55NiCrMoV7 Steel
Steel name: 55NiCrMoV7
Diagram No.: 167
DIN designation: 55NiCrMoV7
Mat.No. (Wr.Nr.) designation: 1.2714
AISI/SAE designation: L6
Chemical composition in weight %: 0.50-0.60% C, 0.10-0.40% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.005% S, 0.80-1.20% Cr, 0.35-0.55% Mo, 0.05-0.15% V, 1.50-1.80% Ni
Steel group: Hot work tool steels
Properties: No data
Applications: Forging dies of all types, hammer forging dies up to largest dimensions, tools for tube and rod extrusion such as rams, bolsters, mandrels, plungers, sleeves, die holders, backing plates, chipping beds, press dies for mould parts, deep engraving dies, containers for die casting presses, hot forming dies, bending and heavy embossing tools, hot mill rolls, hammers and pile drivers, hot punching tools, very hard cold work dies and punches, hot shear blades, blocks for dies, forging saddles, pressing spindles, shrink rings, armoured trim dies, hydro forming tools, plastic moulds, hot gripper and heading dies.
Reference: Not shown in this demo version.
Heat Treatment
Hardening in air: 870 - 900oC
Hardening in oil: 830 - 870oC
Tempering: See the diagram
Tempering Diagram
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.