45CrVMoW58 Steel

Steel name: 45CrVMoW58
Diagram No.: 1490
DIN designation: 45CrVMoW58
Chemical composition in weight %: 0.39%C, 1.5% Cr, 0.5%Mo, 0.7% V, 0.55% W
Steel group: Alloy steels
Applications: No data
Comment: Jominy hardenability curves of grade DIN 45CrVMoW58 steel after quenching (solid curve) and after quenching and tempering (dashed curves) for a specimen modified by adding a cap.
Reference: Not shown in this demo version.

Heat Treatment
Austenitizing: 1100oC

Hardenability Diagram


Click the image to enlarge the diagram.

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.