1.2436 Steel

Steel name: 1.2436
Diagram No.: 1071
Mat.No. (Wr.Nr.) designation: 1.2436
AISI/SAE designation: D6 (D3)
Chemical composition in weight %: 2.05% C, 0.30% Si, 0.80% Mn, 12.70% Cr, 1.10% W
Steel group: Cold work tool steels
Properties: No data
Applications: Steel is recommended for applications demanding maximum wear-resistance, such as blanking and shearing tools for thin, hard materials; long-run press tools; forming tools; moulds for ceramics and abrasive plastics.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 920–1000oC/oil, vacuum, gas, hot bath
Tempering: See the diagram

Tempering Diagram


Click the image to enlarge the diagram.

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.