Chemical Composition of Steels in Weight %

0.002% C, 10.0% Co, 15.0% W
0.002% C, 10.0% Co, 15.0% W
0.005% C, 18.00% Ni, 12.00% Co, 2.00% Mo, 3.00% W, 1.70% Ti, 0.70% V, 0.30% Al
0.009% C, 0.24% Si, 1.17% Mn, 0.014% N
0.01% C, 0.55% Si, 0.11% Mn, 12.30% Cr, 8.89% Ni, 0.98% Mo, 0.83% Ti, 0.57% Al, 75.80% Fe
0.01% C, 13.00% Ni, 15.00% Co, 10.00% Mo, plus Ti, Al, V
0.010% C, 0.011% N, 0.11 %Ti, 0.03% C, 0.11% Nb, 0.35 % Mo, 0.071% C, 0.92% Si, 0.64% Ti, 0.071% C, 0.92% Si, 0.64% Ti
0.013% C, 10.72% Ni, 8.12% Co, 6.49% Mo, 0.60% Ti, 0.06% Al
0.014% C
0.014% C
0.017% C, 0.45% Mn, 0.0021% O2, 0.0014% N2
0.018% C, 2.02% Si, 0.225% Al. 0.012% C, 3.66% Si, 0.225% Al
0.02 wt% C
0.02% C, 0.26% Mo, 0.002% N2
0.02% C, 0.26% Mo, 0.002% N2
0.02% C, 0.38% Si, 1.47% Mn, 0.022% P, 0.001% S, 22.62% Cr, 5.12% Ni, 3.24% Mo, 0.196% N
0.022% C, 0.006% S, 0.007% P, 0.003% Si, 0.002% Cr, 0.003% Mo, <0.001% V, 0.008% Cu, 0.001% Al, 0.001% As, 0.002% N2
0.022% C, 0.15% Mn, 0.035% Al, 0.015% Ti, 0.0038% N, 0.78% Cr
0.022% C, 0.15% Mn, 0.78% Cr, 0.035% Al, 0.015% Ti, 0.0038% N
0.027% C, 1.46% Mn 0.72% Si, 0.012% P, 0.012% S, 18.8% Cr, 10.50% Ni, 0.06% Mo, 0.177% N, 0.002% B. PE16">0.08% C, 0.05% Mn, 17.10% Cr, 42.50% Ni, 3.10% Mo, 1.30% Al, 1.20% Ti
0.03% C, 0.42% Si, 1.65% Mn, 0.017% P, 0.002% S, 24.80% Cr, 21.50% Cr, 2.33% Mo, 0.10% V, 0.12% Cu
0.03% C, 13% Cr, 10% Co, 2% Mo
0.03% C, 13% Cr, 10% Co, 2% Mo
0.03% C, 13% Cr, 10% Co, 2% Mo
0.03% C, 13% Cr, 20% Co, 8% Mo
0.03% C, 13% Cr, 20% Co, 8% Mo
0.03% C, 13% Cr, 20% Co, 8% Mo
0.03% C, 13% Cr, 20% Co, 8% Mo
0.03% C, 13% Cr, 20% Co, 8% Mo
0.03% C, 13% Cr, 20% Co, 8% Mo
0.03% C, 13% Cr, 20% Co, 8% Mo
0.03% C, 13% Cr, 20% Co, 8% Mo
0.03% C, 13% Cr, 20% Co, 8% Mo
0.03% C, 21-23.5% Cr, <1.5% Mn, 2.5-3.5% Mo, 4.5-6.5% Ni, 0.10-0.30% N, <0.040% P, <0.020% S, <1.0% Si. CD3MWCuN steel"><0.03% C, 24-26% Cr, <1.0% Mn, 3.0-4.0% Mo, 6.50-8.50% Ni, 0.20-0.30% N, <0.030% P, <0.025% S, <1.0% Si, 0.50-1.0% W
0.03% C, Fe
0.03% C, max. 0.10% Si, max. 0.10% Mn, max. 0.010% P, max. 0.010% S, 0.05-0.15% Al, 4.60-5.20% Mo, 17.00-19.00% Ni, max. 0.003% B, max. 0.05% Ca, 7.00-8.50% Co, 0.30-0.60% Ti, max. 0.02% Zr
0.03% C, max. 1.00% Si, max. 2.00% Mn, max. 0.030% P, max. 0.015% S, 22.00% Cr, 5.50% Ni, 3.20% Mo, 0.18% N
0.030% C, 21.00-23.00% Cr, 4.50-6.50% Ni, 2.50-3.50% Mo, 0.08-0.20% N. Steel 1.4501">max. 0.03% C, max. 1.00% Si, max. 1.00% Mn, 0.01% S, 0.03% P, 6.00-8.00% Ni, 24.00-26.00% Cr, 3.00-4.00% Mo, 0.50-1.00% Cu, 0.20-0.30% N
0.032% C, 2.02% Mn, 7.23% Ni, 0.47% Cr, 0.25% Si, 0.008% S, 0.011% P, 0.63% Mo, 0.03% Cu
0.034% C, 0.041% Nb, 0.029% N2
0.04% C, 0.39% Nb
0.04% C, 0.39% Nb
0.04% C, 1.17% Mo
0.042% C, 0.71% Si, 1.54% Mn, 17.8% Cr, 9.4% Ni, 0.25% Mo, 0.63% Nb, 0.13% Co
0.05% C, 30.2% Cr, 51.0% Co, 2.20% Mo
0.05% C, max. 1.00% Si, max. 1.00% Mn, max. 0.040%P, max. 0.015% S, 16.00-18.00% Cr
0.05-0.12% C, 0.10-0.80% Si, 0.20-1.35% Mn, max. 0.025% P, max. 0.020% S, 0.035% N, 5.00-7.00% Co, 9.80-11.50% Cr
0.05-0.15% C, max. 0.50% Si, 0.30-0.60% Mn, max. 0.025% P, max. 0.025% S, 1.90-2.60% Cr, 0.87-1.13% Mo
0.057% C, 0.044% Al, 0.006% N
0.057% C, 0.29% Mn, 0.025% S, 0.018% P, 0.002% N2, 0.048% O2
0.06 to 0.09% C, 18% Cr, 8% Ni
0.06 to 0.09% C, 18% Cr, 8% Ni
0.06 to 0.09% C, 18% Cr, 8% Ni
0.06 to 0.09% C, 18% Cr, 8% Ni
0.06% C, 0.43% Si, 1.59% Mn, 0.03% P, 0.01% S, 18.00% Cr, 11.90% Ni, 1.84% Mo
0.06% C, 0.44% Si, 0.41% Mn, 0.022% P, 0.017% S, 12.50% Cr, 0.38% Ni, 0.09% Mo, 0.11% Cu
0.06% C, 0.46% Mn, 0.41% Si, 9.5% Ni, 17.7% Cr, 0.41% Ti
0.06% C, 1.8% Mn, 0.3% Mo, 0.04% Ni
0.06-0.10% C, 0.10-0.40% Si, 0.20-0.60% Mn, max. 0.030% P, max. 0.030% S, 2.00-2.50% Cr, max. 0.35% Ni
0.07% C, 0.50% Si, 1.15% Mn, 11.1% Ni, 17.8% Cr, 0.86% Nb
0.07% C, 0.50% Si, 1.15% Mn, 11.1% Ni, 17.8% Cr, 0.86% Nb
0.07% C, 0.56% Si, 1.60% Mn, 11.9% Ni, 17.3% Cr, 0.50% Ti
0.07% C, 0.56% Si, 1.60% Mn, 11.9% Ni, 17.3% Cr, 0.50% Ti
0.07-0.14% C, <0.50% Si, <0.70% Mn, 10-12.5% Cr, 0.50 Ni, 0.25-0.60% Mo, 0.15-0.30% V, 0.04-0.10% Nb, 1.5-2.5 W, 0.04-0.10% Ni, <0.005% B, 0.3-1.7% Cu, <0.04% Al
0.07-0.14% C, <0.50% Si, <0.70% Mn, 10.00-12.50% Cr, <0.50% Ni, 0.25-0.60% Mo, 0.04-0.10% Nb, 1.50-2.50% W, 0.040-0.10% N, <0.005% B, 0.30-1.70% Cu, <0.04% Al
0.074% C, 9.29% Si, 0.44% Mn, 0.009% P, 0.004% S, <0.005% Al, 9.26% Cr, 0.06% Ni, 2.84% W, 2.95% Co, 0.21% V, 0.056% Nb, <0.005% Ti, 0.0120% B, 0.0130% N
0.076% C, 0.677% Si, 2.02% Mn, 0.026% P, 0.677% S, 17.16% Cr, 2.192% Mo, 12.04% Ni, 0.926% Nb
0.08% C, 0.054% Al, 0.007% N, 0.38% Si, 1.0% Mn, 0.08% Al, 0.045% Nb, 0.007% N, 0.01% (V + Ti)
0.08% C, 0.15% Si, 2.00% Mn, 0.04% P, 14.30% Cr, 20.00% Ni, 2.50% Mo, 2.50% Al, 0.90% Nb, 0.01% B. NF709">Fe-20Cr-25Ni base
0.08% C, 0.51% Mn, 0.505 Si, 17.18% Cr, 4.27% Ni
0.08% C, 0.75% Si, 2.00% Mn, 0.045% S, 0.030% S, 17.00-19.00% Cr
0.08% C, 2.00% Mn, 1.00% Si, 17.00-19.00% Cr, 9.00-13.00% Ni, max. 0.045% P, max. 0.03% S, 0.70% Nb, 0.10% Ta
0.08-0.13% C, 0.45-0.65% Mn, 0.15-0.30% Si, 0.025 (max)% P, 0.025 (max)% S, 1.00-1.40% Cr, 3.00-3.50% Ni, 0.08-0.15% Mo
0.08-0.15% C, max. 0.50% Si, 0.40-0.70% Mn, max. 0.040% P, max. 0.040% S, 2.00-2.50% Cr, 0.90-1.20% Mo
0.083% C, 0.036% Nb
0.083% C, 0.036% Nb
0.083% C, 0.036% Nb
0.09% C, 1.55% Si, 1.06% Mn, 18.4% Ni, 23.3% Cr
0.09% C, max. 1.00% Si, max. 1.00% Mn, max. 0.030% P, max. 0.030% S, 14.00-16.00% Cr, 2.00-2.50% Mo, 6.50-7.75% Ni, 0.75-1.50% Al
0.092% C, 0.20% Si, 1.41% Mn, 0.005% P, 0.004% S, 0.039% Al, 0.0067% N, <0.005% Nb, <0.005% V, <0.0005% B. Steel V">0.094% C, 0.21% Si, 1.44% Mn, 0.005% P, 0.003% S, 0.029% Al, 0.0052% N, <0.005% Nb, 0.10% V, <0.0005% B
0.10 %C, 0.06 %Si, 0.1% Mn, 10.0% Cr, 0.17% Ni, 0.7% Mo, 0.05% Nb, 0.2% V, 0.003% N, 0.008% B, 2.0% W, 3.0% Co, 0.01% Ti, 0.006% Cu, 0.01% Al
0.10% C, <0.005% Si, 1.99% Mn, 0.56% V, 0.03% Al, 0.0049% N
0.10% C, <0.005% Si, 1.99% Mn, 1.60% Mo, 0.03% Al, 0.0049% N
0.10% C, <0.005% Si. 2.00% Mn, 0.40% Mo, 0.30% V, 0.03% Al, 0.0041% N
0.10% C, 0.005% Si, 1.99% Mn, 0.56% V, 0.03% Al, 0.0049% N
0.10% C, 0.005% Si, 2.00% Mn, 0.40% Mo, 0.56% V, 0.03% Al, 0.0040% N
0.10% C, 0.005% Si, 2.00% Mn, 1.59% Mo, 0.56% V, 0.03% Al, 0.0044% N
0.10% C, 0.15-0.50% Si, 0.40-0.80% Mn, 0.020% P, 0.020% S, 2.00-2.50% Cr, 0.90-1.10% Mo, 0.30-0.80% Ni, Nb/Ta">10 x C, 0.05% N
0.10% C, 0.20-0.60% Mn, 0.40% Si, 2.00-2.50% Cr, 0.35% Ni, 0.25% Cu, 0.03% P, 0.03% S
0.10% C, 0.40% Mn, 0.20% Si, 0.13% Ni,8.30% Cr, 0.95% Mo, 0.010% Al, 0.02% S, 0.007% P, 0.20% V, 0.075% Nb, 0.004% Ti, 0.03% N
0.10% C, 0.40% Mn, 0.20% Si, 0.13% Ni,8.30% Cr, 0.95% Mo, 0.010% Al, 0.02% S, 0.007% P, 0.20% V, 0.075% Nb, 0.004% Ti, 0.03% N
0.10% C, 0.50% Mn, 0.25% Si, 3.25% Ni, 1.20% Cr, 0.12% Mo
0.10% C, 0.98% Mn, 2.98% Cr, 1.50% Mo
0.10% C, 15.0% W
0.10% C, 2% Mn, 1% Si
