Alphabetical Index
Chemical Composition
Keyword Search
AFNOR Steels
AISI/SAE Steels
BS Steels
DIN Steels
Wr.Nr. (Mat.No.) Steels
Calculated Diagrams
CCT Diagrams
TTA Diagrams
TTE Diagrams
TTT Diagrams
TTP Diagrams
TTS Diagrams
Alloy Steels
Carbon Steels
Carburizing Steels
Cast Irons
Chromium Steels
Cold Work Tool Steels
High Speed Steels
Hot Work Tool Steels
Low Carbon Steels
Microalloyed Steels
Molybdenum Steels
New Diagrams
Nitriding Steels
Plastic Mould Steels
PM Steels
Stainless Steels
Steel Companies
Structural Steels
Tools Steels
Vanadium Steels
Welding Steels
White Cast Irons
Help
Home
Structural Steels
0.04C-V-Mo Steel
0.04C-V-Mo Steel
0.04C-V-Mo Steel
0.04C-V-Mo Steel
0.04C-Vanadium Steel
0.05C-V-Ti Steel
0.05C-Vanadium Steel
0.06C Steel
0.06C Steel
0.06C-0.45V Steel
0.06C-0.45V Steel
0.06C-Mn-Cu-Ni-Mo-Nb-Ti Steel
0.06C-V Steel
0.06C-V Steel
0.06C-V-Mo Steel
0.06C-V-Mo Steel
0.06C-V-Mo Steel Steel
0.06C-V-Nb-Mo Steel
0.06C-V-Nb-Mo Steel
0.06C-V-Ti Steel
0.06C-Vanadium-Niobium Steel
0.06C-Vanadium-Niobium Steel
0.07C-0.45V Steel
0.07C-0.45V Steel
0.07C-V-Mo Steel
0.07C-V-Mo Steel
0.07C-V-N Steel
0.07C-V-Nb-Mo Steel
0.07C-Vanadium Steel
0.07C-Vanadium-Niobium Steel
0.08C-V Steel
0.08C-Vanadium-Niobium Steel
0.094C-0.30Si-1.32Mn Steel
0.09C-V Steel
0.09C-V Steel
0.09C-V Steel
0.09C-V Steel
0.09C-V-Nb-Mo Steel
0.09C-Vanadium Steel
0.10C-1.63Mn-0.41Mo Weld Metal Steel
0.10C-V Steel
0.10C-V Steel
0.10C-V-Nb-Ti Steel
0.10C-V-Ti Steel
0.10C-Vanadium-Niobium Steel
0.10C-Vanadium-Niobium Steel
0.11C-5.00Ni-0.55Cr-0.47Mo-0.075V Steel
0.11C-V Steel
0.11C-V Steel
0.11C-V Steel
0.11C-Vanadium Steel
0.11C-Vanadium Steel
0.11C-Vanadium Steel
0.11C-Vanadium-Niobium Steel
0.12C-V Steel
0.12C-V Steel
0.12C-V Steel
0.12C-V Steel
0.12C-V-Mo Steel
0.12C-V-Nb-Mo Steel
0.13C-0.16Mn-1.76Cr-0.49Mo-3.08Ni Steel
0.13C-V Steel
0.13C-V Steel
0.13C-V Steel
0.14C-0.26Mn-1.05Cr-0.26Mo-2.21Ni Steel
0.14C-0.3Cr-1.2Mn-0.5Si-0.002B Steel
0.14C-2.43Cr-1.07Mo Steel
0.14C-V Steel
0.14C-V Steel
0.14C-V Steel
0.14C-V-Nb-Mo Steel
0.14C-Vanadium Steel
0.14C-Vanadium Steel
0.15C-0.5Mn Steel
0.15C-V Steel
0.15C-V Steel
0.15C-V Steel
0.15C-V Steel
0.15C-V-Mo Steel
0.15C-V-Ni Steel
0.15C-Vanadium Steel
0.15C-Vanadium Steel
0.16C-0.34Si-1.50Mn-0.035Nb-0.004V-0.015Ti Steel
0.16C-0.34Si-1.50Mn-0.035Nb-0.015Ti-0.037Al Steel
0.16C-V Steel
0.16C-V Steel
0.16C-V-N Steel
0.16C-Vanadium Steel
0.16C-Vanadium Steel
0.16C-Vanadium Steel
0.17C-0.20Si-1.81Mn-0.15(Nb+V+Ti) Steel
0.17C-0.33Si-1.37Mn-0.66Cr-0.77Ni Steel
0.17C-0.33Si-1.37Mn-0.77Ni-0.66Cr Steel
0.17C-1.37Mn-0.66Cr Steel
0.17C-V Steel
0.17C-V Steel
0.17C-V-Mo Steel
0.17C-V-N Steel
0.17C-V-N Steel
0.18C Carbon Steel
0.18C-0.35Si-1.6Mn-0.01P-0.008S-0.006N Steel
0.18C-V-Nb-Mo Steel
0.19C-1.50Mn-1.20Cr-2.50Ni-0.35Mo Steel
0.19C-1.64Mn Steel
0.19C-2.146Si-2.96Mn-0.04Al Steel
0.19C-V-N Steel
0.19C-Vanadium Steel
0.20C-0.28Si-1.25Mn-25 ppm B Steel
0.20C-0.78Mn-0.60Cr-0.16Mo-0.52Ni Steel
0.20C-1.44Mn-0.49Ni-0.16V Steel
0.20C-Vanadium Steel
0.20C-Vanadium Steel
0.21C-V-N Steel
0.22C-0.79Mn-0.50Mo Steel
0.22C-0.79Mn-0.50Mo Steel
0.22C-V Steel
0.23C-0.0021B Steel
0.23C-0.82Mn-1.22Cr-0.53Mo-0.22V Steel
0.23C-V Steel
0.23C-V Steel
0.24C-0.69Mn-0.50Mo-3.35Ni-0.09V Steel
0.24C-1.67Mn-0.22Mo Steel
0.24C-1.67Mn-0.22Mo Steel
0.25C-0.88Mn-0.73Cr-0.88Mo-0.59Ni-0.23V Steel
0.25C-1.2Si-2.0Mn-0.2Cr (+Nb, B, Ti) Steel
0.25C-1.2Si-2.0Mn-0.2Cr-0.08Mo (+Nb, B, Ti) Steel
0.25C-1.5Mn-1.2Si-1.5Ni-0.05Nb Steel
0.25C-1.80Ni-1.50Si-0.40Mo Steel
0.26C-0.57Mn-0.48Mo-2.20Ni-0.09V Steel
0.26C-V Steel
0.26C-V Steel
0.27C-0.84Mn-0.73Cr-0.90Mo-0.60Ni-0.11V Steel
0.2C-1.2Mn-1Cu-0.6Ni Steel
0.2C-1Mn-1Cu-0.25Mo-0.8Ni Steel
0.2C-1Mn-1Cu-0.25Mo-0.8Ni Steel
0.30C-0.30Mn-3.64Ni-l.63Cr-0.49Mo Steel
0.30C-0.95Cr-0.20Mo Steel
0.30C-O.30Mn-3.64Ni-1.63Cr-O.49Mo Steel
0.30C-O.30Mn-3.64Ni-1.63Cr-O.49Mo Steel
0.33C-0.41Mn-1.96Mo Steel
0.33C-0.45Mn-1.97Cr Steel
0.33C-0.84Mn-1.05Cr-1.07Mo-0.26V Steel
0.35%C-0.23Si-0.65Mn-1.11Cr-0.05Mo-0.23Ni-0.11Cu Steel
0.35C-0.37Mn Hypoeutectoid Steel
0.35C-1.40Mn-0.19Mo Steel
0.35C-1.40Mn-0.19Mo Steel
