Alphabetical Index
Chemical Composition
Keyword Search
AFNOR Steels
AISI/SAE Steels
BS Steels
DIN Steels
Wr.Nr. (Mat.No.) Steels
Calculated Diagrams
CCT Diagrams
TTA Diagrams
TTE Diagrams
TTT Diagrams
TTP Diagrams
TTS Diagrams
Alloy Steels
Carbon Steels
Carburizing Steels
Cast Irons
Chromium Steels
Cold Work Tool Steels
High Speed Steels
Hot Work Tool Steels
Low Carbon Steels
Microalloyed Steels
Molybdenum Steels
New Diagrams
Nitriding Steels
Plastic Mould Steels
PM Steels
Stainless Steels
Steel Companies
Structural Steels
Tools Steels
Vanadium Steels
Welding Steels
White Cast Irons
Help
Home
Cast Irons
0.322C-2.52Si-0.43Mn-0.020Sn-0.045Mg Cast Iron
0.44Mn, 0.87Mn, 2.02Mn Cast Irons
0.50Mn Cast Iron
0.5Cr Cast Iron
0.5Cr and 1Cr Cast Irons
0.5Mo Cast Iron
0.7Si, 1.6Si, 2.6Si, 3.5Si, 4.5Si Cast Irons
0Mo Cast Iron
1.00Cr Cast Iron
1.00Mn Cast Iron
1.00Ni, 1.96Ni Cast Irons
1.0Mo Cast Iron
1.44Si Melleable Iron
1.50Mn Cast Iron
1.5Mo Cast Iron
1.6Si Cast Iron
1.7C, 2.28C, 2.54C, 3.34C Cast Irons
1.95C-10.80Cr-3.80Mo Alloyed White Cast Iron
1.95C-10.80Cr-3.80Mo Alloyed White Cast Iron
1.96C-15.40Cr-2.20Mo Alloyed White Cast Iron
1.96C-15.40Cr-2.20Mo Alloyed White Cast Iron
1.98C-20.25Cr-2.14Mo Alloyed White Cast Iron
1.98C-20.25Cr-2.14Mo Alloyed White Cast Iron
11.20Cr Cast Iron
15-2-1 LC White Cast Iron
2.00Cr Cast Iron
2.04C-20.55Cr-0.61Mo Alloyed White Cast Iron
2.04C-20.55Cr-0.61Mo Alloyed White Cast Iron
2.05C-15.60Cr-0.81Mo Alloyed White Cast Iron
2.05C-15.60Cr-0.81Mo Alloyed White Cast Iron
2.08C-15.85Cr Alloyed White Cast Iron
2.08C-15.85Cr Alloyed White Cast Iron
2.08C-20.55Cr-0.01Mo Alloyed White Cast Iron
2.08C-20.55Cr-0.01Mo Alloyed White Cast Iron
2.13C-11.30Cr-1.41Mo Alloyed White Cast Iron
2.13C-11.3Cr-1.41Mo Alloyed White Cast Iron
2.19C-11.65Cr-0.02Mo Alloyed White Cast Iron
2.19C-11.65Cr-0.02Mo Alloyed White Cast Iron
2.25Cr-1Mo Steel
2.25Cr-1Mo Steel
2.41C-12.15Cr-2.45Mo Alloyed White Cast Iron
2.41C-12.15Cr-2.45Mo Alloyed White Cast Iron
2.45C-19.82Cr-2.94Mo Alloyed White Cast Iron
2.45C-19.82Cr-2.94Mo Alloyed White Cast Iron
2.50C-2.50Si-0.85Mn Cast Iron