0.10% C, max. 1.00% Si, max. 2.00% Mn, max. 0.045% P, max. 0.030% S, 26.00-28.00% Cr, 1.30-2.00% Mo, 4.00-5.00% Mo
0.10-0.18% C, 0.10-0.35% Si, 0.40-0.70% Mn, max. 0.030% P, max. 0.035% S, 0.30-0.60% Cr, 0.50-0.70% Mo, 0.22-0.32% V
0.10C-0.1Si-1.5Mn-0.01P-0.004S-0.2Ti-0.2Mo
0.11% C, 0.026% S, 0.014% P, 0.35% Si, 0.48% Mn, 0.11% Ni, 2.24% Cr, 1.05% Mo, O.19% Cu, less than 0.01% Nb, Ti, V, and balance Fe
0.11% C, 0.035% Nb
0.11% C, 0.21% Si, 0.47% Mn, 0.010% S, 0.010% P, 2.29% Cr, 0.14% Ni, 1.02% Mo, 0.18% Cu, <0.01% V
0.11% C, 0.21% Si, 0.47% Mn, 0.010% S, 0.010% P, 2.29% Cr, 0.14% Ni, 1.02% Mo, 0.18% Cu, <0.01% V
0.11% C, 0.43% Si, 0.41% Mn, 0.010% P, 0.012% S, 2.10% Cr, 0.96% Mo, 0.25% Ni, 0.020% Cu, 0.0125% N2
0.11% C, 0.43% Si, 0.41% Mn, 0.010% P, 0.012% S, 2.10% Cr, 0.96% Mo, 0.25% Ni, 0.020% Cu, 0.0125% N2
0.11% C, 0.43% Si, 0.41% Mn, 0.010% P, 0.012% S, 2.10% Cr, 0.96% Mo, 0.25% Ni, 0.020% Cu, 0.0125% N2
0.11% C, 0.43% Si, 0.41% Mn, 0.010% P, 0.012% S, 2.10% Cr, 0.96% Mo, 0.25% Ni, 0.020% Cu, 0.0125% N2
0.11-0.13% C, 0.46-0.48% Mn, 0.24-0.27% Si, 2.06-2.19% Cr, 0.96-1.02% Mo, 0.005-0.02% V
0.11-0.17% C, max. 0.25% Si, 0.80-1.00% Mn, max. 0.020% P, max. 0.015% S, 1.25-1.50% Cr, 0.80-1.00% Mo, 0.20-0.300% V
0.115% C, 0.20% Si, 0.51% Mn, 0.017% P, 0.002% S, 0.07% Al, 8.85% Cr, 0.24% Ni, 0.94% Mo, 0.22% V, 0.95% W, 0.084% N, 0.069% Nb
0.12% C, 0.90-1.20% Si, 0.35-0.75% Mn, max. 0.035% P, max. 0.035% S, 1.60-2.00% Cr, 0.25-0.35% Mo, 0.25-0.35% V
0.12% C, 1.1% Cr, 0.54% Mn, 0.26% Mo, 0.26% Si, 0.17% V, 0.019% S, 0.015% P
0.12% C, max. 1.0% Si, max. 1.50% Mn, 12.50% Cr
0.12% C, max. 1.00% Si, max. 1.00% Mn, max. 0.040% P, max. 0.030% S, 16.00-18.00% Cr, max. 0.50% Ni
0.124% C, 0.02% Si, 9.07% Cr, 0.06% Ni, 0.46% Mo, 1.78% W, 0.063% Nb, 0.19% V, 0.043% Al, 0.003% B, 0.043% N
0.13% C, 0.35% Si, 0.50% Mn, 0.060% P, 0.002% S, 2.28% Cr, 0.24% V, 0.047% Nb, 0.006% Ti, 1.48% W, 0.009% N
0.13% C, 0.47% Mn, 0.19% Si, 0.29% Cr, 0.08% Ni, 0.49% Mo, 0.23% V
0.13% C, 5.00% Cr, 4.00% Mo, 0.20% V. 0.50% C, 5.00% Cr, 5.00% Mo, 0.60% V. 0.70% C, 1.50% Mn, 1.39% Si, 6.00% Cr, 2.00% Mo
0.135% C, 0.25% Si, 0.34% Mn, 0.010% S, 0.013% P, 1.02% Cr, 0.50% Mo, 0.70% W, 0.47% V
0.135% C, 0.25% Si, 0.34% Mn, 0.010% S, 0.013% P, 1.02% Cr, 0.50% Mo, 0.70% W, 0.47% V
0.135% C, 0.25% Si, 0.34% Mn, 0.010% S, 0.013% P, 1.02% Cr, 0.50% Mo, 0.70% W, 0.47% V
0.135% C, 0.25% Si, 0.34% Mn, 0.010% S, 0.013% P, 1.02% Cr, 0.50% Mo, 0.70% W, 0.47% V
0.135% C, 0.25% Si, 0.34% Mn, 0.010% S, 0.013% P, 1.02% Cr, 0.50% Mo, 0.70% W, 0.47% V
0.135% C, 0.25% Si, 0.34% Mn, 0.010% S, 0.013% P, 1.02% Cr, 0.50% Mo, 0.70% W, 0.47% V
0.135% C, 0.25% Si, 0.34% Mn, 0.010% S, 0.013% P, 1.02% Cr, 0.50% Mo, 0.70% W, 0.47% V
0.13C, 5Cr, 4Mo, 0.2V, (0.5C, 5Cr, 5Mo, 0.6V), (0.7C, 1.5Mn, 1.39Si, 6Cr, 2Mo)
0.14% C, <0.50% Si, 0.40-0.70% Mn, 11-13% Cr, 0.80-1.2% Mo, 0.20-0.30% V, <0.20% Nb, 0.8-1.2% W
0.14% C, <0.50% Si, 0.40-0.70% Mn, 11.00-13.00% Cr, 0.80-1.20% Mo, 0.20-03.0% V, <0.20% Nb, 0.80-1.20% W
0.14% C, 0.65% Mn, 0.26% Si, 2.05% Mo, 0.0020% B
0.14% C, 0.65% Mn, 0.26% Si, 2.05% Mo, 0.0020% B
0.148% C, 0.49% Si, 16.00% Mn, 22.07% Cr , 0.47% Ni, 0.56% N, 0.029% P, 0.002% S
0.149% C, 0.392% Si, 2.061% Mn, 0.011% P, 0.002% S, 0.515% Cr, 0.024% Ni, 0.022% Nb, 0.004% V, 0.006% Ti, 0.017% Cu, 0.620% Al, <0.0001%
0.15% C, 0.25-0.50% Si, 1.00-1.40% Mn, max. 0.035% P, max. 0.035% S, 0.40-0.60% Cr, 0.20-0.40% Mo, 1.10-1.40% Ni, 0.06-0.12% V
0.15% C, 0.25-0.50% Si, 1.00-1.40% Mn, max. 0.035% P, max. 0.035% S, 0.40-0.60% Cr, 0.20-0.40% Mo, 1.10-1.40% Ni, 0.06-0.12% V
0.15% C, 0.25-1.00% Si, 0.30-0.60% Mn, max. 0.030% P, max. 0.030% S, 8.00-10.00% Cr, 0.90-1.10% Mo
0.15% C, 0.30-0.50% Si, 0.30-0.60% Mn, max. 0.035% P, max. 0.035% S, 4.50-5.50% Cr, 0.45-0.65% Mo
0.15% C, 0.37% Si, 0.70% Mn, 1.20% Cr, 0.35% Mo, 0.30% V
0.15% C, 0.50-1.00% Si, 0.30-0.60% Mn, max. 0.030% P, max. 0.030% S, 6.00-8.00% Cr, 0.45-0.65% Mo
0.15% C, 0.63% Mn, 0.045% S, 0.04% Nb, 0.0063% N2
0.15% C, 0.63% Mn, 0.045% Si, 0.04% Nb, 0.0063% N2
0.15% C, 1.20% Cr, 0.35% Mo, 0.30% V, 0.70% Mn, 0.37% Si
0.15% C, 1.58% Si, 1.3% Mn, 25% Cr, 19% Ni
0.15% C, 2.262% Cr, 1.15% Mo, 0.66% Mn, 0.30% Si, 0.20% Ni
0.15% C, 2.262% Cr, 1.15% Mo, 0.66% Mn, 0.30% Si, 0.20% Ni
0.15-0.20% C, 0.15-0.35% Si, 0.30-0.50% Mn, max. 0.035% P, max. 0.035% S, 2.70-3.00% Cr, 0.20-0.30% Mo, 0.10-0.20% V
0.162% C, 14.36% Cr, 13.60% Co, 4.20% Mo, 0.48% V
0.162% C, 14.36% Cr, 13.60% Co, 4.20% Mo, 0.48% V
0.162% C, 14.36% Cr, 13.60% Co, 4.20% Mo, 0.48% V
0.168% C, 0.23% Si, 0.22% Mn, 0.008% P, 0.004% S, 0.003% Al, 8.85% Cr, 1.54% Mo, 0.18% Ni, 0.29% V, 0.057% Nb, 0.0092% B, 0.0160% N
0.168% C, 0.23% Si, 0.22% Mn, 0.008% P, 0.004% S, 0.003% Al, 8.85% Cr, 1.54% Mo, 0.18% Ni, 0.29% V, 0.057% Nb, 0.0092% B, 0.0160% N
0.168% C, 0.23% Si, 0.22% Mn, 0.008% P, 0.004% S, 0.003% Al, 8.85% Cr, 1.54% Mo, 0.18% Ni, 0.29% V, 0.057% Nb, 0.0092% B, 0.0160% N
0.17% C, 0.25-0.50% Si, 0.80-1.20% Mn, max. 0.035% P, max. 0.035% S, 0.50-0.80% Cu, max. 0.30% Cr, 0.25-0.40% Mo, 1.00-1.30% Ni, appr. 0.02% Zr
0.17% C, 0.37% Si, 0.35% Mn, 0.022% P, 0.002% S, 13.1% Cr, 0.22% Ni, 0.04% Mo, 0.01% V, 0.18% Cu
0.17% C, 1.37% Mn, 0.26% Si, 0.012% P, 0.001% S, 0.24% Cr, 0.48% Mo, 0.05% Ni, 0.019% V, 0.004% Ti, 0.17% C, 10.5% Cr, 0.50% Mo, 0.85% Ni, 0.60% Mn, 0.20% Nb, 0.25% V, 0.32% Si, 0.05% Al, 0.003% N, 0.005% P
0.17% C, 10.50% Cr, 0.50% Mo, 0.85% Ni, 0.60% Mn, 0.20% Nb, 0.25% V, 0.32% Si, 0.05% Al, 0.003% N, 0.005% P
0.17-0.23% C, 0.20-0.50% Si, 1.40-1.70% Mn, max. 0.035% P, max. 0.035% S, max. 0.015% N, 0.20-0.50% Mn, max. 0.70% Ni, max. 0.20% V
0.17-0.23% C, max. 0.50% Si, max. 1.00% Mn, max. 0.030% P, max. 0.030% S, 10.00-12.50% Cr, 0.80-1.20% Mo, 0.30-0.80% Ni, 0.25-0.35% V
0.17-0.25% C, 0.10-0.50% Si, 0.30-0.80% Mn, max. 0.045% P, max. 0.030% S, 11.00-12.50% Cr, 0.80-1.20% Mo, 0.30-0.80% Ni, 0.40-0.60% W, 0.25-0.35% V
0.17-0.25% C, 0.15-0.35% Si, 0.35-0.85% Mn, max. 0.030% P, max. 0.035% S, 1.20-1.50% Cr, 0.65-0.80% Mo, 0.25-0.35% V
0.17-0.25% C, max. 0.35% Si, 0.50-1.00% Mn, max. 0.020% P, max. 0.020% S, max. 0.05% Al, max. 0.18% Cu, 0.30-0.50% Cr, 0.50-0.80% Mo, 0.60-1.20% Ni, max. 0.03% V
0.17-0.32% C, max. 0.35% Si, 1.00-1.50% Mn, max. 0.020% P, max. 0.020% S, max. 0.30% Cr, 0.45-0.60% Mo, 0.40-0.80% Ni, max. 0.05% Al, max. 0.18% Cu, max. 0.03% V
0.17-3.00% C, 0.10-0.50% Si, 0.15-0.90% Mn, max. 0.035% P, max. 0.035% S, 0.30-13.50% Cr
0.18-0.22% C, max. 1.00% Si, max. 1.00% Mn, max. 0.045% P, max. 0.035% S, 12.00-14.00% Cr
0.19% C, 0.20-0.50% Si, 1.50-1.70% Mn, max. 0.035% P, max. 0.035% S, max. 0.015% N, 0.20-0.50% Mo, max. 0.70% Ni, max. 0.20% V
0.19% C, 0.34% Si, 0.46% Mn, 0.019% P, 0.013% S, 7.87% Cr, 2.02% Mo
0.19% C, 0.74% Mn, 0.30% Si, 0.017% P, 0.014% S, 1.05% Cr, 0.56% Mo, 0.28% V
