Si, 0.10-0.40% Mn, 0.030% P, 0.030% S
1.00-1.10% C, 0.10-0.40% Si, 0.80-1.10% Mn, 0.030% P, 0.030% S, 0.90-1.10% Cr, 1.00-1.30% W
1.00-1.10% C, 0.15-0.30% Si, 1.00-1.20% Mn, 0.035% P, 0.035% S, 0.70-1.00% Cr
1.00-1.10% C, 0.15-0.35% Si, 0.20-0.40% Mn, 0.030% P, 0.030% S, 0.90-1.10% Cr
1.00-1.10% C, 0.30-0.60% Si, 0.40-0.60% Mn, 0.030% P, 0.015% S, 16.50-17.60% Cr, 0.40-0.60% Mo
1.00-1.10% C, 0.45% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.80-4.50% Cr, 5.50-6.50% Mo, 5.90-6.70% W, 2.30-2.60% V
1.00-1.10% C, 3.50-4.25% Cr, 9.00-10.00% Mo, 1.00-1.50% V, 1.25-2.00% W, 7.75-8.75% Co
1.00-1.10% C, 3.80-4.50% Cr, 6.00-7.00% Mo, 1.50-1.80% V, 5.00-6.00% W, 7.50-8.50% Co
1.02% C, 0.18% Si, 0.23% Mn, 0.18% Cr, 0.15% V, 1.05% W
1.02% C, 0.25% Si, 0.33% Mn, 1.50% Cr
1.02% C, 0.30% Si, 0.25% Mn, 3.75% Cr, 8.50% Mo, 1.90% V, 1.75% W
1.02% C, 0.30% Si, 0.25% Mn, 4.10% Cr, 5.00% Mo, 2.40% V, 6.00% W
1.02% C, 0.40% Si, 0.30% Mn, 17.00% Cr, 0.50% Mo
1.02% C, 0.40% Si, 0.30% Mn, 3.80% Cr, 8.60% Mo, 1.90% V, 1.80% W
1.02% C, 0.40% Si, 0.30% Mn, 3.80% Cr, 8.60% Mo, 1.90% V, 1.80% W
1.02% C, 0.40% Si, 0.40% Mn, 3.80% Cr, 8.60% Mo, 1.90% V, 1.80% W
1.02% C, 3.8% Cr, 8.6% Mo, 1.9% V, 1.8% W
1.02% C, 3.80% Cr, 8.60% Mo, 1.90% V, 1.80% W
1.03% C, 0.18% Si, 0.23% Mn, 0.18% Cr, 0.15% V, 1.05% W
1.05% C, 0.20% Si, 0.25% Mn
1.05% C, 0.20% Si, 0.25% Mn
1.05% C, 0.25% Si, 0.30% Mn
1.05% C, 0.25% Si, 0.33% Mn, 1.03% Cr
1.05% C, 0.25% Si, 0.90% Mn, 0.40% Cr
1.05% C, 0.25% Si, 0.96% Mn, 1.00% Cr, 1.15% V
1.05% C, 0.25% Si, 1.00% Mn, 1.00% Cr, 1.00% W
1.05% C, 0.25% Si, 1.10% Mn, 0.90% Cr
1.05% C, 0.30% Si, 0.35% Mn, 1.50% Cr
1.05% C, 0.30% Si, 0.35% Mn, 1.50% Cr
1.05% C, 0.30% Si, 0.35% Mn, 1.50% Cr
1.05% C, 0.30% Si, 0.35% Mn, 1.50% Cr
1.05% C, 0.30% Si, 0.50% Mn, 14.00% Cr, 4.00% Mo
1.05% C, 0.30% Si, 0.50% Mn, 14.00% Cr, 4.00% Mo
1.05% C, 0.30% Si, 0.50% Mn, 14.00% Cr, 4.00% Mo
1.05% C, 0.35% Si, 0.80% Mn, 0.030% P, 0.030% S, 0.40% Cr
1.05% C, 0.40% Si, 0.40% Mn, 16.70% Cr, 0.50% Mo
1.05% C, 0.40% Si, 0.40% Mn, 17.00% Cr, 0.40% Mo
1.05% C, 0.40% Si, 0.40% Mn, 17.00% Cr, 0.40% Mo
1.05% C, 0.40% Si, 0.40% Mn, 17.00% Cr, 0.50% Mo
1.05% C, 0.40% Si, 0.40% Mn, 17.00% Cr, 0.50% Mo
1.05% C, 17.50% Cr, 1.20% Mo, 0.10% V, 1.50% Co
1.05% C, 4.0% Cr, 6.0% Mo, 1.6% V, 5.0% W, 7.8% Co
1.05% C, 4.0% Cr, 6.3% Mo, 2.5% V, 6.3% W
1.05% C, 4.00% Cr, 6.00% Mo, 2.50% V, 6.00% W, 5.00% Co
1.05% C, 4.00% Cr, 6.30% Mo, 2.50% V, 6.30% W
1.05% C, 9.30% Cr, 1.60% Mo, 0.50% V
1.05-1.12% C, 3.60-4.40% Cr, 9.00-10.00% Mo, 1.00-1.30% V, 1.20-1.80% W, 7.50-8.50% Co
1.05-1.15% C, 0.15-0.30% Si, 0.20-0.35% Mn, 0.030% P, 0.030% S, 1.10-1.30% Cr, 0.15-0.25% V, 1.20-1.40% W
1.05-1.15% C, 0.15-0.65% Si, 0.15-0.40% Mn, 3.50-4.25% Cr, 9.00-10.00% Mo, 0.95-1.35% V, 1.15-1.85% W
1.05-1.15% C, 0.45% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.80-4.50% Cr, 3.60-4.00% Mo, 6.60-7.10% W, 1.70-1.90% V, 4.80-5.20% Co
1.05-1.15% C, 0.70% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.50-4.50% Cr, 9.00-10.00% Mo, 7.50-8.50% Co, 0.90-1.30% V, 1.20-1.90% W
1.05-1.15% C, 0.70% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.80-4.50% Cr, 9.00-10.00% Mo, 1.20-1.90% W, 0.90-1.30% V, 7.50-8.50% Co
1.05-1.15% C, 0.70% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.50-4.50% Cr, 9.00-10.00% Mo, 0.90-1.30% V, 1.20-1.90% W, 7.50-8.50% Co
1.05-1.15% C, 0.70% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.50-4.50% Cr, 9.00-10.00% Mo, 0.90-1.30% V, 1.20-1.90% W, 7.50-8.50% Co
1.05-1.15% C, 1.00% Si, 1.00% Mn, 0.045% P, 0.030% S, 14.00-16.00% Cr, 0.40-0.60% Mo, 0.10-0.15% V
1.07% C, 0.40% Si, 0.40% Mn, 17.30% Cr, 1.10% Mo, 0.10% V, 1.50% Co
1.07% C, 0.40% Si, 0.40% Mn, 17.30% Cr, 1.10% Mo, 0.10% V, 1.50% Co
1.08% C, 0.45% Si, 3.85% Cr, 9.50% Mo, 1.20% V, 1.50% W, 8.00% Co
1.08% C, 3.8% Cr, 9.4% Mo, 1.2% V, 1.5% W, 8.0% Co
1.08% C, 3.8% Cr, 9.4% Mo, 1.2% V, 1.5% W, 8.0% Co
1.08% C, 3.80% Cr, 9.40% Mo, 1.20% V, 1.50% W, 8.00% Co
1.08% C, 3.80% Cr, 9.40% Mo, 1.20% V, 1.50% W, 8.00% Co
