DCMX Steel
Steel name: DCMX
Diagram No.: 1815
JIS designation: SKD11 mod.
Chemical composition in weight %: Patent pending
Steel group: Cold work tool steels, matrix type cold work die steels
Properties: DC-Matrix is a matrix type cold work tool steel: only fine carbides are distributed in matrix due to optimum alloy design and production process. DC-Matrix shows high performance in service and ease in mold making as well.
Applications: Blanking punches and trimming edges where main failures are cracking and chipping.
Reference: Not shown in this demo version.
Heat Treatment
Quenching: 1000-10150 C/air
Tempering: Low: 150-200 C/air cooling. High: 480-560 C/air cooling. More than twice tempering.
Diagram note: Specimen: 15 mm cubic, quenching: 1030, AC.
Tempering diagrams
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.