0.19% C, 11.01% Cr, 0.09% Mo, 3.45% W, 2.97% Co, 0.21% V, 0.06% Nb, 0.03% N
0.195% C, 0.071% Si, 0.059% Mn, 27.41% Cr, 9.16% Co
0.20% C, 0.50-0.90% Si, 0.70-1.10% Mn, max. 0.035% P, max. 0.035% S, 0.60-1.00% Cr, 0.20-0.60% Mo, 0.06-0.12% V, 0.06-0.12% Zr
0.20% C, 26.5% Cr, 49.5% Co
0.20-0.28% C, 0.15-0.35% Si, 0.30-0.60% Mn, max. 0.035% P, max. 0.035% S, 1.20-1.50% Cr, 0.50-0.60% Mo, max. 0.060% Ni, 0.15-0.25% V
0.20-0.28% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S, 0.90-1.20% Cr, 0.20-0.35% Mo, max. 0.60% Ni
0.206% C, 0.023% Si, 0.040% Mn, 18.30% Cr, 9.75% Co
0.206% C, 0.023% Si, 0.040% Mn, 18.30% Cr, 9.75% Co
0.21% C, 12.6% Cr, 14.9% Co
0.21% C, 12.6% Cr, 14.9% Co
0.22% C, 0.054% Nb, 0.034% Ti, 0.80% Mn, 0.017% P, 0.003% S, 0.24% Si, 0.60% Cr. 0.43% Ni, 0.21% Mo, 0.022% Al, 92 ppm N
0.22-0.32% C, max. 0.30% Si, 0.15-0.40% Mn, max. 0.015% P, max. 0.018% S, 1.20-1.80% Cr, 0.25-0.45% Mo, 3.40-4.00% Ni, 0.05-0.15% V
0.23% C, 8.1% Mn, 5.3% Al. Steel B">0.20% C, 8.4% Mn, 1.0% Si, 5.6% Al. Steel C">0.24% C, 8.1% Mn, 1.8% Si, 5.3% Al
0.2457% C, 0.0125% P, 0.0092% S, 24.72% Cr, <3 Si+Mn+Ni+Al
0.25% C, 0.40% Si, 0.05% S, 0,20% Cu, 0.04% P
0.25-0.30% C, max. 0.30% Si, 0.35-0.80% Mn, max. 0.015% P, max. 0.018% S, 1.10-1.40% Cr, 0.80-1.10% Mo, 0.50-0.75% Ni, 0.25-0.35% V
0.25-0.35% C, <1.00% Si, 14.00-16.00% Cr, <0.50% Ni, 0.85-1.10% Mo, 0.30-0.50% N
0.26-0.34% C, max. 0.40% Si, 0.30-0.60% Mn, max. 0.035% P, max. 0.030% S, 1.80-2.20% Cr, 0.30-0.50% Mo, 1.80-2.20% V
0.26-0.34% C, max. 0.40% Si, 0.40-0.70% Mn, max. 0.035% P, max. 0.030% S, 2.30-2.70% Cr, 0.15-0.25% Mo, 0.10-0.20% V
0.28-0.34% C, max. 0.30% Si, 0.30-0.80% Cr, max. 0.015% P, max. 0.018% S, 1.10-1.40% Cr, 1.00-1.20% Mo, 0.50-0.75% Ni, 0.25-0.35% V
0.28-0.35% C, max. 0.40% Si, 0.40-0.70% Mn, max. 0.025% P, max. 0.035% S, 2.80-3.40% Cr, 0.30-0.50% Mo
0.28-1.45% C, 0.10-0.60% Si, 0.10-1.15% Mn, max. 0.035% P, max. 0.035% S
0.30% C, (0.16, 0.26 and 0.43% Cr)
0.30% C, 0.30% Mn, 0.30% Si, 2.50% Cr, 2.60% Mo, 1.59% Ni, 0.18% V
0.30% C, 0.30% Mn, 0.30% Si, 2.50% Cr, 2.60% Mo, 1.59% Ni, 0.18% V
0.30% C, 10% Cr, 36% Ni
0.30% C, 10% Cr, 36% Ni
0.30% C, 36% Ni, 10% Cr
0.30% C, 36% Ni, 10% Cr
0.32-0.39% C, <0.40% Si, 0.50-0.80% Mn, 1.11810.035% P, 1.11810.035% S, 1.11810.40% Cr, 1.11810.10% Mo, 1.11810.40% Ni, Cr+Mo+Ni=0.63
0.33% C, 1.12% Mn, 0.24% Ni, 0.11% Cr
0.34% C, 1.40% Si, 1.11% Mn, 24.37% Cr, 19.13% Ni, 0.38% Mo, 0.37% Cu
0.35-0.42% C, 0.80-1.20% Si, 0.25-0.50% Mn, max. 0.03% P, max. 0.02% S, 4.80-5.50% Cr, 1.20-1.50% Mo, 0.85-1.15% V
0.36% C, 0.29% Si, 0.74% Mn, 0.025% P, 0.004% S, 15.50% Cr, 0.76% Ni, 1.05% Mo, 0.06% V, 0.13% Cu
0.36% C, 0.35% Si, 0.74% Mn, 0.026% P, 0.001% S, 15.7% Cr, 0.85% Ni, 0.04% V, 0.07% Cu
0.36% C, 0.84% Si, 0.34% Mn, 0.017% P, 0.001% S, 5.33% Cr, 0.72% Ni, 1.22% Mo, 0.94% V, 0.14% Cu
0.36% C, 0.94% Si, 0.35% Mn, 0.08% S, 0.011% P, 5.06% Cr, 1.52% Mo, 1.03% V
0.36% C, 0.94% Si, 0.35% Mn, 5.06% Cr, 1.62% Mo, 1.03% V, 0.008% S, 0.011% P
0.36% C, 3.15% Ni, 0.88% Cr, 0.40% Mn
0.36% C, 5.7% Cr, 1.6% Mo, 1.1% V, 0.8% Si, 0.2% Mn
0.36% C, 5.7% Cr, 1.6% Mo, 1.1% V, 0.8% Si, 0.2% Mn
0.361% C, 0.35% Si, 0.36% Mn, 0.06% Ni, 5.06% Cr, 1.25% Mo, 0.49% V
0.37% C, 0.22% Si, 0.80% Mn, 0.018% P, 0.006% S, 0.12% Cr, 0.27% Mo
0.37% C, 1.03% Si, 0.33% Mn, 0.014% P, 0.004% S, 5.23% Cr, 0.12% Ni, 0.98% V, 1.28% Mo
0.37% C, 1.93% Mn, 0.35% Si, 1.60% Cr, 0.43% Mo, 0.12% V
0.37% C, 4.90% Cr, 2.90% Mo, 0.45% Mn, 0.61% V, 0.42% Si
0.37-0.44% C, 0.60-0.90% Mn, max. 0.04% P, max. 0.05% S
0.38% C, 0.23% Si, 0.66% Mn, 0.026% P, 0.004% S, 16.06% Cr, 0.61% Ni, 0.07% V, 1.07% Mo, 0.11% Cu, 0.010% Sn, 0.005% Al
0.38% C, 0.38% Si, 0.26% Mn, 0.017% P, 0.002% S, 12.90% Cr, 0.19% Ni, 0.03% Mo, 0.02% V, 0.22% Cu
0.38% C, 0.78% Mn, 0.29% Si, 0.030% S, 0.015% P, 1.01% Cr, 0.14% Mo
0.38% C, 0.78% Mn, 0.29% Si, 0.030% S, 0.015% P, 1.01% Cr, 0.14% Mo
0.38% C, 0.78% Mn, 0.29% Si, 0.030% S, 0.015% P, 1.01% Cr, 0.14% Mo
0.38% C, 0.78% Mn, 0.29% Si, 0.030% S, 0.015% P, 1.01% Cr, 0.14% Mo
0.39% C, 0.58% Si, 0.45% Mn, 0.003% S, 0.018% P, 1.45% Cr, 0.47% MO, 0.13% Ni, 0.70% V, 0.55% W
0.39% C, 0.58% Si, 0.45% Mn, 0.003% S, 0.018% P, 1.45% Cr, 0.47% MO, 0.13% Ni, 0.70% V, 0.55% W
0.39% C, 1.06% Si, 0.32% Mn, 0.019% P, 0.004% S, 4.91% Cr, 0.11% Ni, 1.17% Mo, 0.37% V, 0.011% Ti
0.40% C, 0.24% Si, 0.81% Mn, 0.02% P, 0.007% S, 1.03% Cr, 0.16% Mo
0.40% C, 0.25% Si, 0.70% Mn, 1.85% Ni, 0.80% Cr, 0.25% Mo. Fe-0.3C-4.08Cr steel
0.40% C, 0.25% Si, 0.70% Mn, 1.85% Ni, 0.80% Cr, 0.25% Mo
0.40% C, 0.30% Si, 1.45% Mn, 1.95% Cr, 0.20% Mo, 1.05% Ni. Steel H11">0.37% C, 1.00% Si, 0.38% Mn, 5.15% Cr, 1.30% Mo, 0.40% V. 0.40% C, 0.99% Si, 0.020% P, 0.002% S, 5.13% Cr, 0.11% Ni, 0.96% V, 0.05% W, 1.25% Mo, 0.06% Cu
0.40% C, 1.0% Si, 0.38% Mn, 5.15% Cr, 1.10% V
0.40% C, 1.00% Si, 0.30% Mn, 5.00% Cr, 1.00% V, 1.20% Mo
0.40% C, 1.00% Si, 0.38% Mn, 5.15% Cr, 1.35% Mo, 1.00% V
0.40% C, 1.08% Si, 0.27% Mn, 0.024% P, 0.005% S, 5.35% Cr, 0.22% Ni, 1.08% V, 1.38% Mo, 0.14% Cu
0.42-0.45% C, <0.40% Si, 0.50-0.80% Mn, <0.045% P, <0.045% S, <0.40% Cr, <0.10% Mo, 0.40% Ni, <0.63% = Cr+Mo+Ni
0.45% C, 0.22% Si, O.62% Mn, 0.004% P, O.0038% S
0.46% C, 0.02% Si, 0.02% Mn, 5.22% Cr, 0.01% Cu
0.46% C, 0.27% Mn, max. 0.015% P, max. 0.012% S, 0.37% Si, 3.12% Cr, 0.19% Mo, 0.06% V
0.46% C, 0.40% Si, 0.25% Mn, 0.025% P, 0.019% S, 13.9% Cr, 0.18% Ni, 0.05% V, 0.05% Mo, 0.15% W, 0.07% Cu
0.46-0.52% C, 0.15-0.35% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S
0.47% C, 0.90% Si, 0.97% Mn, 0.010% P, 0.005% S, 34.9% Ni, 24.75% Cr, 0.97% Nb, 0.046% Ti, 0.011% Mo
0.47% C, 0.97% Mn, 0.32% Si, 1.08% Cr, 0.27% Mo, 2.69% Ni, 0.0047% O, 0.0034% N, 0.0033% S, 0.0018% P
0.47% C, max. 1.0% Si, max. 1.0% Mn, 13.50% Cr
0.48% C, 0.20% V, <0.0005% S, <0.0005% O, <0.0005% N
0.48% C, 0.20% V, <0.005% S, <0.005% O, <0.005% N
0.48% C, 0.7% Mn, 0.24% Si, 0.006% P, 0.015% S
0.48% C, 0.88% Si, 0.33% Mn, 0.023% P, 0.013% Cr. 7.90% Cr, 0.21% Ni, 1.47% Mo, 0.46% V, 0.14% Cu
0.49% C, 0.37% Si, 0.28% Mn, 0.037% P, 0.023% S, 12.60% Cr, 0.15% Mo, 0.12% W, 0.35% Ni, 0.07% V, 0.19% Cu
0.50% C, 0.30% Si, 0.70% Mn, 3.25% Cr, 1.40% Mo
0.50% C, 0.37% Mn, max. 0.015% P, max. 0.012% S, 0.37% Si, 5.12% Cr, 0.53% Mo, 0.06% V
0.50% C, 0.50% Si, 0.70% Mn, 3.25% Cr, 1.50% Mo, 0.25% V
0.50% C, 1.0% Si, 0.45% Mn, 8.0% Cr, 1.50% Mo, 0.52% V
0.50% C, 11% W, 4% Cr, 1.5% W
0.50/1.00% C, 4.00/6.00% Cr, 0.50/1.50% Mo, 0.10/0.50% V, 0.10/0.50% Co, 0.10/0.50% W
0.50/1.00% C, 4.00/8.00% Cr, 1.50/3.00% Mo, 0.50/1.50% V, 0.10/0.50% Co, 0.10/0.50% W
0.51% C, 0.27% Si, 0.96% Mn, 0.015% P, 0.025% S, 1.07% Cr, 0.14% V, 0.02% Cu
0.51% C, 0.37% Si, 0.32% Mn, 0.027% P, 0.007% S, 14.4% Cr, 0.12% Ni, 0.010% Mo, 0.03% Cu
0.51% C, 0.89% Si, 0.36% Mn, 0.023% P, 0.002% S, 7.79% Cr, 0.17% Ni, 0.40% V, 1.41% Mn, 0.15% Cu