1.08% C, 3.90% Cr, 9.40% Mo, 1.20% V, 1.50% W, 8.00% Co
1.10% C, 0.23% Si, 0.30% Mn, 1.20% Cr, 0.20% V, 1.30% W
1.10% C, 0.23% Si, 0.30% Mn, 1.20% Cr, 0.20% V, 1.30% W
1.10% C, 0.50% Si, 0.20% Mn, 3.90% Cr, 9.20% Mo, 1.40% W, 7.80% Co, 1.00% V
1.10% C, 0.50% Si, 0.20% Mn, 3.90% Cr, 9.20% Mo, 1.40% W, 7.80% Co, 1.00% V
1.10% C, 0.50% Si, 0.25% Mn, 3.90% Cr, 9.20% Mo, 1.20% V, 1.40% W, 8.00% Co
1.10% C, 0.50% Si, 0.40% Mn, 4.50% Cr, 3.20% Mo, 3.70% W, 8.50% V, 1.80% N
1.10% C, 0.60% Si, 0.30% Mn, 0.060% S, 3.75% Cr, 9.50% Mo, 1.15% V, 1.50% W, 8.25% Co
1.10% C, 0.70% Si, 0.40% Mn, 4.00% Cr, 9.50% Mo, 1.10% V, 1.55% W, 8.00% Co
1.10% C, 0.70% Si, 0.40% Mn, 8.20% Cr, 2.10% Mo, 0.50% V, +Al, Nb
1.10% C, 0.90% Si, 0.40% Mn, 0.005% S, 8.25% Cr, 2.15% Mo, 0.30% V
1.10% C, 0.90% Si, 0.40% Mn, 8.25% Cr, 2.15% Mo, 0.30% V, 0.50% W, 0.15% Ni, 0.75% Nb
1.10% C, 0.90% Si, 0.40% Mn, 8.30% Cr, 2.10% Mo, 0.50% V + Additions
1.10% C, 1.00% Si, 0.35% Mn, 7.90% Cr, 1.50% Mo, 2.20% V, 1.20% W
1.10% C, 1.00% Si, 5.25% Cr, 1.10% Mo, 4.00% V
1.10% C, 1.20% Si, 0.25% Mn, 7.75% Cr, 1.60% Mo, 2.35% V, 1.10% W
1.10% C, 1.20% Si, 0.25% Mn, 7.75% Cr, 1.60% Mo, 2.35% V, 1.10% W
1.10% C, 12.00% Cr, 0.80% W
1.10% C, 17.00% Cr, 0.70% Mo
1.10% C, 3.75% Cr, 9.50% Mo, 1.15% V, 1.50% W, 8.00% Co
1.10% C, 4.00% Cr, 9.50% Mo, 1.00% V, 1.50% W, 8.00% Co
1.10% C, 4.00% Cr, 9.50% Mo, 1.10% V, 1.50% W, 8.00% Co
1.10% C, 7.50% Cr, 1.50% Mo, 2.10% V, 1.10% W
1.10% C, 7.50% Cr, 1.50% Mo, 2.10% V, 1.10% W
1.10% C, 7.50% Cr, 1.50% Mo, 2.10% V, 1.10% W
1.10% C, 7.50% Cr, 1.60% Mo, 2.40% V, 1.15% W
1.10% C, 8.60% Cr, 2.50% Mo, 0.50% V
1.10-1.20% C, 0.15-0.30% Si, 0.20-0.40% Mn, 0.035% P, 0.035% S, 0.15-0.25% Cr, 1.80-2.10% W
1.10-1.20% C, 0.80-1.00% Si, 0.30-0.50% Mn, 0.030% P, 0.030% P, 8.00-9.00% Cr, 1.40-1.60% Mo, 1.90-2.00% V, 1.40-1.60% W
1.10-1.25% C, 0.15-0.30% Si, 0.20-0.40% Mn, 0.030% P, 0.030% S, 0.50-0.80% Cr, 0.07-0.12% V
1.10-1.25% C, 0.15-0.30% Si, 0.20-0.40% Mn, 0.030% P, 0.030% S, 0.50-0.80% Cr, 0.07-0.12% V
1.10% C, 0.90% Si, 0.40% Mn, 8.30% Cr, 2.10% Mo, 0.50% V + Nb, Al
1.13% C, 0.30% Mn, 1.20% Si, 7.75% Cr, 1.10% W, 1.55% Mo, 2.40% V
1.13% C, 1.20% Si, 0.30% Mn, 7.75% Cr, 1.55% Mo, 2.40% V, 1.10% W
1.13% C, 1.20% Si, 0.30% Mn, 7.75% Cr, 1.55% Mo, 2.40% V, 1.10% W
1.13% C, 7.70% Cr, 1.50% Mo, 2.45% V, 1.10% W
1.14% C, 0.88% Si, 0.33% Mn, 0.025% P, 0.007% S, 8.24% Cr, 1.39% Mo, 0.09% Ni, 1.96% V, 1.40% W, 0.050% Cu
1.14% C, 0.88% Si, 0.33% Mn, 0.025% P, 0.007% S, 8.24% Cr, 1.39% Mo, 1.96% V, 1.40% W, 0.05% Cu
1.145% C, 0.552% Si, 0.492% Mn, 16.01% Cr
1.145% C, 0.552% Si, 0.492% Mn, 16.010% Cr
1.15% C, 0.30% Si, 0.50% Mn, 14.50% Cr, 4.00% Mo, 1.20% V
1.15% C, 0.30% Si, 0.50% Mn, 14.50% Cr, 4.00% Mo, 1.20% V
1.15% C, 0.90% Si, 0.40% Mn, 8.50% Cr, 1.50% Mo, 1.95% V, 1.50% W
1.15% C, 0.90% Si, 0.40% Mn, 8.50% Cr, 1.50% Mo, 1.95% V, 1.50% W
1.15% C, 19.00% Cr, 2.10% Mo, 0.60% V, + N
1.15% C, 19.00% Cr, 2.10% Mo, 0.60% V, +N
1.15% C, 7.50% Cr, 1.00% Mo, 2.40% V, 1.00% W
1.15-1.25% C, 0.10-0.30% Si, 0.10-0.40% Mn, 0.030% P, 0.030% S
1.15-1.25% C, 0.10-0.30% Si, 0.10-0.40% Mn, 0.030% P, 0.030% S
1.15-1.25% C, 0.15-0.30% Si, 0.20-0.35% Mn, 0.035% P, 0.035% S, 0.15-0.25% Cr, 0.07-0.12% V, 0.90-1.20% W
1.15-1.25% C, 0.15-0.30% Si, 0.20-0.35% Mn, 0.035% P, 0.035% S, 0.15-0.25% Cr, 0.90-1.10% W
1.15-1.25% C, 0.15-0.30% Si, 0.20-0.35% Mn, 0.035% P, 0.035% S, 0.15-0.25% Cr, 0.07-0.12% V, 0.90-1.10% W
1.15-1.25% C, 0.15-0.30% Si, 0.20-0.35% Mn, 0.035% P, 0.035% S, 0.15-0.25% Cr, 0.90-1.10% W, 0.07-0.12% V
1.15-1.25% C, 0.15-0.30% Si, 0.20-0.35% Mn, 0.15-0.25% Cr, 0.07-0.12% V, 0.90-1.10% W
1.15-1.25% C, 0.15-0.35% Si, 0.20-0.35% Mn, 0.035% P, 0.035% S, 0.15-0.25% Cr, 0.90-1.10% W, 0.07-0.12% V
1.15-1.25% C, 0.45% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.80-4.50% Cr, 4.70-5.20% Mo, 5.90-6.70% W, 2.70-3.20% V
1.17% C, 0.23% Si, 0.30% Mn, 0.65% Cr, 0.10% V
1.18% C, 0.25% Si, 0.30% Mn, 0.70% Cr, 0.10% V
1.18% C, 0.25% Si, 0.30% Mn, 0.70% Cr, 0.10% V
1.2% C, 3.9% Cr, 5.2% Mo, 2.7% V, 7% W
