X165CrMoV12 Steel
Steel name: X165CrMoV12
Diagram No.: 166
DIN designation: X165CrMoV12
Mat.No. (Wr.Nr.) designation: 1.2601
GOST designation: Ch12VMF
Chemical composition in weight %: 1.55-1.75% C, 0.25-0.40% Si, 0.20-0.40% Mn, max. 0.030% P, max. 0.030% S, 11.00-12.00% Cr, 0.50-0.70% Mo, 0.10-0.50% V, 0.40-0.60% W
Steel group: Cold work tool steels
Properties: No data
Applications: High performance blanking, punching, stamping and cutting tools and dies up to 6 mm sheet thickness, thread rollings, chasers and dies, cold forming and bending tools, precision blanking dies, longitudinal and circular shear blades for plastic, paper and metal, milling cutters, reamers, broaches, hobbing tools, tools for drawing, deep drawing and cold extrusion, woodworking tools, pressing tools for the sinters, ceramics and pharmaceutical industries, cold piercers, measuring tools, rolling cutters and shaping wheels, cold pilger mandrels, flanging, straightening and beading rolls, trimming and splitting dies, tools for the cold manufacture of screws, nuts and rivets, plastic moulds.
Reference: Not shown in this demo version.
Heat Treatment
Hardening in oil, air: 980 - 1010oC
Tempering: See the diagram
Tempering Diagram
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.