0.51% C, 0.90% Si, 0.46% Mn, 0.023% P, 0.007% S, 8.26% Cr, 0.17% Ni, 1.19% Mo, 0.11% V, 1.19% W, 0.08% Cu
0.53% C, 0.25% Si, 0.25% Mn, 1.35% Cr, 0.25% V, 2.0% W. Steel O1">0.95% C, 0.25% Si, 1.20% Mn, 0.48% Cr, 0.13% V, 0.55% W. Steel M2">0.90% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 1.90% V, 6.50% W
0.53% C, 0.25% Si, 0.25% Mn, 1.35% Cr, 2.00% W, 0.25% V. O1 steel">0.95% C, 1.1% Mn, 0.6% Cr, 0.6% W. M2 steel">0.90% C, 0.45% Si, 0.40% Mn, 4.15% Cr, 4.95% Mo, 1.90% V, 6.60% W
0.56-0.64% C, 0.75-1.00% Mn, 0.15-0.30% Si, max. 0.035% P, max. 0.04% S, 0.70-0.90% Cr
0.57% C, 1.96% Si, 0.16% Mn, 0.001% P, 0.001% S, 0.041% Al, 1.02% Cr, 0.002% Mo, 0.0018% N, 0.0005% O
0.57% C, 2.0% Si, 0.80% Mn, 0.30% Cr, 0.78% Mo, 0.25% V
0.57% C, 2.0% Si, 0.80% Mn, 0.30% Cr, 0.78% Mo, 0.25% V
0.57% C, 2.0% Si, 0.80% Mn, 0.30% Cr, 0.78% Mo, 0.25% V
0.57% C, 2.0% Si, 0.80% Mn, 0.30% Cr, 0.78% Mo, 0.25% V
0.57% C, 2.0% Si, 0.80% Mn, 0.30% Cr, 0.78% Mo, 0.25% V
0.57% C, 2.0% Si, 0.80% Mn, 0.30% Cr, 0.78% Mo, 0.25% V
0.57% C, 2.0% Si, 0.80% Mn, 0.30% Cr, 0.78% Mo, 0.25% V
0.58% C, 0.36% Si, 0.35% Mn, <0.0018% P, <0.001% S, 14.39% Cr
0.59% C, 0.37% Si, 10.81% Mn, 1.44% Cr, 0.04% Ni
0.5C-25Cr-24.5Ni-1.8W-1.9Si-1.9Mn
0.60% Mn, 0.035% N, Fe
0.62% C, 0.55% Mn, 1.56% Si, 0.006% S, 0.011% P, 0.66% Cr, 0.05% Ni, 0.01% Mo, 0.11% Cu, 0.23% Al, 0.19% V, 0.012% N
0.63% C, 0.34% Si, 0.73% Mn, 0.022% P, 0.002% S, 12.7% Cr, 0.02% Mo
0.64% C, 1.00% Si, 0.55% Mn, 0.020% P, 0.004% S, 7.98% Cr, 1.50% Ni, 0.95% V, 1.35% Mo, 0.09% Cu
0.65% C, 0.27% Mn, max. 0.015% P, max. 0.012% S, 0.37% Si, 5.12% Cr, 0.80% Mo, 0.06% V
0.67% C, 1.06% Si, 0.38% Mn, 0.013% P, 0.002% S, 5.22% Cr, 0.12% Ni, 1.28% Mo, 0.54% V, 0.10% Cu
0.68% C, 0.90% Si, 0.50% Mn, 0.025% P, 0.011% S, 27.80% Cr, 0.28% Ni, 2.13% Mo, 0.07% V, 0.07% W, 0.08% Cu
0.69% C, 17.4% Cr, 14.8% Co
0.70 Mn, 0.26 Si, 0.81 Cr, 1.80 Ni, 0.25 Mo, their carbon contents were 4320 (0.21 C), 4330 (0.31 C), 4340 (0.40 C), 4350 (0.50), 4360 (0.63 C), 4370 (0.71 C), and 4385 (0.84 C)
0.70% C, 0.30% Si, 2.0% Mn, 1.0% Cr, 1.25% Mo
0.70% C, 4.0% Cr, 18.0% W, 1.0% V
0.70-0.85% C, max. 0.35% Si, max. 0.35% Mn, max. 0.15% Cr
0.70-1.0% C, 0.2-0.5% Si, 0.2-0.5% Mn, 2.8-3.5% Cr, <0.2% Mo, <0.1% V. Semi-HSS">0.5-0.8% C, 3.0-6.0% Cr, 4.0-8.0% W(eq), 0.5-1.0% V, eq">W+2Mo
0.74% C, 0.29% Si, 0.24% Mn, 0.025% P, 0.002% S, 3.85% Cr, 0.11% Ni, 0.16% Mo, 17.8% W, 0.15% Co, 0.12% Cu
0.76% C, 0.45% Si, 0.32% Mn, 0.022% P, 0.018% S, 4.33% Cr, 0.12% Ni, 1.00% V, 17.9% W, 0.05% Co, 0.08% Mo, 0.11% Cu
0.77% C
0.78% C, 17.1% Cr, 40.3% Co
0.78% C, 5.6% Cr, 2.1% W, 3.4% Mo, 2.2% V
0.78% C, max. 0.45% Si, max. 0.45% Mn, 4.15% Cr, 1.10% V, 17.95% W
0.78% C, max. 0.45% Si, max. 0.45% Mn, 4.15% Cr, 1.10% V, 17.95% W
0.78% C, max. 0.45% Si, max. 0.45% Si, 4.15% Cr, 1.10% V, 17.95% W
0.79% C, 0.45% Si, 0.40% Mn, 4.15% Cr, 0.65% Mo, 1.55% V, 18.0% W, 4.75% Co
0.79% C, 0.84% Si, 0.25% Mn, 0.012% P, 0.001% S, 4.96% Cr, 0.19% Ni, 0.31% Mo, 0.02% V
0.79% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 0.65% Mo, 1.55% V, 19.0% W, 4.75% Co
0.79% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 0.65% Mo, 1.55% V, 19.0% W, 4.75% Co
0.79% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 0.65% Mo, 1.55% V, 19.0% W, 4.75% Co
0.79% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 0.65% Mo, 1.55% V, 19.0% W, 4.75% Co
0.79% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 0.65% Mo, 1.55% V, 19.0% W, 4.75% Co
0.79% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 0.65% Mo, 1.55% V, 19.0% W, 4.75% Co
0.79% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 0.65% Mo, 1.55% V, 19.0% W, 4.75% Co
0.79% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 0.65% Mo, 1.55% V, 19.0% W, 4.75% Co
0.79% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 0.65% Mo, 1.55% V, 19.0% W, 4.75% Co
0.79% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 0.65% Mo, 1.55% V, 19.0% W, 4.75% Co
0.79% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 0.65% Mo, 1.55% V, 19.0% W, 4.75% Co
0.79% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 0.65% Mo, 1.55% V, 19.0% W, 4.75% Co
0.79% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 0.65% Mo, 1.55% V, 19.0% W, 4.75% Co
0.79% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 0.65% Mo, 1.55% V, 19.0% W, 4.75% Co
0.79% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 0.65% Mo, 1.55% V, 19.0% W, 4.75% Co
0.79% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 0.65% Mo, 1.55% V, 19.0% W, 4.75% Co
0.79% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 0.65% Mo, 1.55% V, 19.0% W, 4.75% Co
0.79% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 0.65% Mo, 1.55% V, 19.0% W, 4.75% Co
0.79% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 0.65% Mo, 1.55% V, 19.0% W, 4.75% Co
0.79% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 0.65% Mo, 1.55% V, 19.0% W, 4.75% Co
0.79% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 0.65% Mo, 1.55% V, 19.0% W, 4.75% Co
0.79% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 0.65% Mo, 1.55% V, 19.0% W, 4.75% Co
0.79% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 0.65% Mo, 1.55% V, 19.0% W, 4.75% Co
0.79% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 0.65% Mo, 1.55% V, 19.0% W, 4.75% Co
0.79% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 0.65% Mo, 1.55% V, 19.0% W, 4.75% Co
0.79% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 0.65% Mo, 1.55% V, 19.0% W, 4.75% Co
0.79% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 0.65% Mo, 1.55% V, 19.0% W, 4.75% Co
0.79% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 0.65% Mo, 1.55% V, 19.0% W, 4.75% Co
0.80% C, 0.85% Si, 0.30% Mn, 3.00% Cr, 0.18% Mo, 0.40% Ni, 0.20% V
0.80% C, 18.7% W, 4.3% Cr, 1.9% V
0.80% C, 5% Cr, 3% (Mo, W), 1% (V, Nb). HSS">1.8% C, 5% Cr, 5% (Mo, W), 5% (V, Nb)
0.80% C
0.80-1.25% C, 11.00-13.00% Mn
0.81% C, 0.30% Mn, max. 0.015% P, max. 0.012% S, 0.30% Si, 2.42% Cr, 0.19% Mo, 0.06% V
0.81% C, 0.37% Mn, max. 0.015% P, max. 0.012% S, 0.30% Si, 3.12% Cr, 0.19% Mo, 0.06% V
0.81% C, 0.37% Mn, max. 0.015% P, max. 0.012% S, 0.30% Si, 3.12% Cr, 0.53% Mo, 0.06% V
0.81% C, 0.37% Mn, max. 0.015% P, max. 0.012% S, 0.40% Si, 4.00% Cr, 0.53% Mo, 0.06% V
0.81% C, 0.37% Mn, max. 0.015% P, max. 0.012% S, 0.40% Si, 5.12% Cr, 0.48% Mo, 0.06% V
0.82% C, 0.45% Si, 0.40% Mn, 3.85% Cr, 8.60% Mo, 1.15% V, 1.75% W
0.82% C, 0.45% Si, 0.40% Mn, 3.85% Cr, 8.60% Mo, 1.15% V, 1.75% W
0.82% C, 0.70% Si, 0.40% Mn, 8.0% Cr, 1.60% Mo, 0.60% V
0.82% C, 0.79% Si, 0.29 Mn%, 0.012% P, 0.005% S, 5.10% Cr, 0.10% Ni, 0.28% Mo, 0.03% V, 0.15% Cu, 0.04% W, 0.82% C, 0.79% Si, 0.29% Mn, 0.012% P, 0.005% S, 5.10% Cr, 0.10% Ni, 0.28% Mo, 0.03% V, 0.15% Cu, 0.012% Al