2.50C-2.50Si-0.85Mn Cast Iron
2.50C-2.50Si-0.85Mn-0.10P-0.10Mo-1.00Ni Cast Iron
2.50C-2.50Si-0.85Mn-0.10P-0.30Mo-1.00Ni Cast Iron
2.50C-2.50Si-0.85Mn-0.10P-0.50Mo-1.00Ni Cast Iron
2.50C-2.50Si-0.85Mn-0.10P-0.50Mo-2.00Ni Cast Iron
2.50C-2.50Si-0.85Mn-0.10P-0.50Mo-3.00Ni Cast Iron
2.50C-2.50Si-0.85Mn-0.10P-0.50Mo-4.00Ni Cast Iron
2.50C-2.50Si-0.85Mn-0.10P-0.50Mo-5.00Ni Cast Iron
2.50C-2.50Si-0.85Mn-0.10P-1.00Mo-1.00Ni Cast Iron
2.50C-2.50Si-0.85Mn-0.10P-1.00Mo-2.00Ni Cast Iron
2.50C-2.50Si-0.85Mn-0.10P-1.00Mo-3.00Ni Cast Iron
2.50C-2.50Si-0.85Mn-0.10P-1.00Mo-4.00Ni Cast Iron
2.50C-2.50Si-0.85Mn-0.10P-1.00Mo-5.00Ni Cast Iron
2.54C-20.22Cr-1.52Mo Alloyed White Cast Iron
2.54C-20.22Cr-1.52Mo Alloyed White Cast Iron
2.55C-12.40Cr-1.25Mo Alloyed White Cast Iron
2.55C-12.40Cr-1.25Mo Alloyed White Cast Iron
2.5C, 3.0C, 3.5C Cast Irons
2.5Si Cast Iron
2.5TC-1Ni-0.1Mo Steel
2.5TC-1Ni-0.5Mo Steel
2.5TC-1Ni-1Mo Steel
2.5TC-2Ni-0.5Mo Steel
2.5TC-2Ni-1Mo Steel
2.5TC-3Ni-0.5Mo Steel
2.5TC-3Ni-1.0Mo Steel
2.5TC-4Ni-0.5Mo Steel
2.5TC-4Ni-1Mo Steel
2.5TC-5Ni-0.5Mo Steel
2.5TC-5Ni-1Mo Steel
2.60C-0.4Mn-1.4Si-B Malleable Iron
2.60C-0.4Mn-1.4Si-B Malleable Iron
2.60C-0.4Mn-1.4Si-B Malleable Iron
2.60C-15.20Cr-1.95Mo Alloyed White Cast Iron
2.60C-15.20Cr-1.95Mo Alloyed White Cast Iron
2.65C-12.65Cr-0.02Mo Alloyed White Cast Iron
2.65C-12.65Cr-0.02Mo Alloyed White Cast Iron
2.67C-14.95Cr Alloyed White Cast Iron
2.67C-14.95Cr Alloyed White Cast Iron
2.67C-15.20Cr-1.09Mo Alloyed White Cast Iron
2.67C-15.20Cr-1.09Mo Alloyed White Cast Iron
2.67C-20.75Cr-0.01Mo Alloyed White Cast Iron
2.67C-20.75Cr-0.01Mo Alloyed White Cast Iron
2.6C, 3.0C, 2.6C Cast Irons
2.6C, 3.0C, 2.6C Cast Irons
2.6C, 3.0C, 3.6 Cast Irons
2.72C-25.15Cr-2.52Mo Alloyed White Cast Iron
2.72C-25.15Cr-2.52Mo Alloyed White Cast Iron
2.73C-0.03Mn-1.25Si-0.015S White Iron
2.75C-0.13Mn-1.21Si-0.008S White Iron
2.84V, 3.70V, 6.78V, 8.73V Cast Irons
2.87C-25.50Cr-1.22Mo Alloyed White Cast Iron
2.87C-25.50Cr-1.22Mo Alloyed White Cast Iron
2.90C-0.60Si-0.70Mn-19.40Cr-2.10Mo-1.00Cu Cast Iron
2.92C-17.59Cr-1.05Nb, 2.96C-17.68Cr-2.71Nb Cast Irons