1.20% C, 0.20% Cr, 0.10% V, 1.00% W
1.20% C, 0.20% Cr, 0.10% V, 1.00% W
1.20% C, 0.20% Si, 0.30% Mn
1.20% C, 0.30% Si, 0.25% Mn, 4.10% Cr, 5.00% Mo, 3.00% V, 6.00% W
1.20% C, 0.30% Si, 0.30% Mn, 11.50% Cr, 1.40% Mo, 1.70% V, 2.40% W
1.20% C, 0.30% Si, 0.30% Mn, 11.50% Cr, 1.40% Mo, 1.70% V, 2.40% W
1.20% C, 0.45% Si, 0.40% Mn, 4.15% Cr, 4.95% Mo, 2.95% V, 3.35% W
1.20% C, 0.70% Cr, 0.10% V
1.20% C, 0.70% Cr, 0.10% V
1.20% C, 0.70% Cr, 0.10% V
1.20% C, 0.70% Cr, 0.10% V
1.20% C, 11.00% Cr, 1.40% Mo, 1.50% V, 2.40% W
1.20% C, 12.00% Cr, 1.40% Mo, 1.70% V, 2.50% W
1.20% C, 12.00% Cr, 1.40% Mo, 2.50% W
1.20% C, 4.00% Cr, 6.50% Mo, 5.20% W, 2.80% V
1.20% C, 4.00% Cr, 5.00% Mo, 3.00% V, 6.20% W
1.20% C, 4.1% Cr, 5.0% Mo, 3.0% V, 6.2% W
1.20% C, 4.20% Cr, 7.50% Mo, 2.90 % V, 4.50% W
1.20% C, 7.80% Cr, 3.25% Mo, 3.50% V, 0.50% W
1.20-1.30% C, 0.15-0.35% Si, 0.25-0.40% Mn, 0.025% P, 0.025% S, 0.40-0.60% Cr, 0.10% Mo, 0.40% Ni
1.20-1.30% C, 1.05-1.25% Si, 0.60-0.80% Mn, 0.035% P, 0.035% S, 1.10-1.30% Cr
1.20-1.30% C, 3.80-4.50% Cr, 3.00-4.00% Mo, 3.20-3.70% V, 9.00-11.00% W, 9.50-10.50% Co
1.20-1.35% C, 0.10-0.30% Si, 0.10-0.35% Mn, 0.030% P, 0.030% S
1.20-1.35% C, 0.45% Si, 0.30% Mn, 0.030% P, 0.030% S, 3.80-4.50% Cr, 3.20-3.90% Mo, 3.20-3.50% V, 9.00-10.00% W, 9.50-10.50% Co
1.20-1.35% C, 0.45% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.80-4.50% Cr, 0.70-1.00% Mo, 11.50-12.50% W, 3.50-4.00% V
1.20-1.35% C, 0.45% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.80-4.50% Cr, 3.20-3.90% Mo, 9.00-10.00% W, 3.00-3.50% V, 9.50-10.50% Co
1.20-1.35% C, max.0.45% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.80-4.50% Cr, 3.20-3.90% Mo, 3.00-3.50% V, 9.00-10.00% W, 9.50-10.50% Co
1.20-1.35% C, max.0.45% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.80-4.50% Cr, 3.20-3.90% Mo, 3.00-3.50% V, 9.00-10.00% W, 9.50-10.50% Co
1.20???1.35% C, max 0.25% Si, 0.15???0.35% Mn, 0.030% P, 0.035% S, max 0.20% Cr, 0.20% Ni
1.21% C, 0.25% Si, 0.30% Mn, 4.10% Cr, 5.00% Mo, 2.90% V, 6.40% W
1.21% C, 4.25% Cr, 5.0% Mo, 3.0% V, 6.0% W
1.22% C, 0.18% Si, 0.20% Mn, 0.10% V
1.23-1.32% C, 0.70% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.80-4.50% Cr, 4.70-5.30% Mo, 2.70-3.20% V, 5.90-6.70% W, 8.00-8.80% Co
1.23-1.33% C, 0.70% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.80-4.50% Cr, 4.70-5.30% Mo, 5.90-6.70% W, 2.70-3.20% V, 8.00-8.80% Co
1.25% C, 0.30% Si, 0.30% Mn, 10.00% Cr, 0.80% Mo, 1.00% V, +Ti
1.25% C, 0.30% Si, 0.30% Mn, 4.00% Cr, 5.00% Mo, 3.00% V, 6.20% W
1.25% C, 0.70% Si, 0.50% Mn, 4.12% Cr, 5.00% Mo, 2.95% V, 6.32% W, 8.38% Co
1.25% C, 0.70% Si, 0.50% Mn, 4.15% Cr, 5.00% Mo, 2.05% V, 6.30% W, 1.00% Co
1.25% C, 0.70% Si, 0.50% Mn, 4.15% Cr, 5.00% Mo, 2.05% V, 6.30% W, 1.00% Co
1.25% C, 0.90% Si, 0.35% Mn, 8.75% Cr, 2.70% Mo, 1.18% Mo, + Additions
1.25% C, 0.90% Si, 0.35% Mn, 8.75% Cr, 2.70% Mo, 1.18% V
1.25% C, 0.90% Si, 0.35% Mn, 8.75% Cr, 2.70% Mo, 1.18% V
1.25% C, 4.00% Cr, 0.80% Mo, 3.60% V, 12.00% W
1.25% C, 4.00% Cr, 8.00% Mo, 2.80% V, 3.50% W
1.25-1.32% C, 0.70% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.80-4.50% Cr, 4.70-5.20% Mo, 5.90-6.70% W, 2.70-3.20% V
1.25-1.32% C, 0.70% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.80-4.50% Cr, 4.70-5.20% Mo, 5.90-6.70% W, 2.70-3.20% V
1.25-1.32% C, 0.70% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.80-4.50% Cr, 4.70-5.20% Mo, 2.70-3.20% V, 5.90-6.70% W
1.25-1.35% C, 0.20-0.30% Si, 0.20-0.40% Mn, 0.035% P, 0.035% S, 0.20% Cr, 4.70-5.20% W
1.25-1.40% C, 0.45% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.80-4.50% Cr, 4.20-5.00% Mo, 5.20-6.00% W, 3.70-4.20% V
1.25-1.50% C, 0.20-0.45% Si, 0.15-0.40% Mn, 3.75-4.75% Cr, 4.25-5.50% Mo, 3.75-4.50% V, 5.25-6.50% W
1.25-1.50% C, 1.00-1.50% Si, 1.60-2.10% Mn, 1.25-1.75% Mo, 1.55-2.05% Ni
1.25-1.55% C, 0.55-1.50% Si, 0.30-1.10% Mn, 0.30% Cr, 0.20-0.30% Mo
1.26% C, 0.25% Si, 0.30% Mn, 4.00% Cr, 3.60% Mo, 3.20% V, 9.30% W, 10.00% Co
1.26% C, 0.25% Si, 0.30% Mn, 4.00% Cr, 3.60% Mo, 3.20% V, 9.30% W, 10.00% Co
