100Cr6 Steel

Steel name: 100Cr6
Diagram No.: 141
EN designation: 100Cr6
Mat.No. (Wr.Nr.) designation: 1.3504
BS designation: S 135
Chemical composition in weight %: 1.00% C, 1.50% Cr
Steel group: Steel for special applications
Properties: No data
Applications: Ball, roller or needle roller bearings, bearing races.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 835oC/oil
Tempering: See the diagram
Diagram note: Heated on 835oC, oil quenched. Test on 1 cm thick specimen.

Diagram Tempering Temperature - Mechanical Properties

Price: 20.00 US $