0.83% C, 0.26% Si, 0.68% Mn, 0.015% P, 0.002% S, 0.55% Cr, 0.05% Ni, 0.15% V
0.85% C, 0.22% Mn, 0.23% Si, 0.009% P, 4.11% Cr, 0.10% Ni, 4.48% Mo, 1.05% V, 0.05% Cu, 0.011-0.012% N
0.85% C, 0.22% Si, 0.65% Mn, 0.016% P, 0.002% S, 3.00% Cr, 0.13% Ni, 0.13% V, 0.48% Mo, 0.12% Cu
0.85% C, 0.27% Mn, 0.31% Si, 4.26% Cr, 0.50% Mo, 17.0% W, 1.26% V
0.85% C, 0.30% Si, 0.54% Mn, 0.020% P, 0.003% S, 4.04% Cr, 0.48% Ni, 1.45% V, 17.0% W, 0.85% Mo, 0.11% Cu
0.85% C, 0.81% Si, 0.33% Mn, 0.010% P, 0.008% S, 2.18% Cr, 0.06% Ni, 0.01% V, 0.53% Mo, 0.011% Al, 0.04% Cu
0.86% C, 0.21% Si, 1.98% Mn, 0.012% P, 0.008% S, 0.33% Cr, 0.10% Ni, 0.05% Mo, 0.09% V, 0.01% W, 0.13% Cu
0.86-0.94% C, max. 0.45% Si, max. 0.40% Mn, max. 0.030% P, max. 0.030% S, 3.80-4.50% Cr, 4.70-5.20% Mo, 1.70-2.00% V, 6.00-6.70% W
0.87% C, 0.27% Mn, max. 0.015% P, max. 0.012% S, 0.40% Si, 5.12% Cr, 0.19% Mo, 0.06% V
0.87% C, 0.29% Mn, 0.37% Si, 4.24% Cr, 5.0% Mo, 6.73% W, 1.88% V
0.87% C, 0.44% Mn, 0.17% Si, 0.013% P, 0.006% S, 0.39% Ni, 0.21% Cr
0.87% C, 0.44% Mn, 0.17% Si, 0.013% P, 0.006% S, 0.39% Ni, 0.21% Cr
0.87% C, 0.44% Mn, 0.17% Si, 0.013% P, 0.006% S, 0.39% Ni, 0.21% Cr
0.87% C, 6.06% W, 4.79% Mo, 4.09% Cr, 1.89% V, 0.42% Si, 0.39% Mn, 0.22% Ni, 0.12% Cu, 0.022% P, 0.007% S, 0.08% RE, 0.06% N
0.88% C, 0.24% Si, 0.26% Mn, 0.027% P, 0.009% S, 3.91% Cr, 0.21% Ni, 1.78% V, 6.25% W, 4.71% Mo, 0.18% Cu
0.88% C, 0.30% Si, 0.38% Mn, 2.15% Cr, 0.28% Mo, 0.10% V
0.88% C, 0.33% Si, 0.35% Mn, 0.009% P, 0.001% S, 0.11% Ni, 4.97% Cr, 0.41% Mo, 0.33% Cu
0.88% C, 0.37% Si, 0.30% Mn, 4.05% Cr, 1.75% V, 6.03% W, 4.85% Mo
0.88% C, 4.0% Cr, 0.80% Mo, 2.50% V, 12.0% W
0.88% C, 4.0% Cr, 0.80% Mo, 2.50% V, 12.0% W
0.88% C, 4.0% Cr, 0.80% Mo, 2.50% V, 12.0% W
0.88% C, 4.0% Cr, 0.80% Mo, 2.50% V, 12.0% W
0.88% C, 4.0% Cr, 0.80% Mo, 2.50% V, 12.0% W
0.88% C, 4.0% Cr, 0.80% Mo, 2.50% V, 12.0% W
0.88% C, 4.0% Cr, 0.80% Mo, 2.50% V, 12.0% W
0.88% C, 4.0% Cr, 0.80% Mo, 2.50% V, 12.0% W
0.88% C, 4.0% Cr, 0.80% Mo, 2.50% V, 12.0% W
0.88% C, 4.0% Cr, 0.80% Mo, 2.50% V, 12.0% W
0.88% C, 4.0% Cr, 0.80% Mo, 2.50% V, 12.0% W
0.88% C, 4.0% Cr, 0.80% Mo, 2.50% V, 12.0% W
0.88% C, 4.0% Cr, 0.80% Mo, 2.50% V, 12.0% W
0.88% C, 4.0% Cr, 0.80% Mo, 2.50% V, 12.0% W
0.88% C, 4.0% Cr, 0.80% Mo, 2.50% V, 12.0% W
0.88% C, 4.0% Cr, 0.80% Mo, 2.50% V, 12.0% W
0.88% C, 4.0% Cr, 0.80% Mo, 2.50% V, 12.0% W
0.88% C, 4.0% Cr, 0.80% Mo, 2.50% V, 12.0% W
0.88% C, 4.0% Cr, 0.80% Mo, 2.50% V, 12.0% W
0.88% C, 4.0% Cr, 0.80% Mo, 2.50% V, 12.0% W
0.88% C, 4.0% Cr, 0.80% Mo, 2.50% V, 12.0% W
0.88% C, 4.0% Cr, 0.80% Mo, 2.50% V, 12.0% W
0.88% C, 4.0% Cr, 0.80% Mo, 2.50% V, 12.0% W
0.88% C, 4.0% Cr, 0.80% Mo, 2.50% V, 12.0% W
0.88% C, 4.0% Cr, 0.80% Mo, 2.50% V, 12.0% W
0.89%C, 0.20%Si, 0.26%Mn, 0.027 %P, 0.001 %S, 3.91% Cr, 4.74% Mo, 1.74% V, and 6.10% W
0.90% C, 0.17% Si, 0.36% Mn, 0.011% P, 0.01% S, 1.45% Cr
0.90% C, 0.26% Si, 0.27% Mn, 0.028% P, 0.003% S, 3.95% Cr, 0.13% Ni, 4.70% Mo, 1.78% V, 6.40% W, 0.13% Cu
0.90% C, 0.39% Si, 0.44% Mn, 0.026% P, 0.007% S, 17.40% Cr, 0.38% Ni, 0.10% V, 0.10% W, 0.93% Al, 0.07% Cu
0.90% C, 0.45% Si, 0.40% Mn, 4.15% Cr, 4.95% Mo, 1.90% V, 6.60% W
0.90% C, 0.45% Si, 0.40% Mn, 4.15% Cr, 4.95% Mo, 1.90% V, 6.60% W
0.90% C, 1.0% Si, 1.0% Mn, 18.0% Cr, 1.10% Mo, 0.10% V
0.90% C, 19.03 wt.% Cr, 1.65 wt.% Mo and 0.66% wt.% Mn
0.90% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 1.90% V, 6.50% W
0.90% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 4.95% Mo, 1.90% V, 6.60% W
0.90% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 4.95% Mo, 1.90% V, 6.60% W
0.90% C, max. 0.45% Si, max. 0.45% Mn, 4.15% Cr, 4.95% Mo, 1.90% V, 6.60% W
0.90% C, max. 0.45% Si, max. 0.45% Mn, 4.15% Cr, 4.95% Mo, 1.90% V, 6.60% W
0.90% C, max. 0.45% Si, max. 0.45% Mn, 4.15% Cr, 4.95% Mo, 1.90% V, 6.60% W
0.90% C, max. 0.45% Si, max. 0.45% Mn, 4.15% Cr, 4.95% Mo, 1.90% V, 6.60% W
0.90% C, max. 0.45% Si, max. 0.45% Mn, 4.15% Cr, 4.95% Mo, 1.90% V, 6.60% W
0.90% C, max. 0.45% Si, max. 0.45% Mn, 4.15% Cr, 4.95% Mo, 1.90% V, 6.60% W
0.90% C, max. 0.45% Si, max. 0.45% Mn, 4.15% Cr, 4.95% Mo, 1.90% V, 6.60% W
0.90% C, max. 0.45% Si, max. 0.45% Mn, 4.15% Cr, 4.95% Mo, 1.90% V, 6.60% W
0.90% C, max. 0.45% Si, max. 0.45% Mn, 4.15% Cr, 4.95% Mo, 1.90% V, 6.60% W
0.90% C, max. 0.45% Si, max. 0.45% Mn, 4.15% Cr, 4.95% Mo, 1.90% V, 6.60% W
0.90% C, max. 0.45% Si, max. 0.45% Mn, 4.15% Cr, 4.95% Mo, 1.90% V, 6.60% W
0.90% C, max. 0.45% Si, max. 0.45% Mn, 4.15% Cr, 4.95% Mo, 1.90% V, 6.60% W
0.90% C, max. 0.45% Si, max. 0.45% Mn, 4.15% Cr, 4.95% Mo, 1.90% V, 6.60% W
0.90% C, max. 0.45% Si, max. 0.45% Mn, 4.15% Cr, 4.95% Mo, 1.90% V, 6.60% W
0.90% C, max. 0.45% Si, max. 0.45% Mn, 4.15% Cr, 4.95% Mo, 1.90% V, 6.60% W
0.91% C, 0.20% Si, 0.32% Mn, 0.024% P, 0.002% S, 3.80% Cr, 0.15% Ni, 4.90% Mo, 1.74% V, 6.10% W, 0.14% Cu
0.91% C, 0.23% Si, 0.24% Mn, 0.026% P, 0.010% S, 4.05% Cr, 0.14% Ni, 1.95% V, 6.25% W, 4.65% Mo, 0.13% Cu
0.91% C, 0.25% Si, 0.30% Mn, 0.024% P, 0.003% S, 3.87% Cr, 0.28% Ni, 4.97% Mo, 1.85% V, 6.20% W, 0.12% Cu
0.91% C, 0.45% Si, 0.40% Mn, 4.15% Cr, 1.90% Ni, 6.30% V, 4.75% Cr
0.92% C, 0.27% Si, 0.68% Mn, 0.014% P, 0.003% S, 1.75% Cr, 0.05% Ni, 0.27% Mo, 0.01% V, 0.03% Cu
0.92% C, 0.30% Si, 6.17% W, 4.79% Mo, 4.00% Cr, 1.85% V
0.92% C, 0.42% Si, 0.27% Mn, 0.027% P, 3.93% Cr, 6.12% W, 4.77% Mo, 0.39% Ni, 1.74% V, 0.17% Cu, 4.59% Co, 0.018% Al, 0.018% N
0.92% C, 0.42% Si, 0.27% Mn, 0.027% P, 3.93% Cr, 6.12% W, 4.77% Mo, 0.39% Ni, 1.74% V, 0.17% Cu, 4.59% Co, 0.018% Al, 0.018% N
0.92% C, 0.42% Si, 0.27% Mn, 0.027% P, 3.93% Cr, 6.12% W, 4.77% Mo, 0.39% Ni, 1.74% V, 0.17% Cu, 4.59% Co, 0.018% Al, 0.018% N
0.93-1.05% C, 0.15-0.35% Si, 0.25-0.45% Mn, 1.35-1.60% Cr
0.93-1.05% C, 0.15-0.35% Si, 0.25-0.45% Mn, 1.35-1.60% Cr
0.93-1.05% C, 0.15-0.35% Si, 0.25-0.45% Mn, 1.35-1.60% Cr
0.94% C, 0.37% Si, 0.40% Mn, 0.023% P, 0.007% S, 17.46% Cr, 0.38% Ni, 0.96% Mo, 0.11% V, 0.09% Cu
0.95% C, 0.018% P, 0.002% S, 0.22% Si, 0.65% Mn, 3.10% Cr, 0.13% Ni, 0.14% V, 0.51% Mo, 0.13% Cu
0.95% C, 0.33% Si, 1.14% Mn, 0.015% P, 0.002% S, 0.45% Cr, 0.17% Ni, 0.48% W, 0.02% Ni, 0.03% Cu
0.95% C, 1.1% Mn, 0.6% Cr, 0.6% W
0.95% C, 1.10% Mn, 0.60% Cr, 0.60% W, 0.10% V. Steel D2">1.55% C, 0.40% Mn, 11.80% Cr, 0.30% Si, 0.80% V, 0.80% Mo
0.965% C, 0.261% Si, 0.29% Mn, 0.0167% P, 0.0128% S, 1.47% Cr, 0.0474% Ni, 0.0261% Al, 0.0755% Cu, 0.0633% Ti
0.98-1.10% C, 0.25-0.45% Mn, 0.15-0.35% Si, max. 0.025% P, max. 0.025% S, 1.30-1.60% Cr
0.98-1.10% C, 0.25-0.45% Mn, 0.15-0.35% Si, max. 0.025% P, max. 0.025% S, 1.30-1.60% Cr
1.00% C, 0.27% Si, 0.48% Mn, 0.019% P, 0.011% S, 4.93% Cr, 0.14% Ni, 0.92% Mo, 0.22% V, 0.12% Cu
1.00% C, 0.30% Si, 0.60% Mn, 5.3% Cr, 1.1% Mo, 0.2% V
1.00% C, 0.50% Si, 0.30% Mn, 10.0% Cr, 0.25% V
1.00% C, 0.50% Si, 0.30% Mn, 10.0% Cr, 0.25% V