1.27% C, 0.55% Si, 0.30% Mn, 0.030% S, 4.20% Cr, 5.00% Mo, 3.10% V, 6.25% W
1.27% C, 0.55% Si, 0.30% Mn, 0.030% S, 4.20% Cr, 5.00% Mo, 3.10% V, 6.25% W
1.27% C, 4.0% Cr, 3.6% Mo, 3.2% V, 9.5% W, 10.0% Co
1.27-1.37% C, 3.70-4.70% Cr, 4.60-5.40% Mo, 2.80-3.30% V, 5.60-6.40% W, 7.50-8.50% Co
1.28% C, 0.4% Mn, 0.13% S, 4.0% Cr, 5.4% Mo, 3.1% V, 6.4% W
1.28% C, 0.45% Si, 0.40% Mn, 4.15% Cr, 0.85% Mo, 3.75% V, 12.00% W
1.28% C, 0.45% Si, 0.40% Mn, 4.15% Cr, 3.55% Mo, 3.25% V, 9.50% W, 10.00% Co
1.28% C, 4.0% Cr, 5.0% Mo, 3.1% V, 6.4% W
1.28% C, 4.00% Cr, 4.90% Mo, 3.00% V, 6.20% W
1.28% C, 4.2% Cr, 5.0% Mo, 3.1% V, 6.4% W, 8.5% Co
1.28% C, 4.20% Cr, 5.00% Mo, 3.10% V, 6.40% W, 8.50% Co
1.28% C, 4.20% Cr, 5.00% Mo, 3.10% V, 6.40% W
1.28% C, 4.20% Cr, 5.00% Mo, 6.40% W, 3.10%V, 8.50% Co
1.28% C, 4.20% Cr, 5.00% Mo, 3.10% V, 6.40% W, 8.50% Co
1.28% C, 4.20% Cr, 5.00% Mo, 3.10% V, 6.40% W
1.28% C, 4.20% Cr, 5.00% Mo, 6.40% W, 3.10% V
1.28% C, 4.28% Cr, 5.00% Mo, 3.10% V, 6.40% W
1.3% C, 4.0% Cr, 6.0% W, 5.0% Mo, 3.0% V, 8.0% Co
1.3% C, 5.0% Cr, 3.0% W, 6.0% Mo, 4.0% V
1.30% C, 0.06 (0.22%)% S, 3.75% Cr, 2.00% V, 6.25% W, 10.50% Mo
1.30% C, 0.06(0.22)% S, 4.05% Cr, 3.05% V, 5.00% Mo, 6.25% W, 8.00% Co
1.30% C, 0.25% Si, 0.30% Mn, 0.25% Cr
1.30% C, 0.25% Si, 0.30% Mn, 0.25% Cr
1.30% C, 0.30% Si, 0.30% Mn, 4.50% Cr, 4.50% Mo, 4.00% V, 5.50% W
1.30% C, 0.35% Si, 0.30% Mn, 4.20% Cr, 5.00% Mo, 3.10% V, 6.30% W
1.30% C, 0.50% Si, 0.30% Mn, 4.10% Cr, 5.00% Mo, 3.10% V, 6.25% W, 8.25% Co
1.30% C, 0.50% Si, 0.30% Mn, 4.10% Cr, 5.00% Mo, 3.10% V, 6.25% W, 8.25% Co
1.30% C, 0.50% Si, 0.30% Mn, 4.20% Cr, 5.00% Mo, 3.00% V, 6.30% W, 8.40% Co
1.30% C, 0.50% Si, 0.30% Mn, 4.20% Cr, 5.00% Mo, 3.00% V, 6.30% W
1.30% C, 0.50% Si, 0.40% Mn, 4.50% Cr, 1.80% Mo, 10.00% V, 1.80% N
1.30% C, 0.60% Si, 0.70% Mn, 0.050% S, 3.75% Cr, 10.50% Mo, 2.00% V, 6.25% W
1.30% C, 4.00% Cr, 3.5% Mo, 3.50% V, 10.00% W, 10.00% Co
1.30% C, 4.00% Cr, 5.00% Mo, 3.00% V, 6.00% W, 8.00% Co
1.30% C, 4.00% Cr, 5.00% Mo, 3.00% V, 6.5% W, 8.00% Co
1.30% C, 4.00% Cr, 5.00% Mo, 3.00% V, 6.5% W
1.30% C, 4.2% Cr, 4.5% Mo, 4.0% V, 5.6% W
1.30% C, 4.20% Cr, 4.50% Mo, 4.00% V, 5.60% W
1.30% C, 4.20% Cr, 5.00% Mo, 3.10% V, 6.40% W, 8.50% Co
1.30% C, 4.20% Cr, 5.00% Mo, 3.10% V, 6.40% W, 8.50% Co
1.30% C, 4.20% Cr, 5.00% Mo, 3.10% V, 6.40% W
1.30-1.40% C, 4.50-5.50% Cr, 5.50-6.50% Mo, 3.60-4.00% V, 2.50-3.50% W
1.30-1.45% C, 0.10-0.30% Si, 0.10-0.35% Mn, 0.030% P, 0.030% S
1.30-1.45% C, 0.45% Si, 0.40% Mn, 0.030% P, 0.030% S, 3.80-4.50% Cr, 0.70-1.00% Mo, 11.50-12.50% W, 3.50-4.50% V, 4.50-5.00% Co
1.32% C, 0.30% Si, 0.25% Mn, 4.50% Cr, 4.40% Mo, 3.85% V, 5.35% W
1.33% C, 0.35% Si, 0.30% Mn, 4.30% Cr, 4.00% Mo, 4.10% V, 5.90% W
1.33% C, 0.45% Si, 0.40% Mn, 4.15% Cr, 4.60% Mo, 3.95% V, 5.60% W
1.35% C, 4.10% Cr, 5.00% Mo, 4.10% V, 5.90% W
1.35% C, 4.20% Cr, 4.50% Mo, 4.00% V, 5.80% W
1.35-1.45% C, 0.15-0.35% Si, 0.25-0.40% Mn, 0.025% P, 0.025% S, 0.20-0.40% Cr, 0.10-0.15% V
1.35-1.50% C, 0.15-0.30% Si, 0.25-0.40% Mn, 0.035% P, 0.035% S, 0.40-0.70% Cr
1.35-1.55% C, 0.15-0.30% Si, 0.20-0.40% Mn, 0.035% P, 0.035% S, 0.20-0.50% Cr, 2.80-3.30% W, 0.20-0.30% V
1.38% C, 0.20% Si, 0.23% Mn
1.38% C, 0.45% Si, 0.40% Mn, 0.00% Cr, 0.85% Mo, 3.75% V, 12.00% W, 4.75% Co
1.40% C, 0.40% Si, 0.40% Mn, 4.70% Cr, 3.50% Mo, 3.70% V
1.40% C, 0.40% Si, 0.40% Mn, 4.70% Cr, 3.50% Mo, 3.70% V
1.40% C, 0.40% Si, 0.40% Mn, 4.70% Cr, 3.50% Mo, 3.70% V
1.40% C, 0.40% Si, 0.40% Mn, 4.70% Cr, 3.50% Mo, 3.70% V
1.40% C, 0.40% Si, 0.40% Mn, 4.70% Cr, 3.50% Mo, 3.70% V
1.40% C, 1.00% Si, 0.60% Mn, 4.60% Cr, 3.20% Mo, 3.70% V
1.40% C, 1.00% Si, 0.60% Mn, 4.60% Cr, 3.20% Mo, 3.70% V
1.40% C, 1.00% Si, 0.60% Mn, 4.60% Cr, 3.20% Mo, 3.70% V
1.40% C, 1.00% Si, 0.60% Mn, 4.60% Cr, 3.20% Mo, 3.70% V
1.40% C, 1.20% Si, 0.30% Mn, 7.80% Cr, 1.30% Mo, 3.80% V, 1.70% W
1.40% C, 15.00% Cr, 2.00% Mo, 4.50% Nb
1.40% C, 6.40% Cr, 1.50% Mo, 3.70% W, 3.50% W, +Nb
1.40-1.50% C, 0.20-0.35% Si, 0.30-0.50% Mn, 0.030% P, 0.030% S, 3.00-3.50% V
