VHSSM50 Steel
Steel name: VHSSM50
Diagram No.: 1795
Mat.No. (Wr.Nr.) designation: 1.3551
AISI/SAE designation: M50
Chemical composition in weight %: 0.80% C, 4.00% Cr, 4.25% Mo, 1.00% V
Steel group: Tool steels
Properties: No data
Applications: Drills and saws for common use. General tools where higher toughness than other high speed steels is required and a lower hardness is acceptable.
Reference: Not shown in this demo version.
Heat Treatment
Hardening: 1080- 1120 ºC. Hardening procedure must involve pre-heating at 400/500 ºC followed by other at 860/880 ºC. After, austenitizing may be conducted, followed by quenching down to room temperature. A protective atmosphere is absolutely necessary.
Tempering: 560 ºC. Double tempering treatments, of at least 2h, are required and after each one tools must cool to room temperature.
Tempering Diagram
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.