X100CrMoV5 Steel

Steel name: X100CrMoV5
Diagram No.: 145
EN designation: X100CrMoV5
Mat.No. (Wr.Nr.) designation: 1.2363
AISI/SAE designation: A2
Chemical composition in weight %: 1.00% C, 5.00% Cr, 1.00% Mo, 0.30% V
Steel group: Tool steels
Properties: No data
Applications: Cutting and stamping dies, gauging, drawing, forming dies.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 980oC/air, gas
Tempering: See the diagram

Tempering Diagram


Click the image to enlarge the diagram.

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.