H-13 Steel

Steel name: H-13
Diagram No.: 1769
Mat.No. (Wr.Nr.) designation: 1.2344
SS designation: SKD61
BS designation: BH 13
AISI/SAE designation: H13
JIS designation: SKD61
Chemical composition in weight %: 0.32-0.45% C, 0.80-1.25% Si, 0.20-0.60% Mn, 4.75-5.50% Cr, 1.10-1.75% Mo, 0.80-1.20% V
Steel group: Hot work tool steels
Properties: No data
Applications: Die casting, dies dummy blocks, extrusion dies - hot, forging dies, heading dies - hot, heavy shear blades, inserts, mandrels, piercing tools - hot, plastic mold dies, punches - hot, swaging dies - hot.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1830-1900° F/to minimize distortion, air cool. For maximum hardness diameters greater than 6” should be quenched in oil. Soak time is 30 minutes per inch of thickness. Minimum of 1 hour. Allow to cool to 125-150° F before tempering.
Tempering: Complete equalization of temperature throughout the tools is essential for good results. Double temper. Recommended temperature is 1000-1200° F.

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.