SX105V Steel

Steel name: SX105V
Diagram No.: 1831
Chemical composition in weight %: 0.75-0.95% C, 0.90-1.10% Si, 0.70-1.00% Mn, 1.00-1.20% Cr, 0.15-0.30% Mo, 0.07-0.10% V. SKS3 steel: 0.95% C, 0.25% Si, 1.05% Mn, 0.75% Cr, 0.75% W.
Steel group: Cold work tool steels
Properties: Low alloy cold work tool steel.
Applications: Blanking dies, bending dies, drawing dies, cutting edges, wear resistant jigs, etc. (properties of the material especially good for cutting edges).
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 825-1075 C
Tempering: 250 C
Diagram note: No data

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.