AISI 2367 Steel
Steel name: AISI 2367
Diagram No.: 1688
AISI/SAE designation: 2367
Chemical composition in weight %: 0.37% C, 0.42% Si, 0.45% Mn, 4.90% Cr, 2.90% Mo, 0.61% V
Steel group: Hot work tool steels
Properties: Hardness distribution of specimens tempered at 500 °C and 600 °C. Dashed red line exhibits the hardness distribution of specimens processed at 600 °C before tempering. Secondary hardening is a result of tempering carried out after austenitization which is followed by rapid cooling resulting of austenite formation. Holding at 600 °C provides formation of secondary carbides before tempering stage. Thus, while the amount of carbides increase the size of carbides decrease. Finer carbides formed in this stage results in higher hardness and toughness.
Applications: No data
Reference: Not shown in this demo version.
Heat Treatment
Hardening: 1050 C, 90 min/N2
Tempering: See the diagram
Tempering Diagram
Click the image to enlarge the diagram.
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.