0.35C-1.80Ni-0.80Cr-0.35Mo-0.20V Steel
0.36C-0.17Mn-0.82Mo Steel
0.37C-0.37Mn-0.57Cr Steel
0.38C-0.28Si-0.90Mn-1.01Cr-0.20Mo-0.12V Steel
0.38C-0.64Mn-0.23Si-0.99Cr Steel
0.38C-0.64Mn-0.23Si-0.99Cr Steel
0.38C-0.73Si-0.63Mn-0.99Cr-0.16Mo Steel
0.39C-0.45Mn-0.74Mo-3.53Ni Steel
0.3C-1Mn-4Cr-0.3V-1Mn Steel
0.3C-3Ni Steel
0.40C-0.42Mn-0.59Mo Steel
0.40C-0.57Mn-0.01Mo-3.49Ni Steel
0.40C-0.78Mn-1.25Cr-0.53Mo-0.22V Steel
0.40C-1.80Ni-0.80Cr-0.25Mo Steel
0.40C-5.00Cr-1.30Mo-0.50V Steel
0.41C-0.60Mn-0.21Mo-3.51Ni Steel
0.42C Steel
0.42C-0.20Mn-0.20Mo Steel
0.42C-0.20Mn-0.21Mo Steel
0.42C-0.8Cr-O.3Mo-1.5Ni Steel
0.42C-1.10Cr Steel
0.42C-1.10Cr Steel
0.42C-1.10Cr Steel
0.44 C Steel
0.44C Steel
0.45C-3.5Cr Steel
0.45C-5Ni Steel
0.46C-1.00Cr-1.00Mo-0.55Ni Steel
0.46C-1.85Ni-1.59Si-0.75Cr-0.43Mo Steel
0.50C-0.53Si-0.23Mn-0.05Cr Steel
0.51C-0.73Mn-0.99Cr-0.45Mo-2.74Ni Steel
0.51C-3.80Si-0.25Mn-0.32Cr Steel
0.53C-0.24Mn-0.32Cr-2.32Ni Steel
0.54C-0.46Mn Steel
0.54C-1.27Si-0.23Mn-0.05Cr Steel
0.55C-0.83Mn-1.01Cr-0.48Mo-1.15Ni Steel
0.55C-1.62Si-0.78Mn-0.77Cr Steel
0.56C-0.26Mn-1.97Ni
0.56C-0.47Mn-0.35Si-0.10Mo-0.10Ni Steel
0.59C-0.20Mn Steel
0.59C-0.25Mn-3.90Ni Steel
0.59C-0.30Mn Steel
0.5Cr0.5Mo Steel
0.61C-1Cr and 0.86C-0.5Mo Steels
0.63C-O.87Mn-O.22Si Steel
0.80C-0.27Si-0.61Mn Steel
0.90C-0.47Mn-0.20V Steel
0.95C-.48Mn-0.95Co Steel
0.97C-1.04Mn-0.32Mo Steel
0.97C-1.04Mn-0.32Mo Steel
004 Steel
005 Steel
006 Steel
007 Steel
032 Steel
034 Steel
038 Steel
041 Steel
045 Steel
081 Steel
082 Steel
085 Steel
091 Steel
092 Steel
09CuPCrNi Steel
09CuPCrNi Steel
09CuPCrNi Steel
09CuPCrNi Steel
09CuPCrNi Steel
09CuPCrNi Steel
09CuPCrNi Steel
09CuPCrNi Steel
1 Cr Steel
1 Cr Steel
1 Cr V Steel
1 Mn+S Steel
1 Mn+S Steel
1 Ni Steel
1 Ni Steel
1-1/2 Mn Mo Steel
1-1/2 Mn Mo Steel
1-1/2 Mn Mo Steel
1-1/2 Mn Mo Steel
1-1/2 Mn Mo Steel
1-1/2 Mn Mo Steel
1-1/2 Mn Ni Steel
1-1/2 Mn Steel
1-1/2 Mn Steel
1-1/2 Mn Steel
1-1/2 Mn Steel
1-1/2 Mn+S Steel
1-1/2 Ni Mn Steel
1-1/2 Ni Steel
1-1/2 Si Cr Steel
1-1/4 Mn Cr Steel
1-1/4 Mn Cr Steel
1-1/4 Mn Cr Steel
1-1/4 Mn Steel
1-1/4 Mn Steel
1-1/4 Mn Steel
1-3/4 Mn Steel
1-3/4 Mn Steel
1-3/4 Mn Steel
1-3/4 Mn+S Steel
1-3/4 Ni Mo Steel
1-3/4 Ni Mo Steel
1-3/4 Ni Mo Steel
1.0037 Steel
1.0045 Steel
1.00C-1.45Cr Steel
1.0461 Steel
1.0481 Steel
1.0482 Steel
1.0482 Steel
1.0501 Steel
1.0501 Steel
1.0503 Steel
1.0503 Steel
1.0505 Steel
1.0528 Steel
1.0528 Steel
1.0535 Steel
1.0535 Steel
1.0540 Steel
1.0562 Steel
1.0601 Steel
1.0601 Steel
1.0603 Steel
1.0605 Steel
1.0614 Steel
1.0615 Steel
1.0615 Steel
1.0915 Steel
1.0987 Steel
1.1106 Steel
1.1127 Steel
1.1132 Steel
1.1133 Steel
1.1140 Steel
1.1144 Steel
1.1157 Steel
1.1157 Steel
1.1160 Steel
1.1165 Steel
1.1165 Steel
1.1167 Steel
1.1170 Steel
1.1172 Steel
1.1172 Steel
1.1174 Steel
1.1174 Steel
1.1178 Steel
1.1178 Steel
1.1179 Steel
1.1179 Steel
1.1180 Steel
1.1180 Steel
1.1181 Steel
1.1181 Steel
1.1183 Steel
1.1183 Steel
1.1191 Steel
1.1191 Steel
1.1191 Steel
1.1192 Steel
1.1192 Steel
1.1193 Steel
1.1193 Steel
1.1194 Steel
1.1194 Steel
1.1199 Steel
1.1201 Steel
1.1201 Steel
1.1203 Steel
1.1203 Steel
1.1204 Steel
1.1204 Steel
1.1206 Steel
1.1209 Steel
1.1209 Steel
1.1211 Steel
1.1211 Steel
1.1217 Steel
1.1219 Steel
1.1219 Steel
1.1219 Steel
1.1221 Steel
1.1221 Steel
1.1223 Steel
1.1223 Steel
1.1231 Steel
1.1237 Steel
1.1237 Steel
1.1237 Steel
1.1240 Steel
1.1241 Steel
1.1248 Steel
1.1248 Steel
1.1248 Steel
1.1249 Steel
1.1249 Steel
1.1249 Steel
1.1251 Steel
1.1251 Steel
1.1251 Steel
1.1253 Steel
1.1253 Steel
1.1253 Steel
1.1269 Steel
1.1269 Steel
1.1273 Steel
1.13C-0.30Mn Steel
1.1520 Steel
1.1520 Steel
1.25Cr0.5Mo Steel
1.2764 Steel
1.5024 Steel
1.5026 Steel
1.5028 Steel
1.5029 Steel
1.5029 Steel
1.5120 Steel
1.5121 Steel
1.5122 Steel
1.5122 Steel
1.5141 Steel
1.5223 Steel
1.5223 Steel
1.5231 Steel
1.5232 Steel
1.5232 Steel
1.5233 Steel
1.5402 Steel
1.5403 Steel
1.5404 Steel
1.5404 Steel
1.5404 Steel
1.5406 Steel
1.5415 Steel
1.5415 Steel
1.5415 Steel
1.5419 Steel
1.5423 Steel
1.5510 Steel
1.5523 Steel
1.5523 Steel
1.5523 Steel
