19MnB4 Steel

Steel name: 19MnB4
Table No.: 1899
DIN designation: 19MnB4
Mat.No. (Wr.Nr.) designation: 1.5523
AISI/SAE designation: 15B21H
EN designation: 19MnB4
UNI designation: 19MnB4
AFNOR designation: 19MnB4
BS designation: 170H20
GOST designation: 20G2R
GB designation: ML20MnB
Chemical composition in weight %: 0.17-0.24% C, max. 0.40% Si, 0.80-1.15% Mn, max. 0.030% P, max. 0.035% S, min. 0.020% Al, 0.0008-0.0050% B
Steel group: Structural steels
Applications: No data
Note: Ac1=710 C, Ac3=830 C, Ms=440 C, Mf=220 C.
Reference: Not shown in this demo version.

Heat Treatment
Quenching: 850-890 C/polymer, water
Tempering: 450-650 C/air

Table Tempering Temperature - Hardness - Mechanical Properties

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.