VKM42 Steel

Steel name: VKM42
Diagram No.: 1793
Mat.No. (Wr.Nr.) designation: 1.3247
EN designation: HS 2-9-1-8
JIS designation: SKH 59
Chemical composition in weight %: 1.10% C, 3.75% Cr, 9.50% Mo, 1.15% V, 1.50% W, 8.00% Co
Steel group: High speed steels
Properties: No data
Applications: End mills, milling cutters, taps, broaches, reamers.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1160-1190 ºC. Hardening procedure must involve pre-heating at 400/500 ºC followed by other at 860/880 ºC. After, austenitizing may be conducted, followed by quenching down to room temperature. A protective atmosphere is absolutely necessary.
Tempering: Tree tempering treatments, of at least 2h, are required and after each one tools must cool to room temperature.

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.