A-6 Steel
Steel name: A-6
Diagram No.: 1761
ASTM designation: A681 (A-6)
UNS designation: T30i06
AISI/SAE designation: A6
Chemical composition in weight %: 0.65-0.75% C, 0.10-0.70% Si, 1.80-2.50% Mn, 0.90-1.40% Cr, 0.90-1.40% Mo
Steel group: Tool steels
Properties: No data
Applications: Bending tools, blanking dies - large, cams, coining dies, feed fingers, forming dies - large.
Reference: Not shown in this demo version.
Heat Treatment
Hardening: 1500-1600° F/cool in still air or in air blast. Allow to cool to 125-150° F before tempering. Soak time is 10 minutes per inch of thickness. Minimum of 30 minutes.
Tempering: Temper for 1 Hr. per inch of thickness with a minimum of 2 Hrs. Recommended temperature is 350-700° F.
Tempering Diagram
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.