AUD61 Steel

Steel name: AUD61
Diagram No.: 1838
JIS designation: SKD61 mod.
Chemical composition in weight %: 0.32-0.42% C, 0.80-1.20% Si, max. 0.50% Mn, 4.50-5.50% Cr, 1.00-1.50% Mo, 0.80-1.20% V
Steel group: Hot work tool steels
Properties: High toughness general purpose hot work tool steel (SKD61 high performance type).
Applications: Due to its excellent toughness and resistance to softening under high temperatures, this steel is used in hot work/warm work forging, die casting, and more recently, in hot stamping molds.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1000-1050 C
Tempering: 550-650 C
Diagram note: No data

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.