1.40-1.60% C, 0.10-0.60% Si, 0.10-0.60% Mn, 11.0-13.0% Cr, 0.70-1.20% Mo, 0.50-1.10% V
1.40-1.60% C, 0.15-0.30% Si, 0.50-0.70% Mn, 0.035% P, 0.035% S, 1.30-1.50% Cr
1.40-1.60% C, 0.40% Si, 0.40% Mn, 0.030% P, 0.030% S, 11.00-13.00% Cr, 0.80-1.20% Mo, 0.20-0.50% V
1.40-1.60% C, 0.40% Si, 0.60% Mn, 0.030% P, 0.030% S, 11.00-13.00% Cr, 0.80-1.20% Mo, 0.50% Ni, 0.20-0.50% V, 0.25% Cu
1.40-1.60% C, 0.40% Si, 0.60% Mn, 11.00-13.00% Cr, 0.80-1.20% Mn, 0.20-0.50% V
1.40-1.60% C, 0.40% Si, 0.60% Mn, 11.00-13.00% Cr, 0.80-1.20% Mo, 0.20-0.50% V
1.40-1.60% C, 0.60% Si, 0.60% Mn, 0.030% P, 0.030% S, 11.00-13.50% Cr, 0.70-1.20% Mo, 0.80-1.10% V, 1.00% Co
1.41% C, 4.2% Cr, 3.6% Mo, 3.4% V, 8.8% W, 11.0% Co
1.42% C, 0.23% Si, 0.33% Mn, 0.55% Cr
1.42% C, 0.30(0.70)% Mn, 0.06(0.22)% S, 4.00% Cr, 5.25% Mo, 4.00% V, 5.50% W
1.42% C, 0.55% Si, 0.30% Mn, 4.00% Cr, 5.25% Mo, 4.00% V, 5.50% W
1.43% C, 0.23% Si, 0.30% Mn, 0.35% Cr, 0.25% V, 3.05% W
1.45% C, 0.25% Si, 0.25% Mn, 4.50% Cr, 5.20% Mo, 3.85% V, 5.50% W
1.45% C, 0.28% Si, 0.40% Mn, 3.25% V
1.45% C, 0.30% Si, 0.40% Mn, 3.25% V
1.45% C, 0.30% Si, 0.40% Mn, 3.25% V
1.45% C, 0.40% Si, 0.40% Mn, 0.13% S, 4.50% Cr, 4.50% Mo, 4.00% V, 5.75% W
1.45% C, 0.90% Si, 1.00% Mn, 0.25% Mo
1.45% C, 0.90% Si, 1.00% Mn, 0.25% Mo
1.45% C, 0.90% Si, 1.00% Mn, 0.25% Mo
1.45% C, 1.00% Si, 0.85% Mn, 0.25% Mo
1.45% C, 14.00% Cr, 2.00% Mo, 4.00% V
1.45-1.60% C, 0.10-0.60% Si, 0.20-0.60% Mn, 0.030% P, 0.030% S, 11.00-13.00% Cr, 0.70-1.00% Mo, 0.70-1.00% V
1.45-1.60% C, 0.10-0.60% Si, 0.20-0.60% Mn, 0.030% P, 0.030% S, 11.00-13.00% Cr, 0.70-1.00% Mo, 0.70-1.00% V
1.45-1.60% C, 0.10-0.60% Si, 0.20-0.60% Mn, 0.030% P, 0.030% S, 11.00-13.00% Cr, 0.70-1.00% Mo, 0.70-1.00% V
1.45-1.60% C, 0.10-0.60% Si, 0.20-0.60% Mn, 0.030% P, 0.030% S, 11.00-13.00% Cr, 0.70-1.00% Mo, 0.70-1.00% V
1.45-1.60% C, 0.10-0.60% Si, 0.20-0.60% Mn, 0.030% P, 0.030% S, 11.00-13.00% Cr, 0.70-1.00% Mo, 0.70-1.00% V
1.45-1.60% C, 0.10-0.60% Si, 0.20-0.60% Mn, 0.030% P, 0.030% S, 11.00-13.00% Cr, 0.70-1.00% Mo, 0.70-1.00% V
1.45-1.60% C, 0.10-0.60% Si, 0.20-0.60% Mn, 0.030% P, 0.030% S, 11.00-13.00% Cr, 0.70-1.00% Mo, 0.70-1.00% V
1.45-1.60% C, 0.10-0.60% Si, 0.20-0.60% Mn, 0.03% P, 0.03% S, 11.00-13.00% Cr, 0.70-1.00% Mo, 0.70-1.00% V
1.46% C, 0.40% Si, 0.40% Mn, 0.13% S, 4.50% Cr, 4.50% Mo, 4.00% V, 5.75% W
1.50% C, 0.010% S, 4.00% Cr, 2.50% Mo, 4.00% V, 2.50% W
1.50% C, 0.07(0.22)% S, 3.75% Cr, 5.25% Mo, 3.10% V, 9.75% W, 8.50% Co
1.50% C, 0.20% Si, 0.40% Mn, 12.00% Cr, 1.00% Mo, 0.35% V
1.50% C, 0.23% Si, 0.60% Mn, 1.40% Cr
1.50% C, 0.25% Si, 0.25% Mn, 0.85% Cr, 0.20% V
1.50% C, 0.25% Si, 0.25% Mn, 11.25% Cr, 0.80% Mo, 0.85% V
1.50% C, 0.25% Si, 0.45% Mn, 0.025% P, 0.010% S, 12.00% Cr, 1.00% Mo, 0.35% V
1.50% C, 0.25% Si, 0.60% Mn, 1.40% Cr
1.50% C, 0.25% Si, 0.60% Mn, 1.40% Cr
1.50% C, 0.30% Si, 0.30% Mn, 12.00% Cr, 0.75% Mo, 0.90% V
1.50% C, 0.30% Si, 0.30% Mn, 12.00% Cr, 0.75% Mo, 0.90% V
1.50% C, 0.30% Si, 0.30% Mn, 12.00% Cr, 0.75% Mo, 0.90% V
1.50% C, 0.30% Si, 12.00% Cr, 0.95% Mo, 0.90% V
1.50% C, 0.30% Si, min. 0.30% Mn, min. 0.060% S, 3.75% Cr, 5.25% Mo, 3.10% V, 9.75% W
1.50% C, 0.40% Si, 0.40% Mn, 12.00% Cr, 0.95% Mo, 1.00% V
1.50% C, 0.40% Si, 0.40% Mn, 12.00% Cr, 0.95% Mo, 1.00% V
1.50% C, 0.50% Si, 0.35% Mn, 11.65% Cr, 0.80% Mo, 2.80% Co
1.50% C, 0.50% Si, 0.35% Mn, 11.65% Cr, 0.80% Mo, 2.80% Co
1.50% C, 1.00% Si, 0.40% Mn, 8.00% Cr, 1.50% Mo, 4.00% V
1.50% C, 1.00% Si, 0.40% Mn, 8.00% Cr, 1.50% Mo, 4.00% V
1.50% C, 12.00% Cr, 0.90% Mo, 0.90% V
1.50% C, 4.0% Cr, 2.5% Mo, 4.0% V, 2.5% W
1.50-1.60% C, 0.10-0.40% Si, 0.15-0.45% Mn, 11.00-12.00% Cr, 0.60-0.80% Mo, 0.90-1.10% V
1.50-1.60% C, 0.15-10.40% Si, 0.15-0.40% Mn, 3.75-5.00% Cr, 4.50-5.25% V, 4.75-5.25% Co, 11.75-13.00% W
1.51% C, 0.32% Si, 0.27% Mn, 0.019% P, 0.016% S, 11.60% Cr, 0.63% Mo, 0.20% Ni, 0.91% V, 0.02% W
1.51% C, 0.32% Si, 0.27% Mn, 0.019% P, 0.016% S, 11.60% Cr, 0.63% Mo, 0.20% Ni, 0.91% V, 0.02% W
1.53% C, 0.25% Si, 0.25% Mn, 4.90% Cr, 5.00% Ni, 6.50% V, 4.90% Co
