DURO-V2 Steel

Steel name: DURO-V2
Diagram No.: 1863
Chemical composition in weight %: No data
Steel group: Plastic mould steels
Properties: DURO series steel is for precision die and mold with a superior balance of toughness and wear resistance. Die steel which has superior fatigue strength and is the toughest in the DURO series.
Applications: No data
Reference: Not shown in this demo version.

Heat Treatment
Austenitizing: No data
Tempering: See the diagram.
Diagram note: No data

Tempering Diagram


Click the image to enlarge the diagram.

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.