Plain dents - Pipeline defects
Figure 1: Plain dents.
Defect name: Plain dents
Record No.: 2765
Type of defect (Internal/Surface): Surface
Defect classification: Other defects
Steel name: Steel
Steel composition in weight %: No data.
Note: Occur due to: Installation/Construction. Ground movement/settling–Buckling. Some rock impingement.
Plain dents are normally not harmful provided they are not extremely large.
Reference: Not shown in this demonstration version.