1.5525 Steel
1.5525 Steel
1.5527 Steel
1.5531 Steel
1.5532 Steel
1.5622 Steel
1.5633 Steel
1.5637 Steel
1.5639 Steel
1.5662 Steel
1.5662 Steel
1.5680 Steel
1.5680 Steel
1.5680 Steel
1.5710 Steel
1.5710 Steel
1.5710 Steel
1.5710 Steel
1.5713 Steel
1.5713 Steel
1.5732 Steel
1.5732 Steel
1.5732 Steel
1.5736 Steel
1.5737 Steel
1.5737 Steel
1.5752 Steel
1.5752 Steel
1.5752 Steel
1.5752 Steel
1.5752 Steel
1.5755 Steel
1.5755 Steel
1.5805 Steel
1.5805 Steel
1.5807 Steel
1.5807 Steel
1.5808 Steel
1.5808 Steel
1.5815 Steel
1.5815 Steel
1.5860 Steel
1.5860 Steel
1.5860 Steel
1.5864 Steel
1.5864 Steel
1.5918 Steel
1.5919 Steel
1.5919 Steel
1.5919 Steel
1.5919 Steel
1.5919 Steel
1.5920 Steel
1.5920 Steel
1.5920 Steel
1.5924 Steel
1.5924 Steel
1.5934 Steel
1.5934 Steel
1.5Ni-Cr-Mo Steel
1.5Ni-Cr-Mo Steel
1.6210 Steel
1.6211 Steel
1.6213 Steel
1.6217 Steel
1.6310 Steel
1.6310 Steel
1.6310 Steel
1.6311 Steel
1.6347 Steel
1.6349 Steel
1.6368 Steel
1.6368 Steel
1.6368 Steel
1.6511 Steel
1.6511 Steel
1.6511 Steel
1.6522 Steel
1.6522 Steel
1.6522 Steel
1.6522 Steel
1.6522 Steel
1.6523 Steel
1.6523 Steel
1.6523 Steel
1.6523 Steel
1.6523 Steel
1.6526 Steel
1.6541 Steel
1.6545 Steel
1.6545 Steel
1.6546 Steel
1.6546 Steel
1.6546 Steel
1.6562 Steel
1.6580 Steel
1.6580 Steel
1.6580 Steel
1.6580 Steel
1.6582 Steel
1.6582 Steel
1.6582 Steel
1.6587 Steel
1.6587 Steel
1.6587 Steel
1.6604 Steel
1.6604 Steel
1.6738 Steel
1.6738 Steel
1.6742 Steel
1.6746 Steel
1.6749 Steel
1.6751 Steel
1.6751 Steel
1.6753 Steel
1.6757 Steel
1.6780 Steel
1.6782 Steel
1.6926 Steel
1.6926 Steel
1.6946 Steel
1.6946 Steel
1.6956 Steel
1.6959 Steel
1.6985 Steel
1.7003 Steel
1.7005 Steel
1.7006 Steel
1.7014 Steel
1.7015 Steel
1.7015 Steel
1.7016 Steel
1.7023 Steel
1.7025 Steel
1.7033 Steel
1.7033 Steel
1.7034 Steel
1.7034 Steel
1.7035 Steel
1.7035 Steel
1.7037 Steel
1.7037 Steel
1.7038 Steel
1.7038 Steel
1.7039 Steel
1.7039 Steel
1.7045 Steel
1.7045 Steel
1.7108 Steel
1.7131 Steel
1.7131 Steel
1.7131 Steel
1.7138 Steel
1.7139 Steel
1.7139 Steel
1.7147 Steel
1.7147 Steel
1.7149 Steel
1.7149 Steel
1.7160 Steel
1.7168 Steel
1.7176 Steel
1.7182 Steel
1.7214 Steel
1.7214 Steel
1.7218 Steel
1.7218 Steel
1.7218 Steel
1.7219 Steel
1.7219 Steel
1.7220 Steel
1.7220 Steel
1.7223 Steel
1.7223 Steel
1.7225 Steel
1.7225 Steel
1.7226 Steel
1.7226 Steel
1.7227 Steel
1.7227 Steel
1.7228 Steel
1.7228 Steel
1.7238 Steel
1.7238 Steel
1.7242 Steel
1.7242 Steel
1.7243 Steel
1.7243 Steel
1.7244 Steel
1.7244 Steel
1.7255 Steel
1.7255 Steel
1.7258 Steel
1.7258 Steel
1.7271 Steel
1.7273 Steel
1.7311 Steel
1.7311 Steel
1.7320 Steel
1.7323 Steel
1.7323 Steel
1.7325 Steel
1.7326 Steel
1.7335 Steel
1.7335 Steel
1.7361 Steel
1.7362 Steel
1.7362 Steel
1.7380 Steel
1.7380 Steel
1.7380 Steel
1.7561 Steel
1.7701 Steel
1.7701 Steel
1.7701 Steel
1.7701 Steel
1.7703 Steel
1.7707 Steel
1.7707 Steel
1.7715 Steel
1.7733 Steel
1.7733 Steel
1.7734 Steel
1.7734 Steel
1.7734 Steel
1.7735 Steel
1.7735 Steel
1.7765 Steel
1.7767 Steel
1.7779 Steel
1.7783 Steel
1.8070 Steel
1.8154 Steel
1.8154 Steel
1.8159 Steel
1.8159 Steel
1.8161 Steel
1.8161 Steel
1.8807 Steel
1.8814 Steel
1.8903 Steel
1.8905 Steel
1.8905 Steel
1.8905 Steel
1.8905 Steel
1.8918 Steel
1.8918 Steel
1.8918 Steel
1.8928 Steel
1.8931 Steel
1.8940 Steel
1/2 Cr Mo V Steel
1/2 Cr Steel
1/2 Cr Steel
1/2 Mo Steel
1/2 Mo Steel
1/2 Ni Steel
1/4 Mo Steel
1/4 Mo Steel
1/4 Mo Steel
1/4 Mo Steel
1/4 Mo Steel
10 CD 9-10 Steel
10 CD 9-10 Steel
10 N 14 Steel
10 N 14 Steel
10 N 8 Steel
10 NC 12 Steel
10 NC 6 Steel
10 NC 6 Steel
100 C 3 Steel
100 C 6 Steel
100 C 6 Steel
100 CD 7 Steel
100 CD 7 Steel
1006/1008 Steel
100A2 Steel
100B2 Steel
100C2 Steel
100Cr6 Steel
100Cr6 Steel
1010 Mo-B Steel
1010 Steel
1010 Steel
1019 Steel
1021 Steel
1021+1Ni/1021+1N+0.75Si Steel
1021+1Ni/1021+1Ni+0.25Mo Steel
1021+1Ni/1021+1Ni+0.5Cr Steel
1021+1Ni/1021+1Ni+0.5Mo Steel
1021+1Ni/1021+1Ni+1Cr Steel
1021+1Ni/1021+1Ni+2Cr Steel
1021+1Ni/1021+1Ni+2Si Steel
1021+1Ni/1021+1Ni+B Steel
1021+Ni/1021+1Ni+Mn Steel
1021/1021 + 1 Ni Steel
102Cr6 Steel
102Cr6 Steel
