420 mod. Steel

Steel name: 420 mod.
Diagram No.: 1069
AISI/SAE designation: 420 modified
Chemical composition in weight %: 0.38% C, 0.90% Si, 0.50% Mn, 13.60% Cr, 0.30% V, 0.00% W
Steel group: Stainless mould steels
Properties: No data
Applications: Whilst steel is recommended for all types of moulding tools, its special properties make it particularly suitable for moulds with the following demands: Corrosion/staining resistance, i.e. for moulding of corrosive materials, e.g. PVC, acetates, and for moulds subjected to humid working/storage conditions. Wear resistance, i.e. for moulding abrasive/ filled materials, including injection-moulded thermosetting grades. Steel is recommended for moulds with long production runs, e.g. disposable cutlery and containers. High surface finish, i.e. for the production of optical parts, such as camera and sunglasses lenses, and for medical containers, e.g. syringes, analysis phials.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1000–1050oC/oil, hot bath, vacuum, gas
Tempering: See the diagram

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.