1.53% C, 0.30% Si, 0.35% Mn, 12.00 Cr, 0.80% Mo, 0.80% V
1.53% C, 0.35% Si, 0.40% Mn, 12.00% Cr, 1.00% Mo, 0.85% V
1.54-1.64% C, 3.70-4.70% Cr, 5.50-6.50% Mo, 3.80-4.30% V, 7.50-8.50% W, 7.50-8.50% Co
1.55% C, 0.070% S, 4.00% Cr, 5.25% Mo, 3.10% V, 10.00% W, 9.00% Co
1.55% C, 0.20% Si, 0.30% Mn, 0.030% P, 0.005% S, 12.00% Cr, 0.80% Mo, 1.00% V
1.55% C, 0.20% Si, 0.30% Mn, 0.030% P, 0.005% S, 12.00% Cr, 0.80% Mo, 1.00% V
1.55% C, 0.30% Si, 0.25% Mn, 12.00% Cr, 0.80% V
1.55% C, 0.30% Si, 0.30% Mn, 11.30% Cr, 0.75% Mo, 0.75% V
1.55% C, 0.30% Si, 0.30% Mn, 11.30% Cr, 0.75% Mo, 0.75% V
1.55% C, 0.30% Si, 0.30% Mn, 12.00% Cr, 0.80% Mo, 0.90% V
1.55% C, 0.30% Si, 0.30% Mn, 4.00% Cr, 5.00% V, 12.00% W, 5.00% Co
1.55% C, 0.30% Si, 0.35% Mn, 0.020% P, 0.005% S, 11.75% Cr, 0.75% Mo, 0.75% V
1.55% C, 0.30% Si, 0.35% Mn, 0.020% P, 0.005% S, 11.75% Cr, 0.85% Mo, 0.30% V
1.55% C, 0.30% Si, 0.35% Mn, 12.00% Cr, 0.75% Mo, 0.90% V
1.55% C, 0.30% Si, 0.35% Mn, 12.00% Cr, 0.75% Mo, 0.90% V
1.55% C, 0.30% Si, 0.35% Mn, 12.00% Cr, 0.75% Mo, 0.90% V
1.55% C, 0.30% Si, 0.35% Mn, 12.00% Cr, 0.75% Mo, 0.90% V
1.55% C, 0.30% Si, 0.40% Mn, 11.30% Cr, 0.80% Mo, 0.80% V
1.55% C, 0.30% Si, 0.40% Mn, 11.30% Cr, 0.80% Mo, 0.80% V
1.55% C, 0.30% Si, 0.40% Mn, 11.50% Cr, 0.70% Mo, 0.10% V
1.55% C, 0.30% Si, 0.40% Mn, 11.50% Cr, 0.70% Mo, 0.10% V
1.55% C, 0.30% Si, 0.40% Mn, 11.50% Cr, 0.70% Mo, 1.00% V
1.55% C, 0.30% Si, 0.40% Mn, 11.50% Cr, 0.70% Mo, 1.00% V
1.55% C, 0.30% Si, 0.40% Mn, 11.80% Cr, 0.80% Mo, 0.80% V
1.55% C, 0.30% Si, 0.40% Mn, 11.80% Cr, 0.80% Mo, 0.80% V
1.55% C, 0.30% Si, 0.40% Mn, 11.80% Cr, 0.80% V, 0.80% Mo
1.55% C, 0.35% Si, 0.35% Mn, 12.00% Cr, 0.90% Mo, 0.90% V
1.55% C, 0.40% Si, 0.20% Mn, 4.00% Cr, 5.25% Mo, 3.10% V, 10.00% W, 9.00% Co
1.55% C, 0.40% Si, 0.40% Mn, 12.00% Cr, 0.90% Mo, 0.90% V
1.55% C, 1.00% Si, 0.65% Mn, 9.00% Cr, 2.00% Mo, 1.95% V, 1.00% Nb, 0.10% N
1.55% C, 1.00% Si, 0.65% Mn, 9.00% Cr, 2.00% Mo, 1.95% V, 1.00% Nb, 0.10% N
1.55% C, 11.50% Cr, 0.80% Mo, 0.80% V
1.55% C, 12.00% Cr, 0.80% Mo, 0.90% V
1.55% C, 12.00% Cr, 0.70% Mo, 1.00% V
1.55% C, 12.00% Cr, 0.75% Mo, 0.90% V
1.55% C, 12.00% Cr, 0.80% Mo, 0.90% V
1.55% C, 12.00% Cr, 0.80% Mo, 0.90% V
1.55% C, 12.00% Cr, 0.80% Mo, 0.90% V
1.55% C, 4.0% Cr, 12% W, 5.0% Co, 5.0% W
1.55% C, 4.00% Cr, 5.00% V, 13.00% W, 5.00% Co
1.55-1.75% C, 0.25-0.40% Si, 0.20-0.40% Mn, 0.030% P, 0.030% S, 11.00-12.00% Cr, 0.070-0.12% V
1.55-1.75% C, 0.25-0.40% Si, 0.20-0.40% Mn, 0.030% P, 0.030% S, 11.00-12.00% Cr, 0.50-0.70% Mo, 0.10-0.50% V, 0.40-0.60% W
1.55-1.75% C, 0.25-0.40% Si, 0.20-0.40% Mn, 0.030% P, 0.030% S, 11.00-12.00% Cr, 0.50-0.70% Mo, 0.40-0.60% W, 0.10-0.50% V
1.55-1.75% C, 0.25-0.40% Si, 0.20-0.40% Mn, 0.035% P, 0.035% S, 11.00-12.00% Cr, 0.50-0.60% Mo, 0.00% Ni, 1.20-1.40% Co
1.55% C, 0.30% Si, 0.30% Mn, 11.50% Cr, 0.70% Mo, 1.00% V
1.57% C, 0.50% Si, 0.30% Mn, 4.00% Cr, 0.50% Mo, 5.00% V, 12.25% W, 5.00% Co
1.58% C, 0.30% Si, 0.25% Mn, 0.024% P, 0.014% S, 11.37% Cr, 0.79% Mo, 1.04% V
1.60% C, 0.06(0.22)% S, 4.00% Cr, 4.90% V, 12.00% W, 5.00% Co
1.60% C, 0.30% Si, 0.30% Mn, 4.25% Cr, 0.75% Mo, 5.00% V, 12.25% W, 5.00% Co
1.60% C, 0.30% Si, 0.30% Mn, min. 0.06% S, 4.0% Cr, 5.0% Co, 4.90% V, 12.0% W
1.60% C, 0.30% Si, 0.50% Mn, 5.00% Cr, 2.30% Mo, 7.00% V
1.60% C, 0.35% Si, 0.30% Mn, 11.50% Cr, 0.60% Mo, 0.30% V, 0.50% W
1.60% C, 0.35% Si, 0.30% Mn, 4.25% Cr, 5.00% V, 12.25% W, 5.00% Co
1.60% C, 12.00% Cr, 0.10% V
1.60% C, 4.8% Cr, 2.0% Mo, 5.0% V, 10.5% W, 8.0% Co
1.60% C, 4.80% Cr, 2.00% Mo, 5.00% V, 10.50% W, 8.00% Co
1.60% C, 4.80% Cr, 2.00% Mo, 5.00% V, 10.50% W, 8.00% Co
1.60% C, 4.80% Cr, 2.30% Mo, 5.10% V, 10.00% W, 7.90% Co
1.64% C, 0.60% Si, 0.30% Mn, 4.80% Cr, 2.00% Mo, 4.80% V, 10.40% W, 8.00% Co
1.64% C, 0.60% Si, 0.30% Mn, 4.80% Cr, 2.00% Mo, 4.80% V, 10.40% W. 8.00% Co
1.65% C, 0.30% Si, 0.30% Mn, 0.025% P, 0.010% S, 12.00% Cr, 0.60% Mo, 0.30% V, 0.50% W
1.65% C, 0.30% Si, 0.30% Mn, 11.50% Cr, 0.60% Mo, 0.30% V, 0.50% W
1.65% C, 0.30% Si, 0.30% Mn, 11.50% Cr, 0.60% Mo, 0.30% V, 0.50% W
