Alphabetical Index
Chemical Composition
Keyword Search
AFNOR Steels
AISI/SAE Steels
BS Steels
DIN Steels
Wr.Nr. (Mat.No.) Steels
Calculated Diagrams
CCT Diagrams
TTA Diagrams
TTE Diagrams
TTT Diagrams
TTP Diagrams
TTS Diagrams
Alloy Steels
Carbon Steels
Carburizing Steels
Cast Irons
Chromium Steels
Cold Work Tool Steels
High Speed Steels
Hot Work Tool Steels
Low Carbon Steels
Microalloyed Steels
Molybdenum Steels
New Diagrams
Nitriding Steels
Plastic Mould Steels
PM Steels
Stainless Steels
Steel Companies
Structural Steels
Tools Steels
Vanadium Steels
Welding Steels
White Cast Irons
Help
Home
White Cast Irons
1.95% C, 10.80% Cr, 3.80% Mo Alloyed White Cast Iron
1.95% C, 10.80% Cr, 3.80% Mo Alloyed White Cast Iron
1.96% C, 15.40% Cr, 2.20% Mo Alloyed White Cast Iron
1.96% C, 15.40% Cr, 2.20% Mo Alloyed White Cast Iron
1.98% C, 20.25% Cr, 2.14% Mo Alloyed White Cast Iron
1.98% C, 20.25% Cr, 2.14% Mo Alloyed White Cast Iron
15-2-1 LC White Cast Iron
2.04% C, 20.55% Cr, 0.61% Mo Alloyed White Cast Iron
2.04% C, 20.55% Cr, 0.61% Mo Alloyed White Cast Iron
2.05% C, 15.60% Cr, 0.81% Mo Alloyed White Cast Iron
2.05% C, 15.60% Cr, 0.81% Mo Alloyed White Cast Iron
2.08% C, 15.85% Cr Alloyed White Cast Iron
2.08% C, 15.85% Cr Alloyed White Cast Iron
2.08% C, 20.55% Cr, <0.01% Mo Alloyed White Cast Iron
2.08% C, 20.55% Cr, <0.01% Mo Alloyed White Cast Iron
2.13% C, 11.30% Cr, 1.41% Mo Alloyed White Cast Iron
2.13% C, 11.30% Cr, 1.41% Mo Alloyed White Cast Iron
2.19% C, 11.65% Cr, 0.02% Mo Alloyed White Cast Iron
2.19% C, 11.65% Cr, 0.02% Mo Alloyed White Cast Iron
2.41% C, 12.15% Cr, 2.45% Mo Alloyed White Cast Iron
2.41% C, 12.15% Cr, 2.45% Mo Alloyed White Cast Iron
2.45% C, 19.82% Cr, 2.94% Mo Alloyed White Cast Iron
2.45% C, 19.82% Cr, 2.94% Mo Alloyed White Cast Iron
2.54% C, 20.22% Cr, 1.52% Mo Alloyed White Cast Iron
2.54% C, 20.22% Cr, 1.52% Mo Alloyed White Cast Iron
2.55% C, 12.40% Cr, 1.25% Mo Alloyed White Cast Iron
2.55% C, 12.40% Cr, 1.25% Mo Alloyed White Cast Iron
2.60% C, 15.20% Cr, 1.95% Mo Alloyed White Cast Iron
2.60% C, 15.20% Cr, 1.95% Mo Alloyed White Cast Iron
2.65% C, 12.65% Cr, 0.02% Mo Alloyed White Cast Iron
2.65% C, 12.65% Cr, 0.02% Mo Alloyed White Cast Iron
2.67% C, 14.95% Cr Alloyed White Cast Iron
2.67% C, 14.95% Cr Alloyed White Cast Iron
2.67% C, 15.20% Cr, 1.09% Mo Alloyed White Cast Iron
2.67% C, 20.75% Cr, <0.01% Mo Alloyed White Cast Iron
2.67% C, 20.75% Cr, <0.01% Mo Alloyed White Cast Iron
2.67% C-15.20% Cr-1.09% Mo Alloyed White Cast Iron
2.72% C, 25.15% Cr, 2.52% Mo Alloyed White Cast Iron
2.72% C, 25.15% Cr, 2.52% Mo Alloyed White Cast Iron
2.73% C, 0.03% Mn, 1.25% Si, 0.015% S White Iron
2.75% C, 0.13% Mn, 1.21% Si, 0.008% S White Iron
2.87% C, 25.50% Cr, 1.22% Mo Alloyed White Cast Iron
2.87% C, 25.50% Cr, 1.22% Mo Alloyed White Cast Iron
2.9% C-0.6% Si-17.0% Cr-Mn-Mo White Cast Iron
2.9% C-0.6% Si-17.0% Cr-Mn-Mo White Cast Iron
2.9% C-0.6% Si-17.0% Cr-Mn-Mo White Cast Iron
2.9% C-0.7% Mn-0.6% Si-17.5% Cr White Cast Iron (Mo Addition)
2.9% C-0.7% Mn-0.6% Si-17.5% Cr White Cast Iron (Mo Addition)
2.9% C-0.7% Mn-0.6% Si-17.5% Cr White Cast Iron (Mo Addition)