1.00% C, 0.50% Si, 0.30% Mn, 10.0% Cr, 0.25% V
1.00% C, 0.50% Si, 0.30% Mn, 10.0% Cr, 0.25% V
1.00% C, 0.50% Si, 0.30% Mn, 10.0% Cr, 0.25% V
1.00% C, 0.50% Si, 0.30% Mn, 10.0% Cr, 0.25% V
1.00% C, 0.50% Si, 0.30% Mn, 10.0% Cr, 0.25% V
1.00% C, 0.50% Si, 0.30% Mn, 10.0% Cr, 0.25% V
1.00% C, 0.50% Si, 0.30% Mn, 10.0% Cr, 0.25% V
1.00% C, 0.50% Si, 0.30% Mn, 10.0% Cr, 0.25% V
1.00% C, 0.50% Si, 0.30% Mn, 10.0% Cr, 0.25% V
1.00% C, 0.50% Si, 0.30% Mn, 10.0% Cr, 0.25% V
1.00% C, 0.50% Si, 0.30% Mn, 10.0% Cr, 0.25% V
1.00% C, 0.50% Si, 0.30% Mn, 10.0% Cr, 0.25% V
1.00% C, 0.50% Si, 0.30% Mn, 10.0% Cr, 0.25% V
1.00% C, 0.50% Si, 0.30% Mn, 10.0% Cr, 0.25% V
1.00% C, 0.50% Si, 0.30% Mn, 10.0% Cr, 0.25% V
1.00% C, 0.50% Si, 0.30% Mn, 10.0% Cr, 0.25% V
1.00% C, 0.50% Si, 0.30% Mn, 10.0% Cr, 0.25% V
1.00% C, 0.50% Si, 0.30% Mn, 10.0% Cr, 0.25% V
1.00% C, 0.50% Si, 0.30% Mn, 10.0% Cr, 0.25% V
1.00% C, 0.50% Si, 0.30% Mn, 10.0% Cr, 0.25% V
1.00% C, 0.50% Si, 0.30% Mn, 10.0% Cr, 0.25% V
1.00% C, 0.50% Si, 0.30% Mn, 10.0% Cr, 0.25% V
1.00% C, 0.50% Si, 0.30% Mn, 10.0% Cr, 0.25% V
1.00% C, 0.8%Si, 0.1% Mn, 17.0% Cr, 0.2% Ni, 0.005% P, 0.025% S and 80.87% Fe
1.00% C, 1.0% Mo, 0.25% V
1.00% C, 1.0% Mo, 0.25% V
1.00% C, 1.0% Mo, 0.25% V
1.00% C, 1.0% Mo, 0.25% V
1.00% C, 1.0% Mo, 0.25% V
1.00% C, 1.0% Mo, 0.25% V
1.00% C, 1.0% Si, 1.0% Mn, 17.0% Cr, 0.75% Mo
1.00% C, 1.00% Si, 1.00% Mn, 17.00% Cr, 0.75% Mo
1.00% C, 1.10% Si, 0.30% Mn, 8.0% Cr, 2.70% Mo, 0.30% V
1.00% C, 5.0% Cr, 1.0% Mn, 1.0% Mo, 0.15-0.50% V
1.00% C, max. 0.005% S, 0.35% Mn, 7.50% Cr, 2.60% Mo, 0.30% V, +Ti
1.00% Cr, 1.0% Mo, 0.25% V
1.00-1.35% C, 0.50-1.00% Si, 11.00-14.00% Mn, max. 0.020% P, max. 0.050% S, max. 0.50% Cr
1.00-2.5% C, 0.1-0.5% Si, 0.5-1.5% Mn, 1.0-2.5% Mn, 4.0-8.0% Cr, 2.0-8.0% Mo, <0.05% P, <0.015% S, 3.0-9.0% V, 2.0-98.0% W
1.02% C, 0.20% Si, 0.23% Mn, 0.10% V
1.02% C, 0.25% Si, 0.33% Mn, 1.50% Cr. Steel S2">0.4 - 0.55% C, 0.9-1.2% Si, 0.3-0.5% Mn, 0.3-0.6% Mo, max. 0.5% V. Steel S5">0.57% C, 2.00% Si, 0.80% Mn, 0.30% Cr, 0.25% V. Steel S7">0.50% C, 0.50%, 0.70% Mn, 3.25% Cr, 1.50% Mo, 0.25% V. Steel H13"> 0.37% C, 1.03% Si, 0.33% Mn, 0.014% P, 0.004% S, 5.23% Cr, 0.12% Ni, 0.98% V, 1.28% Mo. Steel M2">0.90% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 1.90% V, 6.50% W
1.03% C, 0.22% Si, 0.18% Mn, 3.29% Cr, 4.0% Mo, 6.19% W, 1.87% V, 0.034% N
1.03% C, 0.27% Si, 0.32% Mn, 0.021% P, 0.005% S, 3.87% Cr, 0.17% Ni, 2.37% V, 6.27% W, 4.87% Mo, 0.18% Cu. Diameter of 62 mm">1.04% C, 0.25% Si, 0.32% Mn, 0.022% P, 0.004% S, 3.88% Cr, 0.17% Ni, 2.32% V, 6.21% W, 4.83% Mo, 0.18% Cu
1.03% C, 3.29% Cr, 4.98% Mo, 6.19% W, 1.87% V, 0.22% Si, 0.18% Mn, 0.30% Ni
1.033% C, 0.604% Si, 1.199% Mn, 0.013% P, 0.004% S, 1.15% Cr, <0.001% Mo, 0.011% Ni, 0.013% Cu
1.04% C, 0.96% Si, 0.38% Mn, 0.014% P, 0.002% S, 8.16% Cr, 0.11% Ni, 0.27% V, 2.06% Mo, 0.72% Nb
1.05% C, 0.20% Si, 0.25% Mn, 0.15% V
1.05% C, 0.20% Si, 0.25% Mn
1.05% C, 0.20% Si, 0.25% Mn
1.05% C, 0.20% Si, 0.25% Mn
1.05% C, 0.20% Si, 0.25% Mn
1.05% C, 0.20% Si, 0.25% Mn
1.05% C, 0.20% Si, 0.25% Mn
1.05% C, 0.30% Mn, 0.30% Si
1.06% C, 1.02% Si, 0.021% P, 0.005% S, 7.37% Cr, 2.29% V, 0.20% Ni, 1.43% Mo, 0.12% Cu
1.07% C, 0.38% Si, 0.34% Mn, 0.025% P, 0.003% S, 16.60% Cr, 0.49% Ni, 0.51% Mo, 0.05% V, 0.09% Cu
1.07% C, 1.21% Si, 0.28% Mn, 0.026% P, 0.001% S, 8.02% Cr, 0.13% Ni, 2.63% V, 1.14% W, 1.54% Mo, 0.06% Cu
1.08% C, 1.0% Si, 1.0% Mn, 17.0% Cr, 0.60% Mo
1.08% C, 1.0% Si, 1.0% Mn, 17.0% Cr, 0.60% Mo
1.08% C, 1.04% Si, 0.021% P, 0.005% S, 7.32% Cr, 0.19% Ni, 2.28% V, 0.98% W, 1.44% Mo, 0.13% Cu
1.08% C, 3.75% Cr, 8.0% Co, 9.5% Mo, 1.5% W, 1.15% V
1.08% C, 3.75% Cr, 8.0% Co, 9.5% Mo, 1.5% W, 1.15% V
1.08% C, max. 1.0% Si, max. 1.0% Mn, 17.00% Cr, 0.60% Mo
1.0C-0.35Mn-0.25Si-1.4Cr wt% and 1.0C-0.35Mn-1.25Si-1.4Cr
1.10% C, 0.50% Si, 0.40% Mn, 4.50% Cr, 3.20% Mo, 3.70% W, 8.50% V, 1.80% N
1.10% C, 0.70% Si, 0.40% Mn, 4.00% Cr, 9.50% Mo, 1.10% V, 1.55% W
1.10% C, 1.00% Si, 0.021% P, 0.005% S, 7.90% Cr, 2.20% V, 1.15% W, 0.07% Ni, 1.45% Mo, 0.05% Cu
1.10% C, 2.0% Si, 1.0% Mn, 28.0% Cr, 2.25% Mo
1.10% C, 3.80% Cr, 9.50% Mo, 1.50% W, 1.20% V, 8.00% Co
1.11% C, 0.70% Si, 0.39% Mn, 0.016% P, 0.002% S, 4.58% Cr, 1.39% W, 9.46% Mo, 1.37% V, 8.04% Co
1.145% C, 0.552% Si, 0.492% Mn, 16.01% Cr
1.15% C
1.20% C, 17.50% Mn, 9.50% Cr, 2.80% Nb
1.20% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 4.95% Mo, 2.95% V, 6.35% W
1.20% C
1.21% C, 0.86% Si, 0.33% Mn, 0.019% P, 0.001% S, 8.65% Cr, 0.15% Ni, 2.67% Mo, 1.20% V, 0.50% Nb, 0.07% Cu
1.22% C, 1.93% Mn, 0.19% Si, 0.020% P, 0.020% S, 1.52% Cr, 0.36% Mo, 0.17% V
1.25% C, 0.70% Si, 0.50% Mn, 4.15% Cr, 5.0% Mo, 0.50% Ni, 2.95% V, 6.30% W, 1.0% Co
1.269% C, 4.288% C, 3.005% Mo, 5.88% W, 4.56% V, 77.67% Fe
1.28% C, 0.45% Si, 0.40% Mn, 4.15% Cr, 3.55% Mo, 3.25% V, 9.50% W, 10.0% Co
1.28% C, 1.05% Si, 0.43% Mn, 0.036% P, 0.025% P, 24.7% Cr, 1.14% Ni, 0.04% V, 0.06% Mo, 0.14% Cu
1.28% C, 4.0% Cr, 5.0% Mo, 6.4% W, 3.1% V
1.28% C, 4.20% Cr, 5.0% Mo, 6.40% W, 3.10% V, 8.50% Co
1.28% C, 4.20% Cr, 5.0% Mo, 6.40% W, 3.10% V, 8.50% Co
1.28% C, 4.20% Cr, 6.30% W, 5.00% Mo, 3.10% W
1.28% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 3.55% Mo, 3.25% V, 9.50% W, 10.0% Co
1.28% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 3.55% Mo, 3.25% V, 9.50% W, 10.0% Co
1.28% C, max. 0.45% Si, max. 0.40% Mn, 4.15% Cr, 3.55% Mo, 3.25% V, 9.50% W, 10.0% Co
1.29% C, 0.61% Si, 0.26% Mn, 0.019% P, 0.011% S, 3.88% Cr, 0.24% Ni, 3.05% V, 6.30% W, 8.20% Co, 0.03% Ti, 4.95% Mo, 0.09% Cu
1.29% C, 4.03% Cr, 4.43% Mo, 5.26% W, 3.82% V, 0.40% Mn, 0.03% P, 0.02% S
1.30% C, 0.3% Si, 0.3% Mn, 4.5% Cr, 4.5% Mo, 5.5% W, 4.0% V
1.30% C, 4.5% Cr, 4.5% Mo, 5.5% W, 4.0% V
1.30% C, 4.5% Cr, 4.5% Mo, 5.5% W, 4.0% V
1.31% C, 0.70% Si, 0.50% Mn, 4.50% Cr, 3.15% V, 6.70% W, 5.30% Mo
1.31% C, 0.70% Si, 0.50% Mn, 4.50% Cr, 3.15% V, 6.70% W, 5.30% Mo
1.31% C, 0.72% Si, 0.38% Mn, 0.020% P, 0.006% S, 4.16% Cr, 0.20% Ni, 4.16% Cr, 3.00% V, 6.20% W, 0.48% Co, 5.10% Mo, 0.12% Cu
1.31% C, 6.24% W, 5.34% Mo, 4.12% Cr, 3.05% V, 0.56% Si, 0.24% Mn, 0.11% Ni, 0.22% Cu, 749 ppm N
1.31%C, 0.35% Mn, 0.25% Si
1.34% C, 0.22% Si, 0.18% Mn, 3.29% Cr, 4.09% Mo, 6.19% W, 1.87% V, 0.034% Ni, 0.034% N
1.34% C, 0.85% Si, 0.67% Mn, 0.010% P, 0.011% S, 0.25% Cr, 0.14% Ni, 0.01% V, 0.21% Mo, 0.14% Cu
1.36% C, 0.19% Si, 0.58% Mn, 0.021% P, 0.008% S, 1.42% Cr, 0.07% Ni, 0.13% V, 0.16% Cu
1.40% C, 0.23% Si, 0.42% Mn, 11.59% Cr, 0.80% Mo, 0.23% V, 0.96% C, 0.98% Si, 0.41% Mn, 7.23% Cr, 1.93% Mo, 0.24% V
1.40% C, 1% Si, 0.6% Mn, 4.6% Cr, 3.2% Mo, 3.7% V
1.40% C
1.42% C, 0.40% Mn, 0.30% Si, 11.57% Cr, 0.17% Mo, 0.70% V, 0.010% S, 0.018% P
1.44% C, 0.3% Si, 0.4% Mn, 12.2% Cr, 0.84% Mo, 0.43% V, 0.022% P, 0.008% S
1.45% C, 1.15% Si, 0.80% Mn, 0.25% Mo
1.46% C, 1.03% Si, 12.54% Mn
