35NiCr18 Steel

Steel name: 35NiCr18
Diagram No.: 10
DIN designation: 35NiCr18
Mat.No. (Wr.Nr.) designation: 1.5864
Chemical composition in weight %: 0.34% C, 0.23% Si, 0.55% Mn, 0.011% P, 0.022% S, 1.39% Cr, 4.59% Ni
Steel group: Alloy special structural steels
Properties: No data
Applications: Structural components for very heavy demands.
Reference: Not shown in this demo version.

Heat Treatment
Hardening in water: 820-850oC
Hardening in oil: 820-850oC
Tempering: 450-650oC
Diagram note: No data

Diagram Tempering Temperature - Mechanical Properties


Click the image to enlarge the diagram.

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.