2.9% C-0.8% Mn-0.6% Si-17.0% Cr-1.5% Mo-Si--Cu White Cast Iron
2.9% C-0.8% Mn-0.6% Si-17.0% Cr-1.5% Mo-Si--Cu White Cast Iron
2.9% C-0.8% Mn-0.6% Si-17.0% Cr-1.5% Mo-Si--Cu White Cast Iron
2.9% C-0.8% Mn-0.6% Si-17.5% Cr-Ni-Mo White Cast Iron
2.9% C-0.8% Mn-0.6% Si-17.5% Cr-Ni-Mo White Cast Iron
2.9% C-0.8% Mn-0.6% Si-17.5% Cr-Ni-Mo White Cast Iron
2.9% C-0.8% Mn-0.6% Si-17.5% Cr-Ni-Mo-Cu White Cast Iron
2.9% C-0.8% Mn-0.6% Si-17.5% Cr-Ni-Mo-Cu White Cast Iron
2.9% C-0.8% Mn-0.6% Si-17.5% Cr-Ni-Mo-Cu White Cast Iron
2.93C-0.60Si-0.78Mn-17.4Cr-0.04% Mo White Cast Iron
2.95% C, 25.82% Cr, 0.02% Mo Alloyed White Cast Iron
2.95% C, 25.82% Cr, 0.02% Mo Alloyed White Cast Iron
2.96C-0.52Si-0.79Mn-17.5Cr-0.98Cu-1.55Mo White Cast Iron
2.96C-0.93Si-0.79Mn-17.5Cr-0.98Cu-1.55Mo White Cast Iron
20-2-1 LC White Cast Iron
3.25% C, 11.80% Cr, 2.60% Mo Alloyed White Cast Iron
3.25% C, 11.80% Cr, 2.60% Mo Alloyed White Cast Iron
3.39% C, 11.95% Cr, 1.36% Mo Alloyed White Cast Iron
3.39% C, 11.95% Cr, 1.36% Mo Alloyed White Cast Iron
3.40% C, 19.85% Cr, 3.40% Mo Alloyed White Cast Iron
3.40% C, 19.85% Cr, 3.40% Mo Alloyed White Cast Iron
3.51% C, 12.20% Cr, 0.02% Mo Alloyed White Cast Iron
3.51% C, 12.20% Cr, 0.02% Mo Alloyed White Cast Iron
3.51% C, 20.10% Cr, 1.37% Mo Alloyed White Cast Iron
3.51% C, 20.10% Cr, 1.37% Mo Alloyed White Cast Iron
3.52% C, 24.65% Cr, 2.67% Mo Alloyed White Cast Iron
3.52% C, 24.65% Cr, 2.67% Mo Alloyed White Cast Iron
3.56% C, 14.60% Cr, 0.47% Mo Alloyed White Cast Iron
3.56% C, 14.60% Cr, 0.47% Mo Alloyed White Cast Iron
3.58% C, 14.45% Cr Alloyed White Cast Iron
3.58% C, 14.45% Cr Alloyed White Cast Iron
3.58% C, 14.65% Cr, 0.52% Mo Alloyed White Cast Iron
3.58% C, 14.65% Cr, 0.52% Mo Alloyed White Cast Iron
3.62% C, 20.35% Cr, <0.01% Mo Alloyed White Cast Iron
3.62% C, 20.35% Cr, <0.01% Mo Alloyed White Cast Iron
3.66% C, 24.95% Cr, 1.53% Mo Alloyed White Cast Iron
3.66% C, 24.95% Cr, 1.53% Mo Alloyed White Cast Iron
3.70% C, 25.32% Cr, 0.02% Mo Alloyed White Cast Iron
3.70% C, 25.32% Cr, 0.02% Mo Alloyed White Cast Iron
3.81% C, 14.75% Cr, 2.50% Mo Alloyed White Cast Iron
3.81% C, 14.75% Cr, 2.50% Mo Alloyed White Cast Iron
3.94% C, 23.45% Cr, 2.94% Mo Alloyed White Cast Iron
3.94% C, 23.45% Cr, 2.94% Mo Alloyed White Cast Iron
3.96% C, 14.80% Cr, 1.45% Mo Alloyed White Cast Iron
3.96% C, 14.80% Cr, 1.45% Mo Alloyed White Cast Iron
3.96% C, 17.55% Cr, 2.53% Mo Alloyed White Cast Iron
3.96% C, 17.55% Cr, 2.53% Mo Alloyed White Cast Iron
4.08% C, 18.00% Cr, 1.14% Mo Alloyed White Cast Iron
4.08% C, 18.00% Cr, 1.14% Mo Alloyed White Cast Iron
4.10% C, 15.10% Cr Alloyed White Cast Iron
4.10% C, 15.10% Cr Alloyed White Cast Iron
4.10% C, 23.67% Cr, 1.32% Mo Alloyed White Cast Iron
4.10% C, 23.67% Cr, 1.32% Mo Alloyed White Cast Iron
4.13% C, 18.22% Cr, 0.05% Mo Alloyed White Cast Iron
4.13% C, 18.22% Cr, 0.05% Mo Alloyed White Cast Iron
4.31% C, 24.80% Cr, 0.02% Mo Alloyed White Cast Iron
4.31% C, 24.80% Cr, 0.02% Mo Alloyed White Cast Iron
Hi-Chrome Work Rolls (Core)
Hi-Chrome Work Rolls (Shell)
Low Alloy Steel
White Iron Class III (28% Cr)
White Iron Class IIc
White Iron Class IIe