1.46% C, 12.98% Cr, 2.92% Mo, 2.92% V, 2.00% W
1.49% C, 0.19% Si, 0.57% Mn, 0.023% P, 0.008% S, 1.36% Cr, 0.14% Ni, 0.07% Mo, 0.02% V, 0.13% Cu
1.50% C, 0.30% Si, 0.33% Mn, 0.014% P, 0.006% S, 12.0% Cr, 0.16% Ni, 0.31% V, 0.92% Mo, 0.06% Cu
1.50% C, 0.30% Si, 0.50% Mn, 0.10% S, 12.00% Cr, 1.00% V, 0.75% Mo
1.50% C, 1.0% Si, 0.4% Mn, 8.0% Cr, 1.5% Mo, 4.0% V
1.50-2% C, 0.5-1% Si, 0.5-1.5% Mn, 1-1.5% Ni, 5-7% Cr, 2-5% Mo, 1-3% W, 3-5% V
1.50-2.0% C, 0.5-1.0% Si, 0.2-0.5% Mn, 4.0-6.0% Cr, 4.0-6.0% Mo, 0.5-1.0% Ni, 4.0-6.0% V, 0.1-0.5% W
1.50-2.0% C, 5.0-7.0% Cr, 3.0-4.0% Mo, 4.0-5.0% V, 1.5-2.5% W
1.50-2.0% C, 5.0-7.0% Cr, 7.0-10.0% Weg, 0.6-0.7% Mo/(Mo+W), 4.0-6.0% V. Aurora">1.5-2.0% C, 3.0-5.0% Cr, 11.0-14.0% Weg, 0.9-1.0% Mo/(Mo+W), 4.0-6.0% V
1.50-2.5% C; up to 6% W; up to 6% Mo; 3-8% Cr, 4-10% V
1.51% C, 0.32% Si, 0.27% Mn, 0.019% P, 0.016% S, 11.60% Cr, 0.63% Mo, 0.20% Ni, 0.91% V
1.52% C, 0.28% Si, 0.25% Mn, 0.015% P, 0.008% S, 11.30% Cr, 0.23% Ni, 0.95% V, 0.77% Mo, 0.16% Cu
1.53% C, 0.24% Si, 0.25% Mn, 0.016% P, 0.009% S, 11.50% Cr, 0.18% Ni, 0.79% V, 0.77% Mo, 0.22% Cu
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 0.85% V. Steel 1.4718"> 0.45% C, 3.00% Si, max. 0.60% Mn, 9.00% Cr, max. 0.50% Ni
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 0.85% V. Steel D3">2.1% C, 0.3% Mn, 0.3% Si, 12.5% Cr, 0.5% Ni. Steel M1">0.82% C, 0.45% Si, 0.40% Mn, 3.85% Cr, 8.60% Mo, 1.15% V, 1.75% Steel M4">1.3% C, 0.3% Si, 0.3% Mn, 4.5% Cr, 4.5% Mo, 5.5% W, 4.0% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 1.0% Mo, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 1.0% Mo, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 1.0% Mo, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 1.0% Mo, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 1.0% Mo, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 1.0% Mo, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 1.0% Mo, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 1.0% Mo, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 1.0% Mo, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.0% Cr, 1.0% Mo, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.00% Cr, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.00% Cr, 1.00% Mo, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.00% Cr, 1.00% Mo, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.00% Cr, 1.00% Mo, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.00% Mn, 1.00% Mo, 0.85% V
1.55% C, 0.24% Si, 0.26% Mn, 0.026% P, 0.011% S, 12.0% Cr, 0.15% Ni, 0.97% V, 0.06% W, 0.73% Mo, 0.07% Cu
1.55% C, 0.25% Si, 0.21% Mn, 0.019% P, 0.008% S, 11.7% Cr, 0.19% Ni, 0.93% V, 0.79% Mo, 0.19% Cu
1.55% C, 0.32% Si, 0.32% Mn, 12.7% Cr, 0.85% Mo, 0.89% V, 0.12% W, 0.12% Co. PM tool steel">2.45% C, 0.38% Si, 0.41% Mn, 4.8% Cr, 4.8% Mo, 11% V, 1.4% W, 2.1% Co
1.56% C, 0.28% Si, 0.27% Mn, 0.020% P, 0.004% S, 11.77% Cr, 0.17% Ni, 0.73% Mo, 0.95% V, 0.14% W, 0.11% Cu
1.57% C, 0.26% Si, 0.23% Mn, 0.024% P, 0.008% S, 11.75% Cr, 0.19% Ni, 0.95% V, 0.82% Mo, 0.15% Cu
1.58% C, 0.24% Si, 0.25% Mn, 0.025% P, 0.010% S, 11.4% Cr, 0.16% Ni, 0.85% V, 0.12% W, 0.81% Mo, 0.14% Cu
1.5Cr-0.5Mn-0.7C
1.60% C, 0.30% Si, 0.30% Mn, 4.25% Cr, 0.75% Mo, 5.0% V, 12.25% 1.60% C, 0.30% Si, 0.30% Mn, 4.25% Cr, 0.75% Mo, 5.0% V, 12.25% W, 5.0% Co
1.60% C, 0.30% Si, 0.30% Mn, 4.25% Cr, 0.75% Mo, 5.0% V, 12.25% W, 5.0% Co
1.61% C, 0.155% Si, 0.36% Mn, 0.029% S, 0.050% P
1.63% C, 4.66% Cr, 10.54% W, 2.00% Mo, 4.70% V, 7.83% Co
1.65% C, 0.33% Si, 0.30% Mn, 11.5% Cr, 0.60% Mo, 0.30% V, 0.50% W
1.65% C, 0.33% Si, 0.30% Mn, 11.5% Cr, 0.60% Mo, 0.30% V, 0.50% W
1.65% C, 0.33% Si, 0.30% Mn, 11.5% Cr, 0.60% Mo, 0.30% V, 0.50% W
1.65% C, 0.33% Si, 0.30% Mn, 11.5% Cr, 0.60% Mo, 0.30% V, 0.50% W
1.65% C, 0.33% Si, 0.30% Mn, 11.5% Cr, 0.60% Mo, 0.30% V, 0.50% W
1.65% C, 0.33% Si, 0.30% Mn, 11.5% Cr, 0.60% Mo, 0.30% V, 0.50% W
1.65% C, 0.33% Si, 0.30% Mn, 11.5% Cr, 0.60% Mo, 0.30% V, 0.50% W
1.65% C, 0.33% Si, 0.30% Mn, 11.5% Cr, 0.60% Mo, 0.30% V, 0.50% W
1.65% C, 0.33% Si, 0.30% Mn, 11.5% Cr, 0.60% Mo, 0.30% V, 0.50% W
1.65% C, 0.33% Si, 0.30% Mn, 11.5% Cr, 0.60% Mo, 0.30% V, 0.50% W
1.65% C, 0.33% Si, 0.30% Mn, 11.5% Cr, 0.60% Mo, 0.30% V, 0.50% W
1.65% C, 0.33% Si, 0.30% Mn, 11.5% Cr, 0.60% Mo, 0.30% V, 0.50% W
1.65% C, 0.33% Si, 0.30% Mn, 11.50% Cr, 0.60% Mo, 0.30% V, 0.50% W
1.65% C, 0.33% Si, 0.30% Mn, 11.50% Cr, 0.60% Mo, 0.30% V, 0.50% W
1.65% C, 0.33% Si, 0.30% Mn, 11.50% Cr, 0.60% Mo, 0.30% V, 0.50% W
1.65% C, 0.33% Si, 0.30% Mn, 11.50% Cr, 0.60% Mo, 0.30% V, 0.50% W
1.65% C, 0.33% Si, 0.30% Mn, 11.50% Cr, 0.60% Mo, 0.30% V, 0.50% W
1.65% C, 0.33% Si, 0.30% Mn, 11.50% Cr, 0.60% Mo, 0.30% V, 0.50% W
1.65% C, 0.33% Si, 0.30% Mn, 11.50% Cr, 0.60% Mo, 0.30% V, 0.50% W
1.65% C, 0.33% Si, 0.30% Mn, 11.50% Cr, 0.60% Mo, 0.30% V, 0.50% W
1.65% C, 0.33% Si, 0.30% Mn, 11.50% Cr, 0.60% Mo, 0.30% V, 0.50% W
1.65% C, 0.33% Si, 0.30% Mn, 11.50% Cr, 0.60% Mo, 0.30% V, 0.50% W
1.65% C, 0.33% Si, 0.30% Mn, 11.50% Cr, 0.60% Mo, 0.30% V, 0.50% W
1.65% C, 0.33% Si, 0.30% Mn, 11.50% Cr, 0.60% Mo, 0.30% V, 0.50% W
1.66% C, 0.30% Si, 0.35% Mn, 12.00% Cr, 0.60% Mo, 0.90% V, 0.12% Al
1.90% C, 0.58% Mn, 0.65% Si, 0.025% P, 0.010% S, 1.08% Cr, 0.52% Ni, 0.23% Mo, 0.004% V, 0.15% Cu, 0.06% Al
1.93% C, 0.29% Mn, 0.45% Mn, 0.014% P, 0.017% S, 20.9% Cr, 0.22% Ni, 0.07% Mo, 0.57% V, 1.35% W, 0.03% Cu
11Cr-0.4Mo-2W-Cu-V-Nb
18% Cr, 10% Ni, 0.1% B
18% Cr, 10% Ni, 0.1% B
18% Cr, 10% Ni, 0.1% B
18% Cr, 10% Ni
18% Cr, 2.6% C, 1.27% Mo, 0.3% V
18Cr-12Ni
2.00 % C, 12.0 % Cr, 0.4 % Mn
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr, 0.50% Ni
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.25% Si, 0.30% Mn, 11.50% Cr
2.06% C, 0.19% Si, 0.25% Mn, 0.023% P, 0.001% S, 11.4% Cr, 0.12% Ni, 0.05% V, 0.06% Mo, 0.05% Cu
2.10 %C, 1.0 %Si, 0.4 %Mn, 6.8 %Cr, 1.5 %Mo, 5.4 %V
2.10% C, 0.3% Mn, 0.3% Si, 12.5% Cr, 0.5% Ni. Steel H13"> 0.37% C, 1.03% Si, 0.33% Mn, 0.014% P, 0.004% S, 5.23% Cr, 0.12% 2.10% C, 0.3% Mn, 0.3% Si, 12.5% Cr, 0.5% Ni
2.10% C, 0.8% Si, 7% Cr, 5.8% V, 1.5% Mo
2.10% C, 0.8% Si, 7% Cr, 5.8% V, 1.5% Mo
2.10% C, 0.8% Si, 7% Cr, 5.8% V, 1.5% Mo
2.10% C, 0.8% Si, 7% Cr, 5.8% V, 1.5% Mo
2.10% C, 1.0% Si, 0.4% Mn, 6.8% Cr, 1.5% Mo, 5.4% V
2.10% C, 1.0% Si, 0.4% Mn, 6.8% Cr, 1.5% Mo, 5.4% V
2.10% C, 1.0% Si, 0.4% Mn, 6.8% Cr, 1.5% Mo, 5.4% V
2.10% C, 1.0% Si, 0.4% Mn, 6.8% Cr, 1.5% Mo, 5.4% V
2.11 %C, 10.5 %Cr, 0.77 %W, 0.4 %Si, 0.4 Mn, 0.3 Mo
2.12% C, 0.25% Si, 0.40% Mn, 12.00% Cr
2.12% C, 0.25% Si, 0.40% Mn, 12.00% Cr
2.12% C, 0.25% Si, 0.40% Mn, 12.00% Cr
2.12% C, 0.25% Si, 0.40% Mn, 12.00% Cr
2.12% C, 0.25% Si, 0.40% Mn, 12.00% Cr
2.12% C, 0.25% Si, 0.40% Mn, 12.00% Cr
2.12% C, 0.25% Si, 0.40% Mn, 12.00% Cr
2.12% C, 0.25% Si, 0.40% Mn, 12.00% Cr
