0.55C-1.00Cr-3.00Ni-0.30Mo Steel

Steel name: 0.55C-1.00Cr-3.00Ni-0.30Mo
Diagram No.: 1048
AISI/SAE designation: L6
Chemical composition in weight %: 0.55% C, 0.30% Si, 0.50% Mn, 1.00% Cr, 3.00% Ni, 0.30% Mo
Steel group: Tool and mould steels
Properties: No data
Applications: The excellent combination of toughness and wear resistance offered by steel enables it to be used for a great many tooling applications, both hot and cold. It is widely used for moulds in the plastics industry and for a variety of heavy-duty tools exposed to severe pressure, shock loading or bending stresses.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 800–860oC/oil, gas, hot bath
Tempering: See the diagram

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.