2.93C-0.60Si-0.78Mn-17.4Cr-0.04Mo White Cast Iron
2.93C-1.89Si-0.74Mn-0.218P-0.513Mo Iron
2.95C-25.82Cr-0.02Mo Alloyed White Cast Iron
2.95C-25.82Cr-0.02Mo Alloyed White Cast Iron
2.96C-0.52Si-0.79Mn-17.5Cr-0.98Cu-1.55Mo White Cast Iron
2.96C-0.93Si-0.79Mn-17.5Cr-0.98Cu-1.55Mo White Cast Iron
2.97C-2.00Si Grey Cast Iron
2.97C-2.00Si Grey Cast Iron
2.97C-2.02Si-0.82Mn-0.30P Cast Iron
2.9C-0.6Si-17.0Cr-Mn-Mo White Cast Iron
2.9C-0.6Si-17.0Cr-Mn-Mo White Cast Iron
2.9C-0.6Si-17.0Cr-Mn-Mo White Cast Iron
2.9C-0.7Mn-0.6Si-17.5Cr White Cast Iron (Mo Addition)
2.9C-0.7Mn-0.6Si-17.5Cr White Cast Iron (Mo Addition)
2.9C-0.7Mn-0.6Si-17.5Cr White Cast Iron (Mo Addition)
2.9C-0.8Mn-0.6Si-17.0Cr-1.5Mo White Cast Iron
2.9C-0.8Mn-0.6Si-17.0Cr-1.5Mo-Si-Cu White Cast Iron
2.9C-0.8Mn-0.6Si-17.0Cr-1.5Mo-Si-Cu White Cast Iron
2.9C-0.8Mn-0.6Si-17.5Cr-Ni-Mo White Cast Iron
2.9C-0.8Mn-0.6Si-17.5Cr-Ni-Mo White Cast Iron
2.9C-0.8Mn-0.6Si-17.5Cr-Ni-Mo White Cast Iron
2.9C-0.8Mn-0.6Si-17.5Cr-Ni-Mo-Cu White Cast Iron
2.9C-0.8Mn-0.6Si-17.5Cr-Ni-Mo-Cu White Cast Iron
2.9C-0.8Mn-0.6Si-17.5Cr-Ni-Mo-Cu White Cast Iron
2.9TC-0.5Mo Steel
20-2-1 LC White Cast Iron
22.59% Cr Cast Iron
2C-5Cr-5Mo-5W-5V-5Co Steel
2Mo Cast Iron
2Si, 3Si Cast Irons
2Si, 3Si Cast Irons
3.00C-1.85Si-0.73Mn-0.216P-0.249Mo Cast Iron
3.00Mn Cast Iron
3.04C-1.83Si-0.72Mn-0.212P-0.149Mo Cast Iron
3.06C-0.73Si, 3.11C-1.61Si, 3.04C-2.60Si, 3.09C-2.53Si, 3.09C-4.48Si Cast Irons
3.06C-1.79Si-0.57Mn-0.60Mo Cast Iron
3.12C-1.91Si-0.76Mn-0.21P-0.086Mo Cast Iron
3.14C-2.15Si-0.81Mn-0.219P Grey Cast Iron
3.14TC-2.15Si Steel
3.17C-2.0Si-0.75Mn-0.30Mo-0.60Cu Grey Cast Iron
3.1TC-0.09Mo Steel
3.25C-11.80Cr-2.60Mo Alloyed White Cast Iron
3.25C-11.80Cr-2.60Mo Alloyed White Cast Iron
3.29C-2.35Si-0.07Mn-1.90Mo-0.94Ni Cast Iron
3.2C-0.3Mn-2.36Si-4.82Ni-0.4Mo Alloyed Ductile Iron
3.30C-0.3Mn-2.6Si Ductile Iron
3.30C-0.3Mn-2.6Si Ductile Iron
3.30C-0.3Mn-2.6Si Ductile Iron
3.39C-11.95Cr-1.36Mo Alloyed White Cast Iron
3.39C-11.95Cr-1.36Mo Alloyed White Cast Iron
3.3C-0.3Mn-2.45Si-0.6Ni-0.5Mo Alloyed Ductile Iron
