Steel name: TBL PLUS
Diagram No.: 1802
Chemical composition in weight %: 0.31-0.38% C, max. 0.40% Si, 1.20-1.50% Mn, max. 0.040% P, max. 0.030% S, max. 0.50% Cr, 0.0008–0.0040% B
Steel group: Boron steels, structural steels
Properties: Wear protection for agricultural machinery and concrete mixer trucks.
Applications: For use in agricultural machinery, the steels are usually hardened after processing. As a result of alloying with boron, TBL grades can be hardened without diffi culty in water, oil or polymer dispersion. TBL and TBL PLUS are therefore particularly suited to structures which require high wear resistance, e.g. in harrows, packers and plows.
Reference: Not shown in this demo version.
Heat Treatment
The recommended austenitizing temperature is 860°C. The material temperature at the start of quenching in water should be between 815°C and 870°C. If quenching is carried out in oil, the temperature at the beginning should be between 860°C and 910°C.
Tempering Diagram
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.