M-2 Steel

Steel name: M-2
Diagram No.: 1771
Mat.No. (Wr.Nr.) designation: 1.3343
SS designation: 2722
BS designation: BM 2
AISI/SAE designation: M2
JIS designation: SKH9
Chemical composition in weight %: 0.78-1.05% C, 0.20-0.45% Si, 0.15-0.40% Mn, max. 0.030% P, max. 0.030% S, 3.75-4.50% Cr, max. 0.30% Ni, 1.75-2.20% V, 5.50-6.75% W
Steel group: High speed steels
Properties: No data
Applications: Blanking dies, boring tools, broaches, center drills, gear cutters, lamination dies, lathe tools, mandrels, milling cutters, planer tools, punches reamers, router bits, shear blades, taps thread chasers, twist drills, wood knives.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 2225-2275° F (furnace) 2200-2225° F (salt bath)/Quench in air or warm oil. To minimize quenching strains, quench in salt at 1000° F. For maximum wear resistance, harden at 2275° F. For maximum toughness and high hardness, harden at 2200° F.
Tempering: Double tempering is required. The usual tempering time is 2+2 hours. Recommended temperature is 1000-1075° F.

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.