1.40C-4.60Cr-3.20Mo-3.70V Steel
Steel name: 1.40C-4.60Cr-3.20Mo-3.70V
Diagram No.: 1065
Chemical composition in weight %: 1.40% C, 1.00% Si, 0.60% Mn, 4.60% Cr, 3.20% Mo, 3.70% V
Steel group: Cold work tool steels
Applications: Cold rolls requiring high wear resistance and resistance to cracking, form rolls requiring a high wear resistance and resistance to cracking, cutting rolls, circular slitting knives, knives, engineering applications, substrate for surface coating
Reference: Not shown in this demo version.
Heat Treatment
Hardening: 950–1150oC/gas, vacuum, hot bath
Tempering: See the diagram
Diagram note: Tempering graphs without sub-zero treatment after hardening.
Tempering Diagram
Click the image to enlarge the diagram.
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.