X105CrMo17 Steel

Steel name: X105CrMo17
Diagram No.: 1027
DIN designation: X105CrMo17
EN designation: X105CrMo17
Mat.No. (Wr.Nr.) designation: 1.4125
AISI/SAE designation: 440C
Chemical composition in weight %: 1.00% C, 1.00% Si, 1.00% Mn, 17.00% Cr, 0.60% Mo
Steel group: High carbon martensitic stainless steels
Properties: No data
Applications: Ball bearings and races, gage blocks, molds and dies, cutlery, valve components, knives and measuring instruments and other products with highest hardness and wear resistance.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1000-1050oC/oil, air
Tempering: See the diagram

Tempering Diagram


Click the image to enlarge the diagram.

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.