1.65% C, 0.30% Si, 0.40% Mn, 11.50% Cr, 0.55% Mo, 1.30% Co
1.65% C, 0.32% Si, 0.40% Mn, 11.50% Cr, 0.10% V
1.65% C, 0.33% Si, 0.30% Mn, 11.50% Cr, 0.60% Mo, 0.30% V, 0.50% W
1.65% C, 12.00% Cr, 0.50% Mo, 0.50% W, 0.25% V
1.65% C, 12.00% Cr, 0.60% Mo, 0.50% W, 0.30% V
1.69% C, 4.0% Cr, 4.6% Mo, 3.2% V, 6.3% W, 9.0% Co, 2.1% Nb
1.7% C, 0.8% Si, 0.3% Mn, 18.0% Cr, 1.0% Mo, 3.0% V
1.70% C, 0.30% Si, 0.30% Mn, 11.50% Cr, 0.10% V
1.70% C, 0.80% Si, 0.30% Mn, 18.00% Cr, 1.00% Mo, 3.00% V
1.70% C, 0.80% Si, 0.30% Mn, 18.00% Cr, 1.00% Mo, 3.00% V
1.70% C, 0.80% Si, 0.30% Mn, 18.00% Cr, 1.00% Mo, 3.00% V
1.70% C, 1.00% Si, 0.40% Mn, 8.35% Cr, 1.40% Mo, 1.50% Ni, 1.00% V
1.70-1.85% C, 0.75-1.10% Si, 0.35-0.60% Mn, 0.030% S, 4.75-5.75% Cr, 1.10-1.50% Mo, 8.25-9.50% V
1.7220, 1.7226
1.75% C, 0.22% Mn, 13.00% Cr
1.80% C, 0.07% S, 4.25% Cr, 5.00% V, 12.25% W, 5.00% Co
1.80% C, 0.90% Si, 0.50% Mn, 5.25% Cr, 1.35% Mo, 9.00% V
1.80???2.05% C, 0.02???0.45% Si, 0.02???0.45% Mn, 0.03% P, 0.035% S, 11.0???12.50% Cr, 0.50% Ni
1.86% C, 0.34% Si, 0.32% Mn, 0.020% P, 0.008% S, 19.70% Cr, 0.13% Mo, 0.19% Ni, 0.75% V, 0.04% Cu
1.86% C, 0.34% Si, 0.32% Mn, 0.020% P, 0.008% S, 19.70% Cr, 0.13% Mo, 0.19% Ni, 0.75% V, 0.04% Cu
1.9% C, 5.25% Cr, 1.3% Mo, 9.1% V
1.90% C, 0.30% Si, 0.30% Mn, 20.00% Cr, 1.00% Mo, 4.00% V, 0.60% W
1.90% C, 0.30% Si, 0.30% Mn, 20.00% Cr, 1.00% Mo, 4.00% V, 0.60% W
1.90% C, 0.30% Si, 0.30% Mn, 20.00% Cr, 1.00% Mo, 4.00% V, 0.60% W
1.90% C, 0.30% Si, 0.30% Mn, 20.00% Cr, 1.00% Mo, 4.00% V, 0.60% W
1.90% C, 0.60% Si, 0.35% Mn, 20.00% Cr, 1.00% Mo, 4.00% V, 0.65% W
1.90% C, 0.70% Si, 0.30% Mn, 20.00% Cr, 1.00% Mo, 4.00% V, 0.60% W
1.90% C, 0.70% Si, 0.30% Mn, 20.00% Cr, 1.00% Mo, 4.00% V, 0.60% W
1.90% C, 0.70% Si, 0.30% Mn, 20.00% Cr, 1.00% Mo, 4.00% V, 0.60% W
1.90% C, 5.25% Cr, 1.30% Mo, 9.10% V
1.90-2.15% C, 0.20-0.40% Si, 0.20-0.40% Mn, 0.030% P, 0.030% S, 11.50-12.50% Cr, 0.20-0.40% Mo, 0.10-0.20% V, 2.20-2.80% W
1.90-2.20% C, 0.10-0.40% Si, 0.15-0.45% Mn, 11.00-12.00% Cr
1.90-2.20% C, 0.10-0.60% Si, 0.20-0.40% Mn, 0.030% P, 0.030% S, 11.00-13.00% Cr
1.90-2.20% C, 0.10-0.60% Si, 0.20-0.60% Mn, 0.030% P, 0.020% S, 11.00-13.00% Cr
1.90-2.20% C, 0.10-0.60% Si, 0.20-0.60% Mn, 0.030% P, 0.020% S, 11.00-13.00% Cr
1.90-2.20% C, 0.10-0.60% Si, 0.20-0.60% Mn, 0.030% P, 0.030% S, 11.00-13.00% Cr
1.90-2.20% C, 0.10-0.60% Si, 0.20-0.60% Mn, 0.030% P, 0.030% S, 11.00-13.00% Cr
1.90-2.20% C, 0.10-0.60% Si, 0.20-0.60% Mn, 0.030% P, 0.030% S, 11.00-13.00% Cr
1.90-2.20% C, 0.10-0.60% Si, 0.20-0.60% Mn, 0.030% P, 0.030% S, 11.00-13.00% Cr
1.90-2.20% C, 0.10-0.60% Si, 0.20-0.60% Mn, 0.030% P, 0.030% S, 11.00-13.00% Cr
1.90-2.20% C, 0.10-0.60% Si, 0.20-0.60% Mn, 0.040% P, 0.030% S, 11.00-13.00% Cr
2.00% C, 0.20% Si, 1.00% Mn, 2.10% Cr
2.00% C, 0.25% Si, 0.35% Mn, 11.50% Cr
2.00% C, 0.30% Si, 0.30% Mn, 11.50% Cr
2.00% C, 0.30% Si, 0.30% Mn, 12.00% Cr
2.00% C, 0.35% Si, 0.30% Mn, 11.50% Cr
2.00% C, 0.50% Si, 0.30% Mn, 3.80% Cr, 2.50% Mo, 5.10% V, 14.30% W, 11.00% Co
2.00% C, 0.50% Si, 0.30% Mn, 3.80% Cr, 2.50% Mo, 5.10% V, 14.30% W, 11.00% Co
2.00-2.20% C, 0.20-0.40% Si, 0.20-0.40% Mn, 0.035% P, 0.035% S, 11.50-12.50% Cr, 0.30-0.50% Mo, 0.60-0.80% W, 0.80-1.10% Co
2.00-2.25% C, 0.10-0.40% Si, 0.15-0.45% Mn, 0.030% P, 0.030% S, 11.00-12.00% Cr, 0.60-0.80% W
2.00-2.30% C, 0.10-0.40% Si, 0.30-0.60% Mn, 0.030% P, 0.030% S, 11.00-13.00% Cr, 0.60-0.80% W
2.00-2.30% C, 0.10-0.40% Si, 0.30-0.60% Mn, 0.030% P, 0.030% S, 11.00-13.00% Cr, 0.60-0.80% W
2.00-2.30% C, 0.10-0.40% Si, 0.30-0.60% Mn, 0.030% P, 0.030% S, 11.00-13.00% Cr, 0.60-0.80% W
2.00-2.30% C, 0.10-0.40% Si, 0.30-0.60% Mn, 0.030% P, 0.030% S, 11.00-13.00% Cr, 0.60-0.80% W
2.02-2.30% C, 3.70-4.70% Cr, 8.00-8.50% Mo, 4.80-5.10% V, 9.00-10.00% W, 9.00-10.00% Co
2.03% C, 0.39% Si, 0.32% Mn, 11.49% Cr, 0.11% V, 0.78% W
2.03% C, 0.39% Si, 0.32% Mn, 11.49% Cr, 0.11% V, 0.78% W
2.04% C, 0.22% Si, 0.33% Mn, 0.027% P, 0.016% S, 11.50% Cr, 0.11% Mo, 0.11% Ni, 0.65% W
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn,11.50% Cr
