LESCALLOY D6AC VAC-ARC Steel

Steel name: LESCALLOY D6AC VAC-ARC
Diagram No.: 1680
Chemical composition in weight %: 0.46% C, 0.25% Si, 0.75% Mn, 1.10% CR, 0.60% Ni, 1.00% Mo, 0.10% V
Steel group: Structural steels
Properties: Steel is a medium carbon, low alloy, ultra high strength steel primarily designed for high strength structural applications requiring strength levels up to 280,000 psi. This alloy provides a high yield strength to tensile strength ratio, combined with good ductility.
Applications: No data
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1550-1650°F (843-899°C)/oil, salt
Tempering: 300-1200°F (149-649°C)

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.