0.20C-0.78Mn-0.60Cr-0.16Mo-0.52Ni Steel

Steel name: 0.20C-0.78Mn-0.60Cr-0.16Mo-0.52Ni
Diagram No.: 8332
Type of diagram: CCT
Chemical composition in weight %: 0.20% C, 0.78% Mn, 0.60% Cr, 0.16% Mo, 0.52% Ni
Steel group: Structural steels
Note: Austenitizing temperature: 900 C. Cooling curves and CCT diagrams for a steel containing 0.20% C, 0.78% Mn, 0.60% Cr, 0.52% Ni, and 0.16% Mo after austenitizing at 900 C. (A) Conventional CCT diagram and (B) various air cooling rates to approximately Ac1 followed by water quenching.
Reference: Not shown in this demo version.
Loria, E.A. Transformation behaviour on air cooling steel in A3–A1 temperature range. Met. Technol. 1977, 4(1), 490–492.

Transformation Diagram


Click the image to enlarge the diagram.

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.