1030 Mod. Steel
1030 Steel
1035 Mod. Steel
1036 Steel
1040 Steel
1045/1050 Steel
1045/1050+Cu Steel
1045/1050+Cu Steel
1045/1050+Cu Steel
1050 Steel
1055 Mod. Steel
1060 Mod./1065 Mod. Steel
1060 Steel
1060/10B60 Steel
1080 Steel
1086/1095 Steel
1086/1095+0.25V Steel
10B36 Steel
10CrMo5-5 (P4), 10CrMo9-10 (P5A), X10CrMoVNb9-1 (P15E) Steels
10CrMo5-5, 10CrMo9-10, X10CrMoVNb9-1 Steels
10CrMo9-10 Steel
10CrMo9-10 Steel
10CrMo9-10 Steel
10CrMo9-10 Steel
10CrMo9-10 Steel
10Ni-0.1C Steel
10Ni14 Steel
10NiCr6 Steel
10NiCr6 Steel
113 Steel
114 Steel
12 NC 15 Steel
12 ND 16 Steel
120 NCD 5-02 Steel
12Cr1MoV Steel
12CrMo Steel
12CrMo4 Steel
12Ni19 Steel
1335 Steel
1340 Steel
13CrMo4-4 Steel
13CrMo4-4 Steel
13CrMo4-4 Steel
13CrMo4-4 Steel
13CrMo44 Steel
13NiCr6 Steel
13NiCr6 Steel
14 NC 11 Steel
14 NC 11 Steel
14 NC 12 Steel
14 NCD 4 Steel
144 Steel
145V33 Steel
14CrMoV6-9 Steel
14CrMoV6-9 Steel
14MoV6-3 Steel
14MoV6-3 Steel
14MoV6-3 Steel
14Ni6 Steel
14NiCr10 Steel
14NiCr10 Steel
14NiCr14 Steel
14NiCr14 Steel
14NiCr14 Steel
14NiCr18 Steel
14NiCr18 Steel
14NiCrMo13-4 Steel
14NiCrMo13-4 Steel
15 MDV 4-05 Steel
15 MDV 4-05 Steel
15 MDV 4-05 Steel
15 MDV 4-05 Steel
15 NCDV 11 Steel
15 NCDV 11 Steel
150 Steel
1541 Steel
15Cr3 Steel
15Cr3 Steel
15Cr3 Steel
15Cr3 Steel
15Cr3 Steel
15Cr3 Steel
15CrMo Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15Kh2NMFA-A Steel
15Mo3 Steel
15Mo3 Steel
15Mo3 Steel
15Mo3 Steel
15Mo3 Steel
15Mo3 Steel
15NiCr13 Steel
15NiCuMoNb5 Steel
15NiCuMoNb5 Steel
16 MC 5 Steel
16 MC 5 Steel
16 NC 6 Steel
16 NC 6 Steel
16 NCD 13 Steel
16 NCD 13 Steel
16CMnR Steel
16CrMo4 Steel
16CrMo4 Steel
16CrMo4 Steel
16CrMo4 Steel
16CrNi4 Steel
16CrNi4 Steel
16CrNi4 Steel
16CrNi4 Steel
16MND5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCrB5 Steel
16MnCrB5 Steel
16MnCrS5 Steel
16MnCrS5 Steel
16NiCr11 Steel
16NiCr4 Steel
16NiCr4 Steel
16NiCrMo12 Steel
16NiCrMo12 Steel
16NiCrMo2 Steel
16NiCrS4 Steel
17 MV Az 6 Steel
17Cr3 Steel
17Cr3 Steel
17CrNi6-6 Steel
17CrNi6-6 Steel
17CrNiMo6 Steel
17CrNiMo6 Steel
17CrNiMo6 Steel
17CrNiMo6 Steel
17CrNiMo6 Steel
17CrS3 Steel
17MoV8-4 Steel
17MoV8-4 Steel
17NiCrMo6-4 Steel
17NiCrMo6-4 Steel
17NiCrMoS6-4 Steel
17NiCrMoS6-4 Steel
18 C 3 Steel
18 CD 4 Steel
18 CD 4 Steel
18 NCD 6 Steel
18 NCD-4 Steel
18/8 CrNi Steel
183 Steel
18CrMo4 Steel
18CrMo4 Steel
18CrMoS4 Steel
18CrMoS4 Steel
18CrNi8 Steel
18CrNi8 Steel
18CrNi8 Steel
18CrNi8 Steel
18CrNiMo7-6 Steel
18CrNiMo7-6 Steel
18NiCr5-4 Steel
18NiCr5-4 Steel
18NiCrMo5 Steel
18NiCrMo5 Steel
18NiCrMo5 Steel
18NiCrMo5 Steel
18NiCrMo7 Steel
18NiCrMo7 Steel
19 M Nb 6 Steel
1Cr0.5Mo Steel
1F Steel
1K Steel
1M Steel
1N Steel
1Ni Steel
1Ni Steel
2 Si Mn Steel
2 Si Mn Steel
2 Si Mn Steel
2 Si Mo Steel
2-1/2 Nickel Saw Steel
2-1/2Ni-1/2Mo Turbine Rotor Steel
2-1/4 Cr Mo Steel
2-3/4 Nickel Forging Steel
2.25 Cr-1Mo Steel
2.25Cr1Mo Steel
2.25Cr1Mo Steel
2.25Cr1Mo Steel
2.5Ni-Cr-Mo Medium Carbon Steel
2.5Ni-Cr-Mo Medium Carbon Steel
2.7Ni-0.9Cr-0.25Mo-B Steel
20 CDV 5-08 Steel
20 CDV 5-08 Steel
20 NC 6 Steel
20 NC 6 Steel
20 NCD 10 Steel
20 NCD 10 Steel
20 NCD 2 Steel
20 NCD 2 Steel
20 NCD 7 Steel
20 NCD 7 Steel
20 NCD 8 Steel
20 ND 16 Steel
20 ND 16 Steel
20 ND 8 Steel
20 ND 8 Steel
20CrMo2 Steel
20CrMo2 Steel
20CrMoV13-5 Steel
20CrMoV13-5 Steel
20CrNi4 Steel
20CrNi4 Steel
20CrNi4 Steel
20GFL Steel
20Mn5 Steel
20MnCr5 Steel
20MnCr5 Steel
20MnCr5 Steel
20MnCrB5 Steel
20MnCrS5 Steel
20MnMoNi5-5 Steel
20MnMoNi5-5 Steel
20MnMoNi5-5 Steel
20MnMoNi5-5 Steel
20Mo5 Steel
20MoCr4 Steel
20MoCr4 Steel
20MoCr4 Steel
20MoCr4 Steel
20MoCr4 Steel
20MoCr4 Steel
20MoCr4 Steel
20MoCr4 Steel
20MoCr5 Steel
20MoCr5 Steel
20MoCr5 Steel
20MoCr5 Steel
20NiCr6 Steel
20NiCr6 Steel
20NiCrMo14-6 Steel
20NiCrMo14-6 Steel
20NiCrMo2 Steel
20NiCrMo2 Steel
20NiCrMo2-2 Steel
20NiCrMo2-2 Steel
20NiCrMo3 Steel
20NiCrMo3 Steel
20NiMoCr6 Steel
20NiMoCr6-5 Steel
20NiMoCr6-5 Steel
20g Steel
21/4Cr-1Mo Steel
21CrMoV5-11 Steel
21CrMoV5-11 Steel
21CrMoV5-11 Steel
21CrMoV5-11 Steel
21CrMoV5-11 Steel
21CrMoV5-11 Steel
21Mn6AlX1 Steel
21Mn6AlX1 Steel
