Alphabetical Index
Chemical Composition
Keyword Search
AFNOR Steels
AISI/SAE Steels
BS Steels
DIN Steels
Wr.Nr. (Mat.No.) Steels
Calculated Diagrams
CCT Diagrams
TTA Diagrams
TTE Diagrams
TTT Diagrams
TTP Diagrams
TTS Diagrams
Alloy Steels
Carbon Steels
Carburizing Steels
Cast Irons
Chromium Steels
Cold Work Tool Steels
High Speed Steels
Hot Work Tool Steels
Low Carbon Steels
Microalloyed Steels
Molybdenum Steels
New Diagrams
Nitriding Steels
Plastic Mould Steels
PM Steels
Stainless Steels
Steel Companies
Structural Steels
Tools Steels
Vanadium Steels
Welding Steels
White Cast Irons
Help
Home
1.1191 Steel
Steel name: 1.1191
Steel name of producers:
C45E DIN EN 10083-2:2006-10 Germany
C45E DIN EN 10132-3:2000-05 Germany
C45E DIN EN 10250-2:1999-12 Germany
C45E DIN EN 10269:2006-07 Germany
C45E DIN EN 10277-5:2008-06 Germany
C45E DIN EN 10297-1:2003-06 Germany
C45E DIN EN 10305-1:2003-02 Germany
C45E Stahl Eisen List: 2004 Germany
C45E SEW 550:1976-08 Germany
W3-161 BOFORS Sweden
Ck45,GS-Ck45 Buderus Germany
C45E Dillinger Hüttenwerke Germany
Ck45,GS-Ck45 Dirostahl Germany
Ck45 HKM Krupp Mannesmann Germany
Ck45 Hover&Sohn Germany
Ck45 Platestahl Germany
Ck45 Saarstahl Germany
Ck45 Thyssen Edelstahl Service GmbH Germany
TEWCk45 Thyssen Edelstahl Service GmbH Germany
Ck45 Zapp Germany
C45E DIN EN 10083-1:1996-10 Germany
Ck 45 DIN EN 10083-1:1996-10 Germany
C45E DIN EN 10269:1999-11 Germany
C45E DIN EN 10277-5:1999-10 Germany
C45E DIN 1652-4:1990-11 Germany
Ck 45 DIN 1652-4:1990-11 Germany
C45E DIN 17204:1990-11 Germany
Ck 45 DIN 17204:1990-11 Germany
Ck 45 SEL Germany
C45E AFNOR EN 10083-1:1997-02 France
XC48H1 AFNOR EN 10083-1:1997-02 France
C45E AFNOR EN 10269:1999-11 France
C45E BS EN 10083-1:1991 Great Britain
C45E UNE EN 10083-1:1997 Spain
C45E UNI EN 10083-1:1998 Italy
Ck45 DDR-TGL Germany
B10 BOFORS Sweden
W3-1672 BOFORS Sweden
V945 Bohler Uddeholm Austria
UB65 Deutsche Edelstahlwerke (Witten-Krefeld) Germany
Ck45 Hoverstahl Germany
Ck45 Krupp Germany
V945 Bohler Uddeholm Germany
Diagram No.: 4123
Type of diagram: CCT
Mat. No. (Wr. Nr.) designation: 1.1191
Chemical composition in weight %: 0.42-0.50% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.030% P, max. 0.035% S
Steel group: Structural steels
Note: Austenitizing temperature: 850oC, time: 3 min.
Reference: Not shown in this demo version.
Transformation Diagram
Price: 20.00 US $
Buy Online Transformation Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagram Calculating Service
CCT and TTT Diagrams Home
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.