2.05% C, 0.30% Si, 0.80% Mn, 12.70% Cr, 1.10% W
2.05% C, 0.30% Si, 0.80% Mn, 12.70% Cr, 1.10% W
2.1% C, 4.0% Cr, 9.5% W, 8.2% Mo, 5.0% V, 9.5% Co
2.10% C, 0.25% Si, 0.30% Mn, 11.50% Cr, 0.00% Ni, 0.70% W
2.10% C, 0.25% Si, 0.30% Mn, 12.50% Cr, 0.90% Mo, 2.10% V
2.10% C, 0.25% Si, 0.45% Mn, 0.025% Mn, 0.010% S, 13.50% Cr
2.10% C, 0.30% Si, 0.30% Mn, 0.030% P, 0.005% S, 12.00% Cr, 0.70% W
2.10% C, 0.30% Si, 0.30% Mn, 11.50% Cr, 0.70% W
2.10% C, 0.30% Si, 0.30% Mn, 12.00% Cr, 0.70% W
2.10% C, 0.30% Si, 0.30% Mn, 12.00% Cr
2.10% C, 0.30% Si, 0.40% Mn, 12.00% Cr, 0.40% Mo, 1.00% Co
2.10% C, 0.35% Si, 0.35% Mn, 12.00% Cr, 0.70% W
2.10% C, 0.35% Si, 0.35% Mn, 12.00% Cr, 0.70% W
2.10% C, 1.00% Si, 0.40% Mn, 6.80% Cr, 1.50% Mo, 5.40% V
2.10% C, 1.00% Si, 0.40% Mn, 6.80% Cr, 1.50% Mo, 5.40% V
2.10% C, 1.00% Si, 0.40% Mn, 6.80% Cr, 1.50% Mo, 5.40% V
2.10% C, 12.00% Cr, 0.70% W
2.10% C, 12.00% Cr, 0.70% W
2.10% C, 12.00% Cr, 0.80% Mo, 3.80% V
2.10% C, 12.00% Cr, 0.80% W
2.10% C, 12.00% Cr
2.10% C, 12.00% Cr
2.10% C, 12.50% Cr
2.10-2.30% C, 0.15-0.30% Si, 0.25-0.40% Mn, 0.030% P, 0.020% S, 12.50-13.50% Cr, 0.80-1.10% Mo, 3.70-4.00% V
2.12% C, 0.25% Si, 0.45% Mn, 12.00% Cr, 0.70% W
2.15% C, 0.25% Si, 0.30% Mn, 0.070% S, 4.75% Cr, 6.00% V, 13.00% W, 10.00% Co
2.15% C, 0.40% Si, 0.40% Mn, 12.25% Cr, 0.25% V
2.15% C, 0.40% Si, 0.40% Mn, 12.25% Cr, 0.25% V
2.15-2.30% C, 0.15-0.30% Si, 0.25-0.40% Mn, 0.035% P, 0.035% S, 12.00-13.00% Cr, 0.80-1.00% Mo, 2.00-2.30% V
2.15-2.50% C, 0.10-0.60% Si, 0.10-0.60% Mn, 11.50-13.50% Cr, 0.70-1.20% Mo, 3.80-4.40% V
2.20% C, 5.00% Cr, 1.00% Mo, 4.80% V, 0.60% W
2.23% C, 0.23% Si, 0.32% Mn, 12.50% Cr, 0.90% Mo, 1.15% V
2.25% C, 0.90% Si, 0.50% Mn, 0.030% S, 12.80% Cr, 1.30% Mo, 9.25% V
2.25% C, 0.90% Si, 0.50% Mn, 0.030% S, 12.80% Cr, 1.30% Mo, 9.25% V
2.30% C, 0.40% Si, 0.40% Mn, 12.50% Cr, 1.10% Mo, 4.00% V
2.30% C, 0.40% Si, 0.40% Mn, 12.50% Cr, 1.10% Mo, 4.00% Vbr>
2.30% C, 0.40% Si, 0.40% Mn, 4.80% Cr, 3.60% Mo, 8.00% V
2.30% C, 0.40% Si, 13.00% Cr, 1.10% Mo, 4.00% V
2.30% C, 0.60% Si, 0.30% Mn, 12.50% Cr, 1.10% Mo, 4.00% V
2.30% C, 4.00% Cr, 7.00% Mo, 6.50% V, 6.50% W, 10.50% Co
2.30% C, 4.2% Cr, 7.0% Mo, 6.5% V, 6.5% W, 10.5% Co
2.30% C, 4.20% Cr, 7.00% Mo, 6.50% V, 6.50% W, 10.50% Co
2.30% C, 4.20% Cr, 7.00% Mo, 6.50% V, 6.50% W, 10.50% Co
2.30% C, 4.20% Cr, 7.00% Mo, 6.50% V, 6.50% W, 10.50% Co
2.45% C, 0.55% Si, 4.15% Cr, 3.75% Mo, 9.00% V, 1.00% W, 2.00% Co
2.45% C, 0.90% Si, 0.50% Mn, 0.08% S, 5.30% Cr, 1.30% Mo, 9.50% V
2.45% C, 0.90% Si, 0.50% Mn, 0.080% S, 5.30% Cr, 1.30% Mo, 9.50% V
2.45% C, 0.90% Si, 0.50% Mn, 5.20% Cr, 1.10% Mo, 9.75% V
2.45% C, 0.90% Si, 0.50% Mn, 5.20% Cr, 1.30% Mo, 0.75% V
2.45% C, 0.90% Si, 0.50% Mn, 5.25% Cr, 1.35% Mo, 9.80% V
2.45% C, 5.25% Cr, 1.20% Mo, 9.75% V
2.45% C, 5.25% Cr, 1.3% Mo, 9.75% W
2.45% C, 5.25% Cr, 1.30% Mo, 9.75% V
2.45% C, 5.25% Cr, 1.30% Mo, 9.75% V
2.48% C, 4.2% Cr, 3.1% Mo, 8.0% V, 4.2% W
2.5% C, 4.0% Cr, 1.0% W, 4.0% Mo 9.0% V, 2.0% Co
2.50% C, 0.50% Si, 0.30% Mn, 4.20% Cr, 3.10% Mo, 8.00% V, 4.20% W
2.60% C, 0.30% Si, 0.60% Mn, 8.25% Cr, 1.20% Mo, 4.50% V, 0.005% S
2.60% C, 0.30% Si, 0.60% Mn, 8.25% Cr, 1.20% Mo, 4.50% V, 0.005% S
2.60% C, 17.00% Cr, 3.30% V, 2.00% Co
2.70% C, 0.50% Si, 0.50% Mn, 20.00% Cr, 1.00% Mo, 7.20% V, 0.70% W
2.80% C, 0.30% Si, 0.70% Mn, 5.25% Cr, 1.10% Mo, 4.50% V
2.80% C, 0.30% Si, 0.70% Mn, 5.25% Cr, 1.10% Mo, 4.50% V
2.80% C, 0.80% Si, 0.70% Mn, 7.00% Cr, 2.30% Mo, 8.90% V
2.80% C, 0.80% Si, 0.70% Mn, 7.00% Cr, 2.30% Mo, 8.90% V
2.80-3.00% C, 0.15-0.25% Si, 0.20-0.40% Mn, 0.020% P, 0.020% S, 11.50-12.50% Cr
2.90% C, 0.50% Si, 0.50% Mn, 8.00% Cr, 1.50% Mo, 9.80% V
2.90% C, 0.50% Si, 0.50% Mn, 8.00% Cr, 1.50% Mo, 9.80% V
2.90% C, 8.00% Cr, 1.40% Mo, 9.80% V
3.40% C, 5.25% Cr, 14.50% V, 1.30% Mo
10.00% Cr with 13% carbides in the microstructure.
10.00% Cr with 13% carbides in the microstructure.
13.50% Cr, 5.00% Mo, 9.00% Co, 4.00% Ni, 30.00% TiC, Fe is balance
15.00% Ni, 9.00% Co, 6.00% Mo, 30.00% TiC, Fe is balance