21NiCrMo2 Steel
21NiCrMo2 Steel
21NiCrMo2 Steel
21NiCrMo2 Steel
21NiCrMo2 Steel
21NiCrMo2 Steel
22 N 8 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22NiMoCr3-7 Steel
22NiMoCr3-7 Steel
22NiMoCr3-7 Steel
22NiMoCr3-7 Steel
2315 Steel
2330 Steel
2330 Steel
2340 Steel
2340 Steel
23CrMoB3-3 Steel
23CrMoB3-3 Steel
23MnB4 Steel
24CrMo5 Steel
24CrMo5 Steel
24CrMo5 Steel
24CrMoV5-5 Steel
24CrMoV5-5 Steel
24CrMoV5-5 Steel
24CrMoV5-5 Steel
24CrMoV5-5 Steel
24Mn-18Cr-3Ni-0.62N Steel
25 CD 4 Steel
25 CD 4 Steel
25 M 6 Steel
25 M 6 Steel
2512 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMoS4 Steel
25CrMoS4 Steel
25MoCr4 Steel
25MoCr4 Steel
25MoCr4 Steel
26CrMo4 Steel
26NiCr6-4 Steel
26NiCr6-4 Steel
275 Steel
27MnCrB5-2 Steel
27MnCrV4 Steel
27MnCrV4 Steel
28 NCD 6 Steel
28 NCD 6 Steel
280 Steel
28CrMoNiV4-9 Steel
28CrMoNiV4-9 Steel
28Mn6 Steel
28Mn6 Steel
28Mn6 Steel
28NiCrMo7-4 Steel
28NiCrMo7-4 Steel
2910 Steel
295 Steel
29Cr-4Mo Ferritic Stainless Steel
29Cr-4Mo Ferritic Stainless Steel
2H 6D Steel
2H 7C Steel
2H-50 Steel
2H-Cr Steel
2H-Supper Steel
2H-Te Steel
2H-Ultra Steel
2HA Steel
2HB Steel
2HB Steel
2HB Steel
2M Steel
3 Ni Steel
3-1/2 Ni Mo Steel
3-1/2 Ni Steel
3-1/2 Ni Steel
3-1/2 Ni Steel
3-1/4 Cr Mo Steel
3-1/4 Cr Mo Steel
3.5Ni Steel
3.5Ni Steel
3.5Ni-Cr-Mo Steel
3/4 Ni Cr Steel
30 C 5 Steel
30 CAD 6-12 Steel
30 CD 12 Steel
30 CD 12 Steel
30 CND 8 Steel
30 CND 8 Steel
30 CV 5 Steel
30 MS 6 Steel
30 NC 11 Steel
30 NC 11 Steel
30 NC 12 Steel
30 NCD 12 Steel
30 NCD 12 Steel
30 NCD 12 Steel
30 NCD 2 Steel
30 NCD 2 Steel
30 NCD 8 Steel
30 SC 6 Steel
30 SCD 6 Steel
30CrMo4 Steel
30CrMo4 Steel
30CrMoNiV5-11 Steel
30CrMoNiV5-11 Steel
30CrMoV9 Steel
30CrMoV9 Steel
30CrMoV9 Steel
30CrMoV9 Steel
30CrNiMo8 Steel
30CrNiMo8 Steel
30CrNiMo8 Steel
30CrNiMo8 Steel
30CrNiMo8 Steel
30CrNiMo8 Steel
30CrNiMo8 Steel
30CrNiMo8 Steel
30Mn5 Steel
30Mn5 Steel
30Mn5 Steel
30NC1 Steel
30NiCr-11 Steel
30NiCr-11 Steel
30NiCrMo12 Steel
30NiCrMo12 Steel
30NiCrMo2-2 Steel
30NiCrMo2-2 Steel
3120 Steel
3140 Steel
316 Stainless Steel
3190 Steel
31CrMo12 Steel
31CrMo12 Steel
31CrMoV9 Steel
32 C 4 Steel
32 C 4 Steel
32 CND 11 Steel
32 CND 11 Steel
32 NCD 15 Steel
321 Stainless Steel
32CrMo12 Steel
32CrMo12 Steel
32CrMo12 Steel
32CrMo12 Steel
32CrMoV12-10 Steel
32NiCrMo-14-5-X1* Steel
32NiCrMo-14-5-X1* Steel
3310 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34CrAlNi7-10 Steel
34CrAlNi7-10 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrNiMo6 Steel
34CrNiMo6 Steel
34CrNiMo6 Steel
34CrNiMo6 Steel
34CrNiMo6 Steel
34CrNiMo6 Steel
34CrNiMo6 Steel
34CrNiMo6 Steel
34CrS4 Steel
34CrS4 Steel
35 CD 4 Steel
35 CD 4 Steel
35 M 5 Steel
35 M 5 Steel
35 M 6 Steel
35 NC 11 Steel
35 NC 15 Steel
35 NC 15 Steel
35 NC 6 Steel
35 NC 6 Steel
35 NCD 5 Steel
35 NCD 5 Steel
35NiCr18X1 Steel
35NiCr18X1 Steel
36Cr6 Steel
36Cr6 Steel
36CrMn5 Steel
36CrMn5 Steel
36CrNiMo4 Steel
36CrNiMo4 Steel
36CrNiMo4 Steel
36CrNiMo4 Steel
36CrNiMo4 Steel
36NiCr6-4 Steel
36NiCr6-4 Steel
36NiCrMo16 Steel
36NiCrMo16 Steel
37Cr4 Steel
37Cr4 Steel
37Cr4 Steel
37CrS4 Steel
37MnB5 Steel
37MnSi5 Steel
37MnSi5 Steel
37MnSi5 Steel
37MnSi5 Steel
37MnSi5 Steel
37MnSi5 Steel
37MnSi5 Steel
37MnSi5 Steel
37MnSi5 Steel
37MnSi7 Steel
37MnSi7 Steel
37Mo2 Steel
38 C 4 Steel
38 C 4 Steel
38Cr2 Steel
38Cr2 Steel
38Cr4 Steel
38Cr4 Steel
38KhGMA, 40KhGMA, 40KhGMRA Steels
38MnB5 Steel
38Si6 Steel
38Si6 Steel
38Si7 Steel
39NiCrMo3 Steel
39NiCrMo4 Steel
39NiCrMo4 Steel
3M50 BS-1 Steel
3M50BC-1 Steel
3M50BN-1 Steel
3Ni-Cr Steel
3Ni-Cr Steel
3U Steel
4.25Ni-Cr Steel
4.25Ni-Cr Steel
40 CAD 6-12 Steel
40 CAD 6-12 Steel
40 CV 5 Steel
40 CV 5 Steel
40 NC 18 Steel
40 NCD 18 Steel
40 NCD 18 Steel
40 NCD 3 Steel
40 NCD 3 Steel
40 NDCV 18-11 Steel
4027 Steel
4037 Steel
4047 Steel
4068 Steel
40Mn4 Steel
40Mn4 Steel
40NiCrMo18-6 Steel
40NiCrMo18-6 Steel
40NiCrMo2 Steel
40NiCrMo2-2 Steel
40NiCrMo2-2 Steel
40NiCrMo2-2 Steel
40NiCrMo2-2 Steel
40NiCrMo3 Steel
40NiCrMo7 Steel
40NiCrMo7 Steel
40NiCrMo8-4 Steel
41 S 7 Steel
4130 Steel
4137/4140 Steel
4140 Steel
