0.10C-2.50Mn-3.00Cr-1.00Ni Steel

Steel name: 0.10C-2.50Mn-3.00Cr-1.00Ni
Diagram No.: 1077
Chemical composition in weight %: 0.10% C, 2.50% Mn, 3.00% Cr, 1.00% Ni
Steel group: Tool steels
Properties: No data
Applications: Moulds for plastic injection, holder material for forging and die casting dies, holder material for cutting tools, hot runner manifolds, structural components.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 850oC/air
Tempering: See the diagram

Tempering Diagram


Click the image to enlarge the diagram.

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.