1.4028 Steel

Steel name: 1.4028
Diagram No.: 1021
DIN designation: X30Cr13
EN designation: X30Cr13
Mat.No. (Wr.Nr.) designation: 1.4028
AISI/SAE designation: 420F
Chemical composition in weight %: 0.31% C, 1.00% Si, 1.50% Mn, 13.00% Cr
Steel group: Structural steels
Properties: No data
Applications: Dental and surgical instruments, cutlery, pump shafts, gears pinions and cams, steel balls, and various hand tools. Not recommended for vessels containing high pressure gases or liquids or for plastic molds where high surface finishes are required.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 950-1050oC/oil, air
Tempering: See the diagram
Diagram note: Sample size: square 20 mm.

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.