S-5 Steel

Steel name: S-5
Diagram No.: 1777
AISI/SAE designation: S5
UNS designation: T41905
Chemical composition in weight %: 0.50-0.65% C, 1.75-2.25% Si, 0.60-1.00% Mn, 0.10-0.50% Cr, 0.15-0.35% V
Steel group: Tool steels
Properties: No data
Applications: Brake dies, collets, drift pins, hand chisels, knockout pins, pipe cutters, pneumatic tools, punches, rivet sets, shear blades, slitters, swaging dies.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1575-1650° F (water) 1600-1700° F (oil)/In water. In oil. Allow to cool to 125-150° F before tempering. Soak time is 10 minutes per inch of thickness. Minimum of 30 minutes. Oil quenching is preferred for intricate parts.
Tempering: Temper immediately after hardening and quenching. For maximum hardness temper at 300-350° F. For maximum toughness temper at 900-1000° F.

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.