4150 Mod. Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41CrAlMo7-10 Steel
41CrAlMo7-10 Steel
41CrMo4 Steel
41CrMo4 Steel
41CrS4 Steel
41CrS4 Steel
41NiCrMo7-3-2 Steel
41Si7 Steel
42 C 4 Steel
42 C 4 Steel
42Cr4 Steel
42Cr4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrV6 Steel
42CrV6 Steel
42MnV7 Steel
42MnV7 Steel
42MnV7 Steel
42MnV7 Steel
42MnV7 Steel
42MnV7 Steel
4317 Steel
4317/43B17 Steel
4340 Steel
4360 Steel
45 M 5 Steel
45 M 5 Steel
45 MS 6 Steel
45 MS 6 Steel
45 SC 6 Steel
45 SC 6 Steel
45 SCD 6 Steel
45 SCD 6 Steel
45 SCD 6 Steel
453 Steel
454 Steel
45CrMoV6-7 Steel
45CrMoV6-7 Steel
45CrMoV6-7 Steel
45CrMoV6-7 Steel
45CrMoV6-7 Steel
45Mn5 Steel
45MnSi6 Steel
45MnSi6 Steel
4615 Steel
4615/46B15 Steel
4640 Steel
46Cr2 Steel
46Cr2 Steel
46CrS2 Steel
46Si7 Steel
46SiCrMo6-3 Steel
46SiCrMo6-3 Steel
4815 (1.0% C) Steel
4815 Steel
48Si7 Steel
49CrMo4 Steel
49CrMo4 Steel
5 Ni Mo Steel
5 Ni Steel
50 CD 4 Steel
50 CD 4 Steel
50 CV 4 Steel
50 CV 4 Steel
50 NC 2 Steel
50 NC 2 Steel
50 NCD 6 Steel
50 NCD 6 Steel
501 Steel
502 Steel
504 Steel
505 Steel
506 Steel
507 Steel
508 Steel
509 Steel
50CV4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50SiCrMo6 Steel
5140 Steel
5140 Steel
5160 Steel
5160/51B60 Steel
51CrMoV4 Steel
51CrMoV4 Steel
51CrV4 Steel
51CrV4 Steel
51CrV4 Steel
51CrV4 Steel
51CrV4 Steel
51Si7 Steel
51Si7 Steel
52100 Steel
52100 Steel
52CrMo4V Steel
52CrMo4V Steel
52MnCrB3 Steel
52MnCrB3 Steel
52SiCrNi5 Steel
52SiCrNi5 Steel
53MnSi4-X-1 Steel
53MnSi4-X-1 Steel
53MnSiX1 Steel
53MnSiX1 Steel
54SiCr6 Steel
55 NCDV 7-05 Steel
55 NCDV 7-05 Steel
55 S 7 Steel
55 S 7 Steel
55Cr3 Steel
55Cr3 Steel
55Cr3 Steel
55Si3Mn2CrMoVNb Steel
56Si7 Steel
56Si7 Steel
56SiCr7 Steel
58CrV4 Steel
58CrV4 Steel
58CrV4 Steel
58CrV4 Steel
590 MPa Grade Galvannealed Sheet Steel
5Cr0.5Mo Steel
60 NCD 11 Steel
60 NCD 11 Steel
60 SC 7 Steel
60 SC 7 Steel
60Cr3 Steel
60NiCrMo11-03 Steel
60Si7 Steel
60SiCr8 Steel
60SiCrV7 Steel
60SiCrV7 Steel
6145 Steel
6150 Steel
61SiCr7 Steel
61SiCr7 Steel
6NA Steel
6NB Steel
6NC Steel
6ND Steel
6NE Steel
6NF Steel
6NG Steel
6Q Steel
70 C 1 Steel
71Si7 Steel
71Si7 Steel
7CrMoVTiB10-10 (T/P24) Steel
7Nb Steel
7QA Steel
7QB Steel
7QC Steel
7QD Steel
8-10Cr Steels
80A2 Steel
80B2 Steel
80B20 Steel
80C2 Steel
81B40 Steel
8620 Steel
8620/86B20 Steel
8630 Steel
8640 & 8740 Steel
8650/86B50 Steel
8660 Steel
8680/86B80 Steel
8695 Steel
86B45 Steel
8745 Steel
8A Steel
8B Steel
9 Ni Steel
9% Nickel Low Carbon Steel
90 M 5 Steel
90 M 5 Steel
90 MV 8 Steel
90 MV 8 Steel
9260 Steel
9261 Steel
9262 Steel
9420 Steel
9440 Steel
94B17 Steel
95 C 3 Steel
9860 Steel
98B45 Steel
9Ni Steel
9Ni-4Co Ultra-Strength Steel
A 1320 Steel
A1-3 Steel
A508 type RPV Steel
AH36 Steel
AH36 Steel
AISI 1020 Steel
AISI 1020 Steel
AISI 1045, 5140, 4140, 4340 Steels
AISI 1050 Steel
AISI 1080 Steel
AISI 1090 Steel
AISI 3140 Steel
AISI 3140 Steel
AISI 316 Steel
AISI 316 Steel
AISI 4130 Steel
AISI 4130 Steel
AISI 4130 Steel
AISI 4130 Steel
AISI 4130 Steel
AISI 4130 Steel
AISI 4130 Steel
AISI 4140 Steel
AISI 4140 Steel
AISI 4140 Steel
AISI 4140 Steel
AISI 4140 Steel
AISI 4140 Steel
AISI 4140 Steel
AISI 4140 Steel
AISI 4140 Steel
AISI 4140 Steel
AISI 4140 Steel
AISI 4140 Steel
AISI 4140 Steel
AISI 4340 Steel
AISI 4340 Steel
AISI 4340 Steel
AISI 444 Steel
AISI 5140 Steel
AISI 5150H Steel
AISI 8630 mod. Steel
AISI E52100 Steel
AISI/SAE 4340 Steel
AMS 6416 (200-M) Steel
AMS 6416 (300-M) Steel
AMS 6416 (300-M) Steel
AMS 6418 Steel
AMS 6428 and 6434 Steel
API 5CT L80 Steel
API 5CT L80 Steel
API 5CT L80 Steel
API 5L X-60 Steel
API 5L X80 Steel
API X80 Steel
ASTM Grade 91 Steel
ASTM Grade 911 Steel
ASTMA302B Steel
Al killed Steel
Ausa 42CrMo4 Steel
Austenitic Cr-Ni-Mo Steel X5CrNiMo17-13
B-3 Steel
BHT80 Steel
BHW35 Steel
BS 708A37 Steel
BaseMoV Steel
Bohler 25CrMo4 Steel
Bohler P435 Steel
Bohler P435 Steel
C-0.08 Steel
C-0.15 Steel
C-0.3 Steel
C-0.38 Steel
C-0.53 Steel
C-0.94 Steel
C-1.37 Steel
C-Mn Steel Steel
C-Mn Steel Steel
C-Mn Steel Steel
C-Mn Steel Steel
C-Mn Weld Steel
C-Mn Weld Steel
C-Mn Weld Steel
C-Mn Weld Steel
