Big slag inclusion in 42CrMo4 steel


Figure 1: Slag inclusion in steel, scale bar: 2 mm.

Inclusion name: Slag inclusion
Record No.: 1487
Inclusion formula: No data
Inclusion type (Macro/Micro/Nano): Macro
Inclusion type (Exogenous/Indigenous): Exogenous
Inclusion classification: Oxide
Inclusion composition in weight %: No data
Sample: 42CrMo4 steel
Steel composition in weight %: 0.41% C, 0.20% Si, 0.75% Mn, 1.05% Cr, 0.23% Mo.
Note: Structural steel