41x40 Steel

Steel name: 41x40
Diagram No.: 1813
Chemical composition in weight %: 0.40% C, 0.30% Si, 1.50% Mn, max. 0.012% P, 0.060% S, 1.90% Cr, 0.20% Mo
Steel group: Plastic mould steels, tool steels
Properties: Compared to AISI P20 grade, 30% increase in milling speed and 300% increase in drilling speed can be expected.
Applications: Plastic injection molds for thermoplastics. Extrusion dies for thermoplastics. Compression molds.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 870, 1 h/air
Diagram note: Ac1=733 C, Ac3=780 C, Ms=320 C

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.