C-Mn Weld Steel
C-Mn-B Steel
C-Mn-B Steel
C-Mn-Ni Weld Steel
C-Mn-Ni Weld Steel
C-Mn-Ni Weld Steel
C-Mn-Ni Weld Steel
C-Mn-Ni Weld Steel
C-Mn-Ni Weld Steel
C10 Steel
C10 Steel
C100S Steel
C100S Steel
C10E2C Steel
C10E2C Steel
C110 Steel
C125S Steel
C16 Steel
C17E2C Steel
C20 Steel
C35E Steel
C35E Steel
C35EC Steel
C35EC Steel
C35R Steel
C35R Steel
C35RC Steel
C35RC Steel
C36 Steel
C36 Steel
C38 Steel
C40D2 Steel
C40E Steel
C40R Steel
C42 Steel
C43 Steel
C43 Steel
C45 Steel + Microstructures
C45E Steel
C45E Steel
C45E Steel
C45EC Steel
C45EC Steel
C45R Steel
C45R Steel
C45RC Steel
C45RC Steel
C46 Steel
C46 Steel
C50E Steel
C50R Steel
C53 Steel
C55E Steel
C55E Steel
C55R Steel
C55S Steel
C60E Steel
C60R Steel
C60R Steel
C60S Steel
C60S Steel
C75S Steel
C75S Steel
C75S Steel
C90S Steel
CP1100 Steel
CT182 Steel
CT198 Steel
CT198 Steel
CT198 Steel
CTC-08A Steel
Carburized 1320 (0.4% C) Steel
Carburized 1320 (0.6% C) Steel
Carburized 1320 (0.8% C) Steel
Carburized 1320 (1.0% C) Steel
Carburized 1320 (1.2% C) Steel
Carburized 2512 (0.4% C) Steel
Carburized 2512 (0.6% C) Steel
Carburized 2512 (0.8% C) Steel
Carburized 2512 (1.0% C) Steel
Carburized 2512 (1.2% C) Steel
Carburized 3310 (0.4% C) Steel
Carburized 3310 (0.6% C) Steel
Carburized 3310 (0.8% C) Steel
Carburized 3310 (1.0% C) Steel
Cf35 Steel
Cf35 Steel
Cf45 Steel
Cf45 Steel
Cf53 Steel
Cf53 Steel
Cf70 Steel
Cf70 Steel
Characteristic Shapes of Continuous TTT-Diagrams
Ck15 Steel
Ck30 Steel
Ck30 Steel
Ck35 Steel
Ck35 Steel
Ck35 Steel
Ck35 Steel
Ck35 Steel
Ck35 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck50 Steel
Ck55 Steel
Ck55 Steel
Ck55 Steel
Ck55 Steel
Ck60 Steel
Ck60 Steel
Ck60 Steel
Ck60 Steel
Ck75 Steel
Ck75 Steel
Ck85 Steel
Ck85 Steel
Ck85 Steel
Ck85 Steel
Continuous TTA-Diagram for 100Cr6
Corten Steel
Cr-0.5 Steel
Cr-1 Steel
Cr-2 Steel
Cr-4 Steel
CrMoZr Structural Steel
Cu-3 Steel
D6AC Steel
DC04 Steel
DP 600 Steel
DP 780 Steel
DT Steel
Dual-Phase Steel
Dual-Phase Steel
Duplex Stainless Steel
Durapur 1219 Steel
E 36 Steel
E595 Steel
E599 Steel
E602 Steel
ELI Ferritic Stainless Steel
Effect of C on CCT diagram of steel
Effect of Mn on CCT diagram of steel
En 100 Steel
En 100 Steel
En 100 Steel
En 100 Steel
En 100 Steel
En 11 Steel
En 110 Steel
En 111 Steel
En 111 Steel
En 111 Steel
En 111 Steel
En 12 Steel
En 12 Steel
En 13 Steel
En 13 Steel
En 14B Steel
En 15 Steel
En 16 Steel
En 16 Steel
En 160 Steel
En 160 Steel
En 160 Steel
En 17 Steel
En 17 Steel
En 18 Steel
En 19 Steel
En 19 Steel
En 20 Steel
En 20 Steel
En 21 Steel
En 23 Steel
En 23 Steel
En 24 Steel
En 25 Steel
En 26 Steel
En 26 Steel
En 28 Steel
En 30B Steel
En 31 Steel
En 33 Steel
En 33 Steel
En 33 Steel
En 33 Steel
En 34 Steel
En 34 Steel
En 34 Steel
En 34 Steel
En 351 Steel
En 351 Steel
En 351 Steel
En 351 Steel
En 352 Steel
En 352 Steel
En 352 Steel
En 352 Steel
En 353 Steel
En 353 Steel
En 353 Steel
En 353 Steel
En 354 Steel
En 354 Steel
En 354 Steel
En 354 Steel
En 355 Steel
En 355 Steel
En 355 Steel
En 355 Steel
En 36 Steel
En 36 Steel
En 36 Steel
En 36 Steel
En 36 Steel
En 36 Steel
En 36 Steel
En 36 Steel
En 39A Steel
En 39A Steel
En 39A Steel
En 39A Steel
En 39A Steel
En 39A Steel
En 39B Steel
En 39B Steel
En 39B Steel
En 39B Steel
En 39B Steel
En 39B Steel
En 40B Steel
En 42 Steel
En 44 Steel
En 45 Steel
En 47 Steel
Extremely-Low Carbon Bainitic Steel
FH Steel
FIRD Steels
FTW52A Steel
FTW52B Steel
FTW58 Steel
Fe-C-Cr-Mo Steel
Firmodur 1213 Steel
Firmodur 1249 Steel
Formadur 2335 Steel
GS-22CrMo5 Steel
Grain Coarsened HAZ Steel
Grain refined HAZ Steel
HFX 6926 Steel
HFX 6926 Steel
HFX 6928 Steel
HFX 6928 Steel
HFX 7783 Steel
HFX 7783 Steel
HFX 8090 Steel
HSLA Steel Plate
HSLA Steel Plate
HSLA Steel Plate
HSLA-100 Steel
HSLA-100 Steel
HT60 Steel
HY80 7G Steel
HY80 7H Steel
HY80 K1 Steel
HY80 K2 Steel
HY80 K3 Steel
HY80 K4 Steel
HY80 M1 Steel
HY80 N1 Steel
HY80 N2 Steel
HY80 N3 Steel
HY80 N4 Steel
HY80 NA Steel
HY80 NB Steel
HY80 NE38 Steel
HY80 NER38 Steel
HY80 NS63 Steel
HY80 Y1 Steel
HY80 Y4 Steel
Her-Ten60 Steel
Hi-Z Steel
High Strength Weld Metal