3.3C-0.3Mn-2.46Si-1.17Ni-0.4Mo Alloyed Ductile Iron
3.3C-0.3Mn-2.4Si-2.37Ni-0.5Mo Alloyed Ductile Iron
3.3C-0.3Mn-2.57Si-0.7Mo Alloyed Ductile Iron
3.3C-0.3Mn-2.58Si-0.4Mo Alloyed Ductile Iron
3.3C-0.3Mn-2.69Si-0.2Mo Ductile Cast Irons
3.3C-0.3Mn-2.6Si-0.2Mo Alloyed Ductile Iron
3.40C-19.85Cr-3.40Mo Alloyed White Cast Iron
3.40C-19.85Cr-3.40Mo Alloyed White Cast Iron
3.45C-16.01Cr, 3.56C-15.74Cr-0.92Mo, 3.70C-15.93Cr-2.96Mo Cast Irons
3.4C-0.3Mn-2.47Si-0.5Mo Alloyed Ductile Iron
3.4C-0.3Mn-2.4Si-0.5Mo Ductile Iron (Ni Addition)
3.4C-0.3Mn-2.4Si-0.5Mo Ductile Iron (Ni Addition)
3.4C-0.3Mn-2.4Si-0.5Mo Ductile Iron (Ni Addition)
3.4C-0.3Mn-2.6Si Nonalloyed Ductile Iron
3.50Cr Cast Iron
3.51C-12.20Cr-0.02Mo Alloyed White Cast Iron
3.51C-12.20Cr-0.02Mo Alloyed White Cast Iron
3.51C-20.10Cr-1.37Mo Alloyed White Cast Iron
3.51C-20.10Cr-1.37Mo Alloyed White Cast Iron
3.52C-24.65Cr-2.67Mo Alloyed White Cast Iron
3.52C-24.65Cr-2.67Mo Alloyed White Cast Iron
3.56C-14.60Cr-0.47Mo Alloyed White Cast Iron
3.56C-14.60Cr-0.47Mo Alloyed White Cast Iron
3.58C-14.45Cr Alloyed White Cast Iron
3.58C-14.45Cr Alloyed White Cast Iron
3.58C-14.65Cr-0.52Mo Alloyed White Cast Iron
3.58C-14.65Cr-0.52Mo Alloyed White Cast Iron
3.5C-0.2Mn-2.71Si Nonalloyed Ductile Iron
3.5C-0.3Mn-2.69Si-0.4Mo Ductile Cast Iron
3.5C-0.3Mn-3.45Si Nonalloyed Ductile Iron
3.61C-15.92Cr-0.89V, 3.60C-16.11Cr-2.89V Cast Irons
3.62C-20.35Cr-0.01Mo Alloyed White Cast Iron
3.62C-20.35Cr-0.01Mo Alloyed White Cast Iron
3.63C-1.75Si-0.53Mn-0.56P-0.10S Grey Cast Iron
3.66C-24.95Cr-1.53Mo Alloyed White Cast Iron
3.66C-24.95Cr-1.53Mo Alloyed White Cast Iron
3.68C-1.20Si-0.37Mn-0.28P-0.11S-2.03Ni Cast Iron
3.68C-9.70Cr, 3.45C-16.0Cr, 2.3C-25.5Cr Cast Irons
3.6C-0.2Mn-2.83Si Nonalloyed Ductile Iron
3.6C-0.3Mn-2.61Si Ductile Cast Iron
3.6C-0.3Mn-2.75Si Ductile Cast Iron
3.6C-0.3Mn-2.7Si Ductile Cast Iron
3.6C-0.3Mn-3.68Si Nonalloyed Ductile Iron
3.6TC-1.75Si Steel
3.70C-2.30Si-0.25Mn Steel
3.70C-25.32Cr-0.02Mo Alloyed White Cast Iron
3.70C-25.32Cr-0.02Mo Alloyed White Cast Iron
3.72C-2.32Si-0.31Mn-0.50Cr-3.85Ni-1.03Cu Cast Iron