2.12% C, 0.25% Si, 0.40% Mn, 12.00% Cr
2.12% C, 0.25% Si, 0.40% Mn, 12.00% Cr
2.12% C, 0.25% Si, 0.40% Mn, 12.00% Cr
2.12% C, 0.25% Si, 0.40% Mn, 12.00% Cr
2.12% C, 0.25% Si, 0.40% Mn, 12.00% Cr
2.12% C, 0.25% Si, 0.40% Mn, 12.00% Cr
2.12% C, 0.25% Si, 0.40% Mn, 12.00% Cr
2.12% C, 0.25% Si, 0.40% Mn, 12.00% Cr
2.12% C, 0.25% Si, 0.40% Mn, 12.00% Cr
2.12% C, 0.25% Si, 0.40% Mn, 12.00% Cr
2.12% C, 0.25% Si, 0.40% Mn, 12.00% Cr
2.12% C, 0.25% Si, 0.40% Mn, 12.00% Cr
2.12% C, 0.25% Si, 0.40% Mn, 12.00% Cr
2.12% C, 0.25% Si, 0.40% Mn, 12.00% Cr
2.12% C, 0.25% Si, 0.40% Mn, 12.00% Cr
2.12% C, 0.25% Si, 0.40% Mn, 12.00% Cr
2.12% C, 0.25% Si, 0.45% Mn, 12.00% Cr, 0.70% W
2.15% C, max. 0.03% S, 4.75% Cr, 6.00% V, 13.00% W, 10.00% Co
2.25% Cr, 1.50% Mo. 3.00% Cr, 1.50% Mo
2.25Cr1.5Mo
2.25Cr1Mo
2.25Cr-1.6W-V-Nb
2.26% C, 29.98% Cr, 0.52% Si, 0.30% Mn, 0.013% S, 0.025% P, 0.30% Ni, 0.02% Cu, 0.08% Mo, 0.009% Al
2.26% C, 29.98% Cr, 0.52% Si, 0.30% Mn, 0.013% S, 0.025% P, 0.30% Ni, 0.02% Cu, 0.08% Mo, 0.009% Al
2.26% C, 29.98% Cr, 0.52% Si, 0.30% Mn, 0.013% S, 0.025% P, 0.30% Ni, 0.02% Cu, 0.08% Mo, 0.009% Al
2.29% C, 0.50% Si, 0.32% Mn, 0.026% P, 0.019% S, 12.3% Cr, 4.06% V, 1.06% Mo
2.30% C, 1.00% Si, 1.00% Mn, 18.00% Cr, 1.00% Mo. 2.60-2.80% C, 1.00% Si, 1.00% Mn, 26.00% Cr, 1.00% Mo
2.37% C, 12.06% Cr, 1.2% Mo, 4.00% V
2.40% C, 0.35% Si, 0.73% Mn, 0.028% P, 0.034% S, 17.5% C, 1.0% Mo, 1.0% Ni
2.40%C-30%Cr, 2.9% C-27%Cr
2.47% C, 4.15% Cr, 3.62% Mo, 0.41% Si, 8.94% V, 1.13% W, 2.02% Co
2.5% C, 0.4% Mn, 2.1% Si, 5.9% Cr, 0.8% Mo, 1% V (-)
2.50% C, 3.30% Si, 6.20% Cr, 1.42% Ni, 2.20% Mo, 2.60% V, 2.60% Nb, 0.98% W, 0.03% N, 0.04% O, 0.03% P, 0.02% S
2.56% C, 16.80% Cr, 1.77% Ni, 1.93% Mo, 0.008% S, 0.005% S
2.58% C, 16.90% Cr, 1.98% Mo, 1.80% Ni, 1.98% V, 0.007% S, 0.006% P
2.91% C, 0.983% Si, 2.14% Mn, 0.021% P, 0.016% S, 2.9% Cr, 5.11% Ni, 0.95% Mo, 85.1% Fe
2.98% C, 2.46% Si, 0.29% Mn, 1.53% Mo
23Cr-43Ni-7W-0.2Nb-0.1Ti-0.003B
25% Cr, 15% Ni
25% Cr, 18% Ni, 0.09% C
25% Cr
25% Cr
25.0% Cr, 12.0% Ni
25.0% Cr, 12.0% Ni
25.0% Cr, 12.0% Ni
25.0% Cr, 12.0% Ni
25Cr-24Ni-0.27Ti-0.034C
3.00% C, 3.00% Si, 1.00% Mn, 2.00% Cr, 22.00% Ni
3.20% C, 0.52% M, 2.24% Si, 0.53% Cr, 3.49% Ni, 0.56% Mo, 0.2% Cu
3.29% Cr, 4.09% Mo, 6.19% W, 1.87% V, 0.22% Si, 0.18% Mn, 0.034% Ni, 0.034% N, 1.03% C
3.31% C, 0.94% Si, 17.37% Mn, 3.34% Al
3.35% C, 0.63% Si, 0.60% Mn, 0.05% S, 0.05% P, 15.1% Cr, 2.9% Mo
3.54% C, 0.75% Mn, 0.583% Si, 15.15% Cr, 0.10% Mo
3.60% C, 2.50% Si, 0.20% Mn, 2.00% Mo, 0.50% Ni
3.65% C, 2.13% Si, 0.82% Cu, 0.35% Ni, 0.27% Mo, and 0.34% Mn
3.66% C, 2.52% Si, 0.16% Mn, 0.04% P, 0.01% S, 0.03% Cr, 0.51% Cu, 0.04% Mg
3.90% C, 1.09% Mn, 31.60% Cr
4.0% Cr
4.25% C
4.25% C
4.46% C-33.6% Cr-1.19% Mn-0.78% Si-0.022% S-0.028% P
4.50% C, 0.046% Si
77% Ni, 19% Cr, 0.02% C
9Cr-3W-3Co-0.2V-0.05Nb, 0.078% C, 0.05% N
Fe + <0.20% C, <0.020% N, 0.10-0.020% V, 0.15/0.80 % Ni
Fe + 0.015% C, Fe + 0.9% C
Fe + 0.12% C, 0.05% Nb, Fe + 0.18% C, 0.06% V, Fe + 0.20% C, 0.025% Nb, Fe + 0.40% C, 0.13% V, Fe + 0.06% C, 0.12% Ti
Fe - <0.08%C - 17% Cr - 12% Ni - 2.5% Mo
Fe - 1.05% C - 0.25% Mn -0.2% Si
Fe - 3.1% C - 0.8% Mn - 1% Si - 18.6% Cr - 2% Mo
Fe -<0.03% C -22.25% Cr -5.5% Ni -3% Mo -0.2% N
Fe -25Cr-33Ni-1Mn-1Mo-0.05C-0.7Nb-0.2N, AL20-25+Nb -Fe -20.5Cr-25Ni-1Mn-1.5Mo-0.07C-0.26Nb-0.15N
Fe -25Cr-33Ni-1Mn-1Mo-0.05C-0.7Nb-0.2N. AL20-25+Nb">Fe -20.5Cr-25Ni-1Mn-1.5Mo-0.07C-0.26Nb-0.15N
Fe - 0.10C-<0005Si- 1.99Mn-1.60Mo- 0.03Al - 0.0049N (wt-%)
Fe - 0.2% C - 0.75% Mn - 0.55% Ni - 0.5% Cr -0.2% Mo
Fe - 0.2% C - 0.8% Mn - 0.55% Ni - 0.5% Cr - 0.2% Mo
Fe - 0.2% C - 0.8% Mn - 0.55% Ni - 0.5% Cr - 0.2% Mo
Fe - 0.6% C - 0.85% Mn - 0.25% Si - 0.8% Cr
Fe - 0.94% C - 0.51% Mn - 0.32% Si - 1.34% Cr
Fe - 1% C
Fe - 1% C
Fe - 1.0% C binary alloy
Fe - 1.1% C - 8.25% Co - 9.5% Mo - 1.5% W - 3.75% Cr - 1.15% V
Fe - 1.1% C -0.2% Mn - 0.2% Si
Fe - 1.31% C - 0.35% Mn - 0.25% Si
Fe - 1.4% C binary alloy
Fe - 1.45% C - 0.85% Mn - 1.0% Si - 0.25% Mo
Fe - 1.5% C - 12% Cr - 0.9% V - 0.8% Mo
Fe - 2.1% C - 0.25% Mn - 0.25% Si - 0.5% Ni - 12.5% Cr
Fe - 2.1% C - 12.5% Cr - 0.5% Ni
Fe - 2.2% C - 0.9% Mn - 0.5% Si - 12.7% Cr - 0.4% Mo- 0.1% V
Fe - 2.95% C - 0.61% Mn - 29.3% Cr
Fe - 3.11% C - 1.05% Si - 0.41% Mn - 0.12% S -0.052% P
Fe - 3.4% C - 0.9% Mn - 0.9% Si -1.7% Cr - 4.5% Ni - 0.4% Mo
Fe - 4.0% C - 0.3% Si - 0.16% Mn - 0.91% Cr
Fe -0.11% C -0.85% Mn-0.21% S
Fe -0.16% C -1.26% Mn-0.22% Si-0.15% Cr
Fe -0.2% C -0.8% Mn -0.55% Ni -0.5% Cr -0.2% Mo
Fe -0.94% C -0.51% Mn-0.32% Si-1.34% Cr
Fe -1% C - 1.5% Cr
Fe -1.1% C -8.25% Co -9.5% Mo -1.5% W -3.75% Cr -1.15% V
Fe -1.2% C binary alloy
Fe -1.31% C -0.35% Mn-0.25% Si
Fe -1.31% C -0.35% Mn-0.25% Si
Fe -1.31% C -0.35% Mn-0.25% Si
Fe -1.31% C
Fe -2.2% C -0.9% Mn -0.5% Si -12.7% Cr -0.4% Mo -0.1% V
Fe -2.98% C -0.64% Mn -0.85% Si -4.4% Ni -2.34% Cr
Fe -3.1% C -0.8%Mn-1%Si-18.6% Cr -2% Mo
Fe -3.11% C -1.05% Si -0.41% Mn
Fe -3.3% C -0.9% Mn-0.9% Si-1.8% Cr -4.4% Ni -0.4% Mo
Fe -3.3% C -0.9%Mn-0.9%Si-1.8% Cr -4.4% Ni -0.4% Mo
Fe -3.4% C -0.9% Mn-0.9% Si-1.7% Cr -4.5% Ni -0.4% Mo
Fe -3.4% C -0.9%Mn-0.9%Si-1.7% Cr -4.5% Ni -0.4% Mo
Fe -4% C -0.3% Si -0.11% Mn -0.96% C
Fe-0.049C-0.3Mn-0.126V, Fe-0.38C-1.5Mn-0.5Si-O.1V, Fe-0.052C-0.18Mn-0.12Ti
Fe-0.07C-1.35Mn-0.047Ti-0.086Nb
Fe-0.35C-0.9Mo
Fe-0.43C-5.2Cr-1.5Mo-0.9V-1.0Si
Fe-0.4C-25Cr-20Ni
Fe-0.52C-3.8Cr-0.5Mo-lV-18.8W
Fe-0.5C-0.7Mn
Fe-0.7C-14.5Cr-0.9Mo
Fe-0.86C-23.8Cr-1.9Si-2.1 Ni
Fe-0.9C-11.3Cr-0.7Mn-2.95Mo-0.3Si, Fe-1.33C-6.8Cr-2.4Mo-0.2Si
Fe-1% C
Fe-1% C
Fe-1.3%C-4%Cr-5%Mo-3%V-6%W-8%Co
Fe-1.31% C-0.35% Mn-0.25% Si
Fe-1.31%C-0.35%Mn-0.25%Si
Fe-1.34 C-13.1 Mn
Fe-1.7C-1.2Si-1.1Mn-0.8Ni-3.6Cr-1.7Mo-4.7V
Fe-10% TiC
Fe-10% TiC
Fe-10% TiC
Fe-12Cr-0.2C
Fe-13Mn-0.8C
Fe-14Cr-20Ni-2.5Al-0.9Nb base. NF709">Fe-20Cr-25Ni base
Fe-17.37Mn-3.31C- Fe-19Cr-10Ni-0.07C-1.0Nb-0.7Mn-1Si. CF8C-Plus">Fe-19Cr-12Ni-0.07C-0.07Nb-0.4Si-+Mn+N(new heats + 3Cu-1W)
Fe-19Cr-10Ni-0.07C-1.0Nb-0.7Mn-1Si. Steel CF8C-Plus">Fe-19Cr-12Ni-0.07C-0.07Nb-0.4Si-+Mn+N(new heats + 3Cu-1W)
Fe-1C-4.4Cr-l.6V
Fe-2.1C-l4.7Cr-lNb
Fe-2.2%C-0.9%Mn-0.5%Si-12.7%Cr-0.4%Mo-0.1%V
Fe-2.2C-20.5Mo
Fe-2.4C-0.9Si-0.9Mn-0.1 Ni-2.9Cr-3.4Mo-5-9V
Fe-2.4C-5.4Cr-6V
Fe-23.3Mo-1.1C
Fe-26Al-5Cr-1.5Mo-1.0C (at%)
Fe-26Cr-1Ni-0.3C
Fe-29Mn-9Al-2.6C
Fe-2C-12Cr
Fe-3.3C-9.2V-2Si
Fe-3.3C-l6Cr-3Mo-lMn-0.5Si
Fe-30W-4.3C
Fe-4.46C-33.6Cr-1.19Mn-0.78Si-0.022S-0.028P
Fe-5%Cr-5%Mo-5%W-5%V-5%Co-2.0%C
Fe-5%Cr-5%Mo-5%W-5%V-5%Co-2.0%C
Fe-Ni36-B0.008
Fe-0.19C-1.35Mn-0.82Ni-0.51Mo-0.17Cr-0.009Al-0.008Si
Fe-0.25V-0.05C
Fe-0.29C-1.41Si-1.42Mn
Fe-0.75V-0.15C
Fe-0.8C
Fe-0.8C
Fe-0.8C
Fe-1% C-1.5% Cr
Fe-12Cr-0.2C
Fe-1V-0.2C
Fe-2.0C-5.0V-3.0Mo-1.5W-6.5Cr-0.75Si-0.35Mn-1.0Ni-0.003P-0.002S
Fe-2.0C-5.0V-3.0Mo-1.5W-6.5Cr-0.75Si-0.35Mn-1.0Ni-0.003P-0.002S
Fe-4Mo-0.1Nb-0.2C
Fe-4Mo-0.2C
Fe-4Mo-0.2C
Fe-6W-0.23C