IF and IF-TiNb Steels
Influence of C on the CCT Diagram of Steel - (A) 0.06% C and (B) 0.17% C
Influence of Mn on the CCT Diagram of Steel with 0.44% C: (A) 0.66% Mn and (B) 2% Mn
Influence of Mo or Cr on TTT
Isothermal TTA-Diagram
Isothermal TTA-Diagram for 34CrMo4
J-1 Steel
J-2 Steel
J-3 Steel
J-4 Steel
J-6 Steel
K2H-U Steel
KO Steel
KQ (Hi-Z) Steel
KS Steel
KT Steel
Large Forgings Component
Low Carbon Nb Bearing Steels
Low Carbon Steel
Micro-Alloyed Steel
Mn-0 Steel
Mn-1.0 Steel
Mn-2.0 Steel
Mn-C~Mo Dual Phase Steel
Mn-C~Mo Dual Phase Steel
Mn-Si-Al Steel
Mo-0.5 Steel
Mo-1.0 Steel
Mo-1.6 Steel
N-A-XTRA 70 Steel
N-TuFCR130 Steel
N-TuFCR196 Steel
NA Steel
NB Steel
NC Steel
ND Steel
NE Steel
NF Steel
NK Steel
NK-HT 80 Steel
NM Steel
NRIM 431L Steel
NRIM 432M Steel
NRIM 55 Steel
NRIM A-3 Steel
NRIM B-3 Steel
NRIM37 Steel
NS 80 Steel
Nb Microaloyed Steel
Nb Steel
Nb-2 Steel
Nb-3 Steel
Ni-1.0 Steel
Ni-2.5 Steel
Ni-2.5 Steel
Ni-5 Steel
Ni-7 Steel
Ni-9 Steel
Ni-Cr Steel
Nippon Steel
Nitralloy, 135 Mod. Steel
Non-Superhardening Steel
OvaX 500 Steel
Ovako 280T Steel
Ovako 803Q Steel
Ovako 803Q Steel
P295GH Steel
P92 HTRG Steel
P92 Steel
PA Steel
PB Steel
PC Steel
PC52 Steel
PD Steel
PMS 25 Steel
PMS 35 Steel
PO766 Steel
PO768 Steel
PO768 Steel
PO768 Steel
PO795 Steel
PO795 Steel
PO85 Steel
PT181 Steel
PT181 Steel
PT759 Steel
PT759 Steel
PT759 Steel
RS Steel
Rail Steel
S-1 Steel
S-2 Steel
S-3 Steel
S-4 Steel
S-5 Steel
S-6 Steel
S135 Steel
S235JR Steel
S355J2G3 Steel
S355JR Steel
S355N Steel
S355N Steel
S460 Steel
S460M Steel
S50C Steel
S700 Steel
SAE 1038 Steel
SAE 1038 Steel
SAE 1050 Steel
SAE 1075 Steel
SAE 1092 Steel
SAE 1320 Steel
SAE 1513 + Nb Steel
SAE 15B41 Steel
SAE 4024 Steel
SAE 4047 Steel
SAE 52100 Steel
SAE 52100 Steel
SAE 9840 Steel
SAE/AISI 4140-4142 Steels
SAE1020 Steel
SAE15B41H Steel
SCr415 Steel
SCr415 Steel
SM41 Steel
SM41(A) Steel
SM41(B) Steel
SM41A Steel
SM41B Steel
SM50A Steel
SM50B Steel
SM50Y Steel
SS Steel
SS55 Steel
ST52V Steel
Si-0 Steel
Si-0.2 Steel
Si-0.5 Steel
Si-1.0 Steel
Si-1.6 Steel
Si-Mn Steel
Si-Mn-Ti-B Steel
SiMn HT50 Steel
St52-3 Steel
StE 690 Steel
StE47 Steel
StE47 Steel
StE47 Steel
StE47 Steel
StE70 Steel
Steel with 0.33% Ni
Steel with 1.00% Ni
Steel with 2.50% Ni
Steel with 2.50% Ni
Steels 8, 10, 11, 12, 13, 17
Structural Fe-Cr Steel
Structural Steel
Superhardening Steel
T-1 Steel
T-1 Steel
T1 Steel
TBL PLUS Steel
TBL Steel
TTA Diagram of Steel
Tempaloy A-1 Steel
Ti Modified 316 Stainless Steel
Ti-3 Steel
Ti-47Al-2Cr-2Nb-1Mo
Ti-47Al-2Cr-2Nb-1Mo-0.2B
Ti-Oxide Bearing Steel
Ti-Oxide Bearing Steel
Type 304 Steel
Type 304 Steel
Type 321 Steel
Type 347 Steel
U-1 Steel
U-2 Steel
U-3 Steel
UH-1 Steel
UH-2 Steel
UH-3 Steel
UH-4 Steel
UH-5 Steel
UH-6 Steel
ULCB Steel
UNS S31803 Steel
UNS S31803 Steel
USS Airsteel X 200 Steel
USS Cor-Ten Steel Steel
Uranus 50 Duplex Stainless Steel
Uranus 50 Duplex Stainless Steel
V-3 Steel
VAN-80 HSLA Steel
VC140 Steel
VC140 Steel
VC140 Steel
VCMO125 Steel
VCMO125 Steel
VCMO135 Steel
VCMO135 Steel
VCV150 Steel
VCV150 Steel
VMS135 Steel
VZ197 Steel
VZ197 Steel
VZ197 Steel
VZ197 Steel
VZ727 Steel
VZ727 Steel
VZ727 Steel
VZ727 Steel
VZ727 Steel
W ST 3 Steel
WELDOX 1300 Steel
WELL-TEN60 Steel
WELL-TEN60H Steel
WELL-TEN60R Steel
WELL-TEN62 Steel
WELL-TEN74(A) Steel
WELL-TEN74(B) Steel
WELL-TEN80(A) Steel
WELL-TEN80(B) Steel
WELL-TEN80C(A) Steel
WELL-TEN80C(B) Steel
WELL-TEN80S(41) Steel
WELL-TEN80S(43) Steel
WT-60 Steel
WT-80 Steel
WT-80 Steel
WT-80C Steel
Welten 80 Steel
Welten55C Steel
X-80 Steel
X10CrMoVNb9-1 (T/P91) Steel
X10CrWMoVNb9-2 (T/P92) Steel
X12CrCoWVNb12-2-2 (VM12-SHC) Steel
X210Cr12 Steel
X22CrMoV12-1 Steel
X22CrMoV12-1 Steel
X38CrMoV5-1 Steel
X45Mn2 Steel
X5CrNiMo17-13 Steel
X60 Steel
X65 (0.047C-1.23Mn) Steel
X70 Steel
X80 Steel
X8Ni9 Steel
XC 32 Steel
XC 38 Steel
XC 38 Steel
XC 38 Steel
XC 42 Steel
XC 42 Steel
XC 48 Steel
XC 55 Steel
XC 55 Steel
Y1 120 Steel
Y1 120 Steel
YA Steel
YB Steel
YC Steel
YD Steel
YE Steel
YG Steel
YND33 Steel
Z 10 N 5 Steel
Z 10 N 5 Steel
Z 10 N 9 Steel
Z 10 N 9 Steel
Z 120 M 12 Steel