AISI 440C Steel
Steel name: AISI 440C
Table No.: 1719
AISI/SAE designation: 440C
Chemical composition in weight %: 1.00-1.10% C, 0.30-0.60% Si, 0.40-0.60% Mn, max. 0.030% P, max. 0.015% S, 16.50-17.60% Cr, 0.40-0.60% Mo
Steel group: Tool steels
Properties: No data
Applications: Plastic granulator knives, cutlery, bearings, nozzles, valve parts, balls and sears.
Reference: Not shown in this demo version.
Heat Treatment
Hardening: Preheat to 1200° F - 1450° F, soak until uniformly heated, and either transfer or raise furnace temperature to 1850° F -1950° F, and hold 1 (one) hour per inch of greatest thickness. Quench into 150° F oil or air cool.
Tempering: Temper immediately after quenching, before the part has cooled to below 150oF. Double tempering is recommended and the parts should be held a minimum of 2 hours per inch of greatest thickness. Recommended tempering range is 300°F-700°F. Tempering about 700F will result in lower impact strength and reduce corrosion resistance. The tempering table may be used as a guide. However, since 1/2” diameter specimens were used for this test, it may be found that heavier sections are several points lower.
Table Tempering Temperature (F) - Hardness (HRC)
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.