1.70C-18.00Cr-1.00Mo-3.00V Steel

Steel name: 1.70C-18.00Cr-1.00Mo-3.00V
Diagram No.: 1047
Chemical composition in weight %: 1.70% C, 0.80% Si, 0.30% Mn, 18.00% Cr, 1.00% Mo, 3.00% V
Steel group: PM stainless mould steels
Properties: No data
Applications: Steel has been specially developed for high-tech applications. These include products within the electronic industry such as connectors, plugs, switches, resistors, integrated circuits, etc. Steel can also be used in the food processing industry, where a combination of corrosion resistance and wear resistance is required for cutting applications.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1050–1100oC/air, gas, hot bath
Tempering: See the diagram

Tempering Diagram


Click the image to enlarge the diagram.

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.