3.75C-2.40Si-0.33Mn-0.51Cr-1.41Mo-1.03Cu Cast Iron
3.78C-2.26Si-0.24Mn-0.89Cr-0.78Ni-1.50Cu Cast Iron
3.7C-0.4Mn-2.74Si-0.4Mo Ductile Cast Iron
3.7C-0.4Mn-2.75Si Ductile Cast Iron
3.7TC-2Ni Steel
3.81C-14.75Cr-2.50Mo Alloyed White Cast Iron
3.81C-14.75Cr-2.50Mo Alloyed White Cast Iron
3.83C-2.36Si-0.06Mn-2.00Mo-1.62Ni Cast Iron
3.8C-0.4Mn-2.31Si-0.3Mo Ductile Cast Iron
3.8C-0.4Mn-2.32Si Ductile Cast Iron
3.94C-23.45Cr-2.94Mo Alloyed White Cast Iron
3.94C-23.45Cr-2.94Mo Alloyed White Cast Iron
3.96C-14.80Cr-1.45Mo Alloyed White Cast Iron
3.96C-14.80Cr-1.45Mo Alloyed White Cast Iron
3.96C-17.55Cr-2.53Mo Alloyed White Cast Iron
3.96C-17.55Cr-2.53Mo Alloyed White Cast Iron
3TC-0.15Mo Steel
3TC-0.25Mo Steel
3TC-2Si Steel
3TC-2Si Steel
3TC-2Si Steel
4.08C-18.00Cr-1.14Mo Alloyed White Cast Iron
4.08C-18.00Cr-1.14Mo Alloyed White Cast Iron
4.10C-15.10Cr Alloyed White Cast Iron
4.10C-15.10Cr Alloyed White Cast Iron
4.10C-23.67Cr-1.32Mo Alloyed White Cast Iron
4.10C-23.67Cr-1.32Mo Alloyed White Cast Iron
4.13C-18.22Cr-0.05Mo Alloyed White Cast Iron
4.13C-18.22Cr-0.05Mo Alloyed White Cast Iron
4.31C-24.80Cr-0.02Mo Alloyed White Cast Iron
4.31C-24.80Cr-0.02Mo Alloyed White Cast Iron
42CrMo4 Steel
590-MPa Steel
5Cr-0.5Mo Steel
5Cr-0.5Mo Steel
6.27Cr Cast Iron
ADI Cast Iron I
ADI Cast Iron II
Alloy-White-Cast-Iron
Carbidic Nodular Cast Iron I
Carbidic Nodular Cast Iron II
Carbidic Nodular Cast Iron III
Carbidic Nodular Cast Iron IV
Carbidic Nodular Cast Iron V
Ductile Gray Iron
Ductile iron
EN19B Steel
En 13 Steel
FCD 700 Cast Iron
FCD 700 Cast Iron
FCD 700 Cast Iron
FCD40, FD60 Cast Irons
Fe - 30.8Ni - 26.6Cr Alloy
Fe-30.8Ni-26.6Cr Alloy
Gray Cast Iron I
Gray Cast Iron II
HCCI Cast Iron
HCCI Cast Iron
HT60 Steel
High Chromium Cast Iron
High Cr White Cast Iron
Low Silicon Gray Iron
MV11K Steel
MV11K Steel
Mo-Cu Gray Cast Iron
Ni-Mo Ductile Iron
Ni-Mo Ductile Iron
Pearlitic Malleable Cast Iron
Pearlitic Malleable Iron I
Pearlitic Malleable Iron II
Pearlitic Malleable Iron III
Pearlitic Malleable Iron IV
Pearlitic Malleable Iron V
White Iron Class III (28% Cr)
White